The Effect of Mo Particles Addition in Ag-Cu-Ti Filler Alloy on Ti(C,N)-Based Cermet/45 Steel-Brazed Joints

Reliable brazing of Ti(C,N)-based cermet and 45 steel was successfully achieved by using the Mo-particle-reinforced Ag-Cu-Ti composite filler. The effects of Mo content on the interfacial microstructure and mechanical properties of Ti(C,N)-based cermet/45 steel joints were analyzed. The results showed that the joint microstructure was primarily composed of Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2}, Ag(s,s)+Cu(s.s), CuTi+Mo, Ti-based solid solution, and FeTi+Fe{sub 2}Ti. With the increase in Mo content in filler, the thickness of the Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2} layer adjacent to the Ti(C,N)-based cermet decreases, while more blocky Ti-Cu intermetallic were observed in the brazing seam. The shear strength of the joint could be significantly improved by adding suitable amounts of Mo into the Ag-Cu-Ti filler, and the peak value of 263 MPa was achieved when the alloys were brazed with Ag-Cu-Ti+8wt.%Mo composite filler at 920 °C for 20 min.

36 MATERIALS SCIENCE↗

Enhanced Hot Tensile Ductility of Mg-3Al-1Zn Alloy Thin-Walled Tubes Processed Via a Combined Severe Plastic Deformation

In the current study, combined parallel tubular channel angular pressing (PTCAP) and tube backward extrusion (TBE), as a recently developed severe plastic deformation (SPD) method, were applied at 300 °C on a commercial Mg-3Al-1Zn alloy tubes to achieve an ultrafine grained structure. Then, the microstructure, hardness, tensile properties, and fractography evaluations were done at room temperature on the SPD-processed samples. Also, to study the hot tensile ductility of the SPD-processed samples, tensile testing was performed at an elevated temperature of 400 °C, and then, the fractured surface of the tensile samples was studied. It was observed that a bimodal microstructure, with large gains surrounded by many tiny ones, was created in the sample processed by PTCAP followed by TBE. This microstructure led to reach higher hardness and higher strength at room temperature and also led to reach very high elongation to failure (~ 181%) at 400 °C. Also, the value of elongation to failure for this sample was ~ 14.1% at room temperature. The fractographic SEM images showed the occurrence of predominately ductile fracture in the samples pulled at 400 °C. This was mostly due to the nucleation of microvoids and their subsequent growth and coalescence with each other.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on the Properties of CoCrMo Alloy Manufactured by Selective Laser Melting

To obtain medical implants with better mechanical properties, it is necessary to conduct studies on the heat treatment process of the selective laser melting (SLM) manufacturing parts. The differential scanning calorimetry method was used to study the heat treatment process of the phase transition of SLM CoCrMo alloy parts. The tensile properties were tested with a tensile test machine, the quantity of carbide precipitated after heat treatment was measured by energy-dispersive x-ray spectroscopy, and the tensile fracture morphology of the parts was investigated using SEM. The obtained results were: Mechanical properties in terms of elongation and tensile strength of CoCrMo alloy manufactured by SLM that had been heat-treated at 1200 °C for 2 h followed by cooling with water were not only higher than the national standard but also higher than the experimental results of the same batch of castings. The mechanism of fracture of parts manufactured by SLM without heat treatment was brittle fracture, whereas parts which had been heat-treated at 1200 °C for 2 h combined with water cooling and at 1200 °C for 1 h with furnace cooling suffered ductile fracture. This study provides the basis for defining the applications for which CoCrMo alloys manufactured by SLM are suitable within the field of medical implants.

