Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “scanning electron diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,027 records · Page 57

"Thermal Stability of Anodic Hafnium Oxide Nanotube Arrays"

Thermal stability of highly ordered Hafnium oxide, HfO2 nanotube arrays prepared through electrochemical anodization approach in the presence of ammonium fluoride is investigated in a temperature range of room temperature to 900 C in flowing Argon atmosphere. The formation of the HfO2 nanotube arrays was monitored by current density transient characteristics during anodization of hafnium metal foil. Morphologies of the as grown and post-annealed HfO2 nanotube arrays were analyzed by X-ray powder diffraction (XRD), Scanning electron microscopy (SEM) and Transmission electron microscopy (TEM). Although monoclinic HfO2 is thermally stable up to 2000K in bulk, the morphology HfO2 nanotube arrays degraded at 900 C. Detailed X-ray photoelectron spectroscopy (XPS) study revealed that the thermal treatment significantly impact the composition and chemical environment of the core elements (Hf, O and F) of HfO2. Possible reasons for the degradation of the nanotube morphology were discussed based on XPS study and possible future improvements were suggested briefly.

Qiu, Xiaofeng↗

Polysulfide ligand exchange on zinc sulfide nanocrystal surfaces for improved film formation

The physical and chemical properties of nanocrystals can be modified by changing the ligands attached at their surfaces. A ligand exchange procedure with ammonium polysulfides has been developed to replace the native ligands on cubic zinc sulfide nanocrystals. Several mixtures of polysulfides in formamide and other solvents were prepared with different average chain lengths and used to achieve high yield ligand exchange, as confirmed by UV–vis spectroscopy, infrared spectroscopy and X-ray photoelectron spectroscopy. The results show that polysulfide content can be increased with longer surface ligands and that the exchange process yields compositionally pure surfaces before and after high temperature anneals. X-ray diffraction and scanning electron microscopy show that, when annealed in nitrogen at 525 °C, polysulfide ligands lead to average crystal sizes 2–3 times larger than in the un-exchanged control sample. The ligand exchange procedure itself does not alter nanocrystal size. Nanocrystal inks prepared from the exchanged samples form thin films that exhibit superior grain growth, morphology, mass retention, and composition compared to the un-exchanged material. Overall, polysulfide species are demonstrated as alternative ligands for the surfaces of metal chalcogenide nanocrystals which, when incorporated in an efficient ligand-exchange procedure, can improve the quality of ZnS nanocrystal inks.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Senary refractory high-entropy alloy Cr x MoNbTaVW

This paper demonstrates that a senary refractory high-entropy alloy Cr x MoNbTaVW can be tailored over a certain range of Cr content with the BCC structure for different microstructures and physical properties, assisted by CALPHAD simulations. Microstructure characterizations are performed using X-ray diffraction and scanning electron microscopy. Chemical microsegregation during solidification predicted using the Scheil model generally agrees with the experimental results. The lattice constant, density, and Vickers’ micro-hardness of the highentropy alloy samples in the as-cast state are measured and discussed. For Cr x MoNbTaVW, x=2.0 case appears exceeding the upper limit of maintaining a single BCC phase HEA, determined by the XRD patterns. The elemental dependence of the mixing thermodynamic properties (entropy, enthalpy and Gibbs energy) in BCC phase in the senary system is analyzed. The calculated entropy of mixing and enthalpy of mixing for CrMoNbTaVW are 14.7 J/K/mol and -662.5 J/mol respectively.

