Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “sintering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,045 records · Page 58

UO 2 + 5 vol% ZrB 2 nano composite nuclear fuels with full boron retention and enhanced oxidation resistance

The boron isotope ( 10 B) can be used as a neutron absorber in UO 2 to control the reactivity of nuclear fuel pellets, however, the boron source can react with oxygen source in UO 2 to form B 2 O 3 that vaporize readily at temperatures above 1200 °C. Unfortunately, the sintering of UO 2 fuel requires hours holding at high temperature (>1700 °C), resulting in an inevitable B loss during sintering and unpredictable B concentration in final product. It is challenging to incorporate boron through a conventional sintering method. In this work, we demonstrated that spark plasma sintering (SPS), a field assisted sintering technology, can effectively densify UO 2 + 5 vol% ZrB 2 composite fuel pellets by rapid consolidation at 1600 °C for a short duration of 5 min under an applied pressure of 40 MPa. Further, thermogravimetric analysis (TGA) measurements confirm that ZrB 2 is fully retained inside the composite fuel pellets. Inside the composite fuel pellets, nano sized ZrB 2 particles are uniformly distributed along the grain boundaries of the UO 2 matrix. The ZrB 2 particle transforms to a glassy B 2 O 3 phase covering the sample surface and grain boundaries of UO 2 matrix after a simple post-sintering annealing at 1000 °C in flowing Argon gas for 4 h. The formed glassy B 2 O 3 slows down the diffusion of oxygen ions and postpones the onset temperature for oxidation of UO 2 from 400 °C to 550 °C. This study demonstrates the capability of SPS, an advanced fuel manufacturing technique, to achieve a full retention of ZrB 2 in UO 2 oxide fuel and increase oxidation resistance through a simple post-sintering annealing. The reported work holds great engineering potential for development of advanced oxide fuel for nuclear application.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Final-stage densification kinetics of direct current–sinteredZrB2

Final-stage sintering was analyzed for nominally phase pure zirconium diboride synthesized by borothermal reduction of high-purity ZrO2. Analysis was conducted on ZrB2 ceramics with relative densities greater than 90% using the Nabarro–Herring stress–directed vacancy diffusion model. Temperatures of 1900°C or above and an applied uniaxial pressure of 50 MPa were required to fully densify ZrB2 ceramics by direct current sintering. Ram travel data were collected and used to determine the relative density of the specimens during sintering. Specimens sintered between 1900 and 2100°C achieved relative densities greater than 97%, whereas specimens sintered below 1900°C failed to reach the final stage of sintering. The average grain size ranged from 1.0 to 14.7 μm. The activation energy was calculated from the slope of an Arrhenius plot that used the Kalish equation. The activation energy was 162 ± 34 kJ/mol, which is consistent with the activation energy for dislocation movement in ZrB2. The diffusion coefficients for dislocation motion that controls densification were 5.1 × 10−6 cm2/s at 1900°C and 5.1 × 10−5 cm2/s at 2100°C, as calculated from activation energy and average grain sizes. This study provides evidence that the dominant mechanism for final-stage sintering of ZrB2 ceramics is dislocation motion.

36 MATERIALS SCIENCE↗

Binder jet additive manufacturing of ceramic heat exchangers for concentrating solar power applications with thermal energy storage in molten chlorides

