Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ALLOY SYSTEMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,045 records · Page 58

Microstructure and Wear Resistance of FeCrBSi Plasma-Sprayed Coating Remelted by Gas Tungsten Arc Welding Process

Herein, an FeCrBSi coating was fabricated via plasma spray on AISI1045 steel, and subsequently, a gas tungsten arc welding (GTA) process was employed to remelt the coating. The microstructure, microhardness, fracture toughness and surface roughness of the coating before and after remelting were investigated, as well as the wear resistance was tested by a UMT-3-type sliding wear apparatus. The results showed that, upon remelting, most defects in the as-sprayed coating were effectively eliminated, the surface roughness decreased by 43%, and the coating–substrate interface bonding changed from mechanical to metallurgical. The phase composition of the as-sprayed coating was primarily α-Fe and a small amount of hard Fe{sub 3}B phase, while the remelted coating consisted of α-Fe and (Fe,Cr){sub 23}C{sub 6} and a small quantity of CrB. In addition, remelting the coating was found to induce a 287.6% increase in the fracture toughness, a 33.4% increase in the average microhardness, and a 47.5% decrease in the wear volume, while the failure mechanism changed from abrasive wear to fatigue wear upon remelting. Therefore, GTA remelting of plasma-sprayed coating was found to be a feasible method to obtain a coating with good wear resistance.

36 MATERIALS SCIENCE↗

Replacement of Nitrided 33CrMoV Steel with ESR Hot Work Tool Steels for Motorsport Applications: Microstructural and Fatigue Characterization

In this work tensile strength, fatigue resistance and fracture toughness of two electroslag remelted (ESR) tool steels and of 33CrMoV12 ESR steel (both in quenched and tempered condition, as well as nitrided condition) were evaluated. The role of hardness, residual stresses and inclusion sizes on the fatigue behavior was investigated. Tool steels have a tensile strength between about 1900 and 2300 MPa, fracture toughness between 35 and 33 MPa√m, while fatigue strength ranges between 725 and 992 MPa. The tensile strength and fracture toughness of the 33CrMoV12 ESR are, respectively, 1365 MPa and about 150 MPa√m. Nitriding induces a significant increase in fatigue strength from 560 to 980 MPa. These results highlight that appropriate ESR tool steels could replace nitrided steels.

36 MATERIALS SCIENCE↗

The Sliding Wear and Frictional Behavior of M50-10 wt.%(Sn-Ag-Cu) Self-Lubricating Materials at Elevated Temperatures

As the main steel used in the aero-engine main shaft bearings, the tribological properties of M50 can directly affect the performance of aero-engine. The purpose of this study is to design the reasonable composition of Sn-Ag-Cu alloy and investigate the wear mechanisms of M50-10 wt.%(Sn-Ag-Cu) composites (MSACC) prepared by SPS sliding against Si{sub 3}N{sub 4} ball from 25 to 550 °C at 12 N-0.25 m/s. XRD, EPMA, FESEM and EDS mappings are conducted to understand the major mechanisms leading to the improvement in the sliding behavior of MSACC. The results indicate that MSACC with different specifications of Sn-Ag-Cu alloy shows excellent friction and wear properties from 25 to 550 °C compared to M50. M50-10 wt.%(50Sn40Ag10Cu) (MSACC-2) shows the distinguished tribological performance for the lower friction coefficients of 0.22-0.61 and less wear rates of 1.7-4.1 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1}, which is attributed to the formed excellent lubricating structure consisting of the lubricating film with massive Sn-Ag-Cu alloy and intermetallic compounds formed during the friction process, as well as the underneath mixed layer who can well support the lubricating film due to the good intersolubility between the designed Sn-Ag-Cu alloy and M50 (Fe).

