Stressed-Oxidation Lifetime of Different SiC Fiber, CVI Matrix SiC Minicomposites in Air

The stressed-oxidation lifetime properties of several minicomposites composed of single fiber tows with a CVI SiC matrix were compared. The minicomposites were made up of Nicalon(Tm) and Hi-Nicalon(Tm) SiC fibers with carbon or BN interphases. Constant load stress-rupture tests were performed between 600 and 13000 C in air for all of the minicomposite systems. Cyclic load testing was performed on the Hi-Nicalon minicomposite systems. The factors controlling the different lifetime behaviors: fiber rupture properties, interphase oxidation, fiber degradation, and fiber-matrix bonding, are discussed in light of different minicomposite constituents. All of the systems were subject to intermediate temperature embrittlement. The Hi-Nicalon fiber, BN interphase system, performed the best for constant load conditions. For cyclic load conditions, both the BN- interphase and C-interphase minicomposites displayed poor, but different failure behavior.

Morscher, Gregory N.↗

Geodetic Observations of Interseismic Strain Segmentation at the Sumatra Subduction Zone

Deformation above the Sumatra subduction zone, revealed by Global Positioning System (GPS) geodetic surveys, shows nearly complete coupling of the forearc to the subducting plate south of 0.5 deg S and half as much to north. The abrupt change in plate coupling coincides with the boundary between the rupture zones of the 1833 and 1861 (Mw greater than 8) thrust earthquakes. The rupture boundary appears as an abrupt change in strain accumulation well into the interseismic cycle, suggesting that seismic segmentation is controlled by properties of the plate interface that persist occupied through more than one earthquake cycle. Structural evidence indicates that differences in basal shear stress may be related to elevated pore pressure in the north.

Prawirodirdjo, L.↗

Microstructure, Mechanical Properties, Hot-Die Forming, and Joining of 47XD Gamma TiAl Rolled Sheets

The microstructure and mechanical properties, along with the hot-die forming and joining of Ti-47Al-2Nb-2Mn-0.8 vol% TiB, sheets (known as 47XD), produced by a low-cost rolling process, were evaluated. A near-gamma microstructure was obtained in the as-rolled condition. The microstructures of heat-treated sheets ranged from a recrystallized equiaxed near-gamma microstructure at 1,200 to 1,310 C, to a duplex microstructure at 1,350 C, to a fully lamellar microstructure at 1,376 C. Tensile behavior was determined for unidirectionally rolled and cross-rolled sheets for room temperature (RT) to 816 C. Yield stress decreased gradually with increasing deformation temperature up to 704 C; above 704 C, it declined rapidly. Ultimate tensile strength exhibited a gradual decrease up to 537 C before peaking at 704 C, followed by a rapid decline at 816 C. The modulus showed a gradual decrease with temperature, reaching approximately 72% of the RT value at 816 C. Strain to failure increased slowly from RT to 537 C; between 537 C and 704 C it exhibited a phenomenal increase, suggesting that the ductile-brittle transition temperature was below 704 C. Fracture mode changed from transgranular fracture at low temperature, to a mixture of transgranular and intergranular fracture at intermediate temperature, to ductile fracture at 816 C, coupled with dynamic recrystallization at large strains. Creep rupture response was evaluated between 649 and 816 C over the stress range of 69 to 276 MPa. Deformation parameters for steady-state creep rate and time-to-rupture were similar: activation energies of approximately 350 kJ/mol and stress exponents of approximately 4.5. Hot-die forming of sheets into corrugations was done at elevated temperatures in vacuum. The process parameters to join sheets by diffusion bonding and brazing with TiCuNi 70 filler alloy were optimized for test coupons and successfully used to fabricate large truss-core and honeycomb structures. Nondestructive evaluation methods, e.g., ultrasonic C-scans and thermography along with metallography, were used to characterize bond quality. Microstructural evaluation during heat treatment, identification of phases at the braze/matrix interface, determination of shear strengths of brazed joints, and deformation mechanisms during tensile and creep processes will be discussed.

