Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,009 records · Page 56

Design and thermomechanical properties of a γ' precipitate-strengthened Ni-based superalloy with high entropy γ matrix

A novel Ni-based superalloy was designed with γ' precipitate strengthening, controlled γ/γ' lattice misfit and high configurational entropy of the γ matrix for improved high temperature performance up to 800 degrees C. The alloy contains nano-sized γ' precipitates, MC and other grain boundary carbides. Three variants of the alloy were fabricated using vacuum induction melting, a computational-based homogenization cycle for reducing solidification segregation, and thermomechanical processing steps of forging followed by hot rolling to produce plates from which ASTM standard test specimens were extracted. Tensile testing at room temperature and elevated temperatures up to 800 degrees C revealed superior yield stress when compared to Nimonic 105 with good tensile strength values. Furthermore, the three alloys are machinable with maximum stresses comparable to standard practices as determined using deformation mechanisms maps obtained from Gleeble testing and EBSD analysis. Due to the composition of the experimental alloys falling outside the typical range used to populate thermodynamic databases, differences in phase predictions and related temperatures were observed between the experiment and Thermo-Calc predictions. Here, the γ' forming elements Ti and Nb had a similar effect on the γ' precipitates and indirectly contributed to changing the entropy of the γ matrix. Based on the results of this study, these alloys have the potential for use at 800 degrees C in energy structural applications. Definitions related to this novel class of alloys are discussed.

36 MATERIALS SCIENCE↗

Additively-manufactured Al-0.3Zr-0.2Ce-0.2Cu alloy with high creep resistance and electrical conductivity

Here, a new, solute-lean Al-0.3Zr-0.2Ce-0.2Cu (wt.%) alloy is developed for additive manufacturing that overcomes the classical tradeoff between conductivity and creep resistance. The rapid-cooling-enabled supersaturation of Zr, and its uniform distribution in α-Al matrix, along with formation of submicron (Ce,Cu)-rich intermetallic particles on solidification lead to unusually high creep resistance at 200 °C. Near-zero secondary creep rates are achieved up to the alloy yield stress (YS) of 65 MPa at 200 °C in as-fabricated state. The Zr-solute-induced dislocation-climb suppression mechanism underlying this improvement also restricts dynamic recovery above YS, as noted from appreciable primary creep and its transitioning to near-zero secondary creep rates. A combination of relatively coarse, epitaxially-grown α-Al grains, low Zr concentration in α-Al, and the impurity-scavenging effect of Ce to purify α-Al matrix produces high electrical conductivity of ∼48 %IACS. Aging precipitation of L1 2 -Al 3 Zr nanoprecipitates doubles the YS (to ∼150 MPa) at room temperature and increases alloy conductivity to ∼58 %IACS, but loss of solid-solution Zr out of α-Al matrix leads to activation of dislocation climb, degrading the creep properties as compared to the supersaturated Al-Zr solid solution in the as-fabricated state. Compared to L1 2 -Al 3 Zr nanoprecipitates, submicron (Ce,Cu)-rich particles formed on solidification are more effective at impeding dislocation climb, producing a threshold stress for dislocation creep of ∼ 50 MPa at 200 °C. The new alloy design concepts, especially solute-induced dislocation-climb suppression for creep resistance, explored here may pave way for the design of new metallic alloys for thermal/electrical conductors and other high-temperature applications.

Additive Manufacturing↗

Computer-assisted Rheo-forging Processing of A356 Aluminum Alloys

Die casting process has been used widely for complex automotive products such as the knuckle, arm and etc. Generally, a part fabricated by casting has limited strength due to manufacturing defects by origin such as the dendrite structure and segregation. As an attempt to offer a solution to these problems, forging has been used as an alternative process. However, the forging process provides limited formability for complex shape products. Rheo-forging of metal offers not only superior mechanical strength but also requires significantly lower machine loads than solid forming processes. In order to produce semi-solid materials of the desired microstructure, a stirring process is applied during solidification of A356 aluminum molten state. This paper presents the results of an A356 aluminum alloy sample, which were obtained by experiment and by simulation using DEFORM 3D V6.1. Samples of metal parts were subsequently fabricated by using hydraulic press machinery. In order to compare the influence of loading method, two types of samples were fabricated: (1) samples fabricated under direct loading die sets (2) those fabricated under indirect loading die sets. The formability and defects, which were predicted by FEM simulation, were similar to those of samples used in practice.

