At least 1,063 records · Page 59

Understanding How Structure and Crystallinity Affect Performance in Solid-State Batteries Using a Glass Ceramic LiV 3 O 8 Cathode

The rate-limiting step in lithiation/delithiation of solid-state cathode materials is not well understood. Phase-transformation reaction rate, lithium ion diffusion coefficient, and lithium ion concentration have all been shown to affect the discharge and charge performance. All three parameters are affected by the crystal structure and crystallinity of the cathode. In this paper, lithium trivanadate (LiV 3 O 8 ) is selected as a representative cathode for all solid-state thin-film batteries because of its glass ceramic properties at different annealing temperatures, where the crystallinity and preferred orientation vary. The intermediate temperature-treated thin films outperform both the amorphous and the most crystalline thin films. By correlating the cell polarization with both the diffusion coefficient and the lithium ion concentration at different states of charge, we gain insights into the electrochemical performance of the glass ceramic LiV 3 O 8 cathode.

25 ENERGY STORAGE↗

Observation of Potential-Induced Hydration on the Surface of Ceramic Proton Conductors Using In Situ Near-Ambient Pressure X-ray Photoelectron Spectroscopy

Interactions of ceramic proton conductors with the environment under operating conditions play an essential role on material properties and device performance. It remains unclear how the chemical environment of material, as modulated by the operating condition, affects the proton conductivity. Combining near-ambient pressure X-ray photoelectron spectroscopy and impedance spectroscopy, we investigate the chemical environment changes of oxygen and the conductivity of BaZr 0.9 Y 0.1 O 3-δ under operating condition. Changes in O 1s core level spectra indicate that adding water vapor pressure increases both hydroxyl groups and active proton sites at undercoordinated oxygen. Applying external potential further promotes this hydration effect, in particular, by increasing the amount of undercoordinated oxygen. The enhanced hydration is accompanied by improved proton conductivity. Here, this work highlights the effects of undercoordinated oxygen for improving the proton conductivity in ceramics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dehydration Rather Than HF Capture Explains Performance Improvements of Li-Ion Cells by Ceramic Nanoparticles

Instability of nickel-rich layered oxides at high voltages is an impediment to their wider use in Li-ion batteries. HF generated via LiPF 6 hydrolysis accelerates corrosion, further destabilizing the material. Ceramic particles are believed to interfere with this corrosion by scavenging HF. Furthermore, we show that the likely mechanism is, in fact, disruption of the hydrolytic cycle due to adsorption of water on ceramic particles, of which MgO performed the best. We suggest that hydrolysis prevention rather than post factum remediation of hydrolytic damage makes a more efficient strategy for protection of the high-voltage cathodes.

25 ENERGY STORAGE↗

High-Energy All-Solid-State Organic–Lithium Batteries Based on Ceramic Electrolytes

Recent studies have identified unique properties of organic battery electrode materials such as moderate redox potentials and mechanical softness which are uniquely beneficial for all-solid-state batteries based on ceramic electrolytes. Here, we further explore the promise of organic materials and demonstrate a sulfide electrolyte- based organic-lithium battery with a specific energy of 828 Wh kg –1 , rivaling the state-of- the-art of all-solid-state batteries. Two innovation steps are responsible for the accomplishment. First, the combination of lithium anode and the high-capacity cathode material pyrene-4,5,9,10-tetraone ensures a high theoretical specific energy. Second, the microstructure of the organic cathode is optimized with the introduction of cryomilling, a technique common to processing soft materials but not familiar to electrode fabrication. The cathode material utilization increases to 99.5% as a result, up from the 55–89% previously reported for ceramic electrolyte-based solid-state organic batteries. In conclusion, the improvement highlights the special requirements of solid-state organic electrodes for microstructural engineering while preserving the chemical integrity of components.

25 ENERGY STORAGE↗

Nanoscale Ion Transport Enhances Conductivity in Solid Polymer-Ceramic Lithium Electrolytes

