SEARCH · Engineering Papers
Results for “STEELS, STAINLESS - WELDING”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Through-thickness microstructural evolution during grain boundary engineering type thermomechanical processing and its implication on sensitization behavior in austenitic stainless steel
Highlights: • GBE-treated 304L steel exhibits thickness-dependent microstructural evolution. • Degree of sensitization increases from surface to interior in GBE specimen. • Low fractal dimension and large TRD size lead to lesser sensitization at surface. • As-received specimen shows high albeit thickness-independent sensitization behavior. • Higher residual strain leads to higher sensitization at surface of deformed sample. - Abstract: Through-thickness microstructural variations and their synergistic influence on degree of sensitization in grain boundary engineering (GBE) treated 304L stainless steel was compared with solution-annealed and marginally cold-worked (~ 3% thickness reduction) specimens. The solution-annealed specimen has shown higher degree of sensitization due to the presence of lower fraction of Σ3 (as well as other low Σ CSL) boundaries and dominant random high-angle boundaries (RHAGBs) connectivity. However, it has shown thickness-independent sensitization behavior as grain boundary character distribution, residual strain and grain boundary network topology towards thickness direction are similar. Owing to higher residual strain, as revealed by local misorientation analysis, the cold-worked specimen showed maximum degree of sensitization (higher than solution-annealed condition) at surface. The GBE specimen has shown much lower degree of sensitization at surface due to higher-fraction of Σ3 boundaries and discontinuous RHAGBs connectivity. However, increasing fraction of RHAGBs and their connectivity, as confirmed by twinning-related domain and fractal analysis, cause more sensitization at interior of this specimen. In spite of this, the degree of sensitization at the interior of GBE specimen is lower than the solution-annealed or cold-worked specimen. Even though the residual strain in GBE specimen is higher than the solution-annealed condition, the lower degree of sensitization indicates that the grain boundary character distribution and grain boundary network topology have higher implication than residual strain in controlling sensitization.
NanoComposite Stainless Steel Powder Technologies. CRADA Final Report for CRADA Number NFE-11-03444
The objective of this Cooperative Research and Development Agreement (CRADA) between UT-Battelle and MesoCoat Inc., is to utilize and evaluate NanoComposite Stainless Steel Powder as a coating technology for increased wear and corrosion resistance of component material.
Technical Letter Report of Slow-Strain-Rate Tensile Tests on Irradiated Stainless Steels in a PWR Environment
Slow-strain-rate tensile (SSRT) tests have been performed on irradiated specimens in a simulated pressurized water reactor (PWR) environment. The samples are miniature tensile specimens of various austenitic stainless steels (SSs) with different thermal-mechanical treatments commonly used for reactor core internal components. Neutron irradiation was carried out in the BOR-60 reactor, a sodium-cooled, fast breeder reactor in Russia, at ~320°C. The damage doses of the specimens are 5, 10, and 48 dpa (displacements per atom). All irradiated materials show significant irradiation hardening and loss of ductility in the SSRT tests. The yield strengths of cold-worked are higher than that of solution-annealed samples at all doses up to 48 dpa. While the irradiation hardening seems to saturate between ~5 and ~10 dpa, the loss of ductility continues to increase above 10 dpa. Strain softening is also observed for all irradiated materials above 5 dpa. Fractographic examinations show that ductile dimple fracture is the dominant morphology for all SSRT tests in the PWR environment. Small areas of transgranular, mixed mode and cleavage fractures are seen on most fracture surfaces in PWR water tests. Intergranular cracking is also observed in 48-dpa Types 316 and 347 SSs. Cracking susceptibility of the tested materials was evaluated with fracture morphology and time to failure. In general, high-doses cold-worked SSs are more susceptible to transgranular cleavage cracking in the PWR environment. Solution-annealed Type 347 SS is susceptible to intergranular cracking at 45 dpa in the PWR environment.