36 MATERIALS SCIENCE↗

Analysis of Brazing Effect on Hot Corrosion Behavior of a Nickel-Based Aerospace Superalloy

The effects of brazing and use of composite powder mixture as interlayer material on hot corrosion resistance of brazed IN738 superalloy were studied. Brazing was observed to result in significant reduction in the hot corrosion resistance of the superalloy. However, application of composite powder mixture, which consists of additive superalloy powder, enhanced the hot corrosion resistance of brazed samples. It is also found that although the use of composite powder mixture increased hot corrosion resistance of brazed alloy, if the additive powder completely melts, which is possible during brazing, it can significantly reduce the hot corrosion resistance of the brazed joint. Elemental micro-segregation during solidification of the joint with completely melted powder mixture produces chromium-depleted zones and consequently reduces hot corrosion resistance, since a uniform distribution and adequate chromium concentration are necessary to combat hot corrosion. This has not been previously reported in the literature and it is crucial to the use of composite powder mixture for enhancing the properties of brazed superalloys.

36 MATERIALS SCIENCE↗

Development of powder metallurgy 2XXX series Al alloys for high temperature aircraft structural applications

The objective of the present investigation was to improve the strength and fracture toughness combination of P/M 2124 Al alloys in accordance with NASA program goals for damage tolerance and fatigue resistance. Two (2) P/M compositions based on Al-3.70 Cu-1.85 Mg-0.20 Mn with 0.12 and 0.60 wt. pct. Zr were selected for investigation. The rapid solidification rates produced by atomization were observed to prohibit the precipitation of coarse, primary Al3Zr in both alloys. A major portion of the Zr precipitated as finely distributed, coherent Al3Zr phases during vacuum preheating and solution heat treatment. The proper balance between Cu and Mg contents eliminated undissolved, soluble constituents such as Al2CuMg and Al2Cu during atomization. The resultant extruded microstructures produced a unique combination of strength and fracture toughness. An increase in the volume fraction of coherent Al3Zr, unlike incoherent Al20Cu2Mn3 dispersoids, strengthened the P/M Al base alloy either directly by dislocation-precipitate interactions, indirectly by a retardation of recrystallization, or a combination of both mechanisms. Furthermore, coherent Al3Zr does not appear to degrade toughness to the extent that incoherent Al20Cu2Mn3 does. Consequently, the addition of 0.60 wt. pct. Zr to the base alloy, incorporated with a 774K (935 F) solution heat treatment temperature, produces an alloy which exceeds all tensile property and fracture toughness goals for damage tolerant and fatigue resistant applications in the naturally aged condition.

Chellman, D. J.↗

Real-Time X-Ray Transmission Microscopy for Fundamental Studies Solidification

High resolution real-time X-ray Transmission Microscopy, XTM, has been applied to obtain information fundamental to solidification of optically opaque metallic systems. We have previously reported the measurement of solute profile in the liquid, phase growth, and detailed solid-liquid interfacial morphology of aluminum based alloys with exposure times less than 2 seconds. Recent advances in XTM furnace design have provided an increase in real-time magnification (during solidification) for the XTM from 4OX to 16OX. The increased magnification has enabled for the first time the XTM imaging of real-time growth of fibers and particles with diameters of 5 micrometers. We have applied this system to study of the kinetics of formation and morphological evolution of secondary fibers and particles in Al-Bi monotectic alloys to observe a previously unreported velocity dependent thermo-capillary depletion mechanism for Bi rich liquid which can penetrate many fiber diameters into the solid-liquid interface. In this talk we will discuss application of the XTM to the study the fundamentals of monotectic and eutectic solidification, the enhancement of XTM data with precise solid liquid interfacial temperature and thermal gradient measurement techniques, and the application of this technology to the study of the fundamentals of solidification in microgravity,

