Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CHROMIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,027 records · Page 57

Optimization of Process Parameters for the Axial Distortion and Distortion Range During Die Quenching of a Spiral Bevel Gear

The strength of high-duty gears can be improved by carburizing and quenching processes. Quenching distortion is inevitable during the process, and it has direct effects on the precision of the gear. For spiral bevel gear with big diameter and small thickness, die quenching process is applied in the manufacturing to control the distortion in axial direction. Die quenching parameters must be optimized to minimize the distortion while considering non-uniformity of chemical compositions and loads. In this paper, material models of gear material (22CrMoH) built based on the phase transformation kinetics, static mechanical properties and phase transformation plasticity equations. Finite element analysis (FEA) models are conducted to study the whole die quenching process based on the production process. Die quenching experiments and testing of microstructures and distortions are conducted to verify the accuracy of the FEA models. The effects of loads and bottom die obliquity on the final distortion are studied to set the appropriate range and control distortion. The distortion was very sensitive to the bottom die obliquity and some part of load ranges. The distortion changes little when the load of inner die was in the range of 1.38-2.07 MPa and the load of outer die was in the range of 2.07-2.76 MPa. The distortion range is fitted the production requirements by setting the inclination angle of bottom die between 0.12° and 0.29°.

36 MATERIALS SCIENCE↗

Corrosion Response of Ni-19Cr-5Fe in Molten NaCl-MgCl 2 Salt

Ni-based alloys are strong candidates for use in high-temperature molten salt reactors due to their superior corrosion resistance and mechanical stability compared to stainless steels. In this study, the static corrosion behavior of a Ni-19Cr-5Fe model alloy was systematically evaluated in a purified molten NaCl-MgCl 2 salt at 700°C for 30, 240, and 500 h. Post-exposure analyses were conducted to assess microstructural evolution, corrosion depth, and elemental depletion profiles. Corrosion rates, quantified by chromium depletion depth, followed an inverse power-law trend with increasing exposure time, indicating diffusion-limited kinetics. This trend is attributed to limitations in mass transport in the static salt and to the progressive local depletion of reactive chromium species. Coupled electron backscatter diffraction and energy dispersive X-ray spectroscopy analysis further revealed that the grain boundary character significantly influences corrosion susceptibility: high-angle grain boundaries exhibited pronounced Cr depletion and pitting, while low-angle and Σ3 boundaries remained comparatively resistant. These results offer valuable insight into the role of microstructure in corrosion processes and reinforce the importance of time-dependent material evaluation in molten salt environments relevant to advanced reactor designs.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Application of Nuclear Technology to Art Identification Problems: First Annual Report

Throughout the centuries, as man has become increasingly affluent, his interest in antiquities and objects of art, and the price he has been willing to pay for them, has increased. Inevitably, one result has been to attract the unscrupulous to the production and sale of counterfeit paintings, sculptures, and other works of art. The skill of forgers varies but often is highly sophisticated. However, dealers, museum curators, and other experts have also become more skillful in the detection of forgeries. Scientific tools of increasing sensitivity and sophistication have gradually been applied to the examination of the materials of art and archaeology. Such tools frequently support and render more reliable the judgment of the experts. The quality of forgeries may improve further as their makers become acquainted with the new methods of detection and in turn learn to circumvent or confound the methods. Therefore, the development of still more advanced methods of examination has great utility in the art world. This is particularly true if the ultimate effect is to make circumvention of the methods of examination so costly that the economic incentives for producing forgeries may be substantially reduced, if not eliminated.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding the roles of the strategic element cobalt in nickel base superalloys

The United States imports over 90% of its cobalt, chromium, columbium, and tantalum, all key elements in high temperature nickel base superalloys for aircraft gas turbine disks and airfoils. Research progress in understanding the roles of cobalt and some possible substitutes effects on microstructure, mechanical properties, and environmental resistance of turbine alloys is discussed.

