At least 1,045 records · Page 58

FUNCTIONALIZED SILICA AEROGELS: ADVANCED MATERIALS TO CAPTURE AND IMMOBILIZE RADIOACTIVE IODINE

To support the future expansion of nuclear energy, an effective method is needed to capture and safely store radiological iodine-129 released during reprocessing of spent nuclear fuel. Various materials have been investigated to capture and immobilize iodine. In most cases, however, the materials that are effective for capturing iodine cannot subsequently be sintered/densified to create a stable composite that could be a viable waste form. We have developed chemically modified, highly porous, silica aerogels that show sorption capacities higher than 440 mg of I2 per gram at 150 C. An iodine uptake test in dry air containing 4.2 ppm of iodine demonstrated no breakthrough after 3.5 h and indicated a decontamination factor in excess of 310. Preliminary densification tests showed that the I2-loaded aerogels retained more than 92 wt% of I2 after thermal sintering with pressure assistance at 1200 C for 30 min. These high capture and retention efficiencies for I2 can be further improved by optimizing the functionalization process and the chemistry as well as the sintering conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FY-16 Technology Gap Study Technical Report: Analysis of Undissolved Anode Materials of Mark-IV Electrorefiner

The Experimental Breeder Reactor II (EBR-II) is a sodium cooled fast reactor developed at Argonne National Laboratory (ANL). The used fuels from the EBR-II are currently being treated in the Fuel Conditioning Facility (FCF) at the Idaho National Laboratory (INL). The Mark IV (Mk-IV) electrorefiner (ER) is a unit process in the FCF, which is primarily assigned to treating the used driver fuels. The stainless steel anode baskets hold the chopped spent driver fuel segments. During electrorefining, the anode baskets are immersed into the electrolyte and the used fuel is dissolved electrochemically. Perforated sides and bottoms allow the flow of the electrolyte into and out of the anode baskets. The steel cathode is also immersed into the electrolyte and collects the reduced products. The active metal contents in the used fuel (e.g., Cs, Sr, lanthanides, Pu, etc.) reacts with uranium cations in the electrolyte and progressively reports to the electrolyte. Noble metals are mostly retained in the cladding hulls. Varying quantities of zirconium are retained in the cladding hulls depending on the operational conditions of the Mk-IV ER. The undissolved anode materials are removed from the anode baskets and stored for subsequent metal waste form processing. These undissolved materials typically include undissolved fuels, stainless steel cladding, and adhering electrolyte. A couple of hulls are retrieved for chemical analysis and used for estimating the composition of the entire undissolved anode materials. The mass balance attempt based on this practice of estimating the undissolved anode materials has been a challenge due to inherently high sampling errors associated with heterogeneous undissolved material compositions. Responding to the prescribed challenge, this report investigates chemical analysis data as a whole and finds noticeable trends in the compositions of undissolved anode material samples with respect to the mass of the whole undissolved anode materials. Based upon this discovery, an empirical model is proposed.

36 MATERIALS SCIENCE↗

The Pretreatment and Immobilization Test on The Greater Than Class C Spent Ion Exchange Resins from Taiwan Research Reactor - 17177

In this work, the experience on the removal of greater than Class C bead ion exchange resins from Taiwan Research Reactor spent fuel pool was reported. All of the spent ion exchange resins had been flushed, dewatered, and packed into lead-shield containers for 60 drums and pending for stabilization. The meta-kaolin type of geo-polymer was selected to immobilize the ion exchange resin. According to the 'Regulations on Final Disposal of Low Level Radioactive Waste and Safety Management of the Facilities' Act in Taiwan, the immobilization waste form shall meet seven testing items. Herein, several immobilize samples were prepared with the following amounts of ion exchange resin, 6, 12 and 18 wt.%. The compressive strength of the samples ranged from 2.9 to 18.2 MPa. The Cs and Sr ions were effectively trapped by ion exchange resins. After the resins incorporated with the geo-polymer matrix, the captured ions were expected difficult to leach out. However, it is found that at the higher contents of ion exchange resins in the immobilize samples exhibited poor water resistance due to the swelling effect. Several parameters such as the ratios of SiO{sub 2}/Na{sub 2}O and powder/solution also the blast furnace slag dosage were investigated to improve processibility and improve performance. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The DISTINCTIVE University Consortium: Legacy Ponds and Silo Wastes - 18135

