At least 1,027 records · Page 57

A Novel Low-Temperature Fiffusion Aluminide Coating for Ultrasupercritical Coal-Fried Boiler Applications

An ultrasupercritical (USC) boiler with higher steam temperature and pressure is expected to increase the efficiency of the coal-fired power plant and also decrease emissions of air pollutants. Ferritic/martensitic alloys have been developed with good creep strength for the key components in coal-fired USC plants. However, they typically suffer excessive steam-side oxidation, which contributes to one of main degradation mechanisms along with the fire-side corrosion in coal-fired boilers. As the steam temperature further increases in USC boilers, oxidation of the tube internals becomes an increasing concern, and protective coatings such as aluminide-based diffusion coatings need to be considered. However, conventional aluminizing processes via pack cementation or chemical vapor deposition are typically carried out at elevated temperatures (1000-1150 C). Thermochemical treatment of ferritic/martensitic alloys at such high temperatures could severely degrade their mechanical properties, particularly the alloy's creep resistance. The research focus of this project was to develop an aluminide coating with good oxidation resistance at temperatures {le} 700 C so that the coating processing would not detrimentally alter the creep performance of the ferritic/martensitic alloys. Nevertheless, when the aluminizing temperature is lowered, brittle Al-rich intermetallic phases, such as Fe{sub 2}Al{sub 5} and FeAl{sub 3}, tend to form in the coating, which may reduce the resistance to fatigue cracking. Al-containing binary masteralloys were selected based on thermodynamic calculations to reduce the Al activity in the pack cementation process and thus to prevent the formation of brittle Al-rich intermetallic phases. Thermodynamic computations were carried out using commercial software HSC 5.0 for a series of packs containing various Cr-Al binary masteralloys. The calculation results indicate that the equilibrium partial pressures of Al halides at 700 C were a function of Al content in the Cr-Al alloys. Cr-25Al and Cr-15Al were chosen as the masteralloys in the pack cementation process. In contrast to pure Al masteralloy which led to the formation of Fe{sub 2}Al{sub 5} coatings at 650 C, a coating consisting of a thin Fe{sub 2}Al{sub 5} outer layer and an FeAl inner layer was formed at 700 C with the Cr-25Al masteralloy. By switching to the Cr-15Al masteralloy, thin FeAl coatings ({approx}12 {micro}m) containing < 50 at.% Al were achieved at 700 C. The effect of the amount of masteralloys on coating growth was also studied by employing packs containing 2NH{sub 4}Cl-x(Cr-15Al)-(98-x)Al{sub 2}O{sub 3}, where x = 10, 20, 30, 40, 50, 60, and 70 wt.%. It was noticed that when the Cr-15Al masteralloy was increased from 10 to 40 wt.% in the pack, both coating thickness and surface Al content increased, suggesting that gas phase kinetics played an important role in Al deposition. However, with further increase of the masteralloy, solid state diffusion became the rate-limiting factor. The long-term oxidation performance of the aluminide coatings synthesized at 700 C with Cr-25Al and Cr-15Al masteralloys was evaluated in the water vapor environment at 650-700 C. The low-temperature pack coatings demonstrated excellent oxidation resistance at 650 C in humid air after {approx}1.2 yr testing. Longer lifetimes can be expected for these thin coatings due to minimal interdiffusion at this testing temperature. Exposure at 700 C was conducted to accelerate coating failure via increased interdiffusion of Al with the substrate alloy. The coatings also exhibited good oxidation protection up to 6,000-8,000 h at 700 C, with longer testing needed for coating failure to occur. Furthermore, the oxidation results indicate that in addition to the Al reservoir (as determined by the Al content and coating thickness), the initial coating surface quality had a significant impact on the oxidation behavior. In addition, the effect of various pack aluminide coatings on the creep resistance of coated T91 was investigated. Three representative types of coatings with different thicknesses, Al concentrations and phase constituents were included in the creep test. The creep experiments were performed at 650 C in air at uniaxial stress levels of 100-120 MPa. The thick aluminide coating made at 1050 C showed a considerable reduction ({approx} 42%) in the creep rupture life of the coated alloy, due to the decrease of the load-bearing section. In contrast, the low-temperature thin coatings developed in this project did not significantly reduce the creep resistance of the coated T91 alloy, particularly the thin FeAl coating synthesized at 700 C using the Cr-15Al masteralloy.

