Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “IRON OXIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,009 records · Page 56

A model for the biological precipitation of Precambrian iron-formation

A biological model for the precipitation of Precambrian iron formations is presented. Assuming an oxygen deficient atmosphere and water column to allow sufficient Fe solubility, it is proposed that local oxidizing environments, produced biologically, led to precipitation of iron formations. It is further suggested that spheroidal structures about 30 mm in diameter, which are widespread in low grade cherty rion formations, are relict forms of the organic walled microfossil Eosphaera tylerii. The presence of these structures suggests that the organism may have had a siliceous test, which allowed sufficient rigidity for accumulation and preservation. The model involves precipitation of ferric hydrates by oxidation of iron in the photic zone by a variety of photosynthetic organisms. Silica may have formed in the frustules of silica secreting organisms, including Eosphaera tylerii. Iron formates formed, therefore, by a sediment rain of biologically produced ferric hydrates and silica and other organic material. Siderite and hematite formed diagenetically on basin floors, and subsequent metamorphism produced magnetite and iron silicates.

Laberge, G. L.↗

Oxygen Solubility in Aqueous Amine Solvents with Common Additives Used for CO 2 Chemical Absorption

Major sources of anthropogenic CO 2 are power generation and transportation industries where researcher continue to explore CO 2 emission mitigation strategies as applied to these CO 2 sources through carbon capture, utilization, and sequestration (CCUS). The most mature CO 2 capture technology is post-combustion carbon capture (PCCC) using aqueous amine solutions/solvents, however solvent degradation and regeneration costs are slowing the widespread adoption of PCCC. Solvent degradation of the aqueous amine solutions is mainly caused from the temperature gradient between the absorber and stripper columns and common flue gas components such as SOx, NOx, and oxygen (O 2 ). The two main classifications of solvent degradation are thermal degradation, occurring when the amine reacts with itself at elevated temperatures and anaerobic conditions and oxidative degradation. Oxidative degradation reactions can occur from oxygen mass transfer and free radical oxidation. Metals, such as iron from the corrosion of steel structures used in industrial applications such as PCCC, can help to catalyze these reactions. Various oxidative degradation studies have shown how O 2 concentrations in flue gas and, to a lesser extent, temperature influence the extent of oxidative degradation. Accurately measuring the O 2 solubility, commonly referred to as dissolved oxygen (DO), in a quick, continuous, and efficient manner in aqueous amine solvents should contribute to determine the effectiveness of mitigation strategies for oxidative degradation. Knowing that commercial PCCC amine solvents contain components beyond water, amine, carbonate species and CO 2 , this investigation was conducted to determine the oxygen solubility changes of common aqueous amines solutions with commonly used and published solvent additives. The impact of carbon loadings with and without the additives was also examined. A commercial dissolved oxygen probe was used to measure the DO concentrations and compared them against standard Winkler Method titration values. The results show that antifoam shows minimal change in [DO]. MBT yielded lower DO values, and NaVO 3 showed a higher DO concentration due to interferences. These results indicate that most common amine solvent additives should be expected to minimally impact oxygen solubility and amine oxidative degradation.

60 APPLIED LIFE SCIENCES↗

Deep abiotic weathering of pyrite

Pyrite is a ubiquitous iron sulfide mineral that is oxidized by trace oxygen. The mineral has been largely absent from global sediments since the rise in oxygen concentration in Earth’s early atmosphere. We analyzed weathering in shale, the most common rock exposed at Earth’s surface, with chemical and microscopic analysis. By looking across scales from 10 −9 to 10 2 meters, we determined the factors that control pyrite oxidation. Under the atmosphere today, pyrite oxidation is rate-limited by diffusion of oxygen to the grain surface and regulated by large-scale erosion and clast-scale fracturing. We determined that neither iron- nor sulfur-oxidizing microorganisms control global pyrite weathering fluxes despite their ability to catalyze the reaction. This multiscale picture emphasizes that fracturing and erosion are as important as atmospheric oxygen in limiting pyrite reactivity over Earth’s history.