The UK Engineering and Physical Sciences Research Council (EPSRC) sponsored DISTINCTIVE consortium (Decommissioning, Immobilisation and Storage Solutions for Nuclear Waste Inventories) is undertaking 22 science and engineering projects across 11 universities related to the decommissioning of the Legacy Ponds and Silos at Sellafield. These are grouped into three work packages that focus on wasteform durability, effluent treatment and pond and silo sludges. Specific challenges include understanding the durability of intermediate level waste (ILW) glass-ceramic waste forms, studying thermally treated Pu-containing materials, producing and testing new inorganic ion exchange materials including derivatized magnetic nanoparticles for Cs, Sr and U removal from effluent, developing micro- and ultra-filtration methods, providing improved modelling and simulation of sludge disturbance, mobilisation and transport, developing a better understanding of gas hold-up in sludges, exploring methods for sludge characterisation including the use of acoustic backscatter and quartz crystal microbalance techniques and Raman spectroscopy and computer modelling of the interaction of cations with brucite surfaces. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Radioactive Spent Resins Conditioning by the Hot Supercompaction Process at Tihange NPP

Spent ion-exchange media are considered to be problematic waste that, in many cases, requires special approaches and precautions during its immobilization to meet the acceptance criteria for disposal. The waste acceptance criteria define, among others, the quality of waste forms for disposal, and therefore will sometimes define appropriate treatment options. The selection of treatment options for spent ion-exchange materials must consider their physical and chemical characteristics. Basically, the main methods for the treatment of spent organic ion-exchange materials, following to pre-treatment methods are: - Direct immobilization, producing a stable end product by using cement, bitumen, polymer or high integrity containers; - The destruction of the organic compounds by using thermochemical processes or oxidation to produce an inorganic intermediate product that may or may not be further conditioned for storage and/or disposal; - The complete removal of the resin inner structural water by a thermal process, followed by a supercompaction of the hot dried resins. At Tihange Nuclear Power Plant, spent ion-exchange resins were conditioned by embedding in a polymer matrix with a mobile processing installation. For safety and cost reasons, Electrabel, the Belgian Utility, decided to investigate by which process the former one should be replaced. To carry out this mission, Electrabel entrusted Tractebel Engineering with the selection of the most suitable process available on the international market. After a thorough technical economical analysis, Tractebel Engineering selected the Resin Hot Supercompaction Process to be installed at Tihange Nuclear Power Plant. The Resin Hot Supercompaction Process is used to make water free dense homogeneous organic blocks from a wide range of particulate waste. In this process, spent resins are first dewatered and dried to remove the inner structural water content. The drying takes place in a drying vessel that holds the contents of two 200 l drums. In the oil heated drying and mixing unit, the resins are heated to the necessary process temperature for the structural inner water removal and for the hot pressing step. They are then collected into special metal drums, which are automatically provided with a lid and immediately transferred to a high force compactor. After high force compaction, the pellets are transferred to a measuring unit, where the dose rate, height and weight are automatically measured and recorded. A Volume Reduction Factor (VRF) of approximately up to four (depending on the type of resins) is achievable using hot compaction techniques. This paper describes the application of the Resin Hot Supercompaction Process at Tihange Nuclear Power Plant. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