Stephens, J. R.↗

High-temperature steam oxidation study of irradiated FeCrAl defueled specimens

Post irradiation examinations (PIE) were performed on irradiated iron-chromium-aluminum (FeCrAl) specimens. These FeCrAl specimens were fabricated at the US Department of Energy's Oak Ridge National Laboratory (ORNL). The experimental setup involved subjecting FeCrAl cladding, along with UO 2 pellets, to irradiation in the Idaho National Laboratory Advanced Test Reactor (ATR). In parallel, the FeCrAl alloy tubing without UO 2 pellets was irradiated at ORNL's High Flux Isotope Reactor (HFIR). After irradiation, the ATR-irradiated rodlet was transported to an ORNL hot cell, where it was sectioned into multiple samples for the PIE and severe-accident testing. The sectioning process revealed that the fuel was not bonded to the cladding and could be easily detached from sectioned cladding slices. Microstructural analysis of the fuel cross sections demonstrated no significant interaction between the fuel and the cladding. Additionally, high-temperature steam oxidation tests on defueled cladding segments showed minimal oxygen uptake even at 1200 °C. Here, the ATR-irradiated specimens began to exhibit signs of enhanced oxidation upon reaching a temperature of 1300 °C. Furthermore, enhanced oxidation was observed on the inner surface of the ATR-irradiated FeCrAl specimen, which had been subjected to 1300 °C for a duration of 1 min. By contrast, high-temperature steam oxidation experiments indicated that the HFIR-irradiated FeCrAl cladding provided good thermal stability when exposed to 1300 °C for up to 4 h. Comparative analysis encompassing the oxidation behavior of the ATR-irradiated fueled FeCrAl, HFIR-irradiated unfueled FeCrAl, and unirradiated FeCrAl suggests that the fuel–cladding interaction, although not visible via standard microscale electron microscopy measurements, may accelerate the deterioration of FeCrAl cladding in beyond-design-basis accident scenarios.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal Simulation Analysis of Microstructure and Hardness for CrMoV with PWHT in Type IV Region

Welded components of CrMoV steam pipe exhibit a pernicious form of type IV cracking after long-term service at elevated temperature. To investigate the cracking mechanism, the type IV microstructure and hardness were characterized after thermal simulation of post-weld heat treatment. Below 1098 K (825 °C), loss of carbon from the pearlite region was apparent, and the work zone exhibited a slightly lower hardness than the parent material because of a minor amount of austenite transformation. In addition, for peak temperatures above 1133 K (860 °C), additional transformation into austenite occurred and was followed by retransformation into ferrite upon further increasing the temperature. The pearlite formed at 1173 K to 1223 K (900 °C to 950 °C) resulted in an increase of the volume fraction of pearlite and microstructural refinement, which yielded a remarkable increase of hardness in the work zone. For the peak temperature of 1573 K (1300 °C), previous austenite grains were coarsened and alloy carbides were dissolved in the austenite, which significantly hardened the work zone.

36 MATERIALS SCIENCE↗

Influence of temperature and the role of chromium on the kinetics of sulfidation of 310 stainless steel

The sulfidation of 310 stainless steel was studied over the temperature range from 910 K to 1285 K. By adjusting the ratio of hydrogen sulfide, variations in sulfur potential were obtained. The effect of temperature on sulfidation was determined at three different sulfur potentials: 39/sqNm, 0.014/sqNm, and 0.00015/sqNm. All sulfide scales contained one or two surface layers in addition to a subscale. The second outer layer (OL-II), furthest from the alloy, contained primarily Fe-Ni-S. The first outer layer (OL-I), nearest the subscale, contained FE-Cr-S. The subscale consisted of sulfide inclusions in the metal matrix. At a given temperature and sulfur potential, the weight gain data obeyed the parabolic rate law after an initial transient period. The parabolic rate constants obtained at the sulfur potential of 39/sqNm did not show a break when the logarithm of the rate constant was plotted as a function of the inverse of absolute temperature. Sulfidation carried out at sulfur potentials below 0.02/sqNm, however, did show a break at 1145 K, which is termed as the transition temperature. This break was found to be associated with the changes which had occurred in the Fe:Cr ratio of OL-I. Below the transition temperature the activation energy was found to be approximately 125 kj/mole. Above the transition temperature the rate of sulfidation decreased with temperature but dependent on the Fe:Cr ratio in the iron-chromium-sulfide layers of the OL-I. A reaction mechanism consistent with the experimental results has been proposed.

