Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,063 records · Page 59

Magnetic and high frequency properties of nanogranular CoFe-yttrium-doped zirconia films

Soft magnetic nanogranular FeCo-Yttrium-doped Zirconia thin films were fabricated using RF magnetron sputtering at different sputtering power. It was found that film electrical resistivity (ρ) decreased steeply with the increase of sputtering power, while both saturation magnetization (4πM{sub s}) and natural ferromagnetic resonant frequency (ƒ{sub r}) increased with the sputtering power ascending from 100 W to 200 W, but decreased when sputtering power exceeded 200 W. X-ray diffraction analysis and transmission electron microscopy confirmed that the films were nanocrystalline/amorphous composites. A saturation magnetization as high as 15.4 kGs and a ferromagnetic resonance frequency above 3 GHz were obtained.

36 MATERIALS SCIENCE↗

Textured PrCo{sub 5} nanoflakes with large coercivity prepared by low power surfactant-assisted ball milling

The effect of the milling time on the structure, morphology, coercivity, and remanence ratio of textured PrCo{sub 5} nanoflakes produced by low power surfactant-assisted ball milling (SABM) was investigated. The X-ray powder diffraction (XRD) patterns indicate that the SABM PrCo{sub 5} samples are all CaCu{sub 5}-type hexagonal structure. The average grain size is smaller than 10 nm when the SABM time is equal to or longer than 5.5 h. The thickness of nanoflakes is mainly in the range of 50−100 nm while the length is 0.5−5 μm when the SABM time reaches 8 h. For the field-aligned PrCo{sub 5} nanoflakes, the out-of-plane texture is indicated from the increasing (0 0 l) peaks in the XRD patterns, and the easy magnetization direction is perpendicular to the flake surface. The strong texture of PrCo{sub 5} nanoflakes leads to a large coercivity H{sub c} (7.8 kOe) and obvious anisotropic magnetic behaviors for the aligned samples.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of ball milling and annealing conditions on the properties of L1{sub 0} FePt nanoparticles fabricated by a new green chemical synthesis method

In this work, a new green chemical strategy for the synthesis of L1{sub 0} FePt alloy nanoparticles is reported. The precursor is a polycrystalline molecular complex (Fe(H{sub 2}O){sub 6}PtCl{sub 6}), in which Fe and Pt atoms are arranged on alternating planes and milled with NaCl to form nanocrystals. Then the mixture was annealed under reducing atmosphere (5% H{sub 2} and 95% Ar) at temperatures varying from 350 °C to 500 °C for 2 h with a heating rate of 5 °C/min. After the reduction, the mixture was washed with water to remove the NaCl and L1{sub 0} FePt nanoparticles were obtained. The X-Ray Diffraction pattern showed the presence of the characteristic peaks of the fct phase of FePt nanoparticles. Influence of precursor/NaCl ratio and ball milling time on particle size was investigated. Transmission electron microscopy images revealed that smaller precursor/NaCl ratio (10 mg/20 g) and longer milling time (15 h) lead to smaller particle size and narrower size distribution. Milling time does not influence the coercivity much but the decrease of the amount of precursor leads to a decrease of coercivity from 10.8 kOe to 4.8 kOe.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure investigations of hcp phase CoPt thin films with high coercivity

CoPt films have been grown in the past with a high anisotropy in L1{sub 1} or L1{sub 0} phase, and a high coercivity is observed only in L1{sub 0} CoPt films. Recently, we have grown CoPt films which exhibited a high coercivity without exhibiting an ordered phase. In this study, high resolution transmission electron microscopy (HRTEM) investigations have been carried out to understand the strong thickness and deposition pressure dependent magnetic properties. HRTEM studies revealed the formation of an initial growth layer in a metastable hexagonal (hcp) CoPt with high anisotropy. This phase is believed to be aided by the heteroepitaxial growth on Ru as well as the formation of Ru-doped CoPt phase. As the films grew thicker, transformation from hcp phase to an energetically favourable face-centered cubic (fcc) phase was observed. Stacking faults were found predominantly at the hcp-fcc transformation region of the CoPt film. The higher coercivity of thinner CoPt film is attributed to relatively less fcc fraction, less stacking faults, and to the isolated grain structure of these films compared to the thicker films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties and microstructure of Sm-Co/α-Fe nanocomposite thick film-magnets composed of multi-layers over 700 layers

