CHEMICAL WET ETCHING OF AL(x)GA(1-x)N (0≤X≤1) NANOSTRUCTURES.
Abstract not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Abstract not provided.
An apparatus such as an optical modulator includes a buried oxide layer is disposed on a substrate. A microring resonator and an optical waveguide are disposed on the buried oxide layer and within a bonded semiconductor layer. The optical waveguide is optically coupled to the microring resonator and inputs a first optical wave into the microring resonator. An oxide layer is deposited on top of the optical waveguide and the microring resonator. A set of electrodes is disposed adjacent to the microring resonator, and in response to an electrical signal, the set of electrodes modulates the first optical wave into a modulated optical wave of transverse magnetic polarization within the microring resonator and outputs the modulated optical wave to the optical waveguide.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
No abstract prepared.
A facile method is reported to synthesize hollow mesoporous BaFe{sub 12}O{sub 19} spheres using a template-free chemical etching process. Hollow BaFe{sub 12}O{sub 19} spheres were synthesized by conventional spray pyrolysis. The mesoporous structure is achieved by alkaline ethylene glycol etching at 185 °C, with the porosity controlled by the heating time. The hollow porous structure is confirmed by SEM, TEM, and FIB-FESEM characterization. The crystal structure and magnetic properties are not significantly affected after the chemical etching process. The formation mechanism of the porous structure is explained by grain boundary etching. - Graphical abstract: Hollow spherical BaFe{sub 12}O{sub 19} particles are polycrystalline with both grains and grain boundaries. Grain boundaries have less ordered structure and lower stability. When the particles are exposed to high temperature alkaline ethylene glycol, the grain boundaries are etched, leaving small grooves between grains. These grooves allow ethylene glycol to diffuse inside to further etch the grains. As the grain size decreases, gaps appear on the particle surfaces, and a porous structure is finally formed. - Highlights: • Two-step synthesis method for hollow mesoporous BaFe{sub 12}O{sub 19} spheres is proposed. • Porosity of the product can be regulated by controlling the second step of chemical etching. • The crystal structure and magnetic properties are examined to be little affected during the chemical etching. • The mesoporous structure formation mechanism is explained by grain boundary etching.
Tin deposition mitigation employs hydrogen radicals and ions, formed in a hydrogen plasma, to interact with tin to form tin hydride (SnH 4 ) in the gaseous state, which is then pumped away. Surface wave plasma (SWP) technology developed at Illinois generates hydrogen radicals and ions, resulting in tin etch rates that are high enough to keep extreme ultraviolet (EUV) lithographic tools clean. An advantage of an SWP antenna is the ability to generate a high density of hydrogen radicals and hydrogen ions directly at the desired etching location. In situ etching of tin enables high availability EUV tools by maintaining high reflectivity of the multilayer mirror of the collector. Additionally, the SWP is characterized with low ion energies and low electron temperature, such that the multilayer mirror does not suffer any damage from sputtering or implantation of hydrogen ions during operation. Here, experiments elucidating the fundamental processes of tin removal are conducted by varying pressure, power, surface temperature, and gas flow rate in order to observe the etch rate behavior. Our results have shown that the presence of hydrogen ions increases etch rates because ion bombardment weakens Sn–Sn bonds, which, in turn, allows for a higher rate of chemical etching by the radicals. The ion bombardment reduces the number of radicals needed to etch a single tin atom to the range of 10 2 –10 3 . The linear SWP antenna yields plasma densities on the order of 10 17 to 10 18 m -3 and radical densities on the order of 10 18 to 10 19 m -3 , allowing for greater utilization of ion etch enhancement. Etch rates of up to 200 nm/min have been achieved. The surface temperature of the samples is an important factor in the etching process such that the decrease in the surface temperature increases the etch rates and decreases the hydrogen desorption rates. In addition, a kinetic etch model is developed to explain the behavior of etch rates as a function of surface temperature. Furthermore, results from experiments performed in an Illinois NXE:3100 chamber will be discussed.
