Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Sizing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

Influence of Particle Size on Reaction Selectivity in Cyclohexene Hydrogenation and Dehydrogenation over Silica-Supported Monodisperse Pt Particles

The role of particle size during the hydrogenation/dehydrogenation of cyclohexene (10 Torr C{sub 6}H{sub 10}, 200-600 Torr H{sub 2}, and 273-650 K) was studied over a series of monodisperse Pt/SBA-15 catalysts. The conversion of cyclohexene in the presence of excess H{sub 2} (H{sub 2}:C{sub 6}H{sub 10} ratio = 20-60) is characterized by three regimes: hydrogenation of cyclohexene to cyclohexane at low temperature (< 423 K), an intermediate temperature range in which both hydrogenation and dehydrogenation occur; and a high temperature regime in which the dehydrogenation of cyclohexene dominates (> 573 K). The rate of both reactions demonstrated maxima with temperature, regardless of Pt particle size. For the hydrogenation of cyclohexene, a non-Arrhenius temperature dependence (apparent negative activation energy) was observed. Hydrogenation is structure insensitive at low temperatures, and apparently structure sensitive in the non-Arrhenius regime; the origin of the particle-size dependent reactivity with temperature is attributed to a change in the coverage of reactive hydrogen. Small particles were more active for dehydrogenation and had lower apparent activation energies than large particles. The selectivity can be controlled by changing the particle size, which is attributed to the structure sensitivity of both reactions in the temperature regime where hydrogenation and dehydrogenation are catalyzed simultaneously.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Particle Size-Dependent Zero-Field Exchange Bias in LaFeO {sub 3} Nanoparticles

The present communication deals with particle size-dependent zero-field cooled exchange effect in LaFeO{sub 3} (LFO). LFO nanoparticles were prepared by PVA-based sol-gel method. The sample was calcined at different temperatures (700, 750, and 800 {sup ∘}C) to tune the average particle size. The detailed crystal structural and their geometrical parameters were examined by means of Rietveld refinement using x-ray diffraction data. The different techniques such as Scherrer’s method, Williamson Hall method, FESEM, and TEM were applied to accurately determine the average particle size. Zero-field cooled exchange bias and weak ferromagnetism in antiferromagnetic nanoparticles was observed for all samples using hysteresis loop measurement. The training effect was studied to confirm that the loop shift originates due to exchange bias. Exchange bias as well as coercivity are strongly related to the particle size at low and room temperature. The results clearly demonstrate that the process of calcination tailor the overall properties of material which makes it a promising candidate for device applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of particle size and adsorbates on the L{sub 3}, L{sub 2} and L{sub 1} x-ray absorption near edge structure of supported Pt nanoparaticles.

Pt nano-particles from about 1 to 10 nm have been prepared on silica, alkali-silica, alumina, silica-alumina, carbon and SBA-15 supports. EXAFS spectra of the reduced catalysts in He show a contraction of the Pt-Pt bond distance as particle size is decreased below 3 nm. The bond length decreased as much as 0.13 {angstrom} for 1 nm Pt particles. Adsorption of CO and H{sub 2} lead to a increase in Pt-Pt bond distance to that near Pt foil, e.g., 2.77 {angstrom}. In addition to changes in the Pt bond distance with size, as the particle size decreases below about 5 nm there is a shift in the XANES to higher energy at the L{sub 3} edge, a decrease in intensity near the edge and an increase in intensity beyond the edge. We suggest these features correspond to effects of coordination (the decrease at the edge) and lattice contraction (the increase beyond the edge). At the L{sub 2} edge, there are only small shifts to higher energy at the edge. However, beyond the edge, there are large increases in intensity with decreasing particle size. At the L{sub 1} edge there are no changes in position or shape of the XANES spectra. Adsorption of CO and H{sub 2} also lead to changes in the L{sub 3} and L{sub 2} edges, however, no changes are observed at the L1 edge. Density Functional Theory and XANES calculations show that the trends in the experimental XANES can be explained in terms of the states available near the edge. Both CO and H{sub 2} adsorption result in a depletion of states at the Fermi level but the creation of anti-bonding states above the Fermi level which give rise to intensity increases beyond the edge.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Influence of Particle Size on Apparent Diffusivity During Spark Plasma Sintering of Crystalline Powders