Das, G.↗

High Temperature Si-doped BN Interphases for Woven SiC/SiC Composites

The hydrolytic stability of high-temperature deposited Si-doped BN has been shown in the past to be superior in comparison to "pure" BN processed at similar or even higher temperatures. This type of material would be very desirable as a SiC/SiC composite interphase that is formed by chemical infiltration into multi-ply woven preform. However, due to rapid deposition on the preform outer surface at the high processing temperature, this has proven very difficult. To overcome this issue, single plies of woven fabric were infiltrated with Si-doped BN. Three composite panels of different SiC fiber types were fabricated with Si-doped BN interphases including Sylramic, Hi-Nicalon Type S and Sylramic-iBN fiber-types. The latter fiber-type possesses a thin in-situ grown BN layer on the fiber surface. High Si contents (approx. 7 to 10 a/o) and low oxygen contents (less than 1 a/o) were achieved. All three composite systems demonstrated reasonable debonding and sliding properties. The coated Sylramic fabric and composites were weak due to fiber degradation apparently caused during interphase processing by the formation of TiN crystals on the fiber surface. The Hi-Nicalon Type S composites with Si-doped BN interphase were only slightly weaker than Hi-Nicalon Type S composites with conventional BN when the strength on the load-bearing fibers at failure was compared. On the other hand, the Sylramic-iBN fabric and composites with Si-doped BN showed excellent composite and intermediate temperature stress-rupture properties. Most impressive was the lack of any significant interphase oxidation on the fracture surface of stress-ruptured specimens tested well above matrix cracking at 815C.

Morscher, Gregory N.↗

High-Temperature Mechanical Properties of Cr(3+) Doped Sapphire Fibers

High-temperature slow-crack growth of single crystal 10 wt% Cr2O3 - Al2O3 (nominal composition) fibers has been studied by tensile rupture experiments at 1400 C, under different stressing rates (0.5 to 41.5 MPa/s). Slow-crack growth (SCG) is less pronounced with increasing Cr2O3. Rupture stresses increased with the stressing rate from 397 MPa to 515 MPa, resulting in a SCG exponent, N=19. The Cr2O3 composition was analyzed by Energy Dispersed X-Ray Spectra (EDS) and fracture surfaces were studied by scanning electron microscopy (SEM). Results are compared with previous studies on 100-300 ppm Cr3(+) doped sapphire fibers and on commercial sapphire fibers.

Sayir, A.↗

Cooling of Gas Turbines: Effectiveness of Rim Cooling of Blades - 2

An analysis is presented of rim cooling of gas-turbine blades; that is, reducing the temperature at the base of the blade (wheel rim), which cools the blade by conduction alone. Formulas for temperature and stress distributions along the blade are derived and, by the use of experimental stress-rupture data for a typical blade alloy, a relation is established between blade life (time for rupture), operating speed, and amount of rim cooling for several gas temperatures. The effect of blade parameter combining the effects of blade dimensions, blade thermal conductivity, and heat-transfer coefficient is determined. The effect of radiation on the results is approximated. The gas temperatures ranged from 1300F to 1900F and the rim temperature, from 0F to 1000F below the gas temperature. This report is concerned only with blades of uniform cross section, but the conclusions drawn are generally applicable to most modern turbine blades. For a typical rim-cooled blade, gas temperature increases are limited to about 200F for 500F of cooling of the blade base below gas temperature, and additional cooling brings progressively smaller increases. In order to obtain large increases in thermal conductivity or very large decreases in heat-transfer coefficient or blade length or necessary. The increases in gas temperature allowable with rim cooling are particularly small for turbines of large dimensions and high specific mass flows. For a given effective gas temperature, substantial increases in blade life, however, are possible with relatively small amounts of rim cooling.