Corrosion of 316H Stainless Steel in Flowing FLiBe (LiF-BeF 2 )
This milestone was originally envisioned for completion in FY21 and was delayed due to the COVID-19 response and difficulties in fabricating/obtaining fluoride salts. A monometallic type 316H stainless steel thermal convection loop (TCL) was operated for 1000 h with flowing LiFBeF 2 (i.e. FLiBe) salt and a peak temperature of 650°C. In general, the attack was minimal. However, classic mass transfer was not clearly observed with mass losses in both the hot and cold legs. There was an issue with cleaning the loop with water and specimens may have oxidized, which was not an issue with the previous FLiNaK TCL.
Delayed Critical Enriched Uranium Metal, 7-in.-diam. Cylinder with Thin Stainless Steel Top and Bottom Reflectors
Three 7 in. diameter highly enriched uranium (HEU; 93.17 wt % 235 U) metal cylinders were assembled on the vertical assembly machine of the Oak Ridge Critical Experiments Facility (ORCEF) with thin stainless steel reflectors (0.5, 1, and 2 in. thick) on the top and bottom. These experiments were performed during January 13–25, 1965, and used seven operational days at ORCEF. Before these experiments, unreflected and unmoderated 7 in. diameter HEU metal cylinders had been assembled to delayed criticality at ORCEF, and the results were benchmarked in HEU-MET-FAST-051. In addition to the critical experiments, the prompt neutron decay constant was measured via the Rossi-α technique, and those results are also presented in this report. To achieve near-delayed-critical systems, 5 × 5 × 0.03125 in. rectangular uranium metal parts were used on top of 7 in. diameter cylinders inside the top reflector. The delayed critical configuration from the three experiments described herein are acceptable for use as criticality safety benchmark experiments for the International Criticality Safety Benchmark Evaluation Program (ICSBEP), coordinated by the Nuclear Energy Agency, once the uncertainty analysis is completed. Based on previous ICSBEP benchmarks with this enriched uranium metal at ORCEF, the uncertainty in $k_{eff}$ is expected to be as low as ±0.0002. The prompt neutron time decay data could be the basis of an International Reactor Physics Evaluation Program benchmark.
Failure Assessment Diagram for Brazed 304 Stainless Steel Joints
Interaction equations were proposed earlier to predict failure in Albemet 162 brazed joints. Present study demonstrates that the same interaction equations can be used for lower bound estimate of the failure criterion in 304 stainless steel joints brazed with silver-based filler metals as well as for construction of the Failure Assessment Diagrams (FAD).
Analysis of the MST-16 crimp process on cold 304L stainless steel
The purpose of this report is to assess the quality of the MST-16 crimp process through a series of cold experiments and metallographic analyses. Common practice in MST-16 uses a mechanical crimp on 304L stainless steel tubes to prevent radioactive contamination from escaping the tube interior for a variety of experiments. The crimped tubes must pass a leak check to demonstrate their radiological safety. Cold (i.e. non-radioactive samples) 304L tube samples were tested using two different approved crimping devices to assess the quality of the crimps. Each crimp was leak checked, followed by destructive metallographic analysis to determine the quality of both the crimp equipment and procedures used by MST-16 personnel.
The adsorption of argon and nitrogen on stainless steel at 195 deg K and 303 deg K in the pressure range 10 to the minus 8 power to 10 to the minus 7 power torr
Measuring adsorption of argon and nitrogen at low pressures on stainless steel
Fatigue crack growth at elevated temperature 316 stainless steel and H-13 steel
Crack growths were measured at elevated temperatures under four types of loading: pp, pc, cp, and cc. In H-13 steel, all these four types of loading gave nearly the same crack growth rates, and the length of hold time had negligible effects. In AISI 316 stainless steel, the hold time effects on crack growth rate were negligible if the loading was tension-tension type; however, these effects were significant in reversed bending load, and the crack growth rates under these four types of loading varied considerably. Both tensile and compressive hold times caused increased crack growth rate, but the compressive hold period was more deleterious than the tensile one. Metallographic examination showed that all the crack paths under different types of loading were largely transgranular for both CTS tension-tension specimens and SEN reversed cantilever bending specimens. In addition, an electric potential technique was used to monitor crack growth at elevated temperature.