KEY FACTORS THAT INFLUENCE THE PERFORMANCE PROPERTIES OF ARP/MCU SALTSTONE MIXES

At the Saltstone Production Facility (SPF), decontaminated salt solution (DSS) is combined with premix (a cementitious mixture of portland cement (PC), blast furnace slag (BFS) and Class F fly ash (FA)) in a Readco mixer to produce fresh (uncured) Saltstone. After transfer to the Saltstone Disposal Facility (SDF) the hydration reactions initiated during the contact of the premix and salt solution continue during the curing period to produce the hardened waste form product. The amount of heat generated from hydration and the resultant temperature increase in the vaults depend on the composition of the decontaminated salt solution being dispositioned as well as the grout formulation (mix design). This report details the results from Task 3 of the Saltstone Variability Study for FY09 which was performed to identify, and quantify when possible, those factors that drive the performance properties of the projected ARP/MCU Batches. A baseline ARP/MCU mix (at 0.60 water to cementitious materials (w/cm) ratio) was established and consisted of the normal premix composition and a salt solution that was an average of the projected compositions of the last three ARP/MCU batches developed by T. A. Le. This task introduced significant variation in (1) wt % slag, w/cm ratio, and wt % portland cement about the baseline mix and (2) the temperature of curing in order to better assess the dependence of the performance properties on these factors. Two separate campaigns, designated Phase 10 and Phase 11, were carried out under Task 3. Experimental designs and statistical analyses were used to search for correlation among properties and to develop linear models to predict property values based on factors such as w/cm ratio, slag concentration, and portland cement concentration. It turns out that the projected salt compositions contained relatively high amounts of aluminate (0.22 M) even though no aluminate was introduced due to caustic aluminate removal from High Level Waste. Previous studies revealed that increased levels of aluminate in the feed cause a significant increase in the heat generation. For Phase 10, a mix with 0.05 M aluminate was used as a comparison point for the mixes at 0.22 M aluminate. The temperature of curing in Task 3 ranged from 22 C to 75 C. Recent results demonstrated that it is not only the temperature of curing which is important but also the time/temperature sequence of curing. Therefore, this report also focuses on the impact of the sequencing of time and curing temperature on Saltstone properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Conditioning of Boron-Containing Low and Intermediate Level Liquid Radioactive Waste - 12041

Improved cementation of low and intermediate level radioactive waste (ILW and LLW) aided by vortex electromagnetic treatment as well as silica addition was investigated. Positive effects including accelerated curing of boron-containing cement waste forms, improve end product quality, decreased product volume and reduced secondary LRW volume from equipment decontamination were established. These results established the possibility of boron-containing LRW cementation without the use of neutralizing alkaline additives that greatly increase the volume of the final product intended for long-term storage (burial). Physical (electromagnetic) treatment in a vortex mixer can change the state of LRW versus chemical treatment. By treating the liquid phase of cement solution only, instead of the whole solution, and using fine powder and nano-particles of ferric oxides instead of separable ferromagnetic cores for the activating agents the positive effect are obtained. VET for 1 to 3 minutes yields boron-containing LRW cemented products of satisfactory quality. Silica addition at 10 % by weight will accelerate curing and solidification and to decrease radionuclide leaching rates from boron-containing cement products. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Criticality safety analysis on fissile materials in Fukushima reactor cores

The present study focuses on the criticality analysis for geological disposal of damaged fuels from Fukushima reactor cores. Starting from the basic understanding of behaviors of plutonium and uranium, a scenario sequence for criticality event is considered. Due to the different mobility of plutonium and uranium in geological formations, the criticality safety is considered in two parts: (1) near-field plutonium system and (2) far-field low enriched uranium (LEU) system. For the near-field plutonium system, a mathematical analysis for pure-solute transport was given, assuming a particular buffer material and waste form configuration. With the transport and decay of plutonium accounted, the critical mass of plutonium was compared with the initial load of a single canister. Our calculation leads us to the conclusion that our system with the initial loading being the average mass of plutonium in an assembly just before the accident is very unlikely to become critical over time. For the far-field LEU system, due to the uncertainties in the geological and geochemical conditions, calculations were made in a parametric space that covers the variation of material compositions and different geometries. Results show that the LEU system could not remain sub-critical within the entire parameter space assumed, although in the iron-rich rock, the neutron multiplicity is significantly reduced.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