The predictive design of flexible and solvent-free polymer electrolytes for solid-state batteries requires an understanding of the fundamental principles governing the ion transport. In this work, we establish a correlation among the composite structures, polymer segmental dynamics, and lithium ion (Li + ) transport in a ceramic-polymer composite. Elucidating this structure–property relationship will allow tailoring of the Li + conductivity by optimizing the macroscopic electrochemical stability of the electrolyte. The ion dissociation from the slow polymer segmental dynamics was found to be enhanced by controlling the morphology and functionality of the polymer/ceramic interface. The chemical structure of the Li + salt in the composite electrolyte was correlated with the size of the ionic cluster domains, the conductivity mechanism, and the electrochemical stability of the electrolyte. Polyethylene oxide (PEO) filled with lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) or lithium bis(fluorosulfonyl) imide (LiFSI) salts was used as a matrix. A garnet electrolyte, aluminum substituted lithium lanthanum zirconium oxide (Al-LLZO) with a planar geometry, was used for the ceramic nanoparticle moieties. Further, the dynamics of the strongly bound and highly mobile Li + were investigated using dielectric relaxation spectroscopy. The incorporation of the Al-LLZO platelets increased the number density of more mobile Li + . The structure of the nanoscale ion-agglomeration was investigated by small-angle X-ray scattering, while molecular dynamics (MD) simulation studies were conducted to obtain the fundamental mechanism of the decorrelation of the Li + in the LiTFSI and LiFSI salts from the long PEO chain.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Challenging thermodynamics: combining immiscible elements in a single-phase nano-ceramic

Abstract The Hume-Rothery rules governing solid-state miscibility limit the compositional space for new inorganic material discovery. Here, we report a non-equilibrium, one-step, and scalable flame synthesis method to overcome thermodynamic limits and incorporate immiscible elements into single phase ceramic nanoshells. Starting from prototype examples including (NiMg)O, (NiAl)O x , and (NiZr)O x , we then extend this method to a broad range of Ni-containing ceramic solid solutions, and finally to general binary combinations of elements. Furthermore, we report an “encapsulated exsolution” phenomenon observed upon reducing the metastable porous (Ni 0.07 Al 0.93 )O x to create ultra-stable Ni nanoparticles embedded within the walls of porous Al 2 O 3 nanoshells. This nanoconfined structure demonstrated high sintering resistance during 640 h of catalysis of CO 2 reforming of methane, maintaining constant 96% CH 4 and CO 2 conversion at 800 °C and dramatically outperforming conventional catalysts. Our findings could greatly expand opportunities to develop novel inorganic energy, structural, and functional materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals

All materials can suffer from environmental degradation; the rate and extent of degradation depend on the details of the material composition and structure as well as the environment. The corrosion of silicate glasses, crystalline ceramics, and metals, particularly as related to nuclear waste forms, has received a lot of attention. The corrosion phenomena and mechanisms of these materials are different, but also have many similarities. Furthermore, this review compares and contrasts the mechanisms of environmental degradation of glass, crystalline ceramics, and metals, with the goal of identifying commonalities that can seed synergistic activities and advance the current knowledge in each area.

36 MATERIALS SCIENCE↗

Environmental degradation of high-temperature protective coatings for ceramic-matrix composites in gas-turbine engines

Abstract The need for higher efficiencies and performance in gas-turbine engines that propel aircraft in the air, and generate electricity on land, is pushing the operating temperatures of the engines to unprecedented levels. Replacing some of the current hot-section metallic components with ceramic-matrix composites (CMCs) is making that possible. A high-temperature ceramic coatings system, that includes environmental-barrier coatings (EBCs), are needed to protect CMCs. However, these coatings undergo degradation in the highly hostile environment of the gas-turbine engine consisting of a combination of high gas temperatures, pressures, and velocities. In addition, there is the ubiquitous presence of steam (a combustion by-product) and occasional ingestion of calcia-magnesia-aluminosilicates (CMASs) in the form of dust, sand, or ash from the environment. Steam can cause corrosion of EBCs, and the molten CMAS deposits can react with the EBCs resulting in their failure. This article provides a perspective on the understanding of these degradation mechanisms, and possible approaches, guided by that understanding, for mitigating the degradation. An outlook on the future challenges and opportunities is presented.

Padture, Nitin P. (ORCID:0000000166228559)↗

Grain Boundary Effects on Radiation Damage and Tritium Diffusion in Li–Al–O Ceramics from Molecular Dynamics and Experiments