36 MATERIALS SCIENCE↗

Computational design of high entropy alloy coating for hydrogen turbine applications

This project aims to develop novel high entropy alloy (HEA)-based coatings to protect critical components in hydrogen-fueled turbine power system. The HEA-coatings will demonstrate superior performance in hydrogen combustion environment to commercial NiCoCrAlY coating in current natural gas turbine system. The HEA coating facilitates the formation of a protective scale of alpha-alumina to slow down the inward diffusion of oxidizing species and the outward diffusion of metal elements, and possesses ultrahigh corrosion and spallation resistance to prolong the service lifetime of critical components in hydrogen turbine power system. Aimed to accelerate the discovery of novel HEA coating compositions, high throughput computational modeling including CALPHAD and density functional theory and machine learning are performed to predict phase stability, oxygen permeability, oxidation rate constant, coefficient of thermal expansion, and mechanical properties. Based on the modeling and machine learning prediction, experimental validation is performed. Preliminary results will be presented and approaches to minimize oxidation will be discussed.

alloy design↗

Engine Coatings

Increasing the operating temperature of turbine engines reduces fuel consumption and increases engine efficiency. However, engine components must be protected from excessive heat. Lewis Research Center has successfully developed thermal barrier coatings (TBCs), which are deposited on the components. They insulate, offer oxidation and corrosion resistance and increase adherence. Surface temperatures can be reduced by 200 degrees centigrade or more. G. E. Aircraft Engines, a Lewis contractor, now uses a TBC based on the one developed at Lewis, on production engines. The system, which consists of a bond and a top coat extends component life from 1.3 to 2 times. The company is also testing TBCs on components that operate at higher temperatures.

Source record↗

Balloon for Long-Duration, High-Altitude Flight at Venus

A document describes a 5.5-m-diameter, helium-filled balloon designed for carrying a scientific payload having a mass of 44 kg for at least six days at an altitude of about 55 km in the atmosphere of Venus. The requirement for floating at nearly constant altitude dictates the choice of a mass-efficient spherical super-pressure balloon that tracks a constant atmospheric density. Therefore, the balloon is of a conventional spherical super-pressure type, except that it is made of materials chosen to minimize solar radiant heating and withstand the corrosive sulfuric acid aerosol of the Venusian atmosphere. The shell consists of 16 gores of a multilayer composite material. The outer layer, made of polytetrafluoroethylene, protects against sulfuric acid aerosol. Next is an aluminum layer that reflects sunlight to minimize heating, followed by an aluminized polyethylene terephthalate layer that resists permeation by helium, followed by an aromatic polyester fabric that imparts strength to withstand deployment forces and steady super-pressure. A polyurethane coat on the inner surface of the fabric facilitates sealing at gore-to-gore seams. End fittings and seals, and a tether connecting the end fittings to a gondola, are all made of sulfuric-acid-resistant materials.

Hall, Jeffrey↗

Corrosion evaluation of alloys and MCrAlX coatings in molten carbonates for thermal solar applications

Here, stainless steels (SS) 310, 321, 347, Incoloy 800H (In800H), alumina-forming austenitic (AFA-OC6), Ni superalloy Inconel 625 (IN625), and MCrAlX (M: Ni, and/or Co; X: Y, Hf, Si, and/or Ta) coatings were corroded in molten carbonates in N 2 and bone-dry CO 2 atmospheres. Electrochemical tests in molten eutectics K 2 CO 3 -Na 2 CO 3 and Na 2 CO 3 -K 2 CO 3 -Li 2 CO 3 at temperatures higher than 600 °C were evaluated using an open-circuit potential followed by a potentiodynamic polarization sweep to determine the corrosion rates. Because the best-performing alloys at 750 °C were In800H followed by SS310, these two alloys were selected as the substrate material for the MCrAlX coatings. The coatings were able to mitigate corrosion in molten carbonates environments. The corrosion of substrates SS310 and In800H was reduced from ~2500 um/year to 34 um/year when coated with high-velocity oxyfuel (HVOF) NiCoCrAlHfSiY and pre-oxidized (air, 900 °C, 24 h, 0.5 °C/min) before molten carbonate exposure at 700 °C in bone-dry CO 2 atmosphere. Metallographic characterization of the corroded surfaces showed that the formation of a uniform alumina scale during the pre-oxidation seems to protect the alloy from the molten carbonate attack.