We synthesized Sm-Co/α-Fe nanocomposite film-magnets, approximately 10 μm in thickness, composed of 780 layers by the pulse laser deposition method. Transmission electron microscopic observations revealed that the synthesized film is composed of Sm-Co and α-Fe layers with the well-controlled α-Fe thickness of approximately 10–20 nm, which is suitable one predicted by the micromagnetic simulation. In spite of the enhanced interlayer diffusion of Fe and Co by annealing for crystallization, the (BH){sub max} value of 100 kJ/m{sup 3} was obtained at the averaged compositions of Sm/(Sm + Co) = 0.16 and Fe/(Sm + Co + Fe) = 0.47. The α-Fe fraction for obtaining the highest (BH){sub max} value was smaller than that expected from the micromagnetic simulation. Although the annealing for crystallization lay the easy direction of magnetization in the plane, the film is not expected to have strong crystallographic texture.

36 MATERIALS SCIENCE↗

Structure and magnetic properties of low-temperature phase Mn-Bi nanosheets with ultra-high coercivity and significant anisotropy

The microstructure, crystal structure, and magnetic properties of low-temperature phase (LTP) Mn-Bi nanosheets, prepared by surfactant assistant high-energy ball milling (SA-HEBM) with oleylamine and oleic acid as the surfactant, were examined with scanning electron microscopy, X-ray diffraction, and vibrating sample magnetometer, respectively. Effect of ball-milling time on the coercivity of LTP Mn-Bi nanosheets was systematically investigated. Results show that the high energy ball milling time from tens of minutes to several hours results in the coercivity increase of Mn-Bi powders and peak values of 14.3 kOe around 10 h. LTP Mn-Bi nanosheets are characterized by an average thickness of tens of nanometers, an average diameter of ∼1.5 μm, and possess a relatively large aspect ratio, an ultra-high room temperature coercivity of 22.3 kOe, a significant geometrical and magnetic anisotropy, and a strong (00l) crystal texture. Magnetization and demagnetization behaviors reveal that wall pinning is the dominant coercivity mechanism in these LTP Mn-Bi nanosheets. The ultrafine grain refinement introduced by the SA-HEBM process contribute to the ultra-high coercivity of LTP Mn-Bi nanosheets and a large number of defects put a powerful pinning effect on the magnetic domain movement, simultaneously. Further magnetic measurement at 437 K shows that a high coercivity of 17.8 kOe and a strong positive temperature coefficient of coercivity existed in the bonded permanent magnet made by LTP Mn-Bi nanosheets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electroplated L1{sub 0} CoPt thick-film permanent magnets

The fabrication and magnetic characterization of 15-μm-thick electroplated L1{sub 0} CoPt hard magnets with good magnetic properties is reported in this paper. Experimental study of the dependence of the magnets' properties on annealing temperature reveals that an intrinsic coercivity H{sub ci} = ∼800 kA/m (10 kOe), squareness >0.8, and energy product of >150 kJ/m{sup 3} are obtained for photolithographically patterned structures (250 μm × 2 mm stripes; 15 μm thickness) electroplated on silicon substrates and annealed in hydrogen forming gas at 700 °C. Scanning electron microscopy is used to inspect the morphology of both the as-deposited and annealed magnetic layers, and X-ray Diffractometer analysis on the magnets annealed at 700 °C confirm a phase transformation to an ordered L1{sub 0} CoPt structure, with a minor phase of hcp Co. These thick films are intended for microsystems/MEMS applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and structural properties of MnBi multilayered thin films