Triply periodic minimal surface (TPMS) geometries can only be fabricated by additive manufacturing methods and are of interest for heat exchangers. Ceramic TPMS heat exchangers can operate at higher temperatures and pressures with superior performance and increased operating efficiencies compared to metal heat exchangers. The properties of ultra-high temperature ceramic (UHTC) materials are also favorable for heat exchangers and potentially suited to concentrated solar power (CSP) systems, such as those based on a molten chloride salt thermal energy storage (TES) medium used to heat CO 2 in a closed-loop Brayton power cycle. We intended to demonstrate binder jet additive manufacturing feasibility of a UHTC-TPMS structure by printing and sintering a null candidate. We aimed to achieve parts with a relative density ≥ 92 % of theoretical and to provide a TPMS part demonstration. The target density indicates the transition from intermediate to final stage sintering, a requirement to inhibit gas permeability and for sintering complex near net shapes to full density with sinter-HIP technology. The goal of the TPMS part demonstration was to determine if printing and sintering parameters developed from test coupons apply to the complex geometries that will eventually be used in a heat exchanger design. Our objective was to print cubic TPMS parts with a 9 cm 3 volume and sinter it without distorting and cracking. We report we were able to sinter ZrB 2 -MoSi 2 composite parts based on the Schwarz-D TPMS and achieve isotropic shrinkage up to 60 % by volume, resulting in densities ranging from 92 % to 96 % of theoretical.

36 MATERIALS SCIENCE↗

U Metal Oxidation with Steam (U)

The Savannah Rive National Laboratory 9SRNL) is evaluating a method to produce uranium oxide (UO 2 ) from uranium metal using steam. The typical methods for making UO 2 yield powders with particle-size ranges of 1 to 50 micron. The goal of the steam oxidation is to produce a depleted uranium (DU) product with a larger particle size that can be used as a surrogate for testing physical and mechanical process techniques to refine uranium and/or plutonium bearing residues. Several studies in the literature indicated that reactions between uranium metal and steam will yield UO 2 as fine powders in the 160 to 500 °C range, but granular materials form above 500°C. Above 880 °C, a hard compact scale forms on the U metal. Furthermore, sintering of UO 2 occurs at about 1300 °C, but it has been stated that the presence of steam enhances the sintering characteristics of UO 2 . Initial studies into the oxidation of DU metal in an atmosphere of argon and steam have been completed. Oxidation of depleted uranium metal in Ar/steam at 600, 710, 700, and 830 °C yielded at UO 2 product with little or no impurity at each temperature. Although not enough sample was available to perform sieve analysis for particle size distribution, SEM images reveal that a significant volume fraction of the products at 710, 770, and 830 °C exceeds 100 microns. The material produced at 600 °C was too fine for programmatic needs. Questions associated with the UO 2 include morphology of product, mechanical strength of the particles, and performance in milling operations. The size of the samples produced in these tests did not allow for quantitative assessment of particle size of mechanical strength. A qualitative assessment of the particles formed at 710, 770, and 830 °C was that the samples produced at 710 and 770 °C were friable, and the sample produced 830 °C had more mechanical strength. Sintering of the samples in Ar/steam at 970 °C appeared to increase the strength of the particles without changing their general particle size characteristics. Due to the small sample sizes, the increase in strength could not be quantified. If the sintering at 970 °C is inadequate, higher sintering temperatures in Ar/steam can be evaluated. Future work will increase scale of the steam oxidation conditions which yield the most-favorable particle-size distributions with sufficient mechanical strength for programming usage. Further consideration will be given to oxidation temperature, steam addition to the reaction vessel, U metal pretreatment, and sintering conditions after oxidation. The UO 2 production could involve a two-step process where particles are formed in steam at lower temperatures (700-850 °C) and then sintered in Ar/steam at elevated temperatures (950-1200 °C). Larger samples (50-100 g each) will provide sufficient UO 2 product for sieve analysis and assessment of mechanical strength relatives to subsequent milling operations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Densification and properties of alpha-silicon carbide

The sintering behavior of alpha-SiC with B and C sintering aids and without sintering aids was investigated experimentally. The sintering was performed for 30-60 min in argon flow at 2150 and 2200 C. The density of the sintered bars was determined by weighing and measuring the bars, four-point flexure tests were conducted on machined bars, and the Weibull modulus was determined by regression analysis. It is found that type 1 alpha-SiC powder, which does not densify, can be sintered to a high final density (in excess of 96 percent of the theoretical value) using B and C sintering aids. Flexure test results and Weibull modulus data suggest that the strength of the alpha-SiC ceramic is greatly affected by processing flaws and also by inclusions and machining flaws.