Rao, D. B.↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Microstructural characterization during the hot deformation of 1.17C-11.3Cr-1.48V-2.24W-1.35Mo ledeburitic tool steel

The hot-deformation behavior of 1.17C-11.3Cr-1.48V-2.24W-1.35Mo tool steel was studied. Hot-compression tests were carried out in the temperature range of 850-1200 {sup o}C, at strain rates in the range of 0.001-6 s{sup -1}, and field-emission scanning electron microscope and optical microscopy were used for the microstructural characterization, which revealed a very complex precipitation of carbides that depends on the soaking temperature, the soaking time, the stress state, the deformation temperature as well as on the strain rate. A procedure for determining an appropriate soaking temperature, which enables an extension of the safe hot-working range, was developed. The soaking temperature and the time are the key factors controlling the hot workability. A study of the dissolution of ledeburitic carbides showed that there is a limit fraction to which the carbides could be dissolved prior to hot working without any negative influence on the hot workability. A revision of the general opinion about the influence of non-dissolved carbides on the hot workability is given. - Research Highlights: {yields} Procedure for determining of optimal soaking temperature is given. {yields} Apparent activation energies for three temperature and strain rate ranges are given. {yields} And Q at lower T and are increased due to higher amount of secondary carbides. {yields} Optimal fraction of dissolved carbides prior deformation increases hot workability.

36 MATERIALS SCIENCE↗

Reduction of chromium in Ni-base superalloys through element substitution and rapid solidification processing

The reduction in the use of Cr in Ni base superalloys by the combined approaches of both elemental substitution and rapid solidification processing is studied. The elements Si, Zr, Y and Hf were chosen as potential partial substitutes for Cr in Waspaloy and IN 713LC sine their separate addition to other alloys has previously resulted in enhanced oxidation resistance. The roles of Cr and these replacement elements in determining the microstructure and properties are evaluated. The elements Si, Zr, and Y and Hf are used as partial replacements for Cr in the base superalloys and these resultant alloys are processed using rapid solidification techniques. The mechanical properties and oxidation resistance of the processed materials are evaluated. The microstructure is characterized using state of the art techniques (e.g. analytical transmission electron microscopy), and the mechanism by which these structures are produced is determined.

Fraser, H. D.↗

Corrosion resistance investigation of vanadium alloys in liquid lithium

A major concern in using vanadium alloys for first wall/blanket systems in fusion reactors is their activity with regard to nonmetallic impurities in the coolants. This paper presents the results of studying the corrosion resistance in high-purity liquid lithium (with the nitrogen and carbon content of less than 10{sup –3} wt %) of vanadium and vanadium alloys (V–1.86Ga, V–3.4Ga–0.62Si, V–4.81Ti–4.82Cr) both in the initial state and preliminarily irradiated with Ar+ ions with energy of 20 keV to a dose of 10{sup 22} m{sup –2} at an irradiation temperature of ~400°C. The degree of corrosion was estimated by measuring the changes in the weight and microhardness. Corrosion tests were carried out under static isothermal conditions at a temperature of 600°C for 400 h. The identity of corrosion mechanisms of materials both irradiated with Ar ions and not irradiated, which consisted in an insignificant penetration of nitrogen into the materials and a substantial escape of oxygen from the materials, causing the formation of a zone with a reduced microhardness near the surface, was established. The influence of the corrosive action of lithium on the surface morphology of the materials under study was found, resulting in the manifestation of grain boundaries and slip lines on the sample surface, the latter being most clearly observed in the case of preliminary irradiation with Ar ions.

36 MATERIALS SCIENCE↗

Transmission electron microscopy examinations of metal-oxide interface of zirconium-based alloys irradiated in Halden reactor-IFA-638 - 2016-0039

