Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,045 records · Page 58

Effect of Residual Accelerations on the Crystal Growth of II-VI Semiconductors in Low Earth Orbit

The paper compares and summarizes the effects of residual acceleration during crystal growth on the compositional variation of two II-VI solid solution binary alloys (Hg(0.8)Cd(0.2)Te and Hg(0.84)Zn(0.16)Te). The crystals were grown by directional solidification on the second United States Microgravity Payload (USMP-2) and the first United States Microgravity Laboratory (USML-1) missions, respectively. For both alloys, changes in the direction and magnitude of the quasisteady acceleration vector (approximately 0.4- 1 mu g) caused large changes in the radial compositional distribution that demonstrates the importance of residual accelerations, even in the submicrogravity range, for large density gradients in the melt and slow solidification rates. The observed compositional variations will be correlated to changes in the radial flow velocities ahead of the solidification interface.

Gillies, D. C.↗

Pore Formation and Mobility Investigation (PFMI): Concept, Hardware Development, and Initial Analysis of Experiments Conducted Aboard the International Space Station

Porosity in the form of "bubbles and pipes" can occur during controlled directional solidification processing of metal alloys. This is a consequence that 1) precludes obtaining any meaningful scientific results and 2) is detrimental to desired material properties. Unfortunately, several Microgravity experiments have been compromised by porosity. The intent of the PFMl investigation is to conduct a systematic effort directed towards understanding porosity formation and mobility during controlled directional solidification (DS) in a microgravity environment. PFMl uses a pure transparent material, succinonitrile (SCN), as well as SCN "alloyed" with water, in conjunction with a translating temperature gradient stage so that direct observation and recording of pore generation and mobility can be made. PFMl is investigating the role of thermocapillary forces and temperature gradients in affecting bubble dynamics as well as other solidification processes in a microgravity environment. This presentation will cover the concept, hardware development, operations, and the initial results from experiments conducted aboard the International Space Station.

Grugel, Richard N.↗

Pore Formation and Mobility Investigation (PFMI): Concept, Hardware Development and Initial Analysis of Experiments

Porosity in the form of "bubbles and pipes" can occur during controlled directional solidification processing of metal alloys. This is a consequence that 1) precludes obtaining any meaningful scientific results and 2) is detrimental to desired material properties. Unfortunately, several Microgravity experiments have been compromised by porosity. The intent of the PFMI investigation is to conduct a systematic effort directed towards understanding porosity formation and mobility during controlled directional solidification (DS) in a microgravity environment. PFMI uses a pure transparent material, succinonitrile (SCN), as well as SCN "alloyed" with water, in conjunction with a translating temperature gradient stage so that direct observation and recording of pore generation and mobility can be made. PFMI is investigating the role of thermocapillary forces and temperature gradients in affecting bubble dynamics as well as other solidification processes in a microgravity Environment. This presentation will cover the concept, hardware development, operations, and the initial results from experiments conducted aboard the International Space Station. .

Grugel, Richard N.↗

Crystal Growth Using MEPHISTO

The shuttle flight experiment "In Situ Monitoring of Crystal Growth Using MEPHISTO" was accomplished during STS-87 as part of the fourth flight of the United States Microgravity Payload (USMP-4), which was flown from November 19 to December 5, 1997. The data returned from that flight are just now beginning to yield quantitative results. This project is an international collaboration: the furnace system known as MEPHISTO was built in France by CNES (French National Space Agency) and CEA (French Atomic Energy Commission); the principal investigator, Prof. Reza Abbaschian, is from the University of Florida at Gainesville; and numerical and analytical modeling support includes collaborators from the University of New South Wales, Australia, the University of Wisconsin at Milwaukee, the National Institute of Standards and Technology, and the NASA Lewis Research Center. MEPHISTO is a French acronym that translates into English as Materials for the Study of Interesting Phenomena of Solidification on Earth and in Orbit. Since this was the fourth flight of the MEPHISTO furnace, the experiment is referred to as MEPHISTO-4. MEPHISTO-4 was a directional solidification experiment that studied the liquid-to-solid transformation of bismuth alloyed with tin. Directional solidification is a freezing technique common to the processing of the electronic materials used in integrated circuits and detectors, such as silicon and germanium. When liquids are frozen on Earth, they must be cooled. The cooling causes stirring because of density variations in the liquid. This stirring, known as natural convection, influences the quality of the resulting solid. During freezing, regions of high and low concentrations of tin are created. This introduces another important phenomenon: diffusion, or the movement by molecular action of matter from regions of high concentration to regions of lower concentration. In MEPHISTO-4, it is tin that diffuses from the high-concentration region in front of the solid-liquid interface to more distant low-concentration regions.