Wolfenstein, Lincoln↗

The 1999 (Mw 7.1) Hector Mine, California, Earthquake: Near-Field Postseismic Deformation from ERS Interferometry

Interferometric synthetic aperture radar (InSAR) data over the area of the Hector Mine earthquake (Mw 7.1, 16 October 1999) reveal postseismic deformation of several centimeters over a spatial scale of 0.5 to 50 km. We analyzed seven SAR acquisitions to form interferograms over four time periods after the event. The main deformations seen in the line-of-sight (LOS) displacement maps are a region of subsidence (60 mm LOS increase) on the northern end of the fault, a region of uplift (45 mm LOS decrease) located to the northeast of the primary fault bend, and a linear trough running along the main rupture having a depth of up to 15 mm and a width of about 2 km. We correlate these features with a double left-bending, rightlateral, strike-slip fault that exhibits contraction on the restraining side and extension along the releasing side of the fault bends. The temporal variations in the near-fault postseismic deformation are consistent with a characteristic time scale of 135 + 42 or - 25 days, which is similar to the relaxation times following the 1992 Landers earthquake. High gradients in the LOS displacements occur on the fault trace, consistent with afterslip on the earthquake rupture. We derive an afterslip model by inverting the LOS data from both the ascending and descending orbits. Our model indicates that much of the afterslip occurs at depths of less than 3 to 4 km.

Jacobs, Allison↗

Modeling the Thermostructural Stability of Melt-infiltrated Sic/sic Composites

SiC/SiC composites developed by NASA with Sylramic-iBN fibers and melt-infiltrated (MI) SiC-Si matrices have demonstrated 1000-hour rupture life in air at 100 MPa and 1315OC. Recently it has been determined that a major factor controlling the long-term rupture life of these composites is not environment or stress, but an intrinsic microstructural and strength instability caused by a thermally-induced silicon attack of the Sic fibers. The objective of this paper is to present a simple diffusion-based analytical model which predicts well the observed effects of stress-free thermal exposure on the residual tensile strength of Sylramic-iBN/SiC-Si composites. The practical implications of the model for SiC/SiC composites with MI matrices are discussed.

DiCarlo, James A.↗

Tensile Properties of 17-7 PH and 12 MoV Stainless-Steel Sheet under Rapid-Heating and Constant-Temperature Conditions

Results are presented of rapid-heating tests of 17-7 PH and 12 MoV stainless-steel sheet heated to failure at temperature rates from about 1 F to 170 F per second under constant-load conditions. Yield and rupture strengths obtained from rapid-heating tests are compared with yield and tensile strengths obtained from short-time elevated-temperature tensile tests (30-minute exposure). A rate-temperature parameter was used to construct master curves from which yield and rupture stresses or temperatures can be predicted. A method for measuring strain by optical means is described.

Manning, Charles R., Jr.↗

SiC/SiC Life Modeling at Intermediate Temperatures under NASA UEET

Within the NASA UEET program, physics-based residual strength and rupture life models are being developed for a variety of time-temperature-stress-environment conditions for SiC/SiC components such as combustor liners and vanes. During service, a tensile stress condition that could be life-limiting typically occurs on the 'cold side' of these components due to thermal gradients and attachment schemes. An intermediate temperature (600 to 1000 C) stress-rupture model has been developed based on the underlying physical processes, i.e., oxygen penetration through matrix cracks, oxidation of the BN interphase, and subsequent fiber-fiber fusion within crack-bridging tows that eventually fail in time due to time-dependent strength degradation of the weakest fibers. Modifications to the model will be discussed to incorporate different environmental conditions as well as changes in oxidation kinetics due to improved interphase concepts.