36 MATERIALS SCIENCE↗

Influence of Welding Combined Plastic Forming on Microstructure Stability and Mechanical Properties of Friction Stir-Welded Al-Cu Alloy

A new tailor-welded process, which combines stages of welding, plastic forming, and heat treatment strengthening, was developed to produce a friction stir-welded (FSW) Al-alloy joint. The Al-Cu sheets were FSW under different welding parameters and then were plastic-deformed. The microstructural evolution and mechanical properties of the FSW joint were investigated by scanning electron microscopy and tensile tests. It was found that high heat input during FSW and low solution temperature suppress the abnormal grain growth (AGG) of the joint due to the differential in grain size and grain boundary energy. The microstructure heterogeneity of the FSW joint is effectively improved, as no AGG occurs. The retention of fine equiaxed grains and the increase in the density of precipitates result in excellent mechanical properties. The increase in the strength and micro-hardness of the joint mainly depends on the plastic deformation prior to aging treatment.

36 MATERIALS SCIENCE↗

Constitutive Behavior and Forming Limit of Mg-Al-Ca-Gd Alloy Sheets at Room and Elevated Temperatures

The constitutive behavior and forming limit of a newly developed magnesium alloy sheet containing rare earth elements (Mg-Al-Ca-Gd) were investigated. Anisotropic constitutive constants were obtained through tensile tests at various temperatures and strain rates. A modified Grosman equation was adopted to describe the constitutive behavior of the magnesium alloy, taking into account the effects of temperature and strain rate. Results revealed that the proper forming temperature and the strain rate for the newly developed magnesium alloy were 210 °C and 0.001 s{sup −1}, respectively. Forming limit curves at room temperature and 210 °C were, respectively, established by the combination of hemispherical punch tests and theoretical predictions using a modified Marciniak–Kuczynski model. The accuracy of the theoretical prediction of FLD was discussed. The forming limit of Mg-Al-Ca-Gd alloy sheet increased when heated from room temperature to 210 °C.

36 MATERIALS SCIENCE↗

Toward a Biocompatible and Degradable Battery Using a Mg-Zn-Zr Alloy with β-Tricalcium Phosphate Nanocoating as Anode

A biocompatible β-tricalcium phosphate (β-TCP) nanorod coating on Mg-3 wt.%Zn-0.8 wt.%Zr alloy (MZZ) was fabricated by a chemical solution process. The microstructure and corrosion resistance of β-TCP coating on MZZ were studied using scanning electron microscopy, x-ray diffraction, and potentiodynamic polarization. β-TCP-MZZ was used as the anode for Mg battery with simulated body fluid directly acting as the electrolyte. The experimental results indicate that the β-TCP nanorod coating formed on the surface of MZZ alloy protects the matrix and improves the corrosion resistance of MZZ alloy. The Mg battery showed a voltage of 1.05 V for up to 75 days and continued to discharge for 90 days until 0.7 V at 100 μA/cm{sup 2}. This indicates potential practical importance of biodegradable batteries.

36 MATERIALS SCIENCE↗

Corrosion and Mechanical Degradation of Ni-Ti Superelastic Alloy in Neutral Fluoride Solution

The corrosion behavior and mechanical degradation of Ni-Ti superelastic alloy in neutral fluoride solution were investigated with a focus on the effect of temperature during immersion. Corrosion was accelerated by increasing the temperature, and mass loss increased with immersion time. Furthermore, Ti ions (Ni ions) preferentially dissolved in the early (later) stage of immersion. The tensile strength of the immersed specimen decreased when the mass loss was approximately 0.040-0.050 mg/mm{sup 3}. The fracture mechanisms of specimens immersed in 2.0% NaF solution were active path corrosion at room temperature and presumably hydrogen embrittlement at 80 °C. For long-term (e.g., 180 days) immersions at 80 °C, hydrogen embrittlement did not occur, because the absorbed hydrogen diffused to the center of the immersed specimens, rendering the hydrogen distribution comparatively uniform. These findings suggest that the fracture mechanism of immersed specimens can change as a result of the temperature during immersion.