36 MATERIALS SCIENCE↗

B2 Grain Growth Behavior of a Ti-22Al-25Nb Alloy Fabricated by Hot Pressing Sintering

Grain growth behavior of a powder metallurgy (P/M) Ti-22Al-25Nb alloy was investigated by applying a series of isothermal treatment tests over a wide range of temperatures and holding times. An isothermal treatment scheme was conducted in the B2 phase region (1070-1110 °C) and α{sub 2} + B2 phase region (1010-1050 °C) at holding times of 10, 30 min, 1, 2, and 3 h, respectively. The effects of temperature and holding time on the microstructure evolution and microhardness of the P/M Ti-22Al-25Nb alloy at elevated temperatures were evaluated using optical microscope, scanning electron microscope, x-ray diffraction, and Vickers hardness test techniques. The results revealed that the alloy’s treated microstructure was closely linked to temperature and holding time, respectively. The change law of B2 grain growth with holding time and temperature can be well interpreted by the Beck equation and Hillert equation, respectively. The B2 grain growth exponent n and activation energy Q were acquired based on experimental data in the α{sub 2} + B2 and B2 phase regions. In addition, the grain growth contour map for the P/M Ti-22Al-25Nb alloy was constructed to depict variations in B2 grain size based on holding time and temperature.

36 MATERIALS SCIENCE↗

Inverse Thermal Analysis of Ti-6Al-4V Friction Stir Welds Using Numerical-Analytical Basis Functions with Pseudo-Advection

Inverse thermal analysis of Ti-6Al-4V friction stir welds is presented that demonstrates application of a methodology using numerical-analytical basis functions and temperature-field constraint conditions. This analysis provides parametric representation of friction-stir-weld temperature histories that can be adopted as input data to computational procedures for prediction of solid-state phase transformations and mechanical response. These parameterized temperature histories can be used for inverse thermal analysis of friction stir welds having process conditions similar those considered here. Case studies are presented for inverse thermal analysis of friction stir welds that use three-dimensional constraint conditions on calculated temperature fields, which are associated with experimentally measured transformation boundaries and weld-stir-zone cross sections.

36 MATERIALS SCIENCE↗

Friction and Wear Properties of CrSiCN/SiC Tribopairs in Water Lubrication

CrSiCN coatings (3.4 at.% Si) were prepared on 316L stainless steels using unbalanced magnetron sputtering. According to the analysis results of x-ray diffractometer and x-ray photoelectrons spectroscopy, silicon in CrSiCN coatings mainly presented in the amorphous forms of a-SiN, a-SiCN and a-SiC. The hardness and Young’s modulus of CrSiN coatings were 19.4 ± 0.6 and 306.1 ± 5.9 GPa, respectively. In addition, the ball-on-disk sliding tests of CrSiCN/SiC tribopairs were performed in distilled water at varying velocities (0.1-0.5 m/s) and loads (2-12 N). The friction coefficient of tribopairs presented a decreasing trend with respect to velocity at low applied loads (≤ 4 N). To be specific, the low friction coefficient of 0.05-0.14 accompanied with polished wear scar was obtained at high velocities and low loads. Finally, the wear mechanism map of CrSiCN/SiC tribopairs was proposed based on a combination of friction coefficient, wear scar morphology and wear rates of tribopairs.

36 MATERIALS SCIENCE↗

Electrochemical Behavior Assessment of As-Cast Mg-Y-RE-Zr Alloy in Phosphate Buffer Solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}) Using Electrochemical Impedance Spectroscopy and Mott–Schottky Techniques

In the present study, electrochemical behavior of as-cast Mg-Y-RE-Zr alloy (RE: rare-earth alloying elements) was investigated using electrochemical tests in phosphate buffer solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}). X-ray diffraction techniques and Scanning electron microscopy equipped with energy dispersive x-ray spectroscopy were used to investigate the microstructure and phases of the experimental alloy. Different electrochemical tests such as potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS) and Mott–Schottky (M–S) analysis were carried out in order to study the electrochemical behavior of the experimental alloy in phosphate buffer solutions. The PDP curves and EIS measurements indicated that the passive behavior of the as-cast Mg-Y-RE-Zr alloy in phosphate buffer solutions was weakened by an increase in the pH, which is related to formation of an imperfect and less protective passive layer on the alloy surface. The presence of the insoluble zirconium particles along with high number of intermetallic phases of RE elements mainly Mg{sub 24}Y{sub 5} in the magnesium matrix can deteriorate the corrosion performance of the alloy by disrupting the protective passive layer that is formed at pH values over 11. These insoluble zirconium particles embedded in the matrix can detrimentally influence the passivation. The M–S analysis revealed that the formed passive layers on Mg-Y-RE-Zr alloy behaved as an n-type semiconductor. An increase in donor concentration accompanying solutions of higher alkalinity is thought to result in the formation of a less resistive passive layer.