The Underground Corrosion of Selected Type 300 Stainless Steels After 34 Years

Recently, interest in long-term underground corrosion has greatly increased because of the ongoing need to dispose of nuclear waste. Additionally, the Nuclear Waste Policy Act of 1982 requires disposal of high-level nuclear waste in an underground repository. Current contaminant release and transport models use limited available short-term underground corrosion rates when considering container and waste form degradation. Consequently, the resulting models oversimplify the complex mechanisms of underground metal corrosion. The complexity of stainless steel corrosion mechanisms and the processes by which corrosion products migrate from their source are not well depicted by a corrosion rate based on general attack. The research presented here is the analysis of austenitic stainless steels after 33½ years of burial. In this research, the corrosion specimens were analyzed using applicable ASTM standards as well as microscopic and X-ray examination to determine the mechanisms of underground stainless steel corrosion. As presented, the differences in the corrosion mechanisms vary with the type of stainless steel and the treatment of the samples. The uniqueness of the long sampling time allows for further understanding of the actual stainless steel corrosion mechanisms, and when applied back into predictive models, will assist in reduction of the uncertainty in parameters for predicting long-term fate and transport.

36 MATERIALS SCIENCE↗

Formulation and preparation of Hanford Waste Treatment Plant direct feed low activity waste Effluent Management Facility core simulant

The Hanford Waste Treatment and Immobilization Plant (WTP) Low Activity Waste (LAW) vitrification facility will generate an aqueous condensate recycle stream (LAW Melter Off-Gas Condensate, LMOGC) from the off-gas system. The baseline plan for disposition of this stream during full WTP operations is to send it to the WTP Pretreatment Facility, where it will be blended with LAW, concentrated by evaporation and recycled to the LAW vitrification facility. However, during the Direct Feed LAW (DFLAW) scenario, planned disposition of this stream is to evaporate it in a new evaporator in the Effluent Management Facility (EMF) and then return it to the LAW melter. It is important to understand the composition of the effluents from the melter and new evaporator so that the disposition of these streams can be accurately planned and accommodated. Furthermore, alternate disposition of the LMOGC stream would eliminate recycling of problematic components, and would enable less integrated operation of the LAW melter and the Pretreatment Facilities. Alternate disposition would also eliminate this stream from recycling within WTP when it begins operations and would decrease the LAW vitrification mission duration and quantity of glass waste, amongst the other problems such a recycle stream present. This LAW Melter Off-Gas Condensate stream will contain components that are volatile at melter temperatures and are problematic for the glass waste form, such as halides and sulfate. Because this stream will recycle within WTP, these components accumulate in the Melter Condensate stream, exacerbating their impact on the number of LAW glass containers that must be produced. Diverting the stream reduces the halides and sulfate in the recycled Condensate and is a key outcome of this work. This overall program examines the potential treatment and immobilization of this stream to enable alternative disposal. The objective of this task was to formulate and prepare a simulant of the LAW Melter Off-gas Condensate expected during DFLAW operations. That simulant can be used in evaporator testing to predict the composition of the effluents from the Effluent Management Facility (EMF) evaporator to aid in planning for their disposition. This document describes the method used to formulate a simulant of this LAW Melter Off-Gas Condensate stream, which, after pH adjustment, is the feed to the evaporator in the EMF.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Physical, Hydraulic, and Transport Properties of Sediments and Engineered Materials Associated with Hanford Immobilized Low-Activity Waste

Current plans for treatment and disposal of immobilized low-activity waste (ILAW) from Hanford’s underground waste storage tanks include vitrification and storage of the glass waste form in a nearsurface disposal facility. This Integrated Disposal Facility (IDF) is located in the 200 East Area of the Hanford Central Plateau. Performance assessment (PA) of the IDF requires numerical modeling of subsurface flow and reactive transport processes over very long periods (thousands of years). The models used to predict facility performance require parameters describing various physical, hydraulic, and transport properties. This report provides updated estimates of physical, hydraulic, and transport properties and parameters for both near- and far-field materials, intended for use in future IDF PA modeling efforts. Previous work on physical and hydraulic property characterization for earlier IDF PA analyses is reviewed and summarized. For near-field materials, portions of this document and parameter estimates are taken from an earlier data package. For far-field materials, a critical review is provided of methodologies used in previous data packages. Alternative methods are described and associated parameters are provided.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Aging and iodine loading of silver-functionalized aerogels