Abstract:: A theoretical framework is presented to determine an apparent diffusivity D during powder sintering and further elucidate the underlying interrelation between D and shrinkage behaviors of powders. Furthermore, to eliminate the influence of crystalline defects that are typically present in raw powders, complete crystallization of metallic glass powders is performed to allow the investigation of the influence of particle size solely on powder densification. Furthermore, to validate the framework developed, Ti{sub 40.6}Zr{sub 9.4}Cu{sub 37.5}Ni{sub 9.4}Sn{sub 3.1} crystalline alloy powders constituting particles with different sizes are examined to establish a correlation between D and the sintering behaviors of the powders. The findings show that the value of the apparent diffusivity D increases with the increasing particle size, which accelerates powder densification during spark plasma sintering. Furthermore, the results quantitatively support the argument that particle size can affect atomic diffusion during powder sintering.

36 MATERIALS SCIENCE↗

Regulating the properties of activated carbon for supercapacitors: impact of particle size and degree of aromatization of hydrochar

Hydrochar (HC), obtained by the hydrothermal carbonization (HTC) of biomass, is an excellent precursor for preparing activated carbon (AC). However, the effects of the intrinsic properties of HC on the microstructure and electrochemical properties of AC are largely unknown. Here, this study investigates the impact of particle size and the degree of aromatization of in-situ HC on the microstructure and electrochemical properties of AC. Our results show that a large particle size and a high degree of aromatization help protect the HC from overactivation by ZnCl 2 , resulting in an large specific surface area (SSA > 2000 m 2 /g) and high mesopore to micropore volume ratio value ( V mes /V mic > 0.3) of the AC. Electrochemical performance measurements show a maximum specific capacitance of 218 F/g at 0.5 A/g was achieved in all samples where the AC (AC180-10 h) was prepared by activating HC180-10 h with a large size, a high degree of aromatization, and abundant surface oxygen-containing functional groups. After AC180-10 h was assembled into a supercapacitor, the specific capacitance of AC180-10 h still reached 158 F/g at 0.5 A/g, and it showed excellent cycling stability. This study advances the understanding of the impact of HC particle size and degree of aromatization on AC properties, providing new insights into tailoring HC qualities so that improving improve the properties of AC.

36 MATERIALS SCIENCE↗

Indentation size effect in unirradiated and ion-irradiated 800H steel at high temperatures

Nanoindentation is a widespread and useful method for evaluating mechanical properties at the sub-micron length scale. However, the indentation size effect remains a major obstacle to obtain meaningful macroscopic mechanical properties from small volume testing. Here, this work systematically addresses the Indentation Size Effect (ISE) phenomenon as a function of temperature and defect density in an austenitic Fe-Cr-Ni alloy (800H) to establish the baseline for nanoindentation testing of ion-irradiated alloys in environmental conditions. The 800H steel sample was irradiated with 70 MeV Fe 9+ at 450 °C to the total dose of 20.68 dpa. All samples were tested up to 300 °C in order to quantify the effect of temperature on the indentation size effect. It was found that in all cases, the ISE is less pronounced at high temperatures due to the increase of the plastic zone size. For the same grain orientation, the ISE is less pronounced in the irradiated 800H at all temperatures.

36 MATERIALS SCIENCE↗

Particle size effects in metallic microparticle impact-bonding

In cold spray processing of metals, the critical velocity for particle bonding is dependent on both intrinsic material properties, such as density and (spall) strength, and extrinsic process parameters, such as the powder particle size. Here, we specifically isolate and investigate particle size effects on the critical velocity for bonding through laser- induced single particle impact experiments and finite element simulations. We also present a predictive framework to correlate particle size and critical velocity. We show that an increase in particle size leads to an increase in the temperature of the jet formed at the interface of the particle and the substrate. This increased temperature locally decreases the spall strength of the material which, in turn, decreases the critical velocity for larger particles.