14 SOLAR ENERGY↗

Water protection in coke-plant design

Wastewater generation, water consumption, and water management at coke plants are considered. Measures to create runoff-free water-supply and sewer systems are discussed. Filters for water purification, corrosion inhibitors, and biocides are described. An integrated single-phase technology for the removal of phenols, thiocyanides, and ammoniacal nitrogen is outlined.

01 COAL, LIGNITE, AND PEAT↗

Comparison of selective oxidation in Ni-based alloys exposed to PWR primary water and Rhines Pack environments

A mechanistic understanding of corrosion and oxidation processes is crucial to ensure long-term resistance to stress corrosion cracking of Ni-based structural alloys in PWR primary and secondary systems. Aqueous corrosion of complex Ni-based alloys under PWR water conditions as well as gaseous oxidation of low-solute Ni binary alloys at high temperatures (>800 °C) have been studied extensively. However, a significant knowledge gap exists between response of Ni-based alloys in aqueous and gaseous environmental conditions. Selective oxidation at different temperatures was investigated in a series of gaseous Rhines Pack experiments for a high-purity Ni-5Cr binary alloy and a commercial Ni-18Cr-9Fe Alloy 600. Focused ion beam milling enabled the extraction of site-specific specimens containing high-energy grain boundaries. Analytical transmission electron microscopy was employed to analyze the microstructure and chemical composition of the resulting localized oxidation. The oxidation mechanism in the gaseous Rhines Pack atmosphere at 420 °C included the formation of a protective Cr-oxide cap above grain boundaries in all cases. At higher temperatures (600 and 800 °C), penetrative intergranular and transgranular internal oxidation was observed. Direct comparisons are made to corrosion response for these same materials in simulated PWR primary water at 320-360 °C. These results reveal a temperature dependence for gaseous oxidation and indicate mechanistic differences between aqueous and gaseous degradation in Ni-Cr alloys. These results imply that selective intergranular corrosion in PWR water is governed by processes beyond mere oxidation. Consideration of complex corrosion/dissolution processes at surfaces and in open cracks is essential for the better understanding of stress corrosion cracking mechanisms in PWR primary water.

Rhines Pack, Alloy 600, Ni-base alloys, Internal O↗

Computational Modeling and Assessment Of Nanocoatings for Ultra Supercritical Boilers

Coal-fired power plants are a significant part of the nation's power generating capacity, currently accounting for more than 55% of the country's total electricity production. Extending the reliable lifetimes of fossil fired boiler components and reducing the maintenance costs are essential for economic operation of power plants. Corrosion and erosion are leading causes of superheater and reheater boiler tube failures leading to unscheduled costly outages. Several types of coatings and weld overlays have been used to extend the service life of boiler tubes; however, the protection afforded by such materials was limited approximately one to eight years. Power companies are more recently focused in achieving greater plant efficiency by increasing steam temperature and pressure into the advanced-ultrasupercritical (A-USC) condition with steam temperatures approaching 760°C (1400°F) and operating pressures in excess of 35MPa (5075 psig). Unfortunately, laboratory and field testing suggests that the resultant fireside environment when operating under A-USC conditions can potentially cause significant corrosion to conventional and advanced boiler materials1-2. In order to improve reliability and availability of fossil fired A-USC boilers, it is essential to develop advanced nanostructured coatings that provide excellent corrosion and erosion resistance without adversely affecting the other properties such as toughness and thermal fatigue strength of the component material.

01 COAL, LIGNITE, AND PEAT↗

Perspective—Localized Corrosion: Passive Film Breakdown vs Pit Growth Stability

A debate about the critical step in localized corrosion has raged for decades. Some researchers focus on the composition and structure of the passive film associated with the initial breakdown of the film, whereas others consider that the susceptibility to pitting is controlled by the pit growth kinetics and the stabilization of pit growth. The basis for a unified theory of pitting is presented here in which pit stability considerations are controlling under aggressive conditions (harsh electrolytes and extreme environments and/or susceptible microstructures) and the passive film properties and protectiveness are the critical factors in less extreme environments and/or for less susceptible alloys.