36 MATERIALS SCIENCE↗

Effect of Overaging on Fatigue Crack Propagation and Stress Corrosion Cracking Behaviors of an Al-Zn-Mg-Cu Alloy Thick Plate

The fatigue property as well as stress corrosion cracking (SCC) resistance of an Al-Zn-Mg-Cu alloy thick plate in peak-aged and overaged tempers (T7351 and T7651) is systematically investigated by fatigue crack propagation (FCP) test and slow strain rate test (SSRT). Microstructural characterization is examined by transmission electron microscopy and scanning electron microscopy. Results reveal that the T7351 alloy has lower strength but higher electrical conductivity as compared to T7651 alloy. The FCP resistance of T7351 alloy is superior to that of the T7651 alloy due to the coarser precipitates in the highly overaged alloy in which the strain localization is reduced by promoting homogeneous slip. In addition, the SSRT test suggests a higher SCC resistance in T7351 alloy. The enhanced SCC resistance is found to depend on grain boundary precipitate characteristics and crack propagation resistance of the alloys.

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Dynamic Recrystallization and Grain Refinement of Fe-P-C-Si and Fe-P-C-Si-N Steels

Grain refinement is an effective technique to improve the mechanical properties of steels. In the present work, single-pass hot compression experiments have been conducted on two different compositions of high phosphorous steels to study the microstructural evolution and ferrite grain refinement at various strain rates and deformation temperatures, i.e., 0.01-10 s{sup −1} and 750-1050 °C, respectively. Optical metallography has been employed to understand the physical processes that take place during hot deformation process. The results indicate that when these compositions of high phosphorous steels are worked at relatively low temperatures in the intercritical regions, a ferrite grain size of 5-7 µm is obtained. It is observed that the grain size decreases with an increase in strain rate and with the decrease in deformation temperature. Based on the values of stress exponent (n) obtained in the present work, dislocation creep is identified as the deformation mechanism. The activation energies for deformation of these two types of high phosphorous steels have been calculated. The effect of the alloying elements on the stress–strain curve, microstructure, and grain refinement has been discussed.

36 MATERIALS SCIENCE↗

Effect of Plane Strain Compression and Subsequent Recrystallization Annealing on Microstructures and Phase Transformation of NiTiFe Shape Memory Alloy

The effect of plane strain compression and subsequent recrystallization annealing on microstructures and phase transformation of NiTiFe shape memory alloy (SMA) is investigated. Inhomogeneous plastic deformation at various deformation degrees occurs in NiTiFe SMA during plane strain compression. Nanocrystalline phase and amorphous phase increase as the deformation degree increases. B2 austenite, B19′ martensite, nanocrystalline and amorphous phases coexist in the NiTiFe samples subjected to large plastic strain. The static recrystallization mechanisms depend on the microstructures of the deformed NiTiFe samples. The static recrystallization mechanisms deal with nucleation and growth of the recrystallized grains, growth of nanocrystalline phase and crystallization of amorphous phase. Grain size, subgrain boundaries, geometrically necessary dislocation density and Schmid factor are captured on the basis of electron backscattered diffraction data. The process of recrystallization annealing cannot eliminate the deformation texture completely. The slip direction [110] is the most favorable slip direction in the recrystallized NiTiFe sample. Plane strain compression along with subsequent recrystallization annealing changes the phase transformation path of as-rolled NiTiFe SMA, and it results in the decreasing martensite transformation start temperature. The three annealed NiTiFe samples exhibit the similar phase transformation behavior since complete recrystallization annealing leads to the similar microstructures.

36 MATERIALS SCIENCE↗

Influence of Cu/Li Ratio on the Welding Forces and Mechanical Properties of Two Bobbin Tool Friction Stir Welded Al-Cu-Li Alloys

Increasing space activities produce a high number of space objects and lead to increasing collision risks which urges leading industries to look for future removal strategies. Material substitution in order to raise demisability during atmospheric reentry is a possible solution. Modern aluminum lithium alloys are under consideration to replace high-temperature melting materials like titanium. Further, friction stir welding was proposed as suitable joining technology in order to avoid high heat inputs during manufacturing. In this work, two modern Al-Li-Cu alloys, AA 2060 and AA 2196, in peak-aged temper were welded using the stationary shoulder variant of bobbin tool friction stir welding. Identical process parameters led to defect-free welds in both alloys. The macrostructural and microstructural features are shown and analyzed. The welds were mechanically tested to an efficiency of 78 and 70% of the base metal ultimate tensile strength for AA 2060 T8 and AA 2196 T8, respectively. The process forces as well as the thermal cycle experienced by the workpiece material were used to explain the mechanical performance. The difference in composition regarding the Cu/Li ratio of the alloys was taken into account when the mechanical properties were correlated with the thermally affected microstructure of the weldments.