36 MATERIALS SCIENCE↗

Rules for the crystallite size and dislocation density evolution in phases during α-ω transformation in Zr under high-pressure and severe plastic flow

The first in-situ X-ray diffraction (XRD) study of the evolution of the crystallite size and dislocation density in phases during plastic strain-induced phase transformation (PT) is performed utilizing α-ω PT in strongly pre-deformed commercially pure Zr as an important example. Rough diamond anvils (rough-DA) are introduced to intensify all occurring processes during heterogeneous compression of Zr in a diamond anvil cell (DAC). The main rule is found that during α-ω PT the crystallite size and dislocation density in ω-Zr depend solely on the volume fraction of ω-Zr and are independent of pressure, plastic strain tensor, its path, and initial nanostructure. Crystallite size in ω-Zr increases from 10 to 60 nm during the PT, while dislocation density reduces from 1.83×10 15 /m 2 to 0.6×10 15 /m 2 . Rough-DA produce a steady nanostructure in α-Zr before PT with smaller crystallite size and larger dislocation density than smooth-DA, leading to a reduction of the minimum pressure for α-ω PT to a record value 0.67 GPa, 9 times smaller than under hydrostatic loading and 5.1 times lower than the phase equilibrium pressure. In addition to strain, the kinetics of strain-induced PT unexpectedly depends on time. Also, strain-controlled part of kinetics is zero order, in contrast to the first-order kinetics with smooth-DA. The obtained results open a new window for understanding the mutual effects of nanostructure evolution and PT during severe plastic flow in various technological and natural processes. In conclusion, they may bring up economic strategies of producing nanocomposites and single-phase nanostructured materials with optimal properties.

Crystalline size↗

Clumping index estimation with 30°-tilted cameras in row crops: Evaluation of methods and segment size effects

The clumping index (CI) quantifies the spatial distribution of foliage elements and is essential for accurately estimating the plant area index (PAI), canopy radiative transfer, and photosynthesis. Traditionally, the finite-length averaging method (LX), the gap size distribution method (CC), and a combined approach of CC and LX (CLX) have been applied to instruments like TRAC and digital hemispherical photography to estimate CI. However, a comprehensive evaluation of these methods in row crops remains limited, especially regarding the influence of segment size on CI. Meanwhile, digital cameras offer a cost-effective and user-friendly solution for canopy measurements in row crops, yet their application in this context remains underexplored. In this study, we employed a new approach using a 30°-tilted digital camera to estimate CI in corn and soybean fields, applying the LX, CC, and CLX methods. We systematically assessed the performance of these three methods by combining field measurements in real-world fields with simulations using the LESS 3D radiative transfer model. Our results showed that CLX applied to the whole image and 45° segment offered accurate estimation of CI (bias within ±0.1, RMSE < 0.2) and PAI (bias within ±0.4, RMSE < 1) in real-world fields and LESS simulations. The accuracy of the LX method was highly sensitive to segment size, with the best performance observed at the 15° segment (PAI bias within ±0.4). In contrast, the CC method remained stable across different segment sizes, and its performance was generally comparable to that of LX, except at the 15° segment. Across view zenith angles, CI derived from CC generally showed a continuous increase, while those from LX and CLX followed a rising trend at small zenith angles but began to decline at 68°, likely due to an increasing proportion of no-gap segments. Seasonally, LX tended to show decreasing CI during early growth stages but increased as the canopy matured, whereas CC and CLX showed gradually increasing CI before plateauing at peak PAI. The 30°-tilted camera effectively captured CI variations across different angles and growth stages, making it a practical and robust instrument for row crop canopy structure analysis. Furthermore, applying these CI methods to digital cameras offers a low-cost and accessible CI estimation alternative, improving canopy structure monitoring accuracy in row crops.