58 GEOSCIENCES↗

Ultraviolet Photooxidation of Smectite-Bound Fe(II) and Implications for the Origin of Martian Nontronites

Clay minerals detected with orbital and in situ instruments in ancient Martian terrains constrain Mars' climate and aqueous alteration history. Early in its history, Mars experienced an atmospheric redox change and iron-bearing clay minerals may preserve the effects of that transition. Ferrous smectites, the thermodynamically predicted product of chemical weathering of basalts under anoxic conditions, may have undergone oxidation by exposure to chemical oxidants in the atmosphere or regolith, or by direct photooxidation at the surface. To assess these potential oxidation pathways, ferrous trioctahedral smectites of varying initial iron content were synthesized and subjected to oxidation by ultraviolet (UV) irradiation. Experimental UV irradiation under an anoxic atmosphere equivalent to approximately 7 years of flux on the Martian surface caused partial oxidation of smectite-bound Fe (Fe3+/ΣFe = 16–18%) and octahedral sheet contraction. Metal-OH vibrational bands in visible/near infrared (VNIR) reflectance spectra of oxidized smectites changed in band depth and asymmetry with higher iron content. X-ray diffraction patterns of UV irradiated samples indicate the formation of a mixed di- and trioctahedral smectite or a secondary nontronite phase, possibly on the surfaces of higher iron content smectites. These experiments suggest that UV irradiation is able to oxidize structurally bound iron in smectites without the presence of other chemical oxidants. Photooxidation may have influenced the mineralogy, both syndepositionally and postdepositionally, of Martian alteration assemblages formed near the surface and this process needs not be limited to one part of their formation history. Plain Language Summary: Martian mineral assemblages observed with orbiters and rover instruments allow us to understand the planet's past climate and aqueous activity. Hydrated minerals that contain Fe(II) are of particular interest as they would have been affected by the early atmosphere becoming more oxidizing overtime, changing the structural iron into Fe(III). In this study, we synthesized Fe(II) smectites with varying iron content and irradiated them with an ultraviolet (UV) light source to test whether they could be photooxidized. Iron in the smectite minerals was incompletely oxidized by UV radiation after being exposed for the equivalent of approximately 7 years of exposure on the early Mars surface. The smectites with higher iron content showed more changes with photooxidation in their visible/near infrared spectra as well as in their X-ray diffraction patterns, two datasets collected by instruments on currently active Martian missions. These results suggest that UV photooxidation is a plausible contributor to the mineralogy and redox state of clay mineral assemblages observed at the Martian surface.

V. B. Rivera Banuchi↗

Effect of Electrolytes on the Cathode-Electrolyte Interfacial Stability of Fe-Based Layered Cathodes for Sodium-Ion Batteries

Iron (Fe)-based layered oxide cathodes that employ Fe 3+ /Fe 4+ redox reaction present a family of attractive cathode materials for sodium-ion batteries as iron is abundant, low-cost, and environmentally benign. However, their electrochemical performance is not yet satisfactory and requires further improvement. In this study, we investigate the effect of electrolytes on the electrochemical performance of α -NaFeO 2 , a prototypical model of Fe-based layered cathodes. First, we established the critical impact of the poor cathode-electrolyte interfacial stability on cell performances. Systematic electrochemical tests and material characterizations further revealed the degradation mechanism in which the highly reactive Fe 4+ state in the charged Na 1−x FeO 2 electrodes promotes severe electrolyte decomposition and subsequent growth of a thick interface layer that leads to impedance rise and performance degradation. In addition, the superior performance of NaPF 6 over NaClO 4 and the beneficial effect of the FEC additive are reported.

25 ENERGY STORAGE↗

A Directionally Solidified Iron-chromium-aluminum-tantalum Carbide Eutectic Alloy

A eutectic alloy, Fe-13.6CR-3.7Al+9TaC, was directionally solidified in a high gradient furnace, producing a microstructure of alined TaC fibers in an oxidation resistant alpha-iron matrix. Tensile and stress rupture properties, thermal cycling resistance, and microstructures were evaluated. The alloy displays at 1000 C an ultimate tensile strength of 58 MPa and a 100-hour rupture life at a stress of 21 MPa. Thermal cycling to 1100 C induces faceting in the TaC fibers.