deGroh, Henry C., III↗

Directionally Solidified NiAl-Based Alloys Studied for Improved Elevated-Temperature Strength and Room-Temperature Fracture Toughness

Efforts are underway to replace superalloys used in the hot sections of gas turbine engines with materials possessing better mechanical and physical properties. Alloys based on the intermetallic NiAl have demonstrated potential; however, they generally suffer from low fracture resistance (toughness) at room temperature and from poor strength at elevated temperatures. Directional solidification of NiAl alloyed with both Cr and Mo has yielded materials with useful toughness and elevated-temperature strength values. The intermetallic alloy NiAl has been proposed as an advanced material to extend the maximum operational temperature of gas turbine engines by several hundred degrees centigrade. This intermetallic alloy displays a lower density (approximately 30-percent less) and a higher thermal conductivity (4 to 8 times greater) than conventional superalloys as well as good high-temperature oxidation resistance. Unfortunately, unalloyed NiAl has poor elevated temperature strength (approximately 50 MPa at 1027 C) and low room-temperature fracture toughness (about 5 MPa). Directionally solidified NiAl eutectic alloys are known to possess a combination of high elevated-temperature strength and good room-temperature fracture toughness. Research has demonstrated that a NiAl matrix containing a uniform distribution of very thin Cr plates alloyed with Mo possessed both increased fracture toughness and elevated-temperature creep strength. Although attractive properties were obtained, these alloys were formed at low growth rates (greater than 19 mm/hr), which are considered to be economically unviable. Hence, an investigation was warranted of the strength and toughness behavior of NiAl-(Cr,Mo) directionally solidified at faster growth rates. If the mechanical properties did not deteriorate with increased growth rates, directional solidification could offer an economical means to produce NiAl-based alloys commercially for gas turbine engines. An investigation at the NASA Glenn Research Center at Lewis Field was undertaken to study the effect of the directional solidification growth rate on the microstructure, room temperature fracture toughness, and strength at 1027 C of a Ni-33Al-31Cr-3Mo eutectic alloy. The directionally solidified rates varied between 7.6 and 508 millimeters per hour Essentially fault-free, alternating (Cr, Mo)/NiAl lamellar plate microstructures (left photograph) were formed during growth at and below 12.7 mm/hr, whereas cellular microstructures (right photograph) with the (Cr, Mo) phase in a radial spokelike pattern were developed at faster growth rates. The compressive strength at 1027 C continuously increased with increasing growth rate and did not indicate a maxima as was reported for directionally solidified Ni-33Al-34Cr. Surprisingly, samples with the lamellar plate microstructure (left photograph) possessed a room-temperature fracture toughness of approximately 12 MPa(sup square root of m), whereas all the alloys with a cellular microstructure had a toughness of about 17 MPa(sup square root of m). These results are significant since they clearly demonstrate that Ni-33Al-31Cr-3Mo can be directionally solidified at much faster growth rates without any observable deterioration in its mechanical properties. Thus, the potential to produce strong, tough NiAl-based eutectics at commercially acceptable growth rates exists. Additional testing and alloy optimization studies are underway.