36 MATERIALS SCIENCE↗

W/TaC/SiC sandwich stack for high temperature applications

High-temperature stability of the tungsten/tantalum carbide/silicon carbide (W/TaC/SiC) system was examined and compared to the tungsten/silicon carbide (W/SiC) system. Interfacial reactions, surface morphology, and roughness evolutions on thermal annealing at 1000 °C were systematically investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM) and atomic force microscopy (AFM). For the W/SiC system, WC, W 2 C and W 5 Si 3 phases were observed due to severe chemical reaction after 24 h annealing, which led to an inhomogeneous surface structure with several large craters and small pores, thereby increasing surface roughness greatly. On the other hand, there was no tungsten silicide and/or carbide formation upon annealing with a TaC diffusion barrier. The surface structure remained nearly unchanged, and small changes in surface roughness with annealing time, which could be due to the growth of W grains, were noted. Furthermore, both the as-deposited and the 24 h annealed W/TaC/SiC samples presented an excellent interfacial bonding with a dense uniform interface. The results indicate that TaC is a promising diffusion barrier in the W/SiC system for high temperature applications.

36 MATERIALS SCIENCE↗

The transformation of U(VI) and V(V) in carnotite group minerals during dissimilatory respiration by a metal reducing bacterium

Recent results from laboratory and field studies support that dissimilatory metal reducing (DMR) bacteria influence the fate and transport of uranium in anaerobic subsurface environments. To date, most research efforts have focused on the reduction of soluble U(VI) by DMR bacteria to form insoluble uraninite (UO 2 ). Subsurface environments harbor, however, large reservoirs of U(VI) in solid or mineral form. Uranium that is structure-bound in minerals is expected to be more refractory to microbial reduction than soluble U, based on analogy with Fe respiration. The reducibility of U(VI) could impact the fate of U(IV) by controlling mineral precipitation reactions, which has implications for the long-term immobilization of U in subsurface environments. Here, we studied anoxic cultures of Shewanella putrefaciens CN32 incubated with natural carnotite-group minerals by X-ray diffraction, electron microscopy, scanning transmission X-ray microscopy (STXM). Near-edge X-ray absorption fine structure (NEXAFS) spectroscopy measurements at U-N 4,5 , V-L 2,3 , and O-K edges on cultures incubated up to 10 months show that V(V) was reduced to V(IV), whereas U was not reduced. In contrast, V(V) and U(VI) in solution were both completely reduced to lower oxidation states by CN32, as precipitates within the exopolymer surrounding the bacteria. Assays for the toxicity of U and V to CN32 showed that biofilm formation was stimulated at 0.001 M U(VI), and growth was inhibited at concentrations of U(VI) greater than 0.001 M. Vanadium did not inhibit growth or stimulate biofilm formation at any concentration tested. Investigations of the bacteria-mineral and bacteria-metal interface at the nanometer and molecular scales provide new insights into the co-respiration of V and U that help explain their biogeochemical cycling and have implications for subsurface bioremediation of these elements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Reactivity deterioration of NiO/Al{sub 2}O{sub 3} oxygen carrier for chemical looping combustion of coal in a 10 kW{sub th} reactor

A relatively long-term experiment for chemical looping combustion of coal with NiO/Al{sub 2}O{sub 3} oxygen carrier was carried out in a 10 kW{sub th} continuous reactor of interconnected fluidized beds, and 100 h of operation was reached with the same batch of the oxygen carrier. The reactivity deterioration of the oxygen carriers was present during the experimental period. The reactivity deterioration of reacted oxygen carriers at different experimental stages was evaluated using X-ray diffraction (XRD), scanning electron microscope (SEM), and X-ray fluorescence spectrometer. SEM analysis showed no significant change in the morphology of the nickel-based oxygen carrier at the fuel reactor temperature {<=}940 C, but loss of surface area and porosity of reacted oxygen carriers was observed when the fuel reactor temperature exceeded 960 C. The results show that the sintering effect have mainly contributed to the reactivity deterioration of reacted oxygen carriers in the CLC process for coal, while the effects of coal ash and sulfur can be ignored. The oxidization of reduced oxygen carrier with air was an intensive exothermic process, and the high temperature of oxygen carrier particles led to sintering on the surface of oxygen carrier particles in the air reactor. Attention must be paid to control the external circulation of oxygen carrier particles in the interconnected fluidized beds in order to efficiently transport heat from the air reactor to the fuel reactor, and reduce the temperature of oxygen carrier particles in the air reactor. Improvement of reactivity deterioration of reacted oxygen carriers was achieved by the supplement of steam into the fuel reactor. Nevertheless, NiO/Al{sub 2}O{sub 3} is still one of the optimal oxygen carriers for chemical looping combustion of coal if the sintering of oxygen carrier is minimized at the suitable reactor temperature. (author)