36 MATERIALS SCIENCE↗

Following the Morphological Disruption by an Electrolyte of a Buried Interface

A challenge of broad interest in both materials science and biology is the study of interfaces that are buried within a structure, particularly multilayer structures. Despite the enormous costs of corrosion and many decades of corrosion research, details of the mechanisms of various sorts of corrosion are still not clear, in part due to the difficulty in interrogating the interface between the corroding metal and an organic coating, which is typically used to mitigate corrosion. Generally, the performance of such coatings is evaluated by visual inspection after exposure or by modeling impedance data, which is a process not straightforwardly connected to physical interface structures. "Rocking-curve" X-ray scattering measurements provide a means of probing such interfaces due to the ability of X-rays to penetrate materials. Here, variations in the morphology of an interface between a protective coating and a metal substrate due to exposure to an electrolyte are derived from analysis of rocking-curve data in conjunction with atomic force microscopy imaging of the outer coating surface. The interfaces of cross-linked epoxy coatings with aluminum are irreversibly changed after 12 h of contact between the electrolyte solution and the face of the coating. The character of this change varies with the molecule used to cross-link the coating. Since X-ray off-specular scattering is sensitive to changes on the nanometer scale, it is also able to register interface degradation on time scales shorter than those probed by many other techniques, potentially expediting the evaluation of coatings for protection against degradation of the interface.

36 MATERIALS SCIENCE↗

Adhesive and Protective Characteristics of Ceramic Coating A-417 and Its Effect on Engine Life of Forged Refractaloy-26 (AMS 5760) and Cast Stellite 21 (AMS 5385) Turbine Blades

The adhesive and protective characteristics of National Bureau of Standards Coating A-417 were investigated, as well as the effect of the coating on the life of forged Refractaloy 26 and cast Stellite 21 turbine blades. Coated and uncoated blades were run in a full-scale J33-9 engine and were subjected to simulated service operations consisting of consecutive 20-minute cycles (15 min at rated speed and approximately 5 min at idle). The ceramic coating adhered well to Refractaloy 26 and Stellite 21 turbine blades operated at 1500 degrees F. The coating also prevented corrosion of the Refractaloy 26, a corrosion-sensitive nickel-base alloy, and of the Stellite 21, a relatively corrosion-resistant cobalt-base alloy. Although the coating prevented corrosion of both alloys, it had no apparent effect on blade life.

ALLOYS, HEAT-RESISTING↗

Ab Initio Design of High-Entropy Thermal/ Environmental Barrier Coatings

Next generation thermal/environmental barrier coatings (TEBC) require carefully balancing various properties including phase stability, thermal conductivity, coefficient of thermal expansion (CTE), mechanical properties, and resistance against hot corrosion and water vapor recession. This work mainly focuses on rapid design of cost-effective high entropy rare-earth disilicates and aluminum garnets to protect SiC-based ceramic matrix composites and nickel-based superalloys in the hot section of gas turbine engines using density functional theory methods. Our calculations identify several low-cost high entropy TEBC exhibiting ultralow thermal conductivity at 1500 K and desirable CTE while maintaining good mechanical properties, including Er1/2Y3/4Yb3/4Si2O7, Gd1/4Er1/4Y3/4Yb3/4Si2O7, Eu1/4Er1/4Y3/4Yb3/4Si2O7, and (Y1/4Gd1/4Er1/4Yb1/4)3Al5O12. This work also aims to gain fundamental understanding of oxygen diffusion in model disilicates. Minimizing oxidizer (such as water vapor and oxygen) permeability through the EBC layer can significantly decrease the growth rate of thermally grown oxide and extend the service life of the coating system. Oxygen diffusion mechanisms including formation energy of defects under varying oxygen conditions and defect migration energy barriers will be presented.

coefficient of thermal expansion↗

Superhard Nanocrystalline Homometallic Stainless Steel on Steel for Seamless Coatings