Engineered silver-functionalized silica aerogels are being investigated for their potential application in off-gas treatment at a used nuclear fuel reprocessing facility. Reprocessing will release several key volatile radionuclides, including iodine-129. To achieve regulatory compliance, iodine-129 must be removed from any off-gas stream prior to environmental discharge. Ag{sup 0}-functionalized aerogels have been demonstrated to have high iodine-capture capacity, high porosity, and potential for conversion into a waste form. Capture materials used in off-gas treatment may be exposed to a heated, high-humidity, acidic gas stream for months. Extended exposure to this stream could affect sorbent performance. It was the aim of this study to evaluate what impacts might be observed when Ag{sup 0}-functionalized aerogels prepared at Pacific Northwest National Laboratory were contacted with a dry air stream for up to 6 months and then used to adsorb iodine from a synthetic off-gas stream. Results demonstrate that there is some loss of iodine-capture capacity caused by aging, but that this loss is not as marked as for aging of more traditional iodine sorbents, such as silver-impregnated mordenite. Specifically, aging silver-functionalized aerogel under a dry air stream for up to 6 months can decrease its iodine capacity from 41 wt% to 32 wt%. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Summary Report on the Volatile Radionuclide and Immobilization Research for FY2011 at PNNL

The materials development summarized here is in support of the Waste Forms campaign, Volatile Radionuclide task. Specifically, materials are being developed for the removal and immobilization of iodine and krypton, specifically 129I and 85Kr. During FY 2011, aerogel materials were investigated for removal and immobilization of 129I. Two aerogel formulations were investigated, one based on silica aerogels and the second on chalcogen-based aerogels (i.e., chalcogels). A silica aerogel was tested at ORNL for total I2 sorption capacity. It was determined to have 48 mass% capacity while having little physisorbed I2 (I2 not taken up in the aerogel pores). For 85Kr, metal organic framework (MOF) structures were investigated and a new MOF with about 8 mass% capacity for Xe and Kr. The selectivity can be changed from Xe > Kr to Xe < Kr simply by lowering the temperature below 0 C. A patent disclosure has been filed. Lastly, silicon carbide (SiC) was loaded with Kr. The diffusion of Kr in SiC was found to be less than detectable at 500 C.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Review of recent developments in iodine wasteform production

Radioiodine capture and immobilization is not only important to consider during the operation of reactors (i.e., I-131), during nuclear accidents (i.e., I-131 and I-129) or nuclear fuel reprocessing (i.e., I-131 and I-129), but also during disposal of nuclear wastes (i.e., I-129). Most disposal plans for I-129-containing waste forms (including spent nuclear fuel) propose to store them in underground repositories. Here, iodine can be highly mobile and, given its radiotoxicity, needs to be carefully managed to minimize long-term environmental impacts arising from disposal. Typically, any process that has been used to capture iodine from reprocessing or in a reactor is not suitable for direct disposal, rather conversion into a wasteform for disposal is required. The objectives of these materials are to use either chemical immobilization or physical encapsulation to reduce the leaching of iodine by groundwaters. Some of the more recent ideas have been to design capture materials that better align with disposal concepts, making the industrial processing requirements easier. Research on iodine capture materials and wasteforms has been extensive. This review will act as both an update on the state of the research since the last time it was comprehensively summarized, and an evaluation of the industrial techniques required to create the proposed iodine wasteforms in terms of resulting material chemistry and applicability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Near-Complete Retention of Technetium During Vitrification of Hanford Low Activity Waste With Recycle - 17315

Technetium is one of the more volatile radionuclides for which retention in low activity waste (LAW) glass under the high temperature conditions during vitrification can vary depending on feed composition, feed chemistry, and melter operating parameters. High retention of technetium in the glass is desirable in order to minimize the fraction of technetium that is directed to secondary waste streams, which include liquid off-gas treatment system effluents. Consequently, test data are crucial to assess and underpin the assumptions underlying such mass balance projections, the compositions of secondary waste streams, and, in particular, the effects of recycle on increasing the incorporation of technetium in the glass products and minimizing the fraction in non-glass waste forms. Previous testing performed on a scaled melter system that incorporates prototypical off-gas treatment components and real-time recycle of the liquid effluents back to the melter feed demonstrated that recycle resulted in significant increases of the incorporation of technetium into the LAW glass product and behavior that was in good agreement with process models for the system. However, the maximum technetium retention achieved in those tests was less than predicted. Tests conducted in the present work demonstrated, for the first time, near-complete retention of technetium in the LAW glass product with recycle. Holdup of technetium in the vacuum evaporator, which concentrates the liquid effluents prior to their recycle to the melter feed, was identified as the primary reason for the previously observed shortfall. The fate of other volatile constituents was also assessed. In particular, in addition to technetium, rhenium, which is frequently used as a non-radioactive surrogate for technetium, was included in these tests. This allows for a direct comparison of the behavior of rhenium and technetium during vitrification and in the down-stream processes. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