Whittenberger, J. Daniel↗

Weld repair of directionally solidified articles

A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent of the solidus temperature of the base material in a chamber containing a protective gas that inhibits oxidation of the base material. The defect is filled with a filler metal while maintaining the article at the repair temperature. The filling is accomplished by providing a source of the filler metal of substantially the same composition as the base material of the directionally solidified article, and melting the filler metal into the defect progressively while moving the source of the filler metal relative to the article in a direction parallel to the solidification direction. Optionally, additional artificial heat extraction is accomplished in a heat-flow direction that is within about 45 degrees of the solidification direction, as the filler metal solidifies within the defect. The article may thereafter be heat treated.

Smashey, Russell W.↗

Directionally solidified article with weld repair

A directionally solidified nickel-base superalloy article has a defect therein extending parallel to the solidification direction. The article is repaired by removing any foreign matter present in the defect, and then heating the article to a repair temperature of from about 60 to about 98 percent of the solidus temperature of the base material in a chamber containing a protective gas that inhibits oxidation of the base material. The defect is filled with a filler metal while maintaining the article at the repair temperature. The filling is accomplished by providing a source of the filler metal of substantially the same composition as the base material of the directionally solidified article, and melting the filler metal into the defect progressively while moving the source of the filler metal relative to the article in a direction parallel to the solidification direction. Optionally, additional artificial heat extraction is accomplished in a heat-flow direction that is within about 45 degrees of the solidification direction, as the filler metal solidifies within the defect. The article may thereafter be heat treated.

Smashey, Russell W.↗

Projection Method for Flows with Large Density Variations

Numerical models of solidification including a mushy zone are notoriously inefficient; most of them are based on formulations that require the coupled solution of the velocity components in the momentum equation greatly restricting the range of applicability of the models. There are only two models known to the authors that have used a projection or fractional step formulation, but none of these were used to model problems of any significant size. A third model was only applied to a partial mushy zone with no all-fluid region. Our initial attempts at modeling directional solidification in the presence of a developing mushy zone using a projection formulation encountered very serious difficulties once solidification starts. These difficulties were traced to the inability of the method to deal with large local density differences in the vicinity of the fluid-mush interface. As a result, a modified formulation of the projection method has been developed, that maintains the coupling between the body force and the pressure gradient and is presented in this work. The new formulation is shown to be robust and efficient, and can be applied to problems involving very large meshes. This is illustrated in this work through its application to simulations involving Pb-Sb and Pb-Sn alloys.

Heinrich, Juan C.↗

Microstructural Evaluation and Comparison of Solder Samples Processed Aboard the International Space Station

Samples from the In-Space Soldering Investigation (ISSI), conducted aboard the International Space Station (ISS), are being examined for post-solidification microstructural development and porosity distribution. In this preliminary study, the internal structures of two ISSI processed samples are compared. In one case 10cm of rosin-core solder was wrapped around a coupon wire and melted by conduction, whereas, in the other a comparable length of solder was melted directly onto the hot wire; in both cases the molten solder formed ellipsoidal blobs, a shape that was maintained during subsequent solidification. In the former case, there is clear evidence of porosity throughout the sample, and an accumulation of larger pores near the hot end that implies thermocapillary induced migration and eventual coalescence of the flux vapor bubbles. In the second context, when solder was fed onto the wire. a part of the flux constituting the solder core is introduced into and remains within the liquid solder ball, becoming entombed upon solidification. In both cases the consequential porosity, particularly at a solder/contact interface, is very undesirable. In addition to compromising the desired electrical and thermal conductivity, it promotes mechanical failure.