MXenes are 2D materials composed of layered transition metal nitrides or carbides. These materials are synthesized by HF exfoliation from MAX phases (Ti{sub 3}AlC{sub 2}). The 2D nanomaterial was synthesized by the removal of the 'A' element, resulting in a Mxene product (Ti{sub 3}C{sub 2}). MXenes have the general formula M{sub n+1}X{sub n}T{sub x}, where M is an early transition metal, X is Carbon and/or Nitrogen, and T accounts for surface terminated functional groups such as Fluoride, hydroxyl, and oxygen. These materials have very unique properties, similar to graphene, that allows them to be applied in a variety of trace detection techniques including surface-enhanced Raman spectroscopy (SERS). MXenes have also been demonstrated to selectively uptake uranyl ion, UO{sub 2}{sup 2+}. If this property can be combined with SERS or fluorescence detection, it may be possible to use MXenes as the basis for an alternative method to kinetic phosphorescence analysis (KPA) for trace uranyl measurements. Objectives: To confirm that MXene Nano materials are suitable substrates for SERS and sensor development by enhancing Raman signaling. To determine if certain MXene preparation methods yield materials that are more suitable for trace sensing methods. To determine uranyl uptake properties of these MXene materials and test them for analytical signals. Sample Preparation: Preparation of Ti{sub 3}C{sub 2}MXene (at FSU). MXenes were prepared by etching Al from Ti{sub 3}AlC{sub 2} (MAX phase)material. Two etching techniques yield different MXene products: LiF/HCl: Milder reaction, larger MXene flakes. HF: Harsher reaction, smaller flakes, larger layer separation. Products washed to remove etchant, vacuum filtered, and dried. Dried MXene flakes are air-stable. Film preparation for sensor testing (at SRNL): Suspend powder in diH{sub 2}O, purge with Ar, sonicate for 30 min. Centrifuge and collect supernate with suspended particles. Observed LiF-etched Mxene yielded a higher density of particles and darker collected solution. Drop-cast (4 ml) supernate onto slides and dried with Ar. For Rhodamine B (RhB) testing, drop-cast 4 ml drops onto Mxene spots and dried with Ar. Scanning Electron Microscopy conditions: 10 kV Beam energy, high vacuum; Working distance of 8 mm; beam penetration depth appx. 4 microns, beam spot size appx. 2 nanometers. Results: Detection of aluminum correlates with bright spots on image. Presence of aluminum shows that LiF/HCl etching was less thorough than HF etching. Trace Cl detection in LiF images suggests incomplete rinsing. HF has smaller feature size, more layer structure, and increased homogeneity, consistent with expectations. Macroscopic Raman spectroscopy measurements: 532 nm excitation, ∼50 mW with a ∼100 micron spot size (InPhotonics RPB probe). Kaiser Optical Holospec f/1.8 spectrometer with cooled (-60 deg.C) Andor iDus OE420 CCD. LiF 1x supernate showed good signal for trace measurements of Rhodamine B. HF and 1/4x LiF supernates showed little Mxene or Rhodamine B signal. Low deposition densities led to excess background signal from glass slides. For LiF film, response is linear with Rhodamine B concentration over range tested. Will retest with Raman microscope (∼1 micron spot size) to characterize SERS of more dilute LiF and HF etched Mxenes. Conclusions: The LiF etched material was more suitable for macroscopic SERS measurements because it was more concentrated, resulting in a thicker film than the HF etched Mxene and diluted LiF sample. However, the other materials may give greater SERS enhancements, which we hope to determine from measurements with the Raman microscope. From characterization with SEM we concluded that the HF etched Mxene is more uniform/homogenous and has smaller particle size than the LiF etched Mxene. There is still aluminum present in both samples indicating that etching wasn't complete, but the removal of the aluminum was more efficient in the HF method. Path Forward: Observe SERS with Raman microscopy, to obtain better signals for the more diluted samples and be able to compare enhancement effects for the different MXenes. Characterize uranyl sorption into MXene films and test Raman and fluorescence signals. Revisit the etching conditions to improve removal of aluminum. FSU and SRNL will continue to collaborate to create and characterize different Mxene materials and test their usefulness for sensor applications.