Harf, F. H.↗

Elevated Temperature Properties of Titanium Carbide Base Ceramals Containing Nickel or Iron

Elevated-temperature properties of titanium carbide base ceramals containing nickel or iron were determined in oxidation, modulus of rupture, tensile strength, and thermal-shock resistance. These materials followed the general growth law and exhibited two stages in oxidation. The following tensile strengths were found at 2000 degrees F: 13.3 weight percent nickel, 16, 150 pounds per square inch; 11.8 weight percent iron, 12,500 pounds per square inch; unalloyed titanium carbide, 16,450 pounds per square inch. Nickel or iron additions to titanium carbide improved the thermal-shock resistance, nickel more. The path of fracture in tensile and thermal-shock specimens was found to progress approximately 50 percent intergranularly and 50 percent transgranularly.

MATERIALS - TEMPERATURES, HIGH↗

Viscous flow behavior of four iron-containing silicates with alumina, effects of composition and oxidation condition

The viscosity of a magma is an important parameter in connection with its effect on geologic processes such as melt segregation, magma vesiculation, and crystal fractionation. Though most models of geologic processes assume relatively low values for the magma viscosity less than 10,000 poise, it would be useful to have an empirical model for estimating viscosities when the process occurs during continuous cooling to a temperature region where the viscosity is expected to be very high. The considered work has been carried out to provide the experimental measurements of viscosity at low temperatures which would be used in formulating the empirical model. Ten iron-containing silicate compositions have been investigated by Klein et al. (1981), and four of these compositions have been selected for the present study with alumina. The study involves substitutions of Al2O3 for FeOx at Na2O/Al2O3 moles greater than one. For the four iron-containing silicate glasses with alumina, the viscosity at a given temperature is found to increase with increasing (Fe + Al).

Klein, L. C.↗

Oxidation Behavior of Binary Niobium Alloys

This investigation concludes a study to determine the effects of up to 25 atomic percent of 55 alloying additions on the oxidation characteristics of niobium. The alloys were evaluated by oxidizing in an air atmosphere for 4 hours at 1000 C and 2 hours at 1200 C. Titanium and chromium improved oxidation resistance at both evaluation conditions. Vanadium and aluminum improved oxidation resistance at 1000 C, even though the V scale tended to liquefy and the Al specimens became brittle and the scale powdery. Copper, cobalt, iron, and iridium improved oxidation resistance at 1200 C. Other investigations report tungsten and molybdenum are protective up to about 1000 C, and tantalum at 1100 C. The most important factor influencing the rate of oxidation was the ion size of the alloy additions. Ions slightly smaller than the Nb(5+) ion are soluble in the oxide lattice and tend to lower the compressive stresses in the bulk scale that lead to cracking. The solubility of the alloying addition also depends on the valence to some extent. All of the elements mentioned that improve the oxidation resistance of Nb fit this size criterion with the possible exception of Al, whose extremely small size in large concentrations would probably lead to the formation of a powdery scale. Maintenance of a crack-free bulk scale for as long as possible may contribute to the formation of a dark subscale that ultimately is rate- controlling in the oxidation process. The platinum-group metals, especially Ir, appear to protect by entrapment of the finely dispersed alloying element by the incoming Nb2O5 metal-oxide interface. This inert metallic Ir when alloyed in a sufficient amount with Yb appears to give a ductile phase dispersed in the brittle oxide. This scale would then flow more easily to relieve the large compressive stresses to delay cracking. Complex oxide formation (which both Ti and Zr tend to initiate) and valence effects, which probably change the vacancy concentration in the scale, are masked by the overriding tendency for a porous scale.

Barrett, Charles A.↗

IIAB IRON METEORITES: FORMATION AND RELATION TO OTHER METEORITE GROUPS.