Dutta, S.↗

Advanced Ceramic Technology for Space Applications at NASA MSFC

The ceramic processing technology using conventional methods is applied to the making of the state-of-the-art ceramics known as smart ceramics or intelligent ceramics or electroceramics. The sol-gel and wet chemical processing routes are excluded in this investigation considering economic aspect and proportionate benefit of the resulting product. The use of ceramic ingredients in making coatings or devices employing vacuum coating unit is also excluded in this investigation. Based on the present information it is anticipated that the conventional processing methods provide identical performing ceramics when compared to that processed by the chemical routes. This is possible when sintering temperature, heating and cooling ramps, peak temperature (sintering temperature), soak-time (hold-time), etc. are considered as variable parameters. In addition, optional calcination step prior to the sintering operation remains as a vital variable parameter. These variable parameters constitute a sintering profile to obtain a sintered product. Also it is possible to obtain identical products for more than one sintering profile attributing to the calcination step in conjunction with the variables of the sintering profile. Overall, the state-of-the-art ceramic technology is evaluated for potential thermal and electrical insulation coatings, microelectronics and integrated circuits, discrete and integrated devices, etc. applications in the space program.

Alim, Mohammad A.↗

Multilayer ceramic oxide solid electrolyte for fuel cells and electrolysis cells

A unitary layered ceramic structure is disclosed which comprises co-sintered layers. The co-sintered structure comprises a sintered central layer of yttria stabilized zirconia (YSZ) which is about 8 mole percent yttria and having a density of at least about 95% of theoretical, and sintered outer layers of strontium lanthanum manganite (LSM) having the approximate molecular composition La.sub.0.8 Sr.sub.0.2 MnO.sub.3, having a density from about 50 to about 60% of theoretical, and having interconnected porosity from about 40 to 50% with an interconnected pore diameter from about one micron to about five microns. The sintered central layer is sandwiched by and bonded and sintered to the outer layers and is essentially free of significant amounts of manganese. A process for making the unitary composition-of-matter is also disclosed which involves tape casting a LSM tape and then on top thereof casting a YSZ tape. The process comprises presintering LSM powder at 1250.degree. F., crushing the presintered commercially available LSM powder, forming a slurry with the crushed LSM, a binder and solvent, tape casting the slurry and allowing the slurry to air dry. A mixture of commercially available submicron size particle YSZ powder is milled with a dispersant and solvent to disperse the YSZ particles thereby forming a dispersed YSZ slurry. The YSZ slurry is then tape cast on the dried LSM tape. If desired, a third layer of LSM can be cast on top of the dried YSZ layer. After drying the composite LSM/YSZ and LSM/YSZ/LSM tapes are fired at 1300.degree. C. No migration of manganese into the YSZ layer was observed with scanning electron microscope/edax in the sintered multilayer tape.

Schroeder, James E.↗

Multilayer ceramic oxide solid electrolyte for fuel cells and electrolysis cells and method for fabrication thereof

An unitary layered ceramic structure is disclosed which comprises co-sintered layers. The co-sintered structure comprises a sintered central layer of yttria stabilized zirconia (YSZ) which is about 8 mole percent yttria and having a density of at least about 95% of theoretical, and sintered outer layers of strontium lanthanum manganite (LSM) having the approximate molecular composition La.sub.0.8 Sr.sub.0.2 MnO.sub.3, having a density from about 50 to about 60% of theoretical, and having interconnected porosity from about 40 to 50% with an interconnected pore diameter from about one micron to about five microns. The sintered central layer is sandwiched by and bonded and sintered to the outer layers and is essentially free of significant amounts of manganese. A process for making the unitary composition-of-matter is also disclosed which involves tape casting a LSM tape and then on top thereof casting a YSZ tape. The process comprises presintering LSM powder at 1250.degree. F., crushing the presintered commercially available LSM powder, forming a slurry with the crushed LSM, a binder and solvent, tape casting the slurry and allowing the slurry to air dry. A mixture of commercially available submicron size particle YSZ powder is milled with a dispersant and solvent to disperse the YSZ particles thereby forming a dispersed YSZ slurry. The YSZ slurry is then tape cast on the dried LSM tape. If desired, a third layer of LSM can be cast on top of the dried YSZ layer. After drying the composite LSM/YSZ and LSM/YSZ/LSM tapes are fired at 1300.degree. C. No migration of manganese into the YSZ layer was observed with scanning electron microscope/edax in the sintered multilayer tape.