An improved process for the fabrication of random arrays of silicon nanotips has been demonstrated to be feasible. Relative to other such processes, this process offers advantages of low cost and simplicity. Moreover, this process can readily be combined with other processes used to fabricate integrated circuits and other monolithic silicon structures. Arrays of silicon nanotips are subjects of research and development efforts directed toward utilizing them as field emitters in flat-panel displays, vacuum microelectronics, and microwave devices. Other silicon-nanotip-fabrication processes developed thus far predominantly include lithography, etching, and/or elaborate deposition steps followed by oxide sharpening steps and are both process intensive as well as expensive. In addition to being cheaper and simpler, the present process can efficiently produce silicon nanotips that range in height from a few microns to several tens of microns and are distributed over large areas. The process mentioned here can be summarized as consisting of (1) the growth of micro-etch masks on a silicon substrate, followed by (2) etching away of the masks, along with some of the substrate, to make an array of sharp tips. In the first step of the process, a cleaned silicon substrate is subjected to reactive ion etching (RIE) in a certain mixture of oxygen and carbon tetrafluoride under radio-frequency excitation. This process step results in the growth of fluorine based compounds in the form of stumps randomly distributed on the substrate. These stumps are known in the art as polymer RIE grass. The dimensions of these stumps are of the order of hundreds of nanometers, the exact values depending on process time and gas composition. The areal density of the stumps decreases with increasing process time as they grow and merge with neighboring stumps. These stumps constitute the micro-etch masks for the next step of the process. In the second step of the process, the substrate covered with the microetch masks is subjected to deep reactive ion etching (DRIE) process, which consists of cycles of reactive ion etching alternating with passivation (the Bosch process). The gas used in the etching substeps is sulfur hexafluoride (SF6); the gas used in the passivation substeps is octafluorocyclobutane (C4F8). The portions of the substrate directly under the RIE grass stubs are etched more slowly than are the portions between the stubs. Hence, what remains at the end of the process, after the stubs and parts of the substrate have been etched away, are silicon spikes where the stubs were (see figure). In a variation of the process, one starts with a silicon or silicon-on-insulator substrate with the intent to etch through the full thickness of the substrate. That is to say, one chooses the thickness so that the DRIE step releases individual nanotips. Such individual silicon nanotips may have utility as microscopic probes in biomedical applications.
Previously, it was difficult to fabricate deformable mirrors made by piezoelectric actuators. This is because numerous actuators need to be precisely assembled to control the surface shape of the mirror. Two approaches have been developed. Both approaches begin by depositing a stack of piezoelectric films and electrodes over a silicon wafer substrate. In the first approach, the silicon wafer is removed initially by plasmabased reactive ion etching (RIE), and non-plasma dry etching with xenon difluoride (XeF2). In the second approach, the actuator film stack is immersed in a liquid such as deionized water. The adhesion between the actuator film stack and the substrate is relatively weak. Simply by seeping liquid between the film and the substrate, the actuator film stack is gently released from the substrate. The deformable mirror contains multiple piezoelectric membrane layers as well as multiple electrode layers (some are patterned and some are unpatterned). At the piezolectric layer, polyvinylidene fluoride (PVDF), or its co-polymer, poly(vinylidene fluoride trifluoroethylene P(VDF-TrFE) is used. The surface of the mirror is coated with a reflective coating. The actuator film stack is fabricated on silicon, or silicon on insulator (SOI) substrate, by repeatedly spin-coating the PVDF or P(VDFTrFE) solution and patterned metal (electrode) deposition. In the first approach, the actuator film stack is prepared on SOI substrate. Then, the thick silicon (typically 500-micron thick and called handle silicon) of the SOI wafer is etched by a deep reactive ion etching process tool (SF6-based plasma etching). This deep RIE stops at the middle SiO2 layer. The middle SiO2 layer is etched by either HF-based wet etching or dry plasma etch. The thin silicon layer (generally called a device layer) of SOI is removed by XeF2 dry etch. This XeF2 etch is very gentle and extremely selective, so the released mirror membrane is not damaged. It is possible to replace SOI with silicon substrate, but this will require tighter DRIE process control as well as generally longer and less efficient XeF2 etch. In the second approach, the actuator film stack is first constructed on a silicon wafer. It helps to use a polyimide intermediate layer such as Kapton because the adhesion between the polyimide and silicon is generally weak. A mirror mount ring is attached by using adhesive. Then, the assembly is partially submerged in liquid water. The water tends to seep between the actuator film stack and silicon substrate. As a result, the actuator membrane can be gently released from the silicon substrate. The actuator membrane is very flat because it is fixed to the mirror mount prior to the release. Deformable mirrors require extremely good surface optical quality. In the technology described here, the deformable mirror is fabricated on pristine substrates such as prime-grade silicon wafers. The deformable mirror is released by selectively removing the substrate. Therefore, the released deformable mirror surface replicates the optical quality of the underlying pristine substrate.
With increasing demands on device patterning to achieve smaller critical dimensions and pitches for the 5 nm node and beyond, the need for atomic layer etching (ALE) is steadily increasing. In this work, a cyclic fluorocarbon/Ar plasma is successfully used for ALE patterning in a manufacturing scale reactor. Self-limited etching of silicon oxide is observed. The impact of various process parameters on the etch performance is established. The substrate temperature has been shown to play an especially significant role, with lower temperatures leading to higher selectivity and lower etch rates, but worse pattern fidelity. The cyclic ALE approach established with this work is shown to have great potential for small scale device patterning, showing self-limited etching, improved uniformity and resist mask performance.