36 MATERIALS SCIENCE↗

Effect of Ceramic Rolling and Annealing on Mechanical Properties of AlCoCrFeNi{sub 2.1} Eutectic High-Entropy Alloys

It was firstly proved that AlCoCrFeNi{sub 2.1} could optimize the strength-ductility combination by ceramic rolling at room temperature. The technique greatly enhanced the strength of the materials at the price of slight ductility, which is different from the previous studies. When the thickness reduction was 23.06%, the yield strength and compressive strength were 1611.42 and 2212.99 MPa, respectively, with the plastic strain of 28.36%. Such an excellent combination of strength and ductility was attributed to the distribution of the residual stress, the high hydrostatic stress and the shear bands in ceramic rolling process. The plastic strain of the material increased to 38.54%, and the strength reduced to 1900.73 MPa after annealing at 800 °C for 1 h. A lot of like-flower patterns of recrystallized ultrafine grain were observed after annealing at 800 °C due to the sluggish diffusion in HEAs and the effect of ceramic rolling. In addition, after annealing at 800 °C, the fracture mode changed to shearing fracture of microvoid aggregation from cleavage/quasi-cleavage fracture of as-rolled sample due to the deposition of the second phase in the tested sample.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a Ag Micro-Alloyed Mg-5Sn Alloy

Effects of 1.5 wt.% Ag addition and solid solution + artificial ageing at 160 °C on the microstructure and mechanical properties of a Mg-5Sn alloy have been studied. The results show that Ag addition has significantly hardened the solution-treated Mg-5Sn alloy. During the ageing process, the hardness increase rate and the strength and ductility of the Mg-5Sn alloy at each state are also improved by Ag addition. The improved strengthening behavior is primarily attributed to the refinement distribution of the Mg{sub 2}Sn precipitates, the enhanced precipitation process, and the synergistic strengthening effect of Mg{sub 2}Sn and a metastable plate DO{sub 19} phase formed at lower ageing temperature. For each solution-treated alloy, the strength and ductility are higher than the corresponding cast ones. Ageing further enhances the yield strength, and the ductility of the Mg-5Sn-1.5Ag alloy is also increased after ageing. The fracture surfaces of the both peak-aged alloys exhibit the characteristic of a mixture of quasi-cleavage and ductile fracture.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Low-Activation Fe-Cr-V Multicomponent Single-Phase Alloys

A ternary equiatomic and nearly equiatomic alloy composed of the low-activation elements Fe, Cr, and V was designed for potential application as low-activation structural materials for the first wall of fusion reactors. The optimal composition of the multicomponent alloy was determined by minimizing the Gibbs free energy for solid-solution formation. The microstructure, phase stability, and mechanical properties of the equiatomic and optimized Fe-Cr-V alloys were studied. The equiatomic alloy consisted of a body-centered-cubic (BCC) solid-solution phase with a small amount of a face-centered-cubic (FCC) solid-solution phase, whereas the optimized alloy consisted of a single BCC solid-solution phase in the as-cast state. The crystal grains of both alloys were equiaxial. No phase transition was observed in the optimized alloy after homogenization; however, for the equiatomic alloy, the FCC solid-solution phase disappeared and surface relief was observed. The Vickers microhardness and yield strength of the Fe-Cr-V alloys increased after homogenization compared with those of the as-cast alloys.

36 MATERIALS SCIENCE↗

Notch Sensitivity and Failure Behavior of TiAl and K418 Alloys

The notch sensitivity of tensile specimens of TiAl and K418 alloys has been investigated, and the notch strength has been quantitatively analyzed. The fracture surface of the specimens has also been observed and analyzed by scanning electron microscopy (JEOL-6700F). By comparing notch rod tensile specimens and special notch rod tensile specimens, it was found that the basic nature, fracture driving force, and fracture criteria of the brittle TiAl alloy and the ductile K418 alloy are different. The final fracture of the K418 alloy is controlled by strain and not by stress, and the specimens do not exhibit notch sensitivity. However, the final fracture of the TiAl alloy is controlled by stress, and the specimens exhibit small notch sensitivity. For the special notch rod tensile specimens, the K418 specimens do not exhibit notch sensitivity. However, for the TiAl alloy, when the notch depth reaches 10% of the specimen diameter, the tensile strength decreases, and when the notch depth reaches 20% of the specimen diameters, the tensile strength sharply decreases.