Curreri, Peter A.↗

Convection and morphological stability during directional solidification

For growth of a vicinal face at constant velocity, the effect of anisotropic interface kinetics on morphological stability is calculated for a binary alloy. The dependence of the interface kinetic coefficient on crystallographic orientation is based on the motion and density of steps. Anisotropic kinetics give rise to traveling waves along the crystal-melt interface, and can lead to a significant enhancement of morphological stability. The stability enhancement increases as the orientation approaches a singular orientation and as the solidification velocity increases. Shear flows interact with the traveling waves and, depending on the direction of the flow, may either stabilize or destabilize the interface. Specific calculations are carried out for germanium-silicon alloys.

Coriell, Sam R.↗

Experimental Investigations on Solidification of 500-kg Steel Ingots with Laboratory Trials

The present work focuses on the solidification process of large steel ingots. Several complex solidification phenomena in large ingots were investigated by means of experimental hot modeling and cold modeling. In hot modeling, a 500 kg ingot solidified slowly in a specially insulated mold and this slow solidification process simulates the solidification of industrial scale ingots with a weight between 3 and 6 t. Temperature was measured by thermocouples during solidification and curves were plotted, and as-cast structure and macrosegregation of alloying elements were quantified. The A segregates were produced in the laboratory hot trials and quantitatively investigated. Meanwhile, water modeling (cold modeling) using NH{sub 4}Cl solution was conducted with different cooling/heating conditions. Macroscopic crystal growth phenomena, such as dendritic growth, sedimentation of crystals, and convective fluid flow, were directly observed and analyzed, and flow channels were also observed and compared with A segregates in the hot modeling.

36 MATERIALS SCIENCE↗

Effect of Melt Convection and Solid Transport on Macrosegregation and Grain Structure in Equiaxed Al-Cu Alloys

Macrosegregation in metal casting can be caused by thermal and solutal melt convection, and the transport of unattached solid crystals. These free grains can be a result of, for example, nucleation in the bulk liquid or dendrite fragmentation. In an effort to develop a comprehensive numerical model for the casting of alloys, an experimental study has been conducted to generate benchmark data with which such a solidification model could be tested. The specific goal of the experiments was to examine equiaxed solidification in situations where sinking of grains is (and is not) expected. The objectives were: 1) experimentally study the effects of solid transport and thermosolutal convection on macrosegregation and grain size distribution patterns; and 2) provide a complete set of controlled thermal boundary conditions, temperature data, segregation data, and grain size data, to validate numerical codes. The alloys used were Al-1 wt. pct. Cu, and Al-10 wt. pct. Cu with various amounts of the grain refiner TiB2 added. Cylindrical samples were either cooled from the top, or the bottom. Several trends in the data stand out. In attempting to model these experiments, concentrating on experiments that show clear trends or differences is recommended.

Rerko, Rodney S.↗

Quantification and prediction of solidification textures under additive manufacturing conditions

Crystallographic textures are a major determinant of the macroscale anisotropic properties of polycrystalline metallic alloys produced in a wide range of additive manufacturing (AM) processes. Here, we introduce a statistical method that can accurately quantify the degree of orientational order of textures despite the large random fluctuations in the orientation of individual grains inherent in AM processes. The method, demonstrated for laser and resolidification of AlSi thin films, extends Z-scoring to a dynamical regime to assess the statistical significance of observed textures compared to randomly generated ones at different stages of solidification. We further show that, combined with phase-field modeling, this method can be used to infer fundamental anisotropic properties of the solid-liquid interface that are essential for texture prediction, and are compared here to the results of atomistic simulations. In addition, phase-field modeling reveals that, even at rapid AM solidification rates, the observed 〈110〉-dominated textures in the AlSi thin films are controlled predominantly by the anisotropy of the interface free-energy and sheds light on the physical mechanism of grain competition. These results significantly enhance both the existing tools for the quantification and prediction of AM crystallographic textures and our basic understanding of their formation.