Schroeder, James E.↗

Improvements to the Powder Processing of near-Final Shape alnico Magnets

Alnico permanent magnets (PMs), a recent PM system of interest as an attractive rare earth-free PM alternative, have advantageous high operating temperature and magnetic saturation with the potential for utilization in electric machines, e.g. interior-PM motors found in electric vehicles, if current directional solidification methods can be replaced by a true mass production approach. Recently, two unique alnico compositions, termed Full-Co and Co-lean, with improved coercivity, were gas atomized, compression molded, and vacuum sintered (4h at 1240°C) to high densities of 97.8% and 99.3%, respectively. However, the Co-lean remained fine grained isotropic magnets and the Full-Co grains were not textured, lowering magnetic strength in spite of attempts to grow large textured grains by a stress-biased solid state grain alignment method to convert them to high energy anisotropic magnets. It was hypothesized that oxidation during de-binding in air left many prior particle boundary oxides within the sintered microstructure that hindered grain growth and texturing during the stress-biased texturing procedure and prevented the desired abnormal grain growth (AGG). Here we explored a vacuum de-binding step that was linked (in-place) to vacuum sintering and found that the Co-lean exhibited faster uniform grain growth that doubled the average grain size (40 μm to 80 μm). Linked vacuum de-binding and sintering of Full-Co produced some AGG after only 1 h of 1240°C sintering. A new direction for promoting AGG (and stress-biased texturing) in alnico is being explored that utilizes a fundamental analysis of systems with second phase particles that either inhibit or boost grain growth. This effort explores the influence of vacuum de-binding linked to a series of lower sintering temperatures at a fixed time (4h) to see if oxide particle size and volume fraction can be changed to promote AGG conditions in alnico. Surprising qualitative results indicate that AGG may be promoted for vacuum sintering at less than 1200°C.

Rinko, Emily↗

Structure, electrical characteristics, and high-temperature stability of aerosol jet printed silver nanoparticle films

Printed electronics has emerged as a versatile eco-friendly fabrication technique to create sintered nanoparticle (NP) films on arbitrary surfaces with an excellent control over the film microstructure. While applicability of such films for high-temperature applications is not explored previously, herein we report the high-temperature electrical stability of silver (Ag) metal NP films fabricated using an Aerosol Jet based printing technique and demonstrate that this behavior is dictated by changes in the film microstructure. In-situ high temperature (24–500 °C) impedance spectroscopy measurements show that the real part of the impedance increases with increasing temperature up to 150 °C, at which point a decreasing trend prevails until 300 °C, followed again by an increase in impedance. The electrical behavior is correlated with the in-situ grain growth of the Ag NP films, as observed afterwards by scanning electron microscopy and X-ray diffraction (XRD), and could be tailored by controlling the initial microstructure through sintering conditions. Using combined diffraction and spectroscopic analytical methods, it is demonstrated the Aerosol Jet printed Ag NP films exhibit enhanced thermal stability and oxidation resistance. In addition to establishing the conditions for stability of Ag NP films, the results provide a fundamental understanding of the effect of grain growth and reduction in grain boundary area on the electrical stability of sintered NP films.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Characterization of Al–Al{sub 4}C{sub 3} nanocomposites produced by mechanical milling