IMPACT OF TIME / TEMPERATURE CURING CONDITIONS AND ALUMINATE CONCENTRATIONS ON SALTSTONE PROPERTIES

This report addresses the impact of (1) the time and temperature curing conditions (profile) and (2) the impact of higher aluminate concentrations in the decontaminated salt solution on Saltstone processing and performance properties. The results demonstrate that performance properties as well as some of the processing properties of Saltstone are highly sensitive to the conditions of time and temperature under which curing occurs. This sensitivity is in turn dependent on the concentration of aluminate in the salt feed solution. In general, the performance properties and indicators (Young's modulus, compressive strength and total porosity) are reduced when curing is initially carried out under high temperature. However, this reduction in performance properties is dependent on the sequence of temperatures (the time/temperature profile) experienced during the curing process. That is, samples that are subjected to a 1, 2, 3 or 4 day curing time at 60 C followed by final curing at 22 C lead to performance properties that are significantly different than the properties of grouts allowed to cure for 1, 2, 3 or 4 days at 22 C followed by a treatment at 60 C. The performance properties of Saltstone cured in the sequence of higher temperature first are generally less (and in some cases significantly less) than performance properties of Saltstone cured only at 22 C. This loss in performance was shown to be mitigated by increased slag content or cement content in the premix at the expense of fly ash. For the sequence in which the Saltstone is initially cured at 22 C followed by a higher temperature cure, the performance properties can be equal to or greater than the properties observed with curing only at 22 C curing. The results in this report indicate that in order to meaningfully measure and report the performance properties of Saltstone, one has to know the time/temperature profile conditions under which the Saltstone will be cured. This will require thermal modeling and actual time/temperature profiles within the vaults under various pour schedules to determine (1) an average profile of time and temperature under normal processing conditions and (2) a conservative (worst case) time/temperature profile. Samples can then be cast and cured in the laboratory under these time and temperature profiles prior to measurement of the performance properties of the product waste forms From a processing perspective, a higher initial curing temperature decreased the set time to 1 day at both 40 C and 60 C and eliminated any bleed volume that was present for those samples that exhibited bleed at room temperature. However, the bleed water return system in the Saltstone Disposal Facility may remove bleed water before it can be reabsorbed. Aluminate concentrations at levels greater than 0.20 M in these salt solutions can lead to positive or negative effects on the performance properties. At a curing temperature of 22 C, aluminate increases Young's modulus and the compressive strength while reducing the total porosity. This generally corresponds to an improved (decreased) permeability (hydraulic conductivity) for Saltstone which is a positive outcome. On the other hand, with increased aluminate concentration there is a significant increase in heat of hydration that may limit pour schedule and must be considered in estimating the time/temperature profile to which Saltstone will be subjected during curing as discussed above. That is, higher temperatures in the vault (due to the higher heats of hydration) may present a greater challenge in controlling the curing time and temperature profile to achieve the desired performance properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Synthesis of apatite phosphates containing Cs{sup +}, Sr{sup 2+} and RE{sup 3+} ions and chemical durability studies