30°-tilted camera↗

The sampling of nanoparticles of MgO formed when doping an oxygen-rich flame with magnesium: The measurement of the concentrations and size-distributions of these nanoparticles

A technique for measuring the concentrations and size-distributions of nanoparticles of the oxide of Mg (and similar elements with involatile oxides), when an oxygen-rich flame is doped with an appropriate metal is considered in detail. For this purpose a well-characterized, premixed, laminar flat flame of C{sub 2}H{sub 2} + O{sub 2} + N{sub 2} was burnt fuel-lean at 1 atm; the final steady temperature in the burned gas was 2000{+-}30 K. An aqueous solution of, e.g., MgCl{sub 2} was nebulized as a fine spray into the unburned gas fed to the burner, so that the total concentration of Mg atoms in the flame was finally {proportional_to}13 p.p.m. A very pale white turbidity indicated that particles (in fact of MgO) form very quickly in the flame's reaction zone. The technique involved sampling the flame through a hole at the tip of a conical quartz probe. The sample was supersonically expanded to a lower pressure and then diluted; some of the resulting gas was passed into a particle sizer, which measured the concentrations and sizes of the particles from their differential mobilities. This study reports particle size distributions (PSDs) and number densities as measured for different sizes of the sampling orifice, for different dilutions of the sample, and for various pressures inside the probe. In general, it was found that a PSD can be falsified by nanoparticles agglomerating in the sampling line. Such falsification of the measurements can be minimized by(i)Ensuring that the sample of flame gas is diluted as quickly as possible with a large flow of particle-free nitrogen. However, care has to be taken to avoid turbulence in the probe and sampling lines, as well as the consequential deposition of nanoparticles on the walls. (ii)Maintaining a low pressure (<0.5 bar) inside the sampling probe and lines, so that the flow through the sampling orifice is choked and also the collision frequency is low enough for there to be no agglomeration of particles. To achieve a rapid reduction in pressure with minimal disturbance of the flame, a conical probe is desirable. (iii)Sampling a flame through an orifice wider than 0.3 mm to ensure that only a small fraction of the MgO particles are deposited on the quartz around the sampling hole. (iv)Reducing the deposition of particles inside the probe by using cooling water at 90 C. If these guidelines are followed, the sampling of nanoparticles becomes quantitative, in that to within {+-}40% every particle of MgO entering the sampling system is detected. (author)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ observations of reacting Al/Fe 2 O 3 thermite: Relating dynamic particle size to macroscopic burn time

Time-resolved x-ray imaging is used to capture high-resolution images of the Al/Fe 2 O 3 thermite reaction as it proceeds in an extended burn tube. The observed thermite reaction products are generally large, multi-phase composite particles. Image processing algorithms are developed to extract a continuous record of composite particle size as a function of time and distance from the ignition point. Small particles are observed immediately after ignition, followed by a rapid increase in particle size and a gradual decline toward late times. Correlating the dynamic particle size with visible light emission from the reaction, we propose a two-stage mechanism where the combination of early ignition and delayed expansion causes the material closest to the ignition point to undergo substantial coalescence before it begins moving down the tube. We also identify two mechanisms that may contribute to particle size refinement at late times, both based on the collapse of large gas bubbles that are observed preferentially in particles at earlier times. A new approach to extracting burn times from luminous intensity data is explored, and we find that a more nuanced analysis of burn time and luminous intensity may help to improve reactivity assessments when data from in situ studies is unavailable.

36 MATERIALS SCIENCE↗

Circumacenes versus periacenes: HOMO-LUMO gap and transition from nonmagnetic to magnetic ground state with size

Circumacenes and periacenes as zigzag-edged nanographenes differ only in that circumacenes have one extra benzene ring on each of the two armchair sides. Using first principles density functional theory, we show that this slight difference in the boundary shape dramatically affects the critical size at which the open-shell antiferromagnetic state supersedes the closed-shell nonmagnetic state as the ground state. We correlate this critical size to the decreasing HOMO-LUMO gap with the molecular size and discuss implications of the critical size for experimental syntheses of circumacenes and periacenes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Regulation of hair cell and stomatal size by a hair cell-specific peroxidase in the grass Brachypodium distachyon