01 COAL, LIGNITE, AND PEAT↗

Autogenous healing of Engineered Cementitious Composites (ECC) based on MgO-fly ash binary system activated by carbonation curing

Developing self-healing of concrete cracks represents a critical approach for extending material longevity. If demonstrated on concretes with CO 2 stored through carbonation curing, self-healing can further mitigate infrastructure lifecycle emissions. In this study, the self-healing process is investigated on novel Engineered Cementitious Composites (ECC) based on binary blends of reactive MgO cement and siliceous fly ash activated by carbonation. The self-healing was observed under cyclic wetting and drying exposures and was characterized by measurements of resonance frequency, optical microscopy and X-ray computed microtomography (XCT). Thermogravimetric analysis, X-ray powder diffraction and scanning electron microscopy were employed to assist in identifying healing products and mechanisms. It was found that micro-cracks could be autogenously filled in 7 wet-dry cycles, as evidenced by over 95% recovery of resonance frequency and healed crack appearance under optical microscopic observation. Nevertheless, the composite mechanical performance, particularly tensile strength and ductility, did not fully recover with respect to the uncracked specimens. The inadequate post-healing mechanical properties were consistent with XCT observations that indicated low material densities in the cracked area. Based on the chemical and microstructural characterizations, it was determined that nesquehonite crystallites were responsible for the crack filling. Although the nesquehonite filled cracks will be less permeable to invasion of reactive fluids, novel strategies are needed to establish more robust healing capability to completely restore the crack bridging and composite tensile performance.

36 MATERIALS SCIENCE↗

PdAgAu alloy with high resistance to corrosion by H 2 S

PdAgAu alloy films were prepared on porous stainless steel supports by sequential electroless deposition. Two specific compositions, Pd 83 Ag 2 Au 15 and Pd 74 Ag 14 Au 12 , were studied for their sulfur tolerance. The alloys and a reference Pd foil were exposed to 1000 H 2 S /H 2 at 623 K for periods of 3 and 30 hours. The microstructure, morphology and bulk composition of both nonexposed and H 2 S-exposed samples were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). XRD and SEM analysis revealed time-dependent growth of a bulk Pd{sub 4}S phase on the Pd foil during H 2 S exposure. In contrast, the PdAgAu ternary alloys displayed the same FCC structure before and after H 2 S exposure. In agreement with the XRD and SEM results, sulfur was not detected in the bulk of either ternary alloy samples by EDS, even after 30 hours of H 2 S exposure. X-ray photoelectron spectroscopy (XPS) depth profiles were acquired for both PdAgAu alloys after 3 and 30 hours of exposure to characterize sulfur contamination near their surfaces. Very low S 2p and S 2s XPS signals were observed at the top-surfaces of the PdAgAu alloys, and those signals disappeared before the etch depth reached ~ 10 nm, even for samples exposed to H 2 S for 30 hours. The depth profile analyses also revealed silver and gold segregation to the surface of the alloys; preferential location of Au on the alloys surface may be related to their resistance to bulk sulfide formation. In preliminary tests, a PdAgAu alloy membrane displayed higher initial H{sub 2} permeability than a similarly prepared pure Pd sample and, consistent with resistance to bulk sulfide formation, lower permeability loss in H 2 S than pure Pd.