36 MATERIALS SCIENCE↗

The Application of Centrifugal Atomization Method for Preparation of Rapidly Solidified Nd-Fe-B Flakes Used for Production of Permanent Magnets

Nd-Fe-B-type permanent magnets are used in applications that require a high-energy product/volume ratio in order to reduce weight. Automotive industry, hard drives, or wind turbines are just examples of an application where their use can be found. Conventional casting techniques reveal the formation of a high quantity of α-Fe and large Nd-rich regions. On the other hand, new techniques, like strip casting, melt-spinning and centrifugal atomization, produce homogeneous and fine-scaled microstructures. This paper discusses the application of rapid solidification by means of the centrifugal atomization method for preparation of Nd-Fe-B flakes. The effect of alloy composition and various process parameters of centrifugal atomization on the microstructure of rapidly solidified Nd-Fe-B alloy were investigated. The microstructures and the phase composition were examined by metallographic techniques, namely optical and scanning electron microscopy. Additionally, the influence of the processing parameters on the microstructures of as-cast flakes and subsequent magnetic properties of the prepared magnets will be discussed.

36 MATERIALS SCIENCE↗

Optimization of Hot Deformation Parameters and Constitutive Analysis for As-Cast Mg-5Li-3Zn-0.3Y Alloy Using Processing Maps

Hot deformation behavior of as-cast Mg-5Li-3Zn-0.3Y (wt.%) alloy has been studied by establishing processing maps covering the range of 200-450 °C in temperature and 0.001-10 s{sup −1} in strain rate. The map corresponding to the strain of 0.7 reveals that a domain of dynamic recrystallization occurred at 340-400 °C/0.01-0.158 s{sup −1} with its peak efficiency of approximately 31%. Analysis of the flow behaviors and microstructural observations indicated that dynamic recrystallization occurred in the domain, in which fine microstructure can be achieved. The above conditions represent the optimum processing parameters, and the flow instability regimes are also recognized from the maps. The average deformation in the deformed range was 136.414 kJ/mol which is close to that for lattice self-diffusion in magnesium and far smaller than that for as-cast Mg-5.75Zn-0.73Y-0.36Zr (wt.%) alloy. It is believed that a lower activation energy for Mg-5Li-3Zn-0.3Y alloy can partly result from both the weak particle pinning effects and adding Li into the Mg-Zn-Y-Zr alloy. Results of extrusion experiments conducted at 350 °C show that the alloy can be easily extruded with good mechanical properties of the yield strength of 132 MPa, the fracture strength of 215 MPa and the elongation of 20.9%, and the grains can be well refined.

36 MATERIALS SCIENCE↗

Microstructure and Electromagnetic Shielding Properties of Mg-Zn-Ce-Y-Zr Alloys

Microstructure and electromagnetic interference shielding properties of extruded Mg-Zn-Ce-Y-Zr alloys were systematically investigated. A bimodal grain structure of fine recrystallized grains and deformed grains was observed in the alloys. Yttrium (Y) and cerium (Ce) refined the recrystallized grains. Mg-Zn-Ce phase, Mg{sub 3}Zn{sub 3}Y{sub 2} phase and a few precipitates containing Zn and Zr were observed. Y and Ce additions changed the texture of the alloys. When the total rare earth content reached 4 wt.%, the texture was remarkably weaker than other studied alloys. The shielding capacity increased first and then decreased with Y contents. The value of shielding effectiveness for the extruded Mg-5Zn-1Ce-2Y-0.6Zr alloys reached 79-118 dB in the frequency range of 30 MHz-1.5 GHz, which was significantly higher than that of some aluminum alloys. The addition of Y and Ce is effective in improving the shielding capacity in Mg alloys. The electrical conductivity and second phases in the alloys were important in enhancing shielding effectiveness. The texture and precipitation exerted significant effect on electrical conductivity. In addition, subsequently aging treatment evidently improved shielding effectiveness.