The leaf epidermis is the outermost cell layer forming the interface between plants and the atmosphere that must both provide a robust barrier against (a)biotic stressors and facilitate carbon dioxide uptake and leaf transpiration. To achieve these opposing requirements, the plant epidermis developed a wide range of specialized cell types such as stomata and hair cells. While factors forming these individual cell types are known, it is poorly understood how their number and size is coordinated. Here, in this study, we identified a role for BdPRX76/BdPOX, a class III peroxidase, in regulating hair cell and stomatal size in the model grass Brachypodium distachyon. In bdpox mutants prickle hair cells were smaller and stomata were longer. Because stomatal density remained unchanged, the negative correlation between stomatal size and density was disrupted in bdpox and resulted in higher stomatal conductance and lower intrinsic water-use efficiency. BdPOX was exclusively expressed in hair cells suggesting that BdPOX cell autonomously promotes hair cell size and indirectly restricts stomatal length. Cell wall autofluorescence and lignin stainings indicated a role for BdPOX in lignification or crosslinking of related phenolic compounds at the hair cell base. Ectopic expression of BdPOX in the stomatal lineage increased phenolic autofluorescence in guard cell walls and restricted stomatal elongation in bdpox. Together, we highlight a developmental interplay between hair cells and stomata that optimizes epidermal functionality. We propose that cell-type-specific changes disrupt this interplay and lead to compensatory developmental defects in other epidermal cell types.

59 BASIC BIOLOGICAL SCIENCES↗

Prenatal exposure to mixtures of persistent endocrine disrupting chemicals and postnatal body size in British girls

Endocrine disrupting chemical (EDC) exposure is ubiquitous. EDC exposure during critical windows of development may interfere with the body's endocrine system, affecting growth. Previous human studies have examined one EDC at a time in relation to infant growth. By studying mixtures, the human experience can be better approximated. We investigated the association of prenatal exposure to persistent EDCs (per- and polyfluoroalkyl substances (PFAS), polychlorinated biphenyls (PCBs), and organochlorine pesticides (OCPs)) as mixtures with postnatal body size among female offspring. We used a sub-sample of the Avon Longitudinal Study of Parents and Children (N = 425), based in the United Kingdom. We quantified 52 EDCs in maternal serum collected during pregnancy. We used Bayesian kernel machine regression with a random intercept to examine the association of prenatal concentrations of EDC mixtures with longitudinal postnatal body size measures for each EDC class separately (PFAS, PCBs, and OCPs) and for all three classes combined. Weight and height measures at 0, 2, 9, and 19 months were obtained by health professionals as part of routine child health surveillance. The mixture representing all three classes combined (31 chemicals) (n = 301) was inversely associated with postnatal body size. Holding all EDCs in the 31-chemical mixture at the 75th percentile compared to the 50th percentile was associated with 0.15 lower weight-for-age z-score (95% credible interval –0.26, –0.03). Weak inverse associations were also seen for height-for-age and body mass index-for-age scores. Furthermore, these results suggest that prenatal exposure to mixtures of persistent EDCs may affect postnatal body size.

59 BASIC BIOLOGICAL SCIENCES↗

Prediction of the effects of size and morphology on the structure of water around hematite nanoparticles

Compared with macroscopic surfaces, the structure of water around nanoparticles is difficult to probe directly. We used molecular dynamics simulations to investigate the effects of particle size and morphology on the time-averaged structure and the dynamics of water molecules around two sizes of hematite ({alpha}-Fe{sub 2}O{sub 3}) nanoparticles. Interrogation of the simulations via atomic density maps, radial distribution functions and bound water residence times provide insight into the relationships between particle size and morphology and the behavior of interfacial water. Both 1.6 and 2.7 nm particles are predicted to cause the formation of ordered water regions close to the nanoparticle surface, but the extent of localization and ordering, the connectivity between regions of bound water, and the rates of molecular exchange between inner and outer regions are all affected by particle size and morphology. These findings are anticipated to be relevant to understanding the rates of interfacial processes involving water exchange and the transport of aqueous ions to surface sites.