Magnetic and structural properties of MnBi films with thicknesses up to 50 nm were investigated. Thin films of the MnBi LTP (Low Temperature Phase) were fabricated onto silica-glass substrates by sputter-deposition of Bi/Mn multilayer, followed by a subsequent annealing at about 550 °C for 30 min. Coercivity of such thin films is higher than 15 kOe, even though the film thickness is about 10 nm. These thin films show the preferential growth of c-axis of the LTP along the film normal. Moreover, high resolution transmission electron microscopy indicates that the LTP regions of 30–50 nm in size are physically isolated by Bi. The magnetization reversal mechanism of such a LTP region is mainly governed by a coherent rotation mode based on the δM curve measurement.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of stoichiometry and growth temperature on the crystal structure and magnetic properties of epitaxial L1{sub 0} Fe-Pd (001) films

To investigate the crystallographic structure and the magnetic properties as a function of chemical composition (40–62 at. %) and substrate temperature (T{sub s} = 300–550 °C), we fabricated epitaxial FePd films of thickness 20 ± 2 nm by sputtering on MgO (100) single-crystal substrates. The ordering parameter, measured by x-ray diffraction with synchrotron radiation, and the perpendicular anisotropy of the Fe{sub 54}Pt{sub 46} films increased with increasing substrate temperature. For FePd films (T{sub s} = 550 °C) with varied Fe content, a direct correlation between the ordering parameter and the magnetocrystalline anisotropy field is found. The greatest ordering parameter, 0.84, and magnetocrystalline anisotropy field, ∼20 kOe, were obtained for FePd films of Fe concentration 54 at. %, indicating that an off-stoichiometric L1{sub 0} FePd might be preferable for engineering and applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Impact of fluorine based reactive chemistry on structure and properties of high moment magnetic material

The impact of the fluorine-based reactive ion etch (RIE) process on the structural, electrical, and magnetic properties of NiFe and CoNiFe-plated materials was investigated. Several techniques, including X-ray fluorescence, 4-point-probe, BH looper, transmission electron microscopy (TEM), and electron energy loss spectroscopy (EELS), were utilized to characterize both bulk film properties such as thickness, average composition, Rs, ρ, Bs, Ms, and surface magnetic “dead” layers' properties such as thickness and element concentration. Experimental data showed that the majority of Rs and Bs changes of these bulk films were due to thickness reduction during exposure to the RIE process. ρ and Ms change after taking thickness reduction into account were negligible. The composition of the bulk films, which were not sensitive to surface magnetic dead layers with nano-meter scale, showed minimum change as well. It was found by TEM and EELS analysis that although both before and after RIE there were magnetic dead layers on the top surface of these materials, the thickness and element concentration of the layers were quite different. Prior to RIE, dead layer was actually native oxidation layers (about 2 nm thick), while after RIE dead layer consisted of two sub-layers that were about 6 nm thick in total. Sub-layer on the top was native oxidation layer, while the bottom layer was RIE “damaged” layer with very high fluorine concentration. Two in-situ RIE approaches were also proposed and tested to remove such damaged sub-layers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magneto-optical spectroscopy of ferromagnetic shape-memory Ni-Mn-Ga alloy

Magneto-optical properties of single crystal of Ni{sub 50.1}Mn{sub 28.4}Ga{sub 21.5} magnetic shape memory alloy in martensite and austenite phase were systematically studied. Crystal orientation was approximately along (100) planes of parent cubic austenite. At room temperature, the sample was in modulated 10M martensite phase and transformed to cubic austenite at 323 K. Spectral dependence of polar magneto-optical Kerr effect was obtained by generalized magneto-optical ellipsometry with rotating analyzer in the photon energy range from 1.2 to 4 eV, and from room temperature to temperature above the Curie point. The Kerr rotation spectra exhibit prominent features typical for complexes containing Mn atoms. Significant spectral changes during transformation to austenite can be explained by different optical properties caused by changes in density of states near the Fermi energy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Investigation of cellular microstructure and enhanced coercivity in sputtered Sm{sub 2}(CoCuFeZr){sub 17} film