Morscher, Gregory N.↗

Integrated Design Software Predicts the Creep Life of Monolithic Ceramic Components

Significant improvements in propulsion and power generation for the next century will require revolutionary advances in high-temperature materials and structural design. Advanced ceramics are candidate materials for these elevated-temperature applications. As design protocols emerge for these material systems, designers must be aware of several innate features, including the degrading ability of ceramics to carry sustained load. Usually, time-dependent failure in ceramics occurs because of two different, delayedfailure mechanisms: slow crack growth and creep rupture. Slow crack growth initiates at a preexisting flaw and continues until a critical crack length is reached, causing catastrophic failure. Creep rupture, on the other hand, occurs because of bulk damage in the material: void nucleation and coalescence that eventually leads to macrocracks which then propagate to failure. Successful application of advanced ceramics depends on proper characterization of material behavior and the use of an appropriate design methodology. The life of a ceramic component can be predicted with the NASA Lewis Research Center's Ceramics Analysis and Reliability Evaluation of Structures (CARES) integrated design programs. CARES/CREEP determines the expected life of a component under creep conditions, and CARES/LIFE predicts the component life due to fast fracture and subcritical crack growth. The previously developed CARES/LIFE program has been used in numerous industrial and Government applications.

Source record↗

Deleterious Phase Formation in Next- Generation Nickel-Base Superalloys Predicted

Nickel- (Ni-) base superalloy single crystals represent the state-of-the-art for turbine engine airfoil applications because they offer the best balance of properties under the high operating temperatures required for efficient engine operation. Current trends in alloy design take advantage of improved creep rupture strength with the addition of higher levels of refractory elements. In particular, the addition of significantly higher levels of rhenium in third-generation superalloys is key for both microstructural stability and creep rupture strength. Although refractories provide strength benefits, alloys tend to be unstable when their refractory content is high because of topologically close-packed (TCP) phases. The formation of these phases in sufficient amount is detrimental to the performance of these alloys because of their brittle nature and because they deplete the Nirich matrix of potent solid-solution strengthening elements.

Ritzert, Frank J.↗

Creep/Rupture Behavior of Melt-Infiltrated SiC/SiC Composites Being Investigated

The failure behavior of melt-infiltrated SiC/SiC ceramic matrix composites is under investigation at the NASA Glenn Research Center as part of NASA's Ultra-Efficient Engine Technology Program. This material was originally developed under the High Speed Research Office's Enabling Propulsion Materials Program. Creep and rupture data provide accelerated testing information to predict material behavior under engine use situations (1500 to 2400 F). This information gives insights into various material development paths to improve composites as well as improve understanding of failure mechanisms. The left figure shows the fracture surface of a CMC material following over 200 hr of testing at 2400 F. This surface demonstrates the kind of fibrous pullout desirable for maximum crack deflection, hence non-brittle failure. Microscopy suggests that creep and rupture of these materials can best be considered as a probabilistic property, rather than a material property. Fiber failure occurs first in isolated regions, while stronger adjacent fibers remain intact. The right figure shows a region where oxide deposits blur and round the fiber images. Because the oxidation kinetics of SiC are well understood, this oxide scale can be used as a measure of the length of time various regions of the composites have been exposed to the environment, hence providing vital information regarding the sequence of failure. The oxide scale in the right figure indicates an early failure of this tow of fibers, whereas adjacent tows remain oxide free, suggesting failure much later in time. The path of various cracks can be followed throughout the composite in this manner, suggesting failure mechanisms.

Hurst, Janet B.↗

Techniques Optimized for Reducing Instabilities in Advanced Nickel-Base Superalloys for Turbine Blades