This paper provides the results of investigations by transmission electron microscopy (TEM) on the selected materials from in-reactor oxidation tests in the Halden test reactor (Reference No. IFA-638) from 1998 to 2006. The objective of the IFA-638 test was to study the corrosion behavior of modern zirconium-based claddings to high burnup in pressurized water reactor water chemistry and thermal hydraulic conditions. The aim of this paper is to report on the microstructure of selected materials (ZIRLO{sup R}, E635, and Alloy A) after the irradiation to different burnup levels to determine the modifications induced by irradiation and to correlate results to their oxidation behavior. The TEM examinations revealed the nature of secondary phase particles (SPPs) and their modification under irradiation. Four types of SPPs were observed, namely β-niobium precipitates, Zr{sub 0.5}Nb{sub 0.3}Fe{sub 0.2} (mainly in the ZIRLO alloy), Zr(Fe,Nb){sub 2} (in E635), and (Cr,Fe){sub 2}Zr,Nb with varying niobium content (present in Alloy A: Zr-0.58Sn-0.31Nb-0.36Fe-0.26Cr). TEM observations showed that all three materials contained still several precipitates after irradiation and in the case of the ZIRLO alloy even after high burnups. Furthermore, the analysis of the metal side of the interface and its comparison with the oxide side led to the conclusion that all types of precipitates dissolved to some extent under irradiation and that their alloying element content decreased. The dissolution was intensified in the oxide. However, a more detailed examination showed that the β-niobium precipitates dissolved at a slower rate, or knowing that their composition was much richer in niobium, the time needed for the precipitates to become fully depleted from niobium was longer. Regarding the amorphization under irradiation, the b-niobium- and chromium-containing precipitates did not amorphize in the metal part of the interface. This was not the case for the other types of precipitates. Furthermore, these two types of SPP both showed delayed oxidation and due to this behavior the typical crack above the SPP in the oxide was also observed. These results are discussed to gain an improved understanding of the oxidation behavior of materials studied as a function of irradiation and residence time. (authors)

36 MATERIALS SCIENCE↗

Corrosion of oxide dispersion strengthened iron–chromium steels and tantalum in fluoride salt coolant: An in situ compatibility study for fusion and fusion–fission hybrid reactor concepts

Primary candidate classes of materials for future nuclear power plants, whether they be fission, fusion or hybrids, include oxide dispersion strengthened (ODS) ferritic steels which rely on a dispersion of nano-oxide particles in the matrix for both mechanical strength and swelling resistance, or tantalum alloys which have an inherent neutron-induced swelling resistance and high temperature strength. For high temperature operation, eutectic molten lithium containing fluoride salts are attractive because of their breeding capability as well as their relatively high thermal capacity, which allow for a higher average operating temperature that increases power production. In this paper we test the compatibility of Flinak (LiF–NaF–KF) salts on ODS steels, comparing the performance of current generation ODS steels developed at Kyoto University with the commercial alloy MA956. Additionally, pure tantalum was also tested for comparative purposes. In situ data was obtained for temperatures ranging from 600 to 900 °C using a custom-built high temperature electrochemical impedance spectroscopy cell. Results for ODS steels show that steel/coolant interfacial resistance increases from 600 to 800 °C due to an aluminum enriched layer forming at the surface, however an increase in temperature to 900 °C causes this layer to break up and aggressive attack to occur. Performance of current generation ODS steels surpassed that of the MA956 ODS steel, with an in situ impedance behavior similar or better than that of pure tantalum.

36 MATERIALS SCIENCE↗

Improved fracture toughness corrosion-resistant bearing material

A development program was performed to establish whether a corrosion-resistant bearing material, such as a 14Cr steel, could be modified to allow carburization, thereby providing the excellent fracture toughness characteristics feasible with this process. The alloy selected for investigation was AMS 5749. Several modifications were made including the addition of a small amount of nickel for austenite stabilization. While some promising results were achieved, the primary objective of an acceptable combination of case hardness and microstructure was not attained. Because the high chromium content presents a serious problem in achieving a viable carburizing cycle, a number of experimental steels having lower chromium contents (8 to 12%) were produced in laboratory quantities and evaluated. The results were basically the same as those initially obtained with the modified AMS 5749. Corrosion tests were performed on AMS 5749, AISI M50, and 52100 bearing steels as well as some of the lower chromium steels. These tests showed that a reduced chromium level (10 to 12%) provided essentially the same corrosion protection as the 14Cr steels.