Understanding irradiation damage and tritium transport in LiAlO2 ceramics is essential for their deployment in tritium-producing burnable absorber rods (TPBARs). Grain boundaries (GBs) play an important role in governing radiation response and tritium transport in LiAlO2 and its secondary phase LiAl5O8. Using molecular dynamics simulations, we investigated defect evolution and tritium diffusion during displacement cascades in single-crystal and bicrystal LiAlO2 and LiAl5O8 at 600 K. The results reveal that GBs suppress the damage in the LiAlO2 bicrystals as compared to single crystals, via interstitial emission. The effect is more pronounced for Li defects, than for Al and O. In LiAl5O8 the damage reduction due to introduction of GB is less pronounced overall. Tritium diffusion coefficients at GBs are higher by factors of 2–10 relative to diffusion inside grain bulk. The effect is particularly pronounced in LiAlO2, where S5, S17, and S25 GBs promote rapid tritium transport, whereas LiAl5O8 exhibits slower diffusion due to reduced free volume at its GBs. These findings evince a trade-off that while GBs mitigate radiation damage by absorbing interstitials, they simultaneously provide fast pathways for tritium migration which is not desirable for TPBAR application. The mechanistic insights gained here establish a foundation for microstructural design strategies to balance radiation tolerance and tritium retention in ceramic breeder materials.

Roy, Ankit↗

Ammonia-fed reversible protonic ceramic fuel cells with Ru-based catalyst

Abstract The intermediate operating temperatures (~400–600 °C) of reversible protonic ceramic fuel cells (RePCFC) permit the potential use of ammonia as a carbon-neutral high energy density fuel and energy storage medium. Here we show fabrication of anode-supported RePCFC with an ultra-dense (~100%) and thin (4 μm) protonic ceramic electrolyte layer. When coupled to a novel Ru-(BaO) 2 (CaO)(Al 2 O 3 ) (Ru-B2CA) reversible ammonia catalyst, maximum fuel-cell power generation reaches 877 mW cm −2 at 650 °C under ammonia fuel. We report relatively stable operation at 600 °C for up to 1250 h under ammonia fuel. In fuel production mode, ammonia rates exceed 1.2 × 10 −8 NH 3 mol cm −2 s −1 at ambient pressure with H 2 from electrolysis only, and 2.1 × 10 −6 mol NH 3 cm −2 s −1 at 12.5 bar with H 2 from both electrolysis and simulated recycling gas.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Chemical interaction and enhanced interfacial ion transport in a ceramic nanofiber–polymer composite electrolyte for all-solid-state lithium metal batteries

This article reports the synergy between ceramic nanofibers and a polymer, and the enhanced interfacial Li-ion transport along the nanofiber/polymer interface in a solid-state ceramic/polymer composite electrolyte, in which a three-dimensional (3D) electrospun aluminum-doped Li 0.33 La 0.557 TiO 3 (LLTO) nanofiber network is embedded in a polyvinylidene fluoride-hexafluoropropylene (PVDF-HFP) matrix. Strong chemical interaction occurs between the nanofibers and the polymer matrix. Addition of the ceramic nanofibers into the polymer matrix results in the dehydrofluorination of the PVDF chains, deprotonation of the –CH 2 moiety and amorphization of the polymer matrix. Solid-state nuclear magnetic resonance (NMR) spectra reveal that lithium ions transport via three pathways: (i) intra-polymer transport, (ii) intra-nanofiber transport, and (iii) interfacial polymer/nanofiber transport. In addition, lithium phosphate is coated on the LLTO nanofiber surface before the nanofibers are embedded into the polymer matrix. The presence of lithium phosphate at the LLTO/polymer interface further enhances the chemical interaction between the nanofibers and the polymer, which promotes the lithium ion transport along the polymer/nanofiber interface. This in turn improves the ionic conductivity and electrochemical cycling stability of the nanofiber/polymer composite. As a result, the flexible LLTO/Li 3 PO 4 /polymer composite electrolyte membrane exhibits an ionic conductivity of 5.1 × 10 -4 S cm -1 at room temperature and an electrochemical stability window of 5.0 V vs. Li/Li + . A symmetric Li|electrolyte|Li half-cell shows a low overpotential of 50 mV at a constant current density of 0.5 mA cm -2 for more than 800 h. In addition, a full cell is constructed by sandwiching the composite electrolyte between a lithium metal anode and a LiFePO 4 -based cathode. Such an all-solid-state lithium metal battery exhibits excellent cycling performance and rate capability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Gel composite electrolyte – an effective way to utilize ceramic fillers in lithium batteries

Achieving synergy between ion-conducting polymers and ceramics in a composite electrolyte has been proven to be difficult as the complicated ceramic/polymer interface presents challenges to understand and control. In this work, we report a strategy to utilize discrete ceramic fillers to form a gel composite electrolyte with enhanced transport properties for lithium metal batteries. The matrix of the composite membrane is crosslinked poly(ethylene oxide) with bis(trifluoromethane)sulfonimide lithium salt (LiTFSI). The membrane is plasticized with tetraethylene glycol dimethyl ether (TEGDME). The incorporation of doped-lithium aluminum titanium phosphate particles (LICGC™) into the membrane greatly improves the membrane's cycling characteristics against the lithium electrode, exhibiting lower interfacial impedance, lower overpotential and higher rate capability. The underpinnings of the superior performance of the gel composite electrolyte are discussed in depth. LICGC™ can immobilize the TFSI - anions in the polymer matrix and simultaneously promote Li+ transport by increasing the plasticizer to Li + ratio. Further, the transport enhancement is achieved without sacrificing mechanical properties. The composite membrane shows significantly improved handleability and processability. This work sheds light on the design strategy for a safe electrolyte towards stable Li metal batteries.