The High-Speed Research (HSR) Airfoil Alloy program developed fourth-generation single-crystal superalloys with up to an 85 F increase in creep rupture capability over current production airfoil alloys. Recent results have been generated at the NASA Glenn Research Center on these fourth-generation alloys, but in coated form, for subsonic turbine blade applications under NASA's Ultra-Efficient Engine Technology (UEET) Program. One goal for UEET is to optimize the airfoil alloy/thermal barrier coating system for 3100 F turbine inlet temperatures. The state-of-the art turbine blade airfoil system consists of a superalloy single crystal that provides the basic mechanical performance of the airfoil. A thermal barrier coating is used to reduce the temperature of the base superalloy, and a bondcoat is deposited between the base material and the thermal barrier coating. The bondcoat improves the oxidation and corrosion resistance of the base superalloy and improves the spallation resistance of the thermal barrier coating. A commercial platinum aluminide bondcoat was applied to the HSR-developed alloys, and a diffusion zone developed as a result of interaction between the bondcoat and the superalloy. Optimized strength is obtained for superalloys when the refractory element content is high and the limits of microstructural stability are approached or exceeded slightly. For fourthgeneration alloys, instability leads to the formation of topologically close packed (TCP) phases, which form internally in the superalloy, and a secondary reaction zone (SRZ), which forms under the diffusion zone. There was a concern that excessive quantities of either TCP or SRZ might decrease the mechanical properties of the superalloy, with SRZ thought to be particularly detrimental and its formation unpredictable. Thus, an SRZreduction effort was initiated in the NASA UEET Program so that methods developed during the HSR project could be optimized further to reduce or eliminate the SRZ. An SRZ is a three-phase constituent composed of TCP and stringers of gamma phase in a matrix of gamma prime. An incoherent grain boundary separates the SRZ from the gammagamma prime microstructure of the superalloy. The SRZ is believed to form as a result of local chemistry changes in the superalloy due to the application of the diffusion aluminide bondcoat. Locally high surface stresses also appear to promote the formation of the SRZ. Thus, techniques that change the local alloy chemistry or reduce surface stresses have been examined for their effectiveness in reducing SRZ. These SRZ-reduction steps are performed on the test specimen or the turbine blade before the bondcoat is applied. Stressrelief heat treatments developed at NASA Glenn have been demonstrated to reduce significantly the amount of SRZ that develops during subsequent high-temperature exposures. Stress-relief heat treatments reduce surface stresses by recrystallizing a thin surface layer of the superalloy. However, in alloys with very high propensities to form SRZ, stress relief heat treatments alone do not eliminate SRZ entirely. Thus, techniques that modify the local chemistry under the bondcoat have been emphasized and optimized successfully at Glenn. One such technique is carburization, which changes the local chemistry by forming submicron carbides near the surface of the superalloy. Detailed characterizations have demonstrated that the depth and uniform distribution of these carbides are enhanced when a stress relief treatment and an appropriate surface preparation are employed in advance of the carburization treatment. Even in alloys that have the propensity to develop a continuous SRZ layer beneath the diffusion zone, the SRZ has been completely eliminated or reduced to low, manageable levels when this combination of techniques is utilized. Now that the techniques to mitigate SRZ have been established at Glenn, TCP phase formation is being emphasized in ongoing work under the UEET Program. The limitsf stability of the fourth-generation alloys with respect to TCP phase formation are currently being defined along with high-temperature creep rupture properties. In addition, a regression model is being developed at Glenn for the prediction of the presence of TCP phase in the microstructure and SRZ under the diffusion zone. The model is based on a design-of-experiments methodology with emphasis on the potential synergistic effects of alloying elements.

MacKay, Rebecca A.↗

Thermostructural Properties Of Sic/Sic Panels With 2.5d And 3d Fiber Architectures

CMC hot-section components in advanced engines for power and propulsion will typically require high cracking strength, high ultimate strength and strain, high creep- rupture resistance, and high thermal conductivity in all directions. In the past, NASA has demonstrated fabrication of a variety of SiC/SiC flat panels and round tubes with various 2D fiber architectures using the high-modulus high-performance Sylramic-iBN Sic fiber and Sic-based matrices derived by CVI, MI, and/or PIP processes. The thermo- mechanical properties of these CMC have shown state-of-the-art performance, but primarily in the in-plane directions. Currently NASA is extending the thermostructural capability of these SiC/SiC systems in the thru-thickness direction by using various 2.5D and 3D fiber architectures. NASA is also using specially designed fabrication steps to optimize the properties of the BN-based interphase and Sic-based matrices. In this study, Sylramic-iBN/SiC panels with 2D plain weave, 2.5D satin weave, 2.5D ply-to-ply interlock weave, and 3D angle interlock fiber architectures, all woven at AITI, were fabricated using matrix densification routes previously established between NASA and GEPSC for CVI-MI processes and between NASA and Starfire-Systems for PIP processes. Introduction of the 2.5 D fiber architecture along with an improved matrix process was found to increase inter-laminar tensile strength from 1.5 -2 to 3 - 4 ksi and thru-thickness thermal conductivity from 15-20 to 30-35 BTU/ft.hr.F with minimal reduction in in-plane strength and creep-rupture properties. Such improvements should reduce thermal stresses and increase the thermostructural operating envelope for SiC/SiC engine components. These results are analyzed to offer general guidelines for selecting fiber architectures and constituent processes for high-performance SiC/SiC engine components.