Grugel, R. N.↗

Materials Science Research Rack Onboard the International Space Station Hardware and Operations

The Materials Science Research Rack (MSRR) is a research facility developed under a cooperative research agreement between NASA and ESA for materials science investigations on the International Space Station (ISS). MSRR was launched on STS-128 in August 2009, and is currently installed in the U.S. Destiny Laboratory Module. Since that time, MSRR has performed virtually flawlessly, logging more than 620 hours of operating time. The MSRR accommodates advanced investigations in the microgravity environment on the ISS for basic materials science research in areas such as solidification of metals and alloys. The purpose is to advance the scientific understanding of materials processing as affected by microgravity and to gain insight into the physical behavior of materials processing. MSRR allows for the study of a variety of materials including metals, ceramics, semiconductor crystals, and glasses. Materials science research benefits from the microgravity environment of space, where the researcher can better isolate chemical and thermal properties of materials from the effects of gravity. With this knowledge, reliable predictions can be made about the conditions required on Earth to achieve improved materials. MSRR is a highly automated facility with a modular design capable of supporting multiple types of investigations. Currently the NASA-provided Rack Support Subsystem provides services (power, thermal control, vacuum access, and command and data handling) to the ESA developed Materials Science Laboratory (MSL) which accommodates interchangeable Furnace Inserts (FI). Two ESA-developed FIs are presently available on the ISS: the Low Gradient Furnace (LGF) and the Solidification and Quenching Furnace (SQF). Sample-Cartridge Assemblies (SCAs), each containing one or more material samples, are installed in the FI by the crew and can be processed at temperatures up to 1400 C. Once an SCA is installed, the experiment can be run by automatic command or science conducted via telemetry commands from the ground. Initially, 12 SCAs were processed in the first furnace insert for a team of European and US investigators. After these samples were processed the Furnaces Inserts were exchanged and an additional single sample was processed. The processed samples have been returned to Earth for evaluation and comparison of their properties to samples similarly processed on the ground. A preliminary examination of the samples indicates that the majority of the desired science objectives have been successfully met leading to significant improvements in the understanding of alloy solidification processes. Six SCAs were launched on Space Shuttle Mission STS-135 in July 2011 for processing during the Fall of 2011. Additional batches are planned for future processing. This facility is available to support additional materials science investigations through programs such as the US National Laboratory, Technology Development, NASA Research Announcements, and others.

Lehman, John R.↗

The Case for a Heat-Pipe Phase of Planet Evolution on the Moon

The prevalence of anorthosite in the lunar highlands is generally attributed to the flotation of less dense plagioclase in the late stages of the solidification of the lunar magma ocean. It is not clear, however, that these models are capable of producing the extremely high plagioclase contents (near 100%) observed in both Apollo samples and remote sensing data, since a mostly solid lithosphere forms (at 60-70% solidification) before plagioclase feldspar reaches saturation (at approximately 80% solidification). Formation as a floating cumulate is made even more problematic by the near uniformity of the alkali composition of the plagioclase, even as the mafic phases record significant variations in Mg/(Mg+Fe) ratios. These problems can be resolved for the Moon if the plagioclase-rich crust is produced and refined through a widespread episode of heat-pipe magmatism rather than a process dominated by density-driven plagioclase flotation. Heat-pipes are an important feature of terrestrial planets at high heat flow, as illustrated by Io's present activity. Evidence for their operation early in Earth's history suggests that all terrestrial bodies should experience an early episode of heat-pipe cooling. As the Moon likely represents the most wellpreserved example of early planetary thermal evolution in our solar system, studies of the lunar surface and of lunar materials provide useful data to test the idea of a universal model of the way terrestrial bodies transition from a magma ocean state into subsequent single-plate, rigid-lid convection or plate tectonic phases.