Tensile Properties of Austenitic Stainless Steel Tubing with Internal Hydrogen/Tritium
Can microstructure explain the observed influence of hydrogen/tritium on tensile ductility? • Hydrogen is believed to interact with dislocations, grain boundaries, vacancies, and other microstructural features2 • How hydrogen and helium (He) interact with austenitic stainless steels remains a vigorous debate • We hypothesize that: • Hydrogen isotopes and decay helium act like solutes strengthening the steel and promoting planar deformation structures that reduce tensile ductility • These changes in mechanical behavior are not the same for differing microstructures
Thermal Conductivity of AM Fabricated Stainless Steel 316L Part
Thermal properties are an integral part of many diverse engineering applications, and additive manufacturing (AM), particularly laser powder bed fusion (LPBF) is shown to affect thermal properties due to the laser processing parameters. For 316L stainless steel, there is little prior research to determine the effects of the process on thermal properties. In this work, the temperature gradient is shown to create uniform, chess board-like distributions of grains in the build direction. These zones create dislocations which were visualized with EBSD techniques. Processing parameters cause hierarchal grain size distribution, with localized concentrations of small grains and large grains. Thermomechanical stresses in the rapid solidification increases dislocation density during grain formation. Previous research shows a higher density of dislocations decreases local thermal conductivity. Local and bulk thermal conductivity are shown in this work to have statistically lowered values to an average of 10-12 W/m-K compared to 14 W/m-K for conventional 316L.
Cryogenic Thermal Absorptance Measurements on Small-Diameter Stainless Steel Tubing
The Mid Infrared Instrument (MIRI) on the James Webb Space Telescope includes a mechanical cryocooler which cools its detectors to their 6 Kelvin operating temperature. The coolant gas flows through several meters of small-diameter stainless steel tubing, which is exposed to thermal radiation from its environment. Over much of its length this tubing is gold-plated to minimize the absorption of this radiant heat. In order to confirm that the cryocooler will meet MIRI's requirements, the thermal absorptance of this tubing was measured as a function of its environment temperature. We describe the measurement technique and present the results.
Flow boiling transient critical heat flux tests with stainless steel and FeCrAl: Transient correlation implementation, model calibration, and sensitivity analysis
In this study, steady-state and transient internal-flow critical heat flux (CHF) experiments were carried out under two flow conditions, at atmospheric pressure, on 316 stainless steel (316-SS) and iron-chromium-aluminum (FeCrAl) tubes. Slow power transients at a low mass flow (300 kg/m 2 - s) with very low subcooling (X e =-0.0054) generated premature CHFs, which were prevented by faster power transients and high mass flow (1000 kg/m 2 - s). The measured transient CHFs increased linearly with increasing power transients, compared with the steady-state CHF. Yet, the wall superheat at the CHFs decreased with faster power transients. Transient CHF correlations highlighting heterogeneous spontaneous nucleation were calibrated to the measured CHFs and compared with other existing correlations. Transient CHF multipliers were acquired from pool and flow boiling empirical CHF correlations that were generated. The multipliers were applied to the RELAP5-3D nuclear system code to analyze the discrepancies between the measured data and the predicted CHF and post-CHF behavior, which improved peak cladding temperature predictions by 24.6%. A variance-based global sensitivity study perturbing the experimental uncertainties and cladding material thermal properties showed the diminishing influence of flow boiling heat transfer with increasing power transients, highlighting the significance of the volumetric heat capacity for the cladding integrity during transients. Transient CHF correlations were applied to the most limiting design basis accident: a hot-zero-power reactivity-initiated accident on a generic pressurized water reactor RELAP5-3D model.