36 MATERIALS SCIENCE↗

CALPHAD Models to Guide Refractory Alloys Additive Manufacturing: In-Situ Compounds Formation, Nanoparticles, and Impurities Considerations

This technical memorandum (TM) seeks to model and discuss aspects of nanoparticle and micrometer-scale particle or ‘microparticle’ inclusions in refractory metal alloy manufacturing, via a currently used additive manufacturing (AM) method that results in equivalent wt.% addition of dissolved elements in the melt pool composition and subsequent formation of nanometer-scale MC and MO inclusions. Additionally, the authors begin to consider the effects of oxygen (O), a ubiquitous impurity, in AM; and seek to understand a combined optimization of alloying, nano- and micro strengthening and refinement, elemental additions, and even in-situ compounds and alloys species formation. To gain insights, this TM focuses on a pair of refractory alloys currently of interest to NASA: tungsten-rhenium-tantalum carbide (with O impurities) (W-Re-TaC(-O)) and tungsten-rhenium-tantalum-carbon (with O impurities) (W-Re-Ta-C(-O)), which are processed via powder bed fusion (PBF)-SLM.

ICME integrated computational materials engineerin↗

The Addition of Boron to Melt-Spun Fe-6.5%Si Ribbons

Fe-6.5%Si has higher electrical resistivity, lower magnetocrystalline anisotropy, and lower magnetostriction than traditional Fe-3.2%Si silicon steel. The reduced iron losses of Fe-6.5%Si render it a highly favorable candidate for high-speed motors and transformers. However, large-scale production of wide Fe-6.5%Si tape by rapid solidification can be challenging mainly because of its high melting point. In this work, boron is alloyed to Fe-6.5%Si to reduce its melting temperature and interfacial energy to improve the alloy’s processability. Boron additions from 0.01 wt.% to 2.24 wt.% into Fe-6.5%Si and its effect on ribbon thickness, grain size, magnetic, and mechanical properties were studied. Further, minor boron alloying significantly changed the melt pool stability and wetting on the quench wheel and in turn increased the quench rate with minimum impact on the magnetic saturation and ductility. Boron addition of < 0.06 wt.% was also found beneficial to the magnetic property of the alloy by lowering both its hysteresis and eddy current losses.

36 MATERIALS SCIENCE↗

Assessment of Directionally Solidified Eutectic Sm–Fe(Co)–Ti Alloys as Permanent Magnet Materials

Sm–Fe–Ti and Sm–Fe0.8Co0.2–Ti alloys were prepared via arc-melting and directionally solidified on a water-cooled copper hearth. The as-solidified alloys featured cells of the Sm(Fe,Co,Ti)12–Ti(Fe,Co) 2+δ –(α-Fe) lamellar eutectic. The lamellae of Sm(Fe,Co,Ti)12 phase with a crystal structure of the ThMn12 type were less than 0.2 μm thick, and had their [001] easy-magnetization directions oriented along the temperature gradient of the solidification. The eutectic microstructure led to an increased coercivity, especially in the Co-added alloys. Below 250 °C, this coercivity was found not to vary much with temperature with a temperature coefficient of -0.18 %/°C. However, the modest absolute values, reaching only 0.7 kOe, are insufficient for utilization of the directionally solidified alloys as anisotropic permanent magnets.

36 MATERIALS SCIENCE↗

Structural and magnetic properties of ball-milled Ni{sub 11}Co{sub 11}Fe{sub 66}Zr{sub 7}B{sub 4}Cu powders

Thick films of the Ni{sub 11}Co{sub 11}Fe{sub 66}Zr{sub 7}B{sub 4}Cu composition were synthesized via screen printing of the ball-milled ribbons of the above composition for possible use as planar inductors. The ribbons were obtained by rapid solidification. The resulting ribbon samples were annealed at 300 deg. C for 2 h to cause embrittlement. They were found to have soft magnetic properties (4{pi}M{sub s}{approx}13 kG, {delta}H{approx}100 Oe, and H{sub c}<0.5 Oe). The brittle ribbons were ball milled using tungsten carbide vials and stainless steel balls in an inert atmosphere for various milling times. The sample milled for 10 h was found to have a 4{pi}M{sub s} of about 13 kG and a coercivity of about 73 Oe with an average particle size of about 5 {mu}m. The screen printed (as prepared and aligned) samples showed a linewidth ({delta}H) of about 1000 Oe. Similar values were obtained for screen printed films annealed for 1 h at 200 and 400 deg. C.