The IIAB iron meteorites are one of the largest iron meteorite groups that formed by fractional crystallization [1]. Iron meteorites formed over a range of oxygen fugacities (fO2)[2], most formed relatively reduced at~ IW–4to –2.5 (IABs), where IW= iron-wüstite buffer, to relatively oxidized at IW–1(IVBs) [2,3]. While the IIABs contain reduced mineral phases (daubré elite [1]),the fO2for IIABs is poorly constrained. The fO2of iron meteorites may have become more reducing during cooling, with oxidized phases (i.e., chromite) forming at higher temperatures and daubré elite forming at lower temperatures [4]. The O-and Cr-isotope compositions of silicates and chromite in meteorites, including iron meteorites, can determine potential genetic links to other meteorite sand con-strain if a meteorite is from the non-carbonaceous (NC) or carbonaceous (CC) group [e.g., 5–8]. Iron meteorite groups have been identified as being in the NCor CC group using Mo[9]and Ni [10] isotope compositions of their metallic component. Numerous iron meteorites contain minor amounts of silicates and oxides [e.g., 11], but most have not been analyzed for their Cr or Ti isotope compositions, with some exceptions (e.g., IIIABs [6,7],a IIG, and a IIAB[7]). We analyzed the compositions of silicates and chromite in six IIAB iron meteorites to investigate the relationship between IIABs and known meteorite groups, the fO2of IIABs, and the origin of chromite in the IIABs. *full abstract in document

Meteorite↗

Fine-grained Goethite as a Precursor for Martian Gray Hematite

Several isolated deposits of gray, crystalline hematite on Mars were discovered using data returned from the Thermal Emission Spectrometer (TES) instrument aboard the Mars Global Surveyor spacecraft. Christensen et al. provided five testable hypotheses regarding the formation of crystalline hematite on Mars: 1) low-temperature precipitation of Fe oxides/hydroxides from standing, oxygenated, Fe-rich water, followed by subsequent alteration to gray hematite, 2) low-temperature leaching of iron-bearing silicates and other materials leaving a Fe-rich residue laterite-style weathering) which is subsequently altered to gray hematite, 3) direct precipitation of gray hematite from Fe-rich circulating fluids of hydrothermal or other origin, 4) formation of gray hematitic surface coatings during weathering, and 5) thermal oxidation of magnetite-rich lavas. Since this initial work, several authors have examined the hematite deposits to determine their formation mechanism. Lane et al. cited the absence of a 390/ cm absorption in the martian hematite spectrum as evidence for platy hematite grains. Their model for the formation of the deposits includes deposition of any of a variety of iron oxides or oxyhydroxides by aqueous or hydrothermal fluids, burial and metamorphosis to gray platy hematite grains, and exhumation in recent times. Based on a detailed geomorphic examination of the Sinus Meridiani region, Hynek et al. conclude that the most likely method of hematite formation was either emplacement by a hydrothermal fluid or oxidation of a magnetite-rich pyroclastic deposit. Similarly, Arvidson et al., favor a model involving the alteration of pyroclastic deposits by aqueous or hydrothermal fluids. Finally, based on geochemical modeling and an examination of Aram Chaos, Catling and Moore favor emplacement by hydrothermal fluids with a minimum temperature of 100 C. Comparison of the average martian hematite spectrum measured by TES to hematite emissivity spectra for a variety of naturally occurring hematites shows small but potentially important differences. In particular, band shapes, positions and relative band emissivities of hematite spectra vary over the range of samples. These differences imply that the natural variability of thermal infrared hematite spectra has not been fully characterized, especially with respect to the reaction pathway and crystal structure.

T D Glotch↗

Pyrite (001) Interface Chemistry is Controlled by a Sulfoxy Termination

Pyrite (FeS 2 ) is the most common sulfide mineral on Earth, forming through inorganic reactions in the crust and oceanic hydrothermal systems and via microbially driven processes in anaerobic sediments. The pyrite–water interface is the site of a wide range of adsorption and reaction processes in Earth systems including oxidation that dramatically affects the geochemistry of surface waters and influences global carbon and oxygen cycles. Mechanistic geochemical models of pyrite interfacial reactivity, however, are limited by the lack of experimentally derived atomistic structures of the reduced and reacting surfaces. Here, in this work, we reveal the atomic-scale structure of the pyrite (001)-water interface that forms at very low oxygen partial pressures, relevant to suboxic environments in Earth. The interface structure and surface speciation were obtained using the crystal truncation rod method supported by ambient-pressure photoelectron spectroscopy and density functional theory calculations. The surface is dominantly composed of disulfide groups bound to a single oxygen atom, forming a sulfoxy group that has no known molecular or bulk mineral analog. This surface is interpreted as the first step in the oxidative dissolution of pyrite. The sulfoxy group is readily protonated through surface acid–base reactions that alter the structure of interfacial water and the free energy of interfacial reactions. Surface iron sites are not oxidized. Surprisingly, this interface can likely develop in equilibrium with bulk pyrite in some reducing and acidic solutions. This termination is therefore likely representative of pyrite surfaces under a vast range of experimental, industrial and Earth conditions.