Simon, J. I.↗

Metallic Powder Core Tubular Wire (PCTW) Development for Additive Manufacturing

NASA Langley Research Center (LaRC) in Hampton, VA, and the Center for Welding, Joining, and Coating Research (CWJCR) in the Department of Metallurgical and Materials Engineering at the Colorado School of Mines (CSM) in Golden, CO, have collaborated for nearly fifteen years to develop metallic powder core tubular wire (PCTW) feedstock for additive manufacturing (AM) using electron beam deposition. The motivation for this development was to offset dealloying observed during deposition of titanium and aluminum alloy solid wire feedstock in the LaRC electron beam freeform fabrication (EBF3) system and to explore novel alloy compositions by tailoring the powder fill. EBF3 is a fusion-based AM process that is performed under vacuum and is consequently prone to vaporization loss of low vapor pressure alloying elements. Research spanning four graduate student research projects succeeded in developing the basic methodology to fabricate PCTW, the mass balance equations used to define the powder fill, microstructure control through particulate inoculation, and the feasibility of producing metal matrix composite materials. Metallic PCTW is comprised of a thin foil sheath wrapped around a powder blend. Fabrication of PCTW at CSM was accomplished using a tubular wire mill system to first bend a flat strip into a u-shaped cross section, deposit a powder fill, create a lap joint to seal the wire, and draw to final diameter. Powder management systems were developed to ensure uniform mixing of powder constituents and identify feed rates for optimum fill ratios. Processing parameters were successfully developed for titanium and aluminum alloy sheaths to account for material work hardening during drawing. Mass balance equations were developed to account for compositional contributions of the sheath and powder fill. PCTW composition can be adjusted through selection of the sheath or powder materials. PCTWs were successfully developed to offset Al loss in deposits of Ti-6-4 and Mg loss in Al 6061, resulting in deposits that were within the composition limits for each material. Ti-6-4 deposits were fabricated using PCTW comprised of commercially pure (CP) titanium sheath and a fill of pre-alloyed Ti-6-4 powder with additions of elemental Al and V powders. Additions of both elements were required to account for the CP Ti from the sheath, and Al was further enhanced to offset documented losses in EBF3 deposits. For Al 6061 deposits, composition was modulated through the choice of sheath material. The PCTW was made using an Al 5052 sheath to supplement Mg content and a fill composition of pre-alloyed 6061 powder with additions of Si and Cu.The slower solidification rate of the EBF3 process compared with laser powder bed fusion processes can lead to coarse-grained microstructures and mechanical property anisotropy. EBF3deposits of Ti-6-4 exhibited large epitaxially grown β grains, which result in degraded mechanical properties in the deposition direction. Microstructure refinement was achieved through a combination of electron beam modulation and the use of a PCTW designed for Ti-6-4 deposits and modified by the addition of powder made from Fe and B. Resulting deposits exhibited reductions in β grain size, α phase colony intercept length and lath width, and an increased volume fraction of β phase. The mechanism of microstructure refinement was related to precipitation of boride particles. Hardness testing confirmed that mechanical property anisotropy was reduced and an overall increase in hardness was achieved.Metal matrix composite (MMC) materials offer strength and stiffness benefits over unreinforced materials. Two methods were investigated using PCTW technology for producing Al 6061 basedMMC materials; the direct addition of SiC reinforcing particles and the in-situ generation of reinforcements through reaction synthesis of precursor powders. Al 6061 based MMCs reinforced with SiC exhibited particle clustering and formation of aluminum carbides during deposition. The application of a Ni coating to the SiC particles prior to incorporation into the powder fill eliminated aluminum carbide formation and aided particle distribution during deposition. Modulation of beam focus and power further reduced aluminum carbide formation and aided particle distribution. In reaction synthesis, precursor additions undergo an exothermic reaction during deposition to form new ceramic products, generally of finer scale than the initial precursor components. The product phases provide reinforcement in the MMC and act as nucleation sites during solidification, resulting in grain refinement, improved mechanical properties, and reduced susceptibility to solidification cracking. Higher tensile strength and stiffness were demonstrated in Al 6061 based MMCs with 2 vol% reinforcement. These combined research efforts demonstrate the potential of PCTW technology for customizing of alloy composition and achieving microstructure control. A manufacturing process for titanium- and aluminum-based PCTWs was developed based on iterative design, theoretical calculations, and empirical data. PCTW technology successfully mitigated Al loss from Ti-6-4 and Mg loss in Al 6061, resulted in grain refinement in Ti-6-4, and demonstrated fabrication of Al based MMCs