We have investigated the effect of annealing temperature on the microstructure and magnetic properties of Sm{sub 2}(CoCuFeZr){sub 17} films prepared using ion beam sputtering at room temperature. The as-deposited film shows randomly oriented polycrystalline grains and exhibits small coercivity (H{sub C}) of 0.04 T at room temperature. Post annealing of these films at 700 °C under Ar atmosphere shows significant changes in the microstructure transforming it to the development of cellular growth, concomitant with enhanced coercivity up to 1.3 T. The enhanced coercivity is explained using the domain wall pinning mechanism.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Sm(Co{sub 1−x}Ni{sub x}){sub 5} ordered alloy thin films formed on Cr(100) single-crystal underlayers

Sm{sub 17}(Co{sub 1−x}Ni{sub x}){sub 83} (at. %, x = 0, 0.2, 0.8, and 1) alloy thin films are deposited on Cr(100) single-crystal underlayers at temperatures ranging between 100 and 500 °C by molecular beam epitaxy. The effects of substrate temperature and Ni/Co composition on the film growth behavior and the detailed resulting structure are investigated. Formation of epitaxial RT{sub 5} (R: rare earth metal, T: transition metal) ordered crystals is, respectively, recognized for the films with x of 0, 0.2, 0.8, and 1 deposited at temperatures higher than 400, 400, 300, and 300 °C, whereas the films deposited below the respective temperatures consist of amorphous phases. The order degree increases with increasing the substrate temperature and the Ni content. The order degrees of films with x of 0, 0.2, 0.8, and 1 deposited at 500 °C are 0.6, 0.7, 0.8, and 0.9, respectively. A replacement of Co site in SmCo{sub 5} structure with Ni atom is useful for enhancing the formation of RT{sub 5} ordered phase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of the interplay between atomic and magnetic order on the properties of metamagnetic Ni-Co-Mn-Ga shape memory alloys

Ni-Co-Mn-Ga ferromagnetic shape memory alloys show metamagnetic behavior for a range of Co contents. The temperatures of the structural and magnetic transitions depend strongly on composition and atomic order degree, in such a way that combined composition and thermal treatment allows obtaining martensitic transformation between any magnetic state of austenite and martensite. This work presents a detailed analysis of the effect of atomic order on Ni-Co-Mn-Ga alloys through the evolution of structural and magnetic transitions after quench from high temperatures and during post-quest ageing. It is found that the way in which the atomic order affects the martensitic transformation temperatures and entropy depends on the magnetic order of austenite and martensite. The results can be explained assuming that improvement of atomic order decreases the free energy of the structural phases according to their magnetic order. However, it is assumed in this work that changes in the slope—that is, the entropy—of the Gibbs free energy curves are also decisive to the stability of the two-phase system. The experimental transformation entropy values have been compared with a phenomenological model, based on a Bragg–Williams approximation, accounting for the magnetic contribution. The excellent agreement obtained corroborates the magnetic origin of changes in transformation entropy brought about by atomic ordering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase structure and magnetic properties of Mn{sub 3}Ga{sub 2} alloy

In this paper, Mn{sub 3}Ga{sub 2} alloys with high saturation magnetization and high Curie temperatures were prepared by levitation melting high pure Mn and Ga elements followed by annealing. The effect of annealing temperature on phase structure and magnetic properties was investigated by means of x-ray diffraction and a vibrating sample magnetometer. A single phase alloy Mn{sub 3}Ga{sub 2}, which has tetragonal P4/mmm structure, was obtained with an annealing temperature of 773 K and annealing time of 24 h. The hysteresis curve of its easy axis for this single phase alloy shows that the room temperature coercivity and saturation magnetization are 4.18 kOe and 50.81 emu/g, respectively. The thermomagnetic curves indicate that the Curie temperature is about 650 K and a phase transformation occurs above 823 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Post magnetic field annealing effect on magnetic and structural properties of Co{sub 80}Pt{sub 20} nanowires and nanotubes fabricated by electrochemical method