oxidation↗

The reactions of cobalt, iron and nickel in SO-2 atmospheres: Similarities and differences

The reactions of cobalt, iron and nickel in SO2 atmospheres are reviewed and compared. A mixed oxide-sulfide product layer is observed in all cases. Cobalt and nickel exhibits similar behavior. The observed rates are near the sulfidation rates, and the reaction rate is strongly influenced by the outward diffusion of metal through an interconnected sulfide network. A continuous interconnected sulfide is not observed in the oxide-sulfide scales formed on iron, and the reaction rates are more difficult to summarize. The differences and similarities among the three metals are explained in terms of the absence of scale-gas equilibrium and the ratio of the metal diffusivity in the corresponding oxide and sulfide.

Jacobson, N. S.↗

The reactions of cobalt, iron and nickel in SO2 atmospheres Similarities and differences

The reactions of cobalt, iron and nickel in SO2 atmospheres are reviewed and compared. A mixed oxide-sulfide product layer is observed in all cases. Cobalt and nickel exhibit similar behavior. The observed rates are near the sulfidation rates, and the reaction rate is strongly influenced by the outward diffusion of metal through an interconnected sulfide network. A continuous interconnected sulfide is not observed in the oxide-sulfide scales formed on iron, and the reaction rates are more difficult to summarize. The differences and similarities among the three metals are explained in terms of the absence of scale-gas equilibrium and the ratio of the metal diffusivity in the corresponding oxide and sulfide.

Jacobson, N. S.↗

Explorations of the nonheme high-valent iron-oxo landscape: crystal structure of a synthetic complex with an [Fe IV 2 (μ-O) 2 ] diamond core relevant to the chemistry of sMMOH

Methanotrophic bacteria utilize methane monooxygenase (MMO) to carry out the first step in metabolizing methane. The soluble enzymes employ a hydroxylase component (sMMOH) with a nonheme diiron active site that activates O 2 and generates a powerful oxidant capable of converting methane to methanol. It is proposed that the diiron(II) center in the reduced enzyme reacts with O 2 to generate a diferric-peroxo intermediate called P that then undergoes O–O cleavage to convert into a diiron(IV) derivative called Q, which carries out methane hydroxylation. Most (but not all) of the spectroscopic data of Q accumulated by various groups to date favor the presence of an Fe IV 2 (μ-O) 2 unit with a diamond core. The Que lab has had a long-term interest in making synthetic analogs of iron enzyme intermediates. To this end, the first crystal structure of a complex with a Fe III Fe IV (μ-O) 2 diamond core was reported in 1999, which exhibited an Fe∙∙∙Fe distance of 2.683(1) Å. Now more than 20 years later, a complex with an Fe IV 2 (μ-O) 2 diamond core has been synthesized in sufficient purity to allow diffraction-quality crystals to be grown. Finally, its crystal structure has been solved, revealing an Fe∙∙∙Fe distance of 2.711(4) Å for comparison with structural data for related complexes with lower iron oxidation states.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Moessbauer Spectroscopy for Lunar Resource Assessment: Measurement of Mineralogy and Soil Maturity