Marcia S Domack↗

Disorder to Order in Interface Patterns: Thermal Noise to Limit Cycle Transition in Dendrite Sidebranch Formation

Thin sample directional solidification experiments have been carried out in the model succinonitrile-camphor system to examine the origin of secondary branches in dendrite morphologies. Thermal noise at the dendrite tip creates interface instabilities which amplify to form sidebranches. This is accepted as the primary mode of sidebranching in dendritic growth from an undercooled melt and occurs in directional solidification of dendrites. The proposed limit cycle couples the growth of the tip with the initiation of the sidebranch. Directional solidification of curved interfaces is a driven dissipative system with the potential to form a limit cycle. Two sets of experiments were performed, the first holding velocity constant and evolving the gradient and the second imposing oscillating velocities around the natural period of sidebranching. Both experimental methods were found to characterize a transition from disordered sidebranching induced by thermal noise to ordered sidebranching produced by the limit cycle mechanisms. This is the first quantitative measurement of previously hypothesized limit cycle growth. These experiment sets have been quantitatively analyzed for dynamic behavior seen in limit cycles. High-quality data sets of the tip and instability enable the measurement of the FFT and analysis through a power spectrum. At low gradients, the sidebranches are found to be excited by thermal noise far away from the tip. As the gradient increases and velocity is held constant, the distance between the instability and tip decreases until limit cycle growth is found between the tip of the primary dendrite and the first forming sidebranch. An alternative to the deterministic limit cycles seen in experiments of gradient evolution is a limit cycle actively driven through the square wave oscillation of velocity. Crucial observations of the solidified microstructure conclude that this produced periodic interconnected bridges between the primary dendrites. This is a finding with potentially significant implications for commercial applications.

Trevor Lyons↗

Entrapment of Inclusions by Solidified Hooks at the Subsurface of Ultra-Low-Carbon Steel Slab

To understand the mechanism for the entrapment of non-metallic inclusions by curved hooks beneath the surface of continuous casting slabs, the etching of the slab, the observation of hooks and the detection of inclusions on sections vertical and parallel to the slab surface were performed. The location of inclusions and hooks was revealed, and forces acting on the inclusion below a hook were analyzed. Inclusions gathered more below the curved hook than in the overflow zone above the hook. From the observation of hooks and inclusions on sections vertical to the slab surface, the number density of 3 to 5 μm inclusions in the hook zone and no-hook zone was very close, while the number density of > 10 μm inclusions in the hook zone was larger than that in the no-hook zone. From the observation on sections parallel to the slab surface, > 20 μm inclusions were located near the hook line more than in other regions, and the number density of inclusions in the hook zone was more than that in the no-hook zone. The apparent friction coefficient dominated the critical capturing size of inclusions from the solidification front, and the deflection angle, flow velocity, sulfur content and solidification velocity had influences on the size range.

36 MATERIALS SCIENCE↗

Microsegregation Measurement: Methods and Applications

Microsegregation is chemical variation at the microstructural level in a solidified ingot, which can cause undesirable effects on material properties. Its formation is driven by different levels of solute elemental solubility between solid and liquid phases, resulting in solute buildup or depletion in the liquid phase during solidification. Characterization of microsegregation can be essential for understanding its formation and removing it through heat treatment. Measurement is frequently carried out via scanning electron microscope (SEM), though metallographic analysis, mechanical testing and optical radiography have been used. SEM analysis can consist of point measurements on single dendrites, line scans across or along dendrites, elemental maps, and extended line-based or grid-based analyses extending over many dendrites, which can generate large amounts of data. Line-based or grid-based data can be analyzed using scatterplots of element concentrations to visualize segregation behavior and sorting/ranking of data by a single element or a combination of elements, to give compositional profiles as a function of extent of solidification. For both qualitative and quantitative analyses, effects of phase transformations and secondary phases need to be considered as well as sorting of measurement errors when generating compositional profiles. Applications of analysis include determination of partition ratios, examination of solute–element interactions, determination of effects of cooling rate and back diffusion, applications to freckling studies, validations of modeling, and development of heat-treatment profiles.