36 MATERIALS SCIENCE↗

Mechanism of H 2 plasma-enabled reduction of hematite thin films

Hydrogen plasma is gaining significant interest as a promising pathway for direct iron ore reduction and for lowering process temperatures but the reduction mechanism remains poorly understood. In this work we analyzed the plasma and thermal reduction of thin-film hematite (Fe 2 O 3 ) at temperatures below 340 °C using X-ray diffraction and scanning electron microscopy with energy-dispersive X-ray spectroscopy. Plasma reduced the incubation period by an order of magnitude and increased the reduction rate by a factor of 2.6 compared to thermal reduction. Plasma-produced H-atoms facilitate the formation of numerous iron nucleation sites, bypassing the energetically unfavorable dissociative adsorption of H 2 on iron oxide. These iron nuclei can autocatalyze the reduction of the surrounding hematite via a hydrogen spillover mechanism. Our results demonstrate that plasma-derived H-atoms primarily impact the initial nucleation-limited stage. These new insights provide a mechanistic framework that can aid the implementation and optimization of hydrogen plasma-assisted iron oxide reduction at reduced temperatures.

08 HYDROGEN↗

LiMnPO4·Li3V2(PO4)3 composite cathode material derived from Mn(VO3)2 nanosheet precursor

The LiMnPO4·Li3V2(PO4)3/C composite cathode material was synthesized from Mn(VO3)2 nanosheet precursor, which was prepared by a hydrothermal method. The structure and morphology of the composite were systematically investigated by powder X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscope (TEM) and scanning transmission electron microscopy (STEM), etc. The LiMnPO4·Li3V2(PO4)3/C composite material exhibits a low polarization and high specific capacity of 150.7 mAh g-1 at 0.1C in voltage range of 2.5–4.5V, and excellent cycle and rate performance for its stable nanocomposite framework. The composite material dominantly exists in the morphological shape of nanograins and nanorods, which increases the surface area and hence facilitate the electrolyte penetration. The nanoparticle components were even further identified in detail.

Lei, Zhihong↗

Mechanical properties of refractory high-entropy alloys: Experiments and modeling

Refractory high-entropy alloys hold the potential for high-temperature applications beyond the capability of the state-of-the-art Ni-based superalloys, and thus, it is important to study their solid solution formation characteristics and mechanical properties. In this study, designed by CALPHAD method, formation of as-cast arc-melted body-centered cubic MoNbTaTiV was experimentally verified using X-ray diffraction and scanning electron microscopy. The measured density and lattice parameter for MoNbTaTiV are 9.29 g/cm3 and 3.224 Å, which obey the rule of mixtures (ROM). The alloy exhibits high hardness at 443 Hv, high yield strength at 1.4 GPa, and good compressive fracture strength at 2.45 GPa with a fracture strain of ~30% at room temperature. The yield strength and hardness values of this alloy, and other single-phase refractory high-entropy alloys, are estimated using a simple model of solid solution strengthening. Reasonable agreement between modeling prediction and experiments is obtained. In addition, first-principles density functional theory calculations predict an enthalpy of formation of -0.865 kJ/mol for the MoNbTaTiV alloy, with calculated atomic volume and elastic properties (e.g., bulk and elastic moduli) obeying the ROM.

36 MATERIALS SCIENCE↗

Phase relationships in the CeFe 8 Co 3 Ti 1 - y Si y system

We investigated the phase formation behavior of the nominal CeFe 8 Co 3 Ti 1-y Si y system for 0 ≤ y ≤ 0.6 by powder x-ray diffraction and scanning electron microscopy with energy dispersive x-ray spectroscopy for ingots formed by arc-melting then annealing at 1000 °C and quenching to room temperature. The ingots are seen to nearly single phase for y ≤ 0.4 and are multi-phase for y ≥ 0.5 though a compound of the ThMn 12 type does indeed form for all values of y. We also measured the saturation magnetizations (M s ), Curie temperatures (T C ), and magnetic anisotropy fields (H a ) for the y ≤ 0.4 samples and the values of Ms and Ha appear to be nearly identical for all y 0.4. TC, but, is seen to increase about 20 °C in this range for increasing y.