First-order assessment of lunar soil as a resource includes measurement of its mineralogy and maturity. Soils in which the mineral ilmenite is present in high concentrations are desirable feedstock for the production of oxygen at a lunar base. The maturity of lunar soils is a measure of their relative residence time in the upper 1 mm of the lunar surface. Increasing maturity implies increasing load of solar wind species (e.g., N, H, and He-3), decreasing mean grain size, and increasing glass content. All these physicochemical properties that vary in a regular way with maturity are important parameters for assessing lunar soil as a resource. For example, He-3 can be extracted and potentially used for nuclear fusion. A commonly used index for lunar soil maturity is I(sub s)/FeO, which is the concentration of fine-grained metal determined by ferromagnetic resonance (I(sub s)) normalized to the total iron content (as FeO). I(sub s)/FeO has been measured for virtually every soil returned by the Apollo and Luna missions to the Moon. Because the technique is sensitive to both oxidation state and mineralogy, iron Moessbauer spectroscopy (FeMS) is a viable technique for in situ lunar resource assessment. Its utility for mineralogy is apparent from examination of published FeMS data for lunar samples. From the data published, it can be inferred that FeMS data can also be used to determine soil maturity. The use of FeMS to determine mineralogy and maturity and progress on development of a FeMS instrument for lunar surface use are discussed.

Morris, R. V.↗

Non-Fouling, Low Cost Electrolytic Coagulation & Disinfection for Treating Flowback and Produced Water for Reuse

Executive Summary This Final Report is composed of two major sections. The first section presents experimental results obtained in the laboratory during Budget Period 1. The second section presents results from the field test conducted during Budget Period 2. Laboratory Results This research investigated a novel electrochemical process for producing a ferric iron coagulant for use in treating flowback and produced water from hydraulic fracturing and oil production operations. The treatment system improves the effectiveness and lowers the cost of coagulation processes using Fe3+ as the coagulant. The electrolytic coagulant generation (ECG) system uses an electrochemical cell to produce acid and base from oilfield brine solutions. The acid is used to dissolve scrap iron to provide a Fe3+ coagulating agent. The base is used to neutralize the treated water. Compared to conventional electrocoagulation (EC), the main advantage of the ECG system is an order of magnitude lower cost for the source of iron. The second advantage over conventional EC is that it can deliver Fe3+ doses greater than 1 mM, since it is not limited by the amount of dissolved oxygen in the water required to oxidize ferrous to ferric iron. The capital costs for conventional EC and the ECG system are similar, but the operational costs for the ECG system are an order of magnitude lower than conventional EC. The combined costs for iron and electrical energy for treating 1 m3 of FPW with 1 mM Fe3+ is estimated to be $0.87 for conventional EC, and $0.087 for the ECG system. The estimated all-in cost for treating FPW with a 2 mM Fe3+ dose is $0.73/m3 ($0.12/bbl). Field Test Results The field test was conducted at the Paul Foster Central Tank Battery (CTB) in Lea County, New Mexico from November 10, 2022 through December 15, 2022. The feed water to the system was produced water from the Tatanka 1H formation. After approximately two weeks of testing, the initial batch of produced water had been treated and no untreated produced water was available. Thus, after this time, the feed water to the system consisted of previously treated water (i.e., recycled water). The recycled water had nearly all colloidal particles removed, and had a much lower alkalinity due to precipitation of carbonate minerals during the first pass through the system. Although the recycled water was not an ideal test solution due to its low particulate concentrations, its lower alkalinity did allow us to identify the main problem with the treatment system. The main problem with the treatment system was caused by the high alkalinity of the initial feed water (5.4 meq/L) that consumed a significant fraction of the electrochemically generated acid. This resulted in pH values exiting the iron contact tank that were too high to dissolve enough iron to effectively treat the produced water. Tests performed with recycled water with lower alkalinity did not have this issue, and dissolved iron concentrations greater than 20 mM could be achieved. One consistent observation was that effluent water from the iron contact tank was always free of particulates, even when fed with circumneutral solutions. This suggests that there is no need to dissolve high concentrations of iron if all the water to be treated is passed through the scrap iron canister. In this case, dissolved O2 and hypochlorous acid can promote sufficient iron corrosion to provide an effective coagulating agent – even in neutral pH water. This solves the problem resulting from highly alkaline produced water. Modifications to the design of the treatment system were made based on the field test results. These modifications will add minimal additional cost, and were tested in bench-scale laboratory experiments. In short-term testing, the modified treatment process was able to remove colloidal FeS particulates to levels below detection. Long-term, steady state testing will be required to determine whether the modified process is suitable for commercial treatment systems.

54 ENVIRONMENTAL SCIENCES↗