In this work, a mixture of Al–C–Al{sub 4}C{sub 3} nanopowder previously synthesized by mechanical milling and subsequent thermal treatment was used to reinforce the Al matrix. The nanocomposites were fabricated via high-energy ball milling and subsequent sintering process for different periods of time at 550 °C. Hardness and compression tests were performed to evaluate the mechanical properties of the nanocomposites in the as-milled and sintered conditions. According to the results the reinforcement located in the grain boundaries is responsible for the brittle behavior observed in the nanocomposites during the compression test. The combined effect of sintering and precipitation mechanisms produced an evident increase of the strength of the Al matrix at a relatively short sintering time. By using the Rietveld method the crystallite size and microstrain measurements were determined and correlated with the microhardness values. For the proper characterization of the nanoparticles present in the Al matrix, atomic force microscopy and high resolution electron microscopy were used. - Highlights: • Nanostructured Al{sub 4}C{sub 3} reinforcement was fabricated via mechanical milling and heat treatment. • We found a significant increase of the mechanical properties at short sintering times. • The formation of Al{sub 4}C{sub 3} with during sintering time restricted the excessive growth of the crystallite. • Al{sub 4}C{sub 3} located in the grain boundaries causes brittle fracture observed in compression tests. • There is a correlation between, crystallite size and microstrain values with microhardness.

36 MATERIALS SCIENCE↗

Interfacial characterization in carbon nanotube reinforced aluminum matrix composites

In this work, the effects of the sintering parameters, such as temperature and the techniques used (HP and SPS), on CNT/Al composite interfaces are studied. The major role of the native aluminum oxide (Al{sub 2}O{sub 3}) layer covering the aluminum grains is highlighted. It is shown that, for a sintering temperature below 620 °C, the amorphous Al{sub 2}O{sub 3} layer prevents the reaction between aluminum and carbon. For greater sintering temperatures, the breaking of the oxide layer due to its crystallization leads to the formation of aluminum carbide (Al{sub 4}C{sub 3}) by reaction between aluminum and the CNT. The Al{sub 4}C{sub 3} crystals grow perpendicularly to the matrix grain boundaries by thermally activated diffusion of the carbon atoms coming from the CNT. It is also demonstrated that, by limiting the sintering time, which is the case in SPS, it is possible to limit the growth of the Al{sub 4}C{sub 3} crystals and thus to preserve the CNT. - Highlights: • The high reactivity between CNT and Al matrix, resulting Al{sub 4}C{sub 3} formation during the sintering process is highlighted. • We demonstrate, thanks to in-situ TEM observations, that Al{sub 4}C{sub 3} crystals grow into aluminum grains by carbon diffusion. • The native aluminum oxide around the aluminum particles prevents the diffusion of carbon into the aluminum grains. • We show that the protective layer can be broken because of its crystallization, leading to the formation of Al{sub 4}C{sub 3}. • SPS, by limiting the sintering duration, is an interesting way for preparing CNT/Al composites without carbide formation.

36 MATERIALS SCIENCE↗

Chromium segregation at phase boundaries in Cr-doped WC-Co cemented carbides

Highlights: • Experimental evidence of a mixed (W,Cr) carbide layer on WC grain surfaces • Evidence of Cr segregation in the Co-rich binder phase in front of WC grain surfaces • Temperature dependent equilibrium segregation of Cr estimated from atom probe data • Experimental observations supported by predictions from thermodynamic modelling - Abstract: Atom probe tomography has shown (Cr,W)C to be present as a thin WC grain surface layer in an as-sintered Cr-doped WC-Co cemented carbide microstructure slowly cooled from the sintering temperature. The Co-rich binder phase contained a segregation of Cr in front of this surface layer. The mixed carbide layer was not observed when the as-sintered material had been heat treated at 1000 °C for 3000 s and then quickly cooled. A reduced amount of segregated Cr was, however, still present in the binder phase in front of the WC grain surface. These observations are supported by predictions from thermodynamic modelling; (Cr,W)C becomes stable at temperatures below 940 °C in the absence of other secondary carbides. The equilibrium segregation of Cr in the binder phase was estimated to 0.8 and 0.4 monolayer in the as-sintered and heat treated materials, respectively. The energy of segregation was calculated to 0.22 eV/Cr atom from the atom probe data. This value would result in a Cr segregation of 0.3 monolayer at the sintering temperature 1410 °C, provided that the energy of segregation in the Co-rich liquid phase sintering medium is the same as in the Co-rich binder phase. This Cr segregation may explain the WC grain growth inhibiting effect of Cr additions to WC-Co cemented carbide materials.