Highly ordered Co{sub 80}Pt{sub 20} nanowires (NWs) and nanotubes (NTs) have been synthesized by low cost DC electrochemical deposition method with constant stirring during the fabrication process in anodic aluminum oxide nano-templates with average pore diameter of about 200 nm. The structural and magnetic properties of nanostructures have been investigated before and after simple and magnetic field annealing. Magnetic field of 1 T has been applied during annealing process in the direction perpendicular to NWs and NTs axis. X-Ray Diffraction analysis shows face centered cubic (fcc) as the dominant phase for Co{sub 80}Pt{sub 20} NWs and post annealing led to better crystallinity with retained fcc phase. Furthermore, magnetic properties, including saturation magnetization (M{sub s}), squareness ratio (M{sub r}/M{sub s}), and coercivity (H{sub c}), have been investigated as a function of annealing temperature by Vibrating Sample Magnetometer.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Exchange bias magnetism in films of NiFe/(Ni,Fe)O nanocrystallite dispersions

Ni{sub 3}Fe/(Ni,Fe)O thin films having a nanocrystallite dispersion morphology were prepared by a reactive ion beam-assisted deposition technique. The crystallite sizes of these dispersion-based films were observed to decrease from 8.4 ± 0.3 nm to 3.4 ± 0.3 nm as the deposition flow-rate increased from 2.78% to 7.89% O{sub 2}/Ar. Thin film composition was determined using selective area electron diffraction images and Multislice simulations. Through a detailed analysis of high resolution transmission electron microscopy images, the nanocrystallites were determined to be Ni{sub 3}Fe (a ferromagnet), NiO, and FeO (both antiferromagnets). It was determined that the interfacial molar Ni{sub 3}Fe ratio in the nanocrystallite dispersions increased slightly at first, then decreased as the oxygen content was increased; at 7.89% O{sub 2}/Ar, the interfacial molar ratio was essentially zero (only NiO and FeO remained). For nanocrystallite dispersion films grown with O{sub 2}/Ar flow-rate greater than 7.89%, no interfacial (intermixed) Ni{sub 3}Fe phase was detected, which resulted in no measurable exchange bias. Comparing the exchange bias field between the nanocrystallite dispersion films at 5 K, we observed a decrease in the magnitude of the exchange bias field as the nanocrystallite size decreased. The exchange bias coupling for all samples measured set in at essentially the same temperature (i.e., the exchange bias blocking temperature). Since the ferromagnetic/anti-ferromagnetic (FM/AFM) contact area in the nanocrystallite dispersion films increased as the nanocrystallite size decreased, the increase in the magnitude of the exchange bias could be attributed to larger regions of defects (vacancies and bond distortions) which occupied a significant portion of the FM/AFM interfaces in the nanocrystallite dispersion films.

36 MATERIALS SCIENCE↗

Magnetic properties of single-phase MnBi grown from MnBi{sub 49} melt

The single-phase NiAs-type MnBi, embedded in Bi matrix, was grown from homogeneous MnBi{sub 49} melt at low temperatures to prevent the formation of Mn{sub 1.08}Bi. An abrupt magnetization change was observed at ∼240 K. The origin of this change was ascribed to the movement of the Mn atoms between the regular sites and the interstitial sites in the MnBi lattices. The splitting of the x-ray photoelectron lines of MnBi indicates the presence of two binding states of Mn atoms, one of which was ascribed to interstitial Mn atoms. A large coercivity up to 1.79 T at 400 K was observed in the as-grown bulk isotropic MnBi alloys.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