Yun, H. M.↗

Thermomechanical Performance of C and SiC Multilayer, Fiber-Reinforced, CVI SiC Matrix Composites

Hybrid fiber approaches have been attempted in the past to alloy desirable properties of different fiber-types for mechanical properties, thermal stress management, and oxidation resistance. Such an approach has potential for the CrSiC and SiCrSiC composite systems. SiC matrix composites with different stacking sequences of woven C fiber (T300) layers and woven Sic fiber (Hi-NicalonTM) layers were fabricated using the standard CVI process. Delamination occurred to some extent due to thermal mismatch for all of the composites. However, for the composites with a more uniform stacking sequence, minimal delamination occurred, enabling tensile properties to be determined at room temperature and elevated temperatures (stress-rupture in air). Composites were seal-coated with a CVI SiC layer as well as a proprietary C-B-Si (CBS) layer. Definite improvement in rupture behavior was observed in air for composites with increasing SiC fiber content and a CBS layer. The results will be compared to standard C fiber reinforced CVI SiC matrix and Hi-Nicalon reinforced CVI SiC matrix composites.

Morscher, Gregory N.↗

Comparison of AMZIRC and GRCop-84

The mechanical properties of two copper alloys with high thermal conductivity, GRCop-84 and AMZIRC, were compared. These are competing alloys in high temperature, high heat flux applications such as rocket nozzles. The GRCop-84 data presented was taken from previous work. The results of new tensile, creep, and compression tests on AMZIRC are presented. Tests were done on as-received hard drawn material, and on material that had been subjected to a heat treatment designed to simulate a brazing operation at 935 C. As-received AMZIRC was found to have excellent properties at temperatures below 550 C, with room temperature yield and ultimate tensile strengths of about 500 MPa, and ductile failures. By comparison, GRCop-84 s room temperature tensile yield and ultimate strengths are about 200 and 380 MPa respectively. However, the simulated brazing heat treatment substantially decreased the mechanical properties of AMZIRC; and the strength of as-received AMZIRC dropped precipitously as test temperatures exceeded 500 C. The properties of GRCop-84 were not significantly affected by the 935 C heat treatment. As a result, there appear to be advantages to GRCop- 84 over AMZIRC if use or processing temperatures of greater than 500 C are expected. Tensile creep tests were done at 500 and 650 C. At these temperatures, the creep properties of GRCop-84 were superior to AMZIRC s. At equivalent rupture life and stress, GRCop-84 was found to have a 150 C temperature advantage over AMZIRC; for equivalent rupture life and temperature GRCop-84 was two times stronger.

de Groh, Henry C. III↗

Simulated Data for High Temperature Composite Design

The paper describes an effective formal method that can be used to simulate design properties for composites that is inclusive of all the effects that influence those properties. This effective simulation method is integrated computer codes that include composite micromechanics, composite macromechanics, laminate theory, structural analysis, and multi-factor interaction model. Demonstration of the method includes sample examples for static, thermal, and fracture reliability for a unidirectional metal matrix composite as well as rupture strength and fatigue strength for a high temperature super alloy. Typical results obtained for a unidirectional composite show that the thermal properties are more sensitive to internal local damage, the longitudinal properties degrade slowly with temperature, the transverse and shear properties degrade rapidly with temperature as do rupture strength and fatigue strength for super alloys.

Chamis, Christos C.↗