36 MATERIALS SCIENCE↗

A Two-Stage Physical-Based Model for Predicting Flow Stress of As-cast TiAl Alloy Under Hot Deformation Conditions

The hot deformation behavior of Ti-30Al-4.2Mn-4.5Nb-0.2B alloy was investigated using the isothermal compression experiment at temperatures of 1020-1200 °C and strain rates of 0.001-1 s{sup −1}. The flow stress was sensitive to the deformation parameters like temperature and strain rate, which decreases with the increase in temperature and decrease in strain rates. Based on the true stress-true strain data, a two-stage physical-based model was proposed to describe the flow stress curve of as-cast TiAl alloy during hot deformation process. For establishing the model, at first, the flow curves of dynamic recovery (DRV) were modeled by employing stress-dislocation relation and adjusting dislocation annihilation coefficient Ω. Then, the flow curves of dynamic recrystallization (DRX) were modeled by considering the dynamic softening behavior into Avrami equation. Finally, the flow curves in the entire deformation stages could be described by embedding the predicted data of DRV model (i.e., flow stress before the critical strain) into the predicted data by DRX model (i.e., flow stress after the critical strain). The critical strain for initiation of DRX was determined by the double-differentiation method. To evaluate the applicability and effectiveness of DRX kinetics equation, the DRX curves were calculated and were consistent with the microstructure observation. Comparison between the experimental and predicted data shows that the proposed physical-based model can well forecast the flow stress under a wide working domain.

36 MATERIALS SCIENCE↗

Microstructure, Texture, and Mechanical Properties of Ni-W Alloy After Accumulative Roll Bonding

In this study, the microstructure, texture, and mechanical properties evolution of Ni-14W (wt.%) alloy processed up to four cycles of accumulative roll-bonding (ARB) were investigated using electron backscatter diffraction, microhardness measurements, and tensile tests. The initial equiaxed grains, with an average size of 10 μm, underwent a strong refinement after ARB processing. The elongated ultrafine grains were parallel to the rolling direction, with a grain thickness of 0.2 µm. The texture after ARB processing was characterized by the typical rolling components (Copper, S and Brass), which showed a tendency toward stabilization after four cycles. The microhardness increased substantially (+ 86%) and seemed to saturate after three cycles. The tensile tests demonstrated that Ni-14W samples subjected to ARB processing exhibited high strength (> 1200 MPa after three ARB cycles) and very poor ductility.

36 MATERIALS SCIENCE↗

Comparison of Different Processing Routes for the Synthesis of Semiconducting AlSb

AlSb is a low-cost, high-band-gap semiconducting material, yet largely limited in its potential due to difficulty in the synthesis of single-phase AlSb. The present work compares different processing routes in their potency to produce bulk and nanocrystalline AlSb. Vacuum arc melting has been successfully employed, for the first time, to synthesize single-phase bulk AlSb. Owing to high vapor pressure of Sb, an optimum amount of excess Sb (3%) needs to be added to achieve single-phase line compound AlSb. Two methods, viz. mechanical alloying of elemental powders and mechanical milling of cast alloy, have been used to synthesize nanocrystalline AlSb. Nanocrystalline AlSb could be produced after ball milling the cast alloy; however, prolonged milling results in the appearance of Sb along with a non-stoichiometric Al-Sb-O oxide. Mechanical alloying of Al and Sb does not lead to appearance of single-phase AlSb, and the mixture largely consists of starting material and amorphous products. Therefore, the effectiveness of a synthesis route in producing single-phase AlSb is governed by the tendency of oxygen pickup during the processing.

36 MATERIALS SCIENCE↗