36 MATERIALS SCIENCE↗

A Comprehensive Analysis of Macrosegregation Formation During Twin-Roll Casting

A two-phase Eulerian–Eulerian volume-averaged model is used to predict the formation of macrosegregation during the twin-roll casting of inoculated Al-4 wt pct Cu alloys. For low solid fractions, the equiaxed crystals are modeled according to the submerged object approach. However, above a given transition limit, they are assumed to behave like a viscoplastic material. This means that the solid phase behaves as a coherent structure that can influence the motion of the liquid. Such approach allows one to take into account the flow dynamics arising from the occurrence of both solidification and hot rolling simultaneously, which usually occurs in twin-roll casting. Therefore, it is possible to explain the origin of the macrosegregation patterns obtained in the simulations based on the relative motion between the phases. Compression-induced expulsion of segregated melt is observed as a result of the deformation of the solidifying shells. Such occurrence leads to a negative macrosegregation region in the outer part of the as-cast strip. Then, because the solute-enriched melt is squeezed out toward adjacent regions, two positively segregated bands can be found near the center of the domain. Furthermore, it is shown how solidification-induced feeding weakens the absolute value of the negative and positive segregation bands.

36 MATERIALS SCIENCE↗

Characterization of Inclusions in 3rd Generation Advanced High-Strength Steels

Samples taken from laboratory-produced 3rd generation advanced high-strength steels, solidified at a low cooling rate, have been investigated to study the characteristics of non-metallic inclusions. Two steels, containing 2 and 5 pct Mn content, were produced for this purpose. A higher number of total inclusions were observed in 5 pct Mn steel. The four main types of inclusions observed were Al{sub 2}O{sub 3}, AlN, MnS, and AlSiMn-oxide. These classes were divided into subclasses according to variations in their chemistry. The major subclasses of AlN inclusions are either plate-like or regular in shape and have different size distributions. Thermodynamic calculations suggest that plate-like AlN inclusions are formed at the initial stage of solidification, while faceted/regular-shaped inclusions are precipitated toward the end of solidification. Moreover, it was found that the size of nitride inclusions is related to their N content. This phenomenon is discussed from the viewpoint of nucleation theory.

36 MATERIALS SCIENCE↗

Closure of Internal Porosity in Continuous Casting Bloom During Heavy Reduction Process

To investigate the closure behavior of internal porosity (also referred to as internal void) in continuous casting bloom during heavy reduction (HR) and thus provide theoretical guidance for minimizing this kind of internal defect more effectively with HR, a three-dimensional (3D) mechanical model was developed based on the predicted temperature field by a 2D heat transfer model. With this 3D mechanical model, closure behaviors of internal porosity in continuous casting bloom during HR at and after the strand solidification end under different process conditions were numerically studied. It was found that the void axis length decreased significantly along the bloom thickness direction and increased slightly along the casting and bloom width directions after HR, and the influence of the initial void size on the void closure was not obvious. With a decrease of temperature difference between the bloom surface and center, HR efficiency for minimizing internal void decreased, while the required reduction force significantly increased. Compared with blooms with a uniform temperature distribution of 1100 °C, the void closure index after HR implemented at the strand solidification end was increased by ~ 25 pct. Compared with a conventional flat roll, the application of a convex roll during HR could contribute to minimizing the internal porosity more effectively and significantly enhance the reduction capacity of the withdrawal and straightening units. The void closure index of η{sub s} and η{sub v} (where η{sub s} and η{sub v} were defined based on the variation of the void aspect ratio and the void volume, respectively) was closely related to the equivalent strain (ε{sub eq}) and the hydrostatic integration parameter (Q), respectively, and two mathematical equations were derived to quantitatively describe the relationship of η{sub s} − ε{sub eq} and η{sub v} − Q.

36 MATERIALS SCIENCE↗