This project studied and implemented methods to form GaN p-n diodes using selective area regrowth to achieve selective area doping. Successful selective area doping of GaN p-n diodes is an enabling factor to realize more advanced devices such as vertical transistors. The general challenge to selective area regrowth of GaN is that the primary etch method, inductively coupled plasma (ICP), damages the crystal and causes high leakage when didoes are formed by regrowth on the etched surface. Our approach used low damage etch methods following ICP etch to remove crystal damage and reduced leakage in the regrown diode. This project demonstrated 1.6 kV etched-and-regrown GaN p-n diodes using planar (non-selective) regrowth and 840 V etched-and-regrown p-n diodes using selective area regrown. Enabling factors were use of a low-damage reactive ion etch (RIE) to remove damage caused by the primary ICP etch combined with a multi-step junction terminal extension (JTE) process. Deep level defect investigation quantitatively correlated a deep level near the middle of the GaN band gap with ICP etch-induced leakage that was greatly mitigated by using a slow, low damage RIE process. This research is economically feasible for commercialization because the processes used in this project, including substrate type and source, epitaxial crystal growth and fabrication techniques are all standard to the GaN semiconductor industry. The fundamental understanding and foundational ability to produce kV-class GaN p-n diodes through etch-and-regrowth provides a path to realize high power, high efficiency GaN power switches that can significantly outperform commercial devices for next-generation electrical power conversion and transmission systems.
Techniques are evaluated for chemical, electrochemical, and thermal etching of thoria dispersed (TD) nickel alloys. An electrochemical etch is described which yielded good results only for large grain sizes of TD-nickel. Two types of thermal etches are assessed for TD-nickel: an oxidation etch and vacuum annealing of a polished specimen to produce an etch. It is shown that the first etch was somewhat dependent on sample orientation with respect to the processing direction, the second technique was not sensitive to specimen orientation or grain size, and neither method appear to alter the innate grain structure when the materials were fully annealed prior to etching. An electrochemical etch is described which was used to observe the microstructures in TD-NiCr, and a thermal-oxidation etch is shown to produce better detail of grain boundaries and to have excellent etching behavior over the entire range of grain sizes of the sample.
The development of plasma processing technology of superconducting radio frequency (SRF) cavities not only provides a chemical free and less expensive processing method, but also opens up the possibility for controlled modification of the inner surfaces of the cavity for better superconducting properties. The research was focused on the transition of plasma etching from two dimensional flat surfaces to inner surfaces of three dimensional (3D) structures. The results could be applicable to a variety of inner surfaces of 3D structures other than SRF cavities. Understanding the A r/C L plasma etching mechanism is crucial for achieving the desired modification of Nb SRF cavities. In the process of developing plasma etching technology, an apparatus was built and a method was developed to plasma etch a single cell Pill Box cavity. The plasma characterization was done with the help of optical emission spectroscopy. The Nb etch rate at various points of this cavity was measured before processing the SRF cavity. Cylindrical ring-type samples of Nb placed on the inner surface of the outer wall were used to measure the dependence of the process parameters on plasma etching. The measured etch rate dependence on the pressure, rf power, dc bias, temperature, CI2 concentration and diameter of the inner electrode was determined. The etch rate mechanism was studied by varying the temperature of the outer wall, the dc bias on the inner electrode and gas conditions. In a coaxial plasma reactor, uniform plasma etching along the cylindrical structure is a challenging task due to depletion of the active radicals along the gas flow direction. The dependence of etch rate uniformity along the cylindrical axis was determined as a function of process parameters. The formation of dc self-biases due to surface area asymmetry in this type of plasma and its variation on the pressure, rf power and gas composition was measured. Enhancing the surface area of the inner electrode to reduce the asymmetry was studied by changing the contour of the inner electrode. The optimized contour of the electrode based on these measurements was chosen for SRF cavity processing.