Bamberger, E. N.↗

Fireside Corrosion Behaviors of Super304H and HR3C in Coal Ash/Gas Environment with Different SO{sub 2} Contents at 650 °C

The corrosion behaviors of Super304H and HR3C used for USC boiler applications were investigated in simulated coal ash/gas environments with 0.1 and 1.5% of SO{sub 2} at 650 °C for 500 h. The results indicated that the increase in SO{sub 2} accelerated the corrosion rate and the spalling tendency of the corrosion layer in both tested alloys. Fe{sub 2}O{sub 3}, Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} main peaks were revealed by XRD on Super304H, but on HR3C only the Cr{sub 2}O{sub 3} peak showed a high intensity. The SO{sub 2} content did not affect the corrosion product composition of any of the alloys, but accelerated the inner sulfidation and the spallation on Super304H. No obvious internal sulfidation was observed on HR3C in either SO{sub 2} content. Based on the experimental results, the alloy corrosion mechanism and the influence of sulfur content on the corrosion process were discussed.

36 MATERIALS SCIENCE↗

Magnetic and structural properties of nanostructured Fe–20Al–2Cr powder mixtures

Nanostructured Fe–20Al–2Cr (wt.%) powders have been prepared using high energy planetary ball-mill. Changes in structural, morphological and magnetic properties of the powders during mechanical alloying (MA) and during subsequent annealing have been examined by X-ray diffraction, scanning electron microscopy (SEM) and vibrating sample magnetometer (VSM). The observed structural and microstructural changes have been related to several processes occurring during MA. After MA, the material becomes significantly disordered and refines to nanoscale grain sizes (~ 14 nm). The obtained bcc α-Fe(Al,Cr) solid solution shows a ferromagnetic behavior. Upon subsequent annealing at 400 °C, α-Fe{sub 2}O{sub 3} and spinel oxides are formed at the surface of particles, while structural defects disappeared as Fe(Al,Cr) solid solution becomes more ordered and grain growth occurs. The saturation magnetization (Ms) shows lower values after annealing, attributed to the formation of metal oxides with low magnetic moment. - Graphical abstract: Display Omitted - Highlights: • Nanostructured Fe–Al–Cr powders were prepared by MA. • Careful analysis of the XRD patterns by using the Rietveld refinement • The lattice distortion is evidenced by the increase of both the lattice parameter and the static Debye Waller parameter. • Annealing at 400 °C stabilizes the microstructure at the nanometer range and leads to the formation of Fe{sub 3}O{sub 4} and Fe{sub 2}O{sub 3} oxides. • Both the milled and annealed samples are ferromagnetic.

36 MATERIALS SCIENCE↗

Effects of high temperature treatment on microstructure and mechanical properties of laser-clad NiCrBSi/WC coatings on titanium alloy substrate

Laser-clad composite coatings on the Ti6Al4V substrate were heat-treated at 700, 800, and 900 °C for 1 h. The effects of post-heat treatment on the microstructure, microhardness, and fracture toughness of the coatings were investigated by scanning electron microscopy, X-ray diffractometry, energy dispersive spectroscopy, and optical microscopy. The wear resistance of the coatings was evaluated under dry reciprocating sliding friction at room temperature. The coatings mainly comprised some coarse gray blocky (W,Ti)C particles accompanied by the fine white WC particles, a large number of black TiC cellular/dendrites, and the matrix composed of NiTi and Ni{sub 3}Ti; some unknown rich Ni- and Ti-rich particles with sizes ranging from 10 nm to 50 nm were precipitated and uniformly distributed in the Ni{sub 3}Ti phase to form a thin granular layer after heat treatment at 700 °C. The granular layer spread from the edge toward the center of the Ni{sub 3}Ti phase with increasing temperature. A large number of fine equiaxed Cr{sub 23}C{sub 6} particles with 0.2–0.5 μm sizes were observed around the edges of the NiTi supersaturated solid solution when the temperature was further increased to 900 °C. The microhardness and fracture toughness of the coatings were improved with increased temperature due to the dispersion-strengthening effect of the precipitates. Dominant wear mechanisms for all the coatings included abrasive and delamination wear. The post-heat treatment not only reduced wear volume and friction coefficient, but also decreased cracking susceptibility during sliding friction. Comparatively speaking, the heat-treated coating at 900 °C presented the most excellent wear resistance. - Highlights: • TiC + WC reinforced intermetallic compound matrix composite coatings were produced. • The formation mechanism of the reinforcements was analyzed. • Two precipitates were generated at elevated temperature. • Cracking susceptibility and microhardness of the coatings were improved. • Post-heat treatment enhances wear resistance of the coatings.

36 MATERIALS SCIENCE↗