36 MATERIALS SCIENCE↗

Improvement microstructural and damage characterization of ceramic composites Y{sub 2}O{sub 3} – V{sub 2}O{sub 5} with MgO nano particles

Compacted samples of Y{sub 2}O{sub 3}-V{sub 2}O{sub 5} – MgO Nano – particles wt. % sintered at different sintering temperature (700, 900, 1100, 1300) ) C° for 2 hours under static air were investigated by x-ray diffraction and differential thermal analysis(DTA), to identify the phase present .Microstructure examination achieved by scanning electron microscopy .Sintered density and porosity were measured for all sintered samples .Compression was tested too and the Brake down voltage and dielectric strength were measure for all sintered samples .The clear improvement were noticed in both microstructure and damage characterization respectively after existing the MgO Nano-particles, by increasing in about 30% in sintered density and 25% for the compressive strength .The improvement also noticed on both brake down voltage and dielectric strength.

36 MATERIALS SCIENCE↗

Effect of thermal treatments on electrochemical behavior of binder jetted 17-4 PH stainless steel

Binder jetted 17–4 PH stainless steel was post-processed to relate heat treatment, microstructure, and corrosion in 3.5 wt% NaCl. Specimens were sintered at 1380 or 1400 °C, solution-annealed at 1055 °C for 1 h, and aged at 482 °C for 1 h. Here, as-sintered parts showed α′-martensitic matrix with a δ-ferrite network and Cu-rich precipitates in ferrite; inclusions (MnS, NbC) promoted localized attack. solutionizing redistributed elements and reduced ferrite, while aging generated coherent Cu nano-precipitates. Corrosion resistance was highly sensitive to post-processing in which aged specimens exhibited the lowest corrosion current density and formed a thicker, stable Cr 2 O 3 -rich passive film, whereas sintered specimens degraded most. Pitting potential depended on sintering temperature and microstructure, with 1400 °C sintering yielding more positive pitting potentials and the best overall performance after aging. Although the 1400-solutionized condition showed a relatively noble pitting response versus 1380-solutionized, it displayed unstable corrosion kinetics attributed to an imperfect passive film linked to higher NbC density. XPS depth profiles corroborated these trends, showing thicker, more continuous Cr 2 O 3 in aged states and discontinuous/thinning oxides in less resistant conditions. Practically, high-temperature sintering (∼1400 °C) followed by solutionizing and aging is recommended, with further gains expected from reducing NbC/MnS populations and porosity via powder and process control.

36 MATERIALS SCIENCE↗

Development of direct ink write radially graded alumina/zirconia

Functionally graded materials (FGMs) are of interest in multiple fields, yet many materials combinations are limited by coefficient of thermal expansion (CTE) mismatch. Here, a radially graded alumina/yttria-doped zirconia (Al 2 O 3 /8YZ) FGM is used to demonstrate processing strategies to mitigate CTE and sintering behavior differences between these oxides. FGM materials are especially sensitive to ink stability during printing, as all components (in this case, Al 2 O 3 and 8YZ) must be stabilized in the same dispersant or additive solution. Thus, this system is also ideal to demonstrate ink optimization best practices. Materials were characterized throughout processing to correlate the effects of common additives on both the ceramic particle suspensions and final sintered components. Aggregation observed in the initial additive-containing suspensions were present in the sintered component. The differences in sintering onset temperature and shrinkage rate resulted in internal stresses within the sintered component, which ultimately caused mechanical failure of the component under low stress. In conclusion, a processing strategy was recommended to mitigate the sintering behavior mismatch of alumina and 8 wt% yttria-stabilized zirconia.