This paper focuses on the applications of a color etchant for aluminum alloys named Weck's reagent. The Al phase shows different colors from location to location after being etched by Weck's reagent. It is proved that Weck's reagent is very sensitive to the micro-segregations of Ti, Si and Mg in Al alloys so that characterization of the micro-segregations can be qualitatively realized which is usually done by electronic probe techniques. With the help of this characterization method, we are able to evaluate solid fractions for the semi-solid processed Al alloy with a better accuracy by excluding the Al grain growth during water quenching. To understand this reagent better, the color change during etching is investigated by applying different etching times at room temperature (25 °C). Among those results, 12 s shows the best color contrast after etching. Finally, we repeat the 12 second etching for four times through repeating a polishing–etching process. The result exhibits that Weck's reagent has a satisfying re-producibility with stable color and color distribution for the four times etching result. The second part of this study covers the coloring mechanism of Weck's reagent by characterizing the etched surface via various characterization methods. - Highlights: • The applications of Weck's reagent for Al alloys are introduced in detail. • Detailed relationship between micro-segregations in Al phase and the color difference revealed by Weck's reagent are studied. • Etching time has a strong influence on the color revealed by Weck's reagent. • Besides micro-segregation, grain boundaries can also be visualized by Weck's reagent, which was proved by EBSD analysis.
For the 45 nm technology node and beyond, a major challenge is to achieve reasonably high photoresist ash rates while minimizing the loss of the silicon (Si) substrate and its nitride (Si{sub 3}N{sub 4}). Accordingly, an objective of this work is to characterize the photoresist strip rate under varying conditions of H{sub 2} plasma and the effects of these conditions on Si and Si{sub 3}N{sub 4} etch rates. In addition, we discuss in detail the fundamental mechanisms of the reactions between H atoms and the above substrates and successfully reconcile the process trends obtained with the reaction mechanisms. In this work, photoresist, Si, and Si{sub 3}N{sub 4} films were exposed to downstream pure-H{sub 2} discharges and their removal rates were characterized by ellipsometry as a function of the following parameters: substrate temperature, reactor pressure, H{sub 2} flow rate, and source power. The authors found that the H{sub 2}-based dry ash and Si{sub 3}N{sub 4} etch are both thermally activated reactions, evidenced by the steady increase in etch rate as a function of temperature, with activation energies of {approx}5.0 and {approx}2.7 kcal/mol, respectively. The Si substrate exhibits a rather unique behavior where the etch rate increases initially to a maximum, which occurs at {approx}40 deg. C, and then decreases upon a further increase in temperature. The decrease in the Si etch rate at higher temperatures is attributed to the activation of competing side reactions that consume the chemisorbed H atoms on the Si surface, which then suppresses the Si-etch step. The photoresist and Si{sub 3}N{sub 4} removal rates increase initially with increasing pressure, reaching maxima at {approx}800 and 2000 mTorr, respectively, beyond which the removal rates drop with increasing pressure. The initial increase in removal rate at the low-pressure regime is attributed to the increased atomic-hydrogen density, whereas the decrease in ash rate at the high-pressure regime could be attributed to the recombination of H atoms that could occur by various mechanisms. At temperatures where the reaction rates are relatively fast, the photoresist and Si removal rates both increase continuously with the H{sub 2} flow rate, indicating that both reactions are in the supply-limited regime. For the range of process conditions explored here, we find that the etch rates of Si are generally much higher than those for Si{sub 3}N{sub 4} with Si:Si{sub 3}N{sub 4} etch-rate ratios that vary from 25 to >>520. Based on the process trends obtained here, we have identified a process window--high temperature and intermediate pressure--that attains relatively high photoresist ash rates and low Si and Si{sub 3}N{sub 4} etch rates.
A reactive ion etching process with alternating Cl{sub 2} and H{sub 2} exposures has been shown to chemically etch CoFe film that is an integral component in magnetoresistive random access memory (MRAM). Starting with systematic thermodynamic calculations assessing various chemistries and reaction pathways leading to the highest possible vapor pressure of the etch products reactions, the potential chemical combinations were verified by etch rate investigation and surface chemistry analysis in plasma treated CoFe films. An ∼20% enhancement in etch rate was observed with the alternating use of Cl{sub 2} and H{sub 2} plasmas, in comparison with the use of only Cl{sub 2} plasma. This chemical combination was effective in removing metal chloride layers, thus maintaining the desired magnetic properties of the CoFe films. Scanning electron microscopy equipped with energy-dispersive x-ray spectroscopy showed visually and spectroscopically that the metal chloride layers generated by Cl{sub 2} plasma were eliminated with H{sub 2} plasma to yield a clean etch profile. This work suggests that the selected chemistries can be used to etch magnetic metal alloys with a smooth etch profile and this general strategy can be applied to design chemically based etch processes to enable the fabrication of highly integrated nanoscale MRAM devices.