36 MATERIALS SCIENCE↗

A New Method for Optimizing Hot Processing Parameters of Mg-6.0Zn-0.5Mn-0.5Er Alloy Based on Kinetic Model of Dynamic Recrystallization and Processing Map

Hot deformation behavior of the cast-homogenized Mg-6.0Zn-0.5Mn-0.5Er alloy was studied using dynamic recrystallization (DRX) kinetic model and processing map. The compressing tests were conducted in the temperature range of 250-450 °C and strain rates of 0.001-1 s{sup −1}. According to the evolution of microstructures, under lower strain rates, the main DRX mechanism of Mg-6.0Zn-0.5Mn-0.5Er alloy is continuous DRX (CDRX); twinning induced DRX (TDRX) and CDRX both become the main DRX mechanism under higher strain rates. The DRX kinetics model of Mg-6.0Zn-0.5Mn-0.5Er alloy is calculated as X{sub DRX}=1−exp[−1.9463(((ε−ε{sub c})/(ε{sup ∗}))){sup 1.4608}], which is corresponding to the microstructure evolutions of DRX under different deformation conditions. The contour map of DRX was proposed based on the calculation results of DRX kinetics model. The processing maps are constructed to predict processing parameters of the alloy, and the predictability was evaluated combining with the contour map of DRX and dynamic materials model (DMM) processing map. It is deduced from the microstructures evolution and processing map that the optimum processing domain is mainly at 380-450 °C and 0.01-0.001 s{sup −1}, and 410-420 °C and 0.01-1 s{sup −1}.

36 MATERIALS SCIENCE↗

Systematic Insight into Chloride Concentration, Applied Potential and Time Effect on the Passive Film of Cu-Zn-Ni Ternary Alloy in Alkaline Solution

The effects of chloride concentration, applied potential and time on the passive film of Cu-Zn-Ni ternary alloy in alkaline solution were systematically investigated using potentiodynamic and potentiostatic polarizations, electrochemical impedance spectroscopy, Mott–Schottky analysis, laser confocal microscopy, atomic force microscopy and x-ray photoelectron spectroscopy. Results showed that the pitting potential decreased as a linear function of log(a{sub Cl{sup −}}), and the size of pits extended faster in the horizontal direction than in the vertical direction. The passive oxide film formed on Cu-Zn-Ni alloy mainly exhibited p-type semiconductor behavior, which was consistent with cuprous and nickel oxide, the main components in the film. The density of cation vacancy (approximately 10{sup 20}-10{sup 21} cm{sup −3}) increased with potentiostatic time but reduced by the increasing potentials. The kinetics of passive film growth followed a parabolic law D = m * t{sup n}, where m is a constant considered as the initial growth rate and n is the time exponent. Subsequent to the formation of a compact and coherent passive film at higher potential, it was hard for an ion to migrate or for an aggressive ion to penetrate, which indicated better corrosion resistance for passive film formed under higher potential.

36 MATERIALS SCIENCE↗

Microstructures and Mechanical Behavior of Ti{sub 3}SiC{sub 2}/Al{sub 2}O{sub 3}-Ni Composites Synthesized by Pulse Discharge Sintering