Lamm, Benjamin W. [Oak Ridge National Laboratory (↗

Preparation and characterization of novel foamed porous glass-ceramics

Foamed glass-ceramics without using foaming agent have been synthesized in a novel glass system of SrO-CaO-Al{sub 2}O{sub 3}-TiO{sub 2}-B{sub 2}O{sub 3}-SiO{sub 2}-P{sub 2}O{sub 5}-M{sub x}O{sub y} (where M = Ba, Mg, La, Ce and Ni) by a simple process of powder sintering. The glass and glass-ceramics are characterized by dilatometry, differential scanning calorimetry (DSC), heating stage microscopy (HSM), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), optical microscopy and Fourier transformed infrared spectroscopy (FTIR). All the glasses formed are amorphous and the glass transition temperature and dilatometric softening temperature of these glasses are found to be in the range 673–678 °C and 706–728 °C respectively. The glasses are highly stable as indicated by the DSC evaluated glass stability parameters of the range 195–240 °C. Quantitative sintering study of glass powder compacts revealed swelling in the samples with NiO and CeO{sub 2} corresponding to a geometry change of 75 and 108% around 900 °C respectively. With reference to this finding the glass powder compacts are heated to 900 °C and the foamed glass-ceramics are obtained. Characteristic crystalline silicate phases have been identified in the XRD studies and their microstructures are recorded by FESEM. Optical microscope study of the foamed samples revealed formation of bigger foamed cavity with residual pores in samples with NiO and CeO{sub 2} in comparison to samples with BaO, MgO and La{sub 2}O{sub 3}. The mean pore diameters of the samples with NiO and CeO{sub 2} are determined to be 43 and 32 μm, and their respective porosities are 2.34 and 1.82 cm{sup 3}/g respectively. Thus NiO and CeO{sub 2} are found to be very effective to obtain foamed glass-ceramics without using foaming agent by the viscous flow sintering of fine glass powder compacts along with the reduction of the respective polyvalent ions. - Highlights: • Synthesis of foamed porous glass-ceramics without foaming agent by sintering method • Only powder compact yielded foamed porous glass-ceramics but bulk glass did not. • Glasses containing NiO and CeO{sub 2} exhibited significant foaming efficiency. • Bloating of entrapped gas during viscous flow sintering is the origin of foaming. • Residual void created pores in the sintered glass-ceramics as evidenced in FESEM.

36 MATERIALS SCIENCE↗

Understanding the effects of fabrication process on BaZr 0.9 Y 0.1 O 3– δ grain-boundary chemistry using atom probe tomography

Proton-conducting oxides, such as BaZr 0.9 Y 0.1 O 3–δ (BZY10), are receiving significant scientific attention for application in a variety of electrochemical applications. It has been shown that the synthesis route has a significant effect on the ionic behavior of these materials, especially the grain boundaries (GB). In this study, laser-pulsed atom probe tomography (APT) is used to characterize the GB chemistry of BZY10 samples prepared by four different methods: (1) spark plasma sintering (SPS), (2) conventional sintering followed by high-temperature annealing (HT), (3) conventional sintering with NiO used as a sintering aid (SSR-Ni), and (4) solid-state reactive sintering of oxide precursor powders with NiO as a reactive sintering aid (SSRS-Ni). Oxygen depletion (corresponding to oxygen vacancy accumulation) was observed at every GB in this study, consistent with the positive space-charge GB region commonly assigned to these materials. In contrast to the consistent trends associated with oxygen depletion, cation constituents showed varying segregation/depletion behaviors. The samples that used NiO revealed Ni preferentially segregating to the GB. The most common impurities in BZY10 are Al, Fe, Mg, Si, and Sr, all of which generally accumulate at GBs. In order to quantify these chemical trends, the APT method was optimized for this material supplemented with understanding from density functional theory (DFT). Finally, this APT study reveals the complexity of BZY10 GB chemistry and shows that even adjacent GBs in the same material can sometimes show surprisingly different GB chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