25 ENERGY STORAGE↗

Crystallographic and magnetic identification of secondary phase in orientated Bi{sub 5}Fe{sub 0.5}Co{sub 0.5}Ti{sub 3}O{sub 15} ceramics

The fabrication of highly-oriented polycrystalline ceramics of Bi{sub 5}Fe{sub 0.5}Co{sub 0.5}Ti{sub 3}O{sub 15}, prepared via molten salt synthesis and uniaxial pressing of high aspect ratio platelets is reported. Electron backscatter images show a secondary phase within the ceramic which is rich in cobalt and iron. The concentration of the secondary phase obtained from scanning electron microscopy is estimated at less than 2% by volume, below the detection limit of x-ray diffraction (XRD). The samples were characterized by x-ray diffraction, polarization-electric field measurements, superconducting quantum interference device as a function of sample orientation and vibrating sample magnetometry as a function of temperature. It is inferred from the data that the observed ferromagnetic response is dominated by the secondary phase. This work highlights the importance of rigorous materials characterisation in the study of multiferroics as small amounts of secondary phase, below the limit of XRD, can lead to false conclusions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Room temperature dielectric and magnetic properties of Gd and Ti co-doped BiFeO{sub 3} ceramics

Room temperature dielectric and magnetic properties of BiFeO{sub 3} samples, co-doped with magnetic Gd and non-magnetic Ti in place of Bi and Fe, respectively, were reported. The nominal compositions of Bi{sub 0.9}Gd{sub 0.1}Fe{sub 1–x}Ti{sub x}O{sub 3} (x = 0.00-0.25) ceramics were synthesized by conventional solid state reaction technique. X-ray diffraction patterns revealed that the substitution of Fe by Ti induces a phase transition from rhombohedral to orthorhombic at x > 0.20. Morphological studies demonstrated that the average grain size was reduced from ∼1.5 μm to ∼200 nm with the increase in Ti content. Due to Ti substitution, the dielectric constant was stable over a wide range of high frequencies (30 kHz to 20 MHz) by suppressing the dispersion at low frequencies. The dielectric properties of the compounds are associated with their improved morphologies and reduced leakage current densities probably due to the lower concentration of oxygen vacancies in the compositions. Magnetic properties of Bi{sub 0.9}Gd{sub 0.1}Fe{sub 1–x}Ti{sub x}O{sub 3} (x = 0.00-0.25) ceramics measured at room temperature were enhanced with Ti substitution up to 20% compared to that of pure BiFeO{sub 3} and Ti undoped Bi{sub 0.9}Gd{sub 0.1}FeO{sub 3} samples. The enhanced magnetic properties might be attributed to the substitution induced suppression of spiral spin structure of BiFeO{sub 3}. An asymmetric shifts both in the field and magnetization axes of magnetization versus magnetic field curves was observed. This indicates the presence of exchange bias effect in these compounds notably at room temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Nd:AlN polycrystalline ceramics: A candidate media for tunable, high energy, near IR lasers

We present processing and characterization of Nd-doped aluminum nitride (Nd:AlN) polycrystalline ceramics. We compare ceramics with significant segregation of Nd to those exhibiting minimal segregation. Spatially resolved photoluminescence maps reveal a strong correlation between homogeneous Nd doping and spatially homogeneous light emission. The spectroscopically resolved light emission lines show excellent agreement with the expected Nd electronic transitions. Notably, the lines are significantly broadened, producing near IR emission (~1077 nm) with a remarkable ~100 nm bandwidth at room temperature. We attribute the broadened lines to a combination of effects: multiple Nd-sites, anisotropy of AlN and phonon broadening. These broadened, overlapping lines in a media with excellent thermal conductivity have potential for Nd-based, tunable lasers with high average power.