Graphical abstract: New chemically durable hydroxy and fluoro apatite phosphate wasteforms CsLa{sub 0.8}Nd{sub 0.1}Sm{sub 0.1}Sr{sub 3}(PO{sub 4}){sub 3}OH and CsLa{sub 0.7}Nd{sub 0.1}Sm{sub 0.1}Eu{sub 0.1}Sr{sub 3}(PO{sub 4}){sub 3}F are fabricated. Display Omitted Highlights: ► Novel apatite phosphates CsLaSr{sub 3}P{sub 3}(PO{sub 4}){sub 3}OH and CsLaSr{sub 3}(PO{sub 4}){sub 3}F are reported. ► New hydroxyapatite wasteform CsLa{sub 0.8}Nd{sub 0.1}Sm{sub 0.1}Sr{sub 3}P{sub 3}O{sub 12}OH is fabricated. ► Fluoro analogue CsLa{sub 0.7}Nd{sub 0.1}Sm{sub 0.1}Eu{sub 0.1}Sr{sub 3}P{sub 3}O{sub 12}F incorporates ‘Eu{sup 3+}’. ► Negligible leachability of Cs and rare earth ions demonstrated. -- Abstract: Crystallization of Cs, Sr and selected rare earth ions in apatite phosphate structure was investigated. Compounds of the formula CsLaSr{sub 3}(PO{sub 4}){sub 3}OH (CSOH), CsLaSr{sub 3}(PO{sub 4}){sub 3}F (CSF) and the simulated waste forms of the compositions CsLa{sub 0.8}Nd{sub 0.1}Sm{sub 0.1}Sr{sub 3}(PO{sub 4}){sub 3}OH (CNSOH) and CsLa{sub 0.7}Nd{sub 0.1}Sm{sub 0.1}Eu{sub 0.1}Sr{sub 3}(PO{sub 4}){sub 3}F (CNSEF) were synthesized and characterized by powder XRD, TGA and SEM techniques. The leachability behaviour of the single phases was studied for a period of one month by MCC-5 test using powder specimen. The leachability of Cs and other rare earth ions was found to be negligible. The leach rates (LR{sub i}) of Sr and P were observed as follows: CSOH – LR{sub Sr} = 10{sup −3}–10{sup −4} g/m{sup 2}/d, LR{sub P} = 10{sup −4} g/m{sup 2}/d; CSF – LR{sub Sr} = 10{sup −3}–10{sup −5} g/m{sup 2}/d, LR{sub P} = 10{sup −4}–10{sup −5} g/m{sup 2}/d; CNSOH and CNSEF – LR{sub Sr} = 10{sup −3}–10{sup −4} g/m{sup 2}/d, LR{sub P} = 10{sup −4}–10{sup −5} g/m{sup 2}/d.

36 MATERIALS SCIENCE↗

Structure and thermodynamics of calcium rare earth silicate oxyapatites, Ca 2 RE 8 (SiO 4 ) 6 O 2 (RE = Pr, Tb, Ho, Tm)

Calcium rare earth silicate oxyapatites, (Ca 2 RE 8 (SiO 4 ) 6 O 2 ), are of interest as components of glass-ceramic nuclear waste forms. To assess their long-term behavior in a geologic repository, it is essential to determine their structure and thermodynamic stability at relevant conditions. Here, in this work, we performed detailed structural and thermodynamic investigations on Ca 2 Pr 8 (SiO 4 ) 6 O 2 , Ca 2 Tb 8 (SiO 4 ) 6 O 2 , Ca 2 Ho 8 (SiO 4 ) 6 O 2 , and Ca 2 Tm 8 (SiO 4 ) 6 O 2 by high energy synchrotron powder X-ray diffraction combined with Rietveld analysis and high temperature oxide melt drop solution calorimetry. Enthalpies of formation from constituent oxides (ΔH f,ox ) were determined to be -765.1 ± 22.8 kJ/mol for Ca 2 Pr 8 (SiO 4 ) 6 O 2 ; -638.9 ± 20.5 kJ/mol for Ca 2 Tb 8 (SiO 4 ) 6 O 2 ; -643.3 ± 10.3 kJ/mol for Ca 2 Ho 8 (SiO 4 ) 6 O 2 ; and -403.2 ± 5.1 kJ/mol for Ca 2 Tm 8 (SiO 4 ) 6 O 2 . These thermodynamic parameters were used in assessing the thermochemical stability of these phases in the presence of water vapor from room temperature to 600 K, as encountered in the subsurface environments of a geological repository.

36 MATERIALS SCIENCE↗