36 MATERIALS SCIENCE↗

Spark plasma sintered, MoNbTi-based multi-principal element alloys with Cr, V, and Zr

MoNbTi, MoNbTiZr, CrMoNbTiZr, and MoNbTiVZr multi-principal element alloys (MPEAs) were fabricated via spark plasma sintering (SPS) and investigated for use in high-strength applications. The fabrication method by SPS and powder metallurgy differs from those presented in the prior literature, where most MPEAs are fabricated using arc melting (AM) methods. Here cryogenic milling was used to maximize potential defect sinks (grain boundaries) for radiation resistance and to increase ultimate tensile strength through the Hall-Petch effect. SPS was chosen for consolidation in order to maintain a fine-grained structure during densification. Each alloy was characterized using x-ray diffraction and scanning electron microscopy for phase identification and compositional homogeneity. The base ternary alloy MoNbTi presented a predominantly single BCC system with minor cubic phases. The introduction of additional alloying elements—Zr, V, and Cr—heightened the phase complexity and increased the fractions of a secondary BCC phase and an HCP phase from Zr. The addition of Cr induced a larger fraction of the Laves phase to form. The addition of V caused the precipitation of small Mo inclusions. Thermodynamic analysis was performed to understand the separation of phases in each alloy. Discrepancies among the phase predictions generated by thermodynamic models, phases previously presented in the literature, and the characterization results suggest that MPEA fabrication methods, especially solid-state methods, require significant investigation to ensure that alloys can remain stable throughout their anticipated service lifetimes.

36 MATERIALS SCIENCE↗

Sonochemical synthesis of highly luminescent Ln 2 O 3 :Eu 3+ (Y, La, Gd) nanocrystals

In this study, sonication of Ln(CH 3 COO) 3 ·H 2 O, Eu(CH 3 COO) 3 ·H 2 O and NaOH dissolved in the ionic liquid-butyl-3-methylimidazolium bis(trifluoromethane)sulfonylamide lead to Ln(OH) 3 :Eu (Ln: Gd, La, Y) nanoparticles. Subsequent calcination at 800 °C for 3 h allowed to obtain Ln 2 O 3 :Eu nanopowders. Gd 2 O 3 and Y 2 O 3 were obtained in the C-type lanthanide sequioxide structure, whereas La 2 O 3 crystallized in the A-type. Structure, morphology, and luminescent properties of the nano-oxides were investigated by powder X-ray diffraction (PXRD), scanning electron microscopy (SEM), dispersive X-ray (EDX), and photoluminescence (PL). SEM studies revealed that the synthesized Gd 2 O 3 :Eu, La 2 O 3 :Eu, and Y 2 O 3 :Eu formed nano-spindle, -sheets, and -rods in shape, respectively. The nanoscale materials show very efficient red emission due to the intraconfigurational f–f transitions of Eu 3+ . The quantum yields for Ln 2 O 3 :Eu (5%) were determined to be 4.2% for Ln=Gd, 13.8% for Ln=Y and 5.2% for Ln=La. The asymmetric ratio I 02 /I 01 of Eu 3+ varies from 5.3 for Gd 2 O 3 , to 5.6 for Y 2 O 3 to 6.5 for La 2 O 3 , which increased the color chromaticity.