36 MATERIALS SCIENCE↗

Effect of Mg-Bearing Oxide(+TiN) Inclusion on Microstructure of Fe-16 Mass Pct Cr Ferritic Alloy and Its Evolution During Heating at 1573 K (1300 °C)

Both the effects of Mg-bearing oxide and Mg-bearing oxide +TiN inclusions on the microstructures of Fe-16 mass pct Cr alloy should be clarified. In this paper, the effects of Mg-bearing oxide(+TiN) inclusions on the microstructures of Fe-16 mass pct Cr ferritic alloy and changes due to the inclusions during heating at 1573 K (1300 °C) were studied by manual and automatic SEM-EDS analyses. Three alloys were used as specimens. The inclusions were Al{sub 2}TiO{sub 4} +TiN with a small amount of TiN in alloy #1, Al{sub 2}(Mg, Ti)O{sub 4} in alloy #2 and Al{sub 2}(Mg, Ti)O{sub 4} +TiN in alloy #3. The average grain size was smaller, and the ratio of columnar grains was lower in the as-cast alloy #2 and as-cast alloy #3 than that in the as-cast alloy #1. This is attributed to the heterogeneous nucleation of delta ferrite on Al{sub 2}(Mg, Ti)O{sub 4} during solidification. Refinement of the microstructures of ferritic steel by Mg-bearing oxide + multi-TiN inclusions is proposed. Changes in composition, aspect ratio, and size distribution of inclusions in each alloy during heating were investigated systematically. Mg-bearing oxide(+TiN) was dispersed in both the as-cast alloys and heated alloys, which contributed to microstructural refinement of the heated alloys through the pinning effect.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Additively manufactured Ni-20Cr to V functionally graded material: Computational predictions and experimental verification of phase formations

Throughout this work, a database for the Cr-Ni-V system was constructed by modeling the binary Cr-V and ternary Cr-Ni-V systems using the CALPHAD approach aided by density functional theory (DFT)-based first-principles calculations and ab initio molecular dynamics (AIMD) simulations. To validate this new database, a functionally graded material (FGM) using Ni-20Cr and elemental V was fabricated using directed energy deposition additive manufacturing (DED AM) and experimentally characterized. The deposited Ni-20Cr was pure fcc phase, while increasing the amount of V across the gradient resulted in the formation of sigma phase, followed by the bcc phase. The experimentally measured phase data was compared with computational predictions made using a Cr-Ni-V thermodynamic database from the literature as well as the database developed in the present work. The newly developed database was shown to better predict the experimentally observed phases due to its accurate modeling of binary systems within the database and the ternary liquid phase, which is critical for accurate Scheil calculations.

36 MATERIALS SCIENCE↗

Evolution of the microstructure and hardness of a rapidly solidified/melt-spun AZ91 alloy upon aging at different temperatures

The effect of aging at different temperatures on a rapidly solidified/melt-spun AZ91 alloy has been investigated in depth. The microstructures of as-spun and aged ribbons with a thickness of approximately 60 {mu}m were characterized using X-ray diffraction, transmission electron microscopy and laser optical microscopy; microhardness measurements were also conducted. It was found that the commercial AZ91 alloy undergoes a cellular/dendritic transition during melt-spinning at a speed of 34 m/s. A strengthening effect due to aging was observed: a maximum hardness of 110 HV/0.05 and an age-hardenability of 50% were obtained when the ribbon was aged at 200 deg. C for 20 min. The {beta}-Mg{sub 17}Al{sub 12} phase exhibits net and dispersion types of distribution during precipitation. The dispersion of precipitates in dendritic grains or cells is the main source of strengthening.

36 MATERIALS SCIENCE↗