High-purity Ti{sub 3}SiC{sub 2} and Ti{sub 3}SiC{sub 2}/Al{sub 2}O{sub 3}-Ni composites with different Al{sub 2}O{sub 3}-Ni contents were fabricated using pulse discharge sintering (PDS) of a mechanical alloyed powder mixture. The synthesis process of monolithic Ti{sub 3}SiC{sub 2} was studied through displacement temperature–time (DTT) curve, displacement rate–time and displacement rate–temperature diagrams obtained during the PDS process. It was found that TiC{sub x} and Ti{sub 5}Si{sub 3}C{sub y} are the intermediate phases and the PDS process completed after 20 min at 1350 °C. The results showed that in Ti{sub 3}SiC{sub 2}/Al{sub 2}O{sub 3}-Ni composite, the Ni part of Al{sub 2}O{sub 3}-Ni leads to decomposition of Ti{sub 3}SiC{sub 2} to TiC{sub x}, Ti{sub 5}Si{sub 3}C{sub y} and Ni(Si){sub x}. No evidence was detected in the reaction between Al{sub 2}O{sub 3} and Ti{sub 3}SiC{sub 2}. The density and hardness of the composites are higher than monolithic Ti{sub 3}SiC{sub 2} due to the production of reinforcing phases. The composite showed lower flexural strength and higher compressive strength than monolithic Ti{sub 3}SiC{sub 2}.

36 MATERIALS SCIENCE↗

Optimization of Process Parameters for the Axial Distortion and Distortion Range During Die Quenching of a Spiral Bevel Gear

The strength of high-duty gears can be improved by carburizing and quenching processes. Quenching distortion is inevitable during the process, and it has direct effects on the precision of the gear. For spiral bevel gear with big diameter and small thickness, die quenching process is applied in the manufacturing to control the distortion in axial direction. Die quenching parameters must be optimized to minimize the distortion while considering non-uniformity of chemical compositions and loads. In this paper, material models of gear material (22CrMoH) built based on the phase transformation kinetics, static mechanical properties and phase transformation plasticity equations. Finite element analysis (FEA) models are conducted to study the whole die quenching process based on the production process. Die quenching experiments and testing of microstructures and distortions are conducted to verify the accuracy of the FEA models. The effects of loads and bottom die obliquity on the final distortion are studied to set the appropriate range and control distortion. The distortion was very sensitive to the bottom die obliquity and some part of load ranges. The distortion changes little when the load of inner die was in the range of 1.38-2.07 MPa and the load of outer die was in the range of 2.07-2.76 MPa. The distortion range is fitted the production requirements by setting the inclination angle of bottom die between 0.12° and 0.29°.

36 MATERIALS SCIENCE↗

Control of Carbon Content in Ultrafine Cemented Carbide by Heat Treatment in Reducing Atmospheres Containing Carbon Oxides

In this work, the method of control of carbon content in the ultrafine-grained cemented carbide alloy was proposed. The treating of the WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} compacts was made in a CO + CO{sub 2} gas mixture at CO concentrations from 0 to 80 vol.% during 50 min at the initial stage of the conventional sintering at a temperature of 700 °C. Conditions for increasing and decreasing the carbon content are CO concentrations of CO in gas mix more than 65 vol.% and less than 35 vol.%, respectively. It is shown that even a small deviation from the stoichiometric carbon content (0.3 wt.%) leads to an increase in porosity and a multiple decrease in the strength of the ultrafine-grained cemented carbide. A comparative analysis with literature data showed that the obtained ultrafine-grained solid alloy WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} with stoichiometric composition is not inferior in hardness and toughness to the analogs obtained by hot pressing and electrospark sintering.

36 MATERIALS SCIENCE↗

Sliding Wear Behavior of Spark-Plasma-Sintered Fe-Based Amorphous Alloy Coatings on Cu-Ni Alloy

This paper reports on the processing of Fe{sub 48}Cr{sub 15}Mo{sub 14}Y{sub 2}C{sub 15}B{sub 6} amorphous alloy coatings on Cu-10%Ni (wt.%) alloy using spark plasma sintering. The amorphous alloy coatings were sintered at temperatures ranging from 575 to 675 °C at a pressure of 50 MPa. The development of microstructure, phases, and wear properties with sintering temperature of the coatings is investigated. The sintered coatings were found to be near fully dense with hardness close to that of the sintered bulk amorphous alloy. X-ray analysis indicated increasing degree of devitrification of the amorphous coatings with increasing sintering temperature. The wear behavior of the coatings is significantly influenced by the sintering temperature with volume wear rate first decreasing in the temperature range of 575-650 °C and then increasing above 650 °C. The variation in wear behavior is explained based on relative stability of the protective surface layer and embrittlement of the surface with the sintering temperature.