Localized orientation gradients in additively manufactured stainless steel 316H structures
The high solidification rates during additive manufacturing cause highly localized thermal and strain gradients. The effect of these gradients on the evolution of local orientation misorientations within a grain is not well understood. In this study, stainless steel 316H parts were fabricated via laser powder bed fusion using three different energy densities: 43, 71, and 135 J/mm 3 . Electron backscatter diffraction showed that the maximum misorientations of the grains can be up to 25° along the build direction. Misorientation gradients (RM g ) within grains are process-dependent and can change from 0.036°/μm to 0.015°/μm with increased volumetric energy densities. In conclusion, the characterized misorientation gradients are an indication of the level of dislocations and, to an extent, the plastic deformation resulting from the rapid solidification during laser powder bed fusion.
Comparison of the Booster Interface Temperature in Stainless Steel (SS) V-Channel Versus the Aluminum (Al) Y-Channel Primer Chamber Assemblies (PCAs): Appendices - Volume 2
NASA's Technical Fellow for Propulsion, requested a technical assessment of the performance improvement achieved by the introduction of the stainless steel (SS) V-channel compared to the aluminum (Al) Y-channel Primer Chamber Assembly (PCA) design. The SS V-channel PCA was developed for NASA's Mars Science Laboratory (MSL) Project. The principle focus of the assessment was to measure the transient temperature at the booster interface with both designs. This document contains the Appendices to the Volume I main report.
A Comparison of Solidification Structures and Submicroscale Cellular Segregation in Rapidly Solidified Stainless Steels Produced via Two-Piston Splat Quenching and Laser Powder Bed Fusion
Fusion-based additive manufacturing techniques leverage rapid solidification (RS) conditions to create parts with complex geometries, unique microscale/nanoscale morphological features, and elemental segregation. Three custom composition stainless steel alloys with varying chromium equivalence to nickel equivalence ratio (Cr eq /Ni eq ) between 1.53 and 1.95 were processed using laser powder bed fusion (LPBF) and/or two-piston splat quenching (SQ) to produce solidification rates estimated between 0.4 and 0.8 m/s. Both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to collect high-resolution images, electron backscatter diffraction (EBSD) phase identification, and measure cellular segregation. Similar features were observed in both LPBF and SQ samples including phase and microstructure, nanoscale oxide particles, cell size, and segregation behavior. However, dislocation pileup was observed along the cell boundaries only in the LPBF austenite solidified microstructure. Targeted adjustment of the SQ feedstock Cr and Ni concentrations, within the ASTM A240 specification for 316L resulted in no observable impact on the cell size, oxide particle size, or magnitude of segregation. Also, the amount of Ni segregation in the ferrite solidified microstructures did not significantly differ, regardless of Cr/Ni eq or processing technique. Here, SQ is demonstrated as capable of simulating RS rates and microstructures similar to LPBF for use as an alternative screening tool for new RS alloy compositions.
Shock compression behavior of stainless steel 316L octet-truss lattice structures
Lattice structures offer desirable mechanical properties for applications of energy absorption and impact mitigation but limited research has been carried out on their shock compression behavior. In this work, the shock compression behavior of stainless steel 316L (SS316L) octet-truss lattice structures was investigated through experimental techniques and numerical simulations. Plate impact experiments with high-speed imaging were conducted at impact velocities of 270 – 390 m/s on lattice specimens with 5x5x10 unit cell geometries additively manufactured (AM) using direct metal laser sintering. High-speed imaging together with digital image correlation was used to extract full-field measurements and define a two-wave structure consisting of an elastic wave and planar compaction (shock) wave which propagated along the impact direction. A linear shock velocity versus particle velocity relation was found to approximate the measurements with a unit slope and a linear fit constant equal to the crushing speed. Furthermore, the shock velocity versus particle velocity relation, full-field measurements, and elastic limit together with the Eulerian form of the Rankine-Hugoniot jump conditions were used to find relations for the stress and internal energy behind the shock. Stress behind the shock increased with relative density and particle velocity, and specific internal energy converged to a single curve similar to that of bulk AM SS316L. Explicit finite element analysis using the Johnson-Cook constitutive model demonstrated similar shock behavior observed in experiments and a linear shock velocity versus particle velocity relation and corresponding Hugoniot calculations were found to be in agreement with experimental results. Numerical simulations confirmed negligible effects of exterior versus interior measurements and further validated the application of one-dimensional shock theory.