The objective of this work is to deposit nanocrystalline stainless steel onto steel substrates (homometallic) for enhanced wear and corrosion resistance. Homometallic coatings provide superior adhesion, and it has been shown that ultrafine-grained materials exhibit the increased hardness and decreased permeability desired for protective coatings. Nanocrystals will be produced by controlling nucleation and growth and use of an ion beam during deposition by e-beam evaporation or sputtering. Phase I is depositing 31 6L nanocrystalline stainless steel onto 31 6L stainless steel substrates. These coatings exhibit hardnesses comparable to those normally obtained for ceramic coatings such ZrO2, and possess the superior adhesion of seamless, homometallic coatings. Hardening the surface with a similar material also enhances adhesion, by avoiding problems associated with thermal and lattice mismatch. So far we have deposited nanocrystalline homometallic 316L stainless steel coatings by varying the ions and the current density of the ion beams. For all deposition conditions we have produced smooth, uniform, superhard coatings. All coatings exhibit hardness of at least 200% harder than that of bulk materials. Our measurements indicate that there is a direct relationship between nanohardness and the current density of the ion beam. Stress measurements indicate that stress in the films is increasingly proportional to current density of the ion beam. TEM, XPS, and XRD results indicate that the coated layers consist of FCC structure nanocrystallites with a dimension of about 10 to 20 nm. The Ni and Mo concentration of these coating are lower than those of bulk 316L but the concentration of Cr is higher.

Tobin, Eric J.↗

Replacement for a Flex Hose Coating at the Space Shuttle Launch Pad

Aerocoat AR-7 is a coating that has been used to protect stainless steel flex hoses at NASA's Kennedy Space Center launch complex and hydraulic lines of the mobile launch platform (MLP). This coating has great corrosion control performance and low temperature application. AR-7 was developed by NASA and produced exclusively for NASA but its production has been discontinued due to its high content of volatile organic compounds (VOC) and significant environmental impact. The purpose of this project was to select and evaluate candidate coatings to find a replacement coating that is more environmentally friendly, with similar properties to AR-7. No coatings were identified that perform the same as AR-7 in all areas. Candidate coatings failed in comparison to AR-7 in salt fog, beachside atmospheric exposure, pencil hardness, Mandrel bend, chemical compatibility, adhesion, and ease of application tests. However, two coatings were selected for further evaluation.

Whitten, Mary↗

NASA and ESA Collaboration on Alternative to Nitric Acid Passivation: Parameter Optimization of Citric Acid Passivation for Stainless Steel Alloys

National Aeronautics and Space Administration (NASA) Headquarters chartered the Technology Evaluation for Environmental Risk Mitigation Principal Center (TEERM) to coordinate agency activities affecting pollution prevention issues identified during system and component acquisition and sustainment processes. The primary objectives of NASA TEERM are to: Reduce or eliminate the use of hazardous materials or hazardous processes at manufacturing, remanufacturing, and sustainment locations. Avoid duplication of effort in actions required to reduce or eliminate hazardous materials through joint center cooperation and technology sharing. Corrosion is an extensive problem that affects the National Aeronautics and Space Administration (NASA) and the European Space Agency (ESA). The damaging effects of corrosion result in steep costs, asset downtime affecting mission readiness, and safety risks to personnel. Consequently, it is vital to reduce corrosion costs and risks in a sustainable manner. NASA and ESA have numerous structures and equipment that are fabricated from stainless steel. The standard practice for protection of stainless steel is a process called passivation. Passivation is defined by The American Heritage Dictionary of the English Language as to treat or coat (a metal) in order to reduce the chemical reactivity of its surface. Passivation works by forming a shielding outer (metal oxide) layer that reduces the impact of destructive environmental factors such as air or water. Consequently, this process necessitates a final product that is very clean and free of iron and other contaminants. Typical passivation procedures call for the use of nitric acid; however, there are a number of environmental, worker safety, and operational issues associated with its use. Citric acid is an alternative to nitric acid for the passivation of stainless steels. Citric acid offers a variety of benefits including increased safety for personnel, reduced environmental impact, and reduced operational cost. The primary objective of this effort is to qualify citric acid as an environmentally-preferable alternative to nitric acid for the passivation of stainless steel alloys. While citric acid use has become more prominent in industry, there is little evidence that citric acid is a technically sound passivation agent, especially for the unique and critical applications encountered by NASA and ESA.