36 MATERIALS SCIENCE↗

Additive manufacturing of AISI M2 tool steel by binder jetting (BJ): Investigation of microstructural and mechanical properties

The presented research demonstrates for the first time the successful processing of AISI M2 tool steel by binder jetting, a promising additive manufacturing technique capable of producing complex shapes with minimal residual stresses and isotropic properties. The optimal printing parameters were explored by varying processing parameters such as the binder saturation (45 %–105 %), binder set time (0 to 10 s), targeted bed temperature (50–60 °C), oscillator (2600–2750 rpm), recoater (20–28 mm/s), and roller speeds (200–300 rpm). Microstructural characterization and evaluation of mechanical properties of binder jetted parts were performed using x-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) to study their chemical composition, powder morphology, microstructure, carbide morphologies, relative density, hardness, compressive strength, and ductility. Two powder sizes (5 and 10 μm) were used, and sintering was performed at varying temperatures (1270, 1280, and 1300 °C) and durations (60 and 120 min), followed by a furnace, air, and water cooling. An optimum hardness of ~970 HV was obtained when parts were sintered at 1270 °C for 60 min, followed by water quenching. Impressive compressive strength of ~ 3580 MPa was observed in the sample sintered at 1280 °C for 60 min duration, followed by air cooling. Furnace-cooled parts showed the highest density of ~95 %, whereas the relative density of air- and water-cooled parts varied between ~91 to 93.50 %, respectively. The microstructure of sintered samples revealed the formation of M 6 C stable carbide, M 2 C metastable carbide, MC as a secondary carbide, and a-Fe matrix, which contributed to the observed increase in mechanical properties.

36 MATERIALS SCIENCE↗

Oxidation behavior of U-Si compounds in air from 25 to 1000 C

The air oxidation behavior of U 3 Si 2 , USi, and U 3 Si 5 is studied from room temperature to 1000 C. Moreover, the onsets of breakaway oxidation for each compound are identified during synthetic air ramps to 1000 C using thermogravimetric analysis. Isothermal air oxidation tests are performed below and above the breakaway oxidation onset to discern the oxidation kinetic behavior of these candidate accident tolerant fuel forms. Uranium metal is tested in the same manner to provide a reference for the oxidation behavior. We present thermogravimetric, x-ray diffraction, and scanning electron microscopy analysis here along with a discussion of the oxidation behavior of these materials and the impact of the lack of oxidation resistance to their deployment as accident tolerant nuclear fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High-throughput ion irradiation of additively manufactured compositionally complex alloys

Several advanced nuclear reactor designs promise efficiency and safety improvements over the current reactor fleet but are limited by the current set of ASME code-qualified materials. Novel alloys including high-entropy alloys (HEAs), and more broadly compositionally complex alloys (CCAs), have shown promising irradiation-tolerance. However, the vast range of alloy compositions adds to an already time-consuming alloy development process. In this study, to accelerate the development of novel alloys for nuclear applications, a high-throughput (HTP) methodology has been employed. Additive manufacturing has been used to produce a compositional array of unary, binary, ternary, and quaternary alloys, including several CCAs, which span the Cr-Fe-Mn-Ni composition space. Additionally, the compositional array was homogenized at 1000°C for 24 hours and each sample was irradiated using 4-MeV Ni2+ ions at room temperature to a peak damage of 50 dpa, as estimated using SRIM, at the University of Wisconsin Ion Beam Laboratory. A custom XY stage was built to accommodate the large compositional array and half of each sample was masked during irradiation enabling both the irradiated and unirradiated properties of each alloy to be characterized side-by-side. Each alloy was characterized using X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and nanoindentation. CALPHAD simulations spanning the entire Cr-Fe-Mn-Ni composition space at 1000°C were performed to compare predicted equilibrium phases with phases identified experimentally from the unirradiated regions of each alloy. Nanoindentation measurements indicate radiation-induced hardening ranging from ~1-1.5 GPa in each of Cr-Fe-Mn-Ni CCAs, which is relatively insensitive to modest changes in alloy composition and comparable to hardening observed in neutron irradiated Cr-Fe-Mn-Ni CCAs in the literature. Overall, a substantial time savings was realized by employing HTP synthesis, irradiation, and characterization in this study compared to conventional techniques, the implications of which are discussed.

36 MATERIALS SCIENCE↗