36 MATERIALS SCIENCE↗

In-situ transmission electron microscopy study of oxygen vacancy ordering and dislocation annihilation in undoped and Sm-doped CeO 2 ceramics during redox processes

Ceria (CeO 2 ) based ceramics have been widely used for many applications due to their unique ionic, electronic, and catalytic properties. We report our findings in investigating into the redox processes of undoped and Sm-doped CeO 2 ceramics stimulated by high-energy electron beam irradiation within a transmission electron microscope (TEM). The reduced structure with oxygen vacancy ordering has been identified as the CeO 1.68 (C-Ce 2 O 3+δ ) phase via high-resolution TEM. The reduction of Ce 4+ to Ce 3+ has been monitored by electron energy-loss spectroscopy. The decreased electronic conductivity of the Sm-doped CeO 2 (Sm 0.2 Ce 0.8 O 1.9 , SDC) is revealed by electron holography, as positive electrostatic charges accumulated at the surfaces of SDC grains under electron beam irradiation, but not at CeO 2 grains. The formation of the reduced CeO 1.68 domains corresponds to lattice expansion compared to the CeO 2 matrix. Therefore, the growth of CeO 1.68 nuclei builds up strain inside the matrix, causing annihilation of dislocations inside the grains. By using in-situ high-resolution TEM and a fast OneView camera recording system, we investigated dislocation motion inside both CeO 2 and SDC grains under electron beam irradiation. The dislocations prefer to dissociate into Shockley partials bounded by stacking faults. Then, the partials can easily glide in the {111} planes to reach the grain surfaces. Even the Lomer-Cottrell lock can be swept away by the phase change induced strain field. Our results revealed the high mobility of dislocations inside CeO 2 and SDC grains during their respective redox processes

36 MATERIALS SCIENCE↗

Thermal conductivity evaluation of ion irradiated Si 3 N 4 and ZrN ceramics using spatial domain thermoreflectance

Nitride ceramics have been investigated for different applications in the nuclear industry, such as space nuclear power, fusion reactor diagnostics and plasma heating, inert matrix fuels, and accident tolerant fuels. Although thermal conductivity remains one of the most important properties to track following irradiation, traditional techniques such as laser flash and xenon flash are limited to bulk sample characterization, which requires lengthy and cost-consuming neutron irradiation. This work used spatial domain thermoreflectance (SDTR) for the micrometer-scale measurement of thermal conductivity in 15 MeV Ni ion-irradiated silicon nitride and zirconium nitride from 1 to 50 dpa and 300 to 700 °C. Here, the SDTR-measured unirradiated thermal conductivity was found to be consistent with the published data on bulk samples. Electrically conductive ZrN exhibits modest reduction after irradiation which is minimal at the highest irradiation temperatures. In electrically insulating Si 3 N 4 , the reduction is more significant and unlike ZrN, the reduction remains significant even at a higher irradiation temperature. The thermal resistance evolution following irradiation was compared with lattice swelling, which was determined using grazing incidence x-ray diffraction, and radiation-induced defects were observed using transmission electron microscopy. A saturation value was observed between 15 and 50 dpa for thermal conductivity degradation in both nitride ceramics and a direct correlation with high-temperature defect recombination was observed, as well as the potential presence of additional carrier scattering mechanisms.

36 MATERIALS SCIENCE↗

Effects of a refractory metal protective barrier on uranium carbonitride ceramic–metallic composites exposed to a high temperature hydrogen environment

Uranium nitride has been under consideration at NASA and the Department of Energy for nuclear thermal propulsion applications intended for deep space exploration vehicles. It is critical to the success of the technology development that the behavior of the fuel system is properly characterized in operational environments. This body of work fabricated ceramic metal composites consisting of uranium ceramic fuel in a molybdenum and molybdenum–tungsten metal matrix, both with and without an exterior molybdenum barrier. Specimens were introduced to a high temperature hydrogen environment and characterized through x-ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy to identify characteristic changes. A portion of the specimens was fabricated with a 1.27 mm thick molybdenum barrier in order to isolate the material from the hydrogen environment. Instability of the uranium nitride occurred as low as 2073 K, leading to aggressive instability approaching 2658 K. Carbon reactions with the metal matrix were observed as well as alloying between the uranium and metal matrix constituents. The liquid uranium resulting from the instability of the uranium nitride was observed to attack the grain boundaries of the refractory metal, resulting in the formation of a liquid uranium molybdenum eutectic melt. Specimens encased in a barrier experienced similar results. The authors conclude this is a significant challenge to applications of this cermet at these temperatures. Alternate configurations with resilient hermetic seals or lower temperature applications such as power reactors may have more success.

36 MATERIALS SCIENCE↗