citric acid passivation↗

Slag Penetration into Refractory Lining of Slagging Coal Gasifier

The impurities in coal are converted into molten slag typically containing SiO2, FeO, CaO, and Al2O3 when coal feedstock is burned in slagging gasifiers. The slag flows down the gasifier sidewalls, dissolves, and penetrates and reacts with the refractory lining that protects the stainless steel shell of the gasifier from elevated temperatures (1300–1600°C). Refractories composed primarily of Cr2O3 have been found most resistant to slag corrosion, but they continue to fail performance requirements because of low resistance to spalling. Post-mortem analysis of high-chromia refractory bricks collected from commercial gasifiers suggests that the spalling is affected by the depth of slag penetration that is in turn affected by the wettability and interconnected porosity of the refractory as well as the slag viscosity. Laboratory tests were conducted to measure the viscosity of slags (Wyoming Powder River Basin [PRB], Pocahontas #3, and Pittsburgh #8), their contact angle on refractories (chromia-alumina [Aurex 75SR] and high-chromia [Serv 95 and Aurex 95P]), and the apparent porosity of selected refractories. In addition, the depth of slag penetration as a function of time and temperature was determined for various refractory-slag combinations. The results of laboratory tests were used to develop a refractory material that has high resistance to penetration by molten slag and thus has a potential to have a substantially longer service life than the materials currently being used.

01 COAL, LIGNITE, AND PEAT↗

Process Control Approach to Implement High Waste Loading Glass Formulations for Hanford Low Activity Waste Vitrification - 18435

Acceptable glass formulations for vitrification of Hanford low activity waste (LAW) at The Hanford Tank Waste Treatment and Immobilization Plant (WTP) must meet a variety of product quality, processability, and waste loading requirements. The glass formulation development work underpinning the WTP baseline LAW glasses was captured in a vitrification process control approach developed by the Vitreous State Laboratory (VSL) and Atkins Energy Federal EPC, Inc. that permits the calculation of the glass formulation required for each particular batch of LAW delivered to the LAW vitrification facility. Since that time, we have developed a wide range of glass formulations that achieve considerably higher waste loadings and which therefore are more economically attractive in terms of reduced amounts of glass produced and decreased time for treatment. That work was done in support of the Department of Energy's Office of River Protection program that is examining options to optimize the LAW facility and LAW glass waste form. Implementation of these high waste loading formulations at the WTP requires the development of a new LAW vitrification process control algorithm, which is the subject of this paper. Waste loadings in LAW glasses are typically limited by either the alkali loading for LAW with low sulfate content or the SO{sub 3} loading for LAW with high sulfate content. In the former case, waste loadings are limited by refractory corrosion and glass corrosion on the vapor hydration test (VHT) and product consistency test (PCT), all of which tend to increase with higher alkali concentrations. In the latter case, waste loadings are limited by the formation of a molten sulfate phase in the melter, which has deleterious effects. The LAW vitrification process control strategy must mitigate these effects while optimizing waste loadings. Given the composition of any LAW stream, the new LAW vitrification process control algorithm permits the calculation of a suitable high waste loading glass composition and the required glass forming additives such that all processing, waste loading, and product quality requirements are met. This algorithm was developed from data for a large number of glasses that were formulated, and characterized with respect to a variety of properties affecting processability and product quality; many of these formulations were also subjected to melter testing to verify acceptable processing characteristics, processing rates, and the absence of secondary sulfate phase formation. This paper describes the development of the present algorithm, comparisons to the present lower waste loading baseline WTP process control approach, and plans for further development and testing. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Hydrothermal Corrosion of First-Generation Dual-Purpose Coatings on Silicon Carbide for Accident-Tolerant Fuel Cladding

In this study, four different commercial coatings, TiN, Cr, CrN, and Cr/CrN (multilayer) were deposited by physical vapor deposition (PVD) on high resistivity chemical vapor deposited (CVD) SiC for the dual purpose of corrosion mitigation and fission gas hermeticity. The coatings were exposed for up to 2600 hours in flowing high temperature (288-350°C), high purity, liquid water with dissolved hydrogen (0.15-3ppm) or dissolved oxygen (1-2ppm). The Cr/CrN coatings did not adhere well and spalled quickly during exposure. In oxygenated conditions, none of the coatings were protective . CrN coatings spalled preferentially at defect sites, but reacted slowly enough in the absence of defects to potentially be chemically protective. TiN coatings fully oxidized within a few hundred hours and spalled. In hydrogen, all the coatings were chemically stable. Coating failures were identified and attributed to localized spallation, potentially related to coating defects. Coating improvements are recommended to reduce spallation and improve coating protection for future generations of dual-purpose coatings.

36 MATERIALS SCIENCE↗