54 ENVIRONMENTAL SCIENCES↗

Cobalt nanoparticles confined in carbon matrix for probing the size dependence in Fischer-Tropsch synthesis

The size effect of the metallic Co (Co 0 ) over supported catalysts for Fischer-Tropsch synthesis (FTS) has imposed great importance for developing a high-performance catalyst. However, the lack of well-structured catalysts makes the clarification of the intrinsic size-dependence of Co 0 still a challenge. In this work, the Co/C catalysts with Co 0 particles from 8.4 ± 1.9 to 74.8 ± 11.6 nm were synthesized by well-controlled pyrolysis of ZIF-67. Based on different characterizations, Co/C catalysts via pyrolyzing ZIF-67 above 450 °C were confirmed as Co0 entrapped in partially graphitized carbon matrix polished by a certain amount of pyridinic and graphitic N and a small portion of adsorbed oxygen. Without the limitation of high-temperature reduction and the dispersion-reducibility dependence, the intrinsic size effect of Co 0 on the activity and product selectivity of FTS was rigorously revealed, and the critical size was determined to be 10.5 ± 1.9 nm.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Numerical study of the effect of propped surface area and fracture conductivity on shale gas production: Application for multi-size proppant pumping schedule design

Hydraulic fracturing is a technique extensively used in the oil and gas industry, where water, proppant (sand) and additives are injected into unconventional reservoirs to enhance the recovery of shale hydrocarbon. Although some previous studies have developed pumping schedules that maximize gas production for a single-size proppant, there are very few studies that consider the effect of varying proppant diameters across pumping stages on shale gas production. Motivated by this, we carried out an extensive sensitivity analysis to determine the effect of different proppant diameters on the average fracture conductivity (FC), average propped surface area (PSA) and cumulative shale gas production volume. We found out that the cumulative shale gas production volume depends on both the average PSA and average FC. We also found out that small-diameter proppant resulted in higher average PSA and lower average FC, whereas large-diameter proppant resulted in lower average PSA and higher average FC. Hence, we designed a multi-size proppant pumping schedule considering both of these parameters into account for simultaneously propagating multiple fractures to maximize shale gas production from unconventional reservoirs. Since the size of injected proppant particles determines the average PSA and average FC for the propped hydraulic fractures, we developed a novel framework called Sequentially Interlinked Modeling Structure (SIMS) to predict the average PSA, average FC and cumulative shale gas production volume at the end of 10 years for a given pumping schedule. Then, we used this SIMS framework to obtain a multi-size proppant pumping schedule that maximizes shale gas production. In closing, we demonstrated that the obtained pumping schedule gives a cumulative shale gas production volume greater than the values obtained from the existing pumping schedules.

03 NATURAL GAS↗

Aperture size distribution, length, and preferential location of bed-parallel veins in shale

Bed-parallel, calcite-filled veins (BPVs) are common in shale formations, and although they have been widely described in other studies, little is known about their population aperture size distribution. To address this knowledge gap, we analyzed BPV sizes in outcrops and cores from the Vaca Muerta Formation, Neuquén Basin, Argentina; in two cores from the Marcellus Formation, Appalachian Basin, northeast Pennsylvania; and in one core from the Wolfcamp Shale, Delaware Basin, West Texas. Nine out of ten aperture size populations follow a negative exponential distribution, with one following a weak power law. Bed-parallel vein size distribution and intensity vary among formations and within the same shale. We define three groups of distributions: (1) Vaca Muerta outcrops, with the highest BPV intensity and the largest BPVs (cumulative frequency of 4.9 BPVs per meter [BPVs/m] for apertures 0.265 mm to 8.7 cm); (2) Vaca Muerta cores with a similar BPV intensity overall but with no apertures wider than 1.2 cm; and (3) Vaca Muerta, Wolfcamp, and Marcellus cores with the fewest BPVs (cumulative frequency up to 0.63 BPVs/m) and very few wider than 1 cm. Aperture and length in two outcrop data sets are weakly positively correlated and follow power laws with exponents of 0.44 and 0.49. Mechanical interfaces at boundaries between different lithologies exert a strong control on BPV location, with 65–75% of observed interfaces having BPVs along them. Only 25–30% of the BPVs occur at observed material interfaces, however, and unless subtle, unobserved mechanical layering is present, other factors must also control location. BPV intensity and organic richness (TOC) from Vaca Muerta well logs are correlated in some instances but not in others, indicating TOC is not always a good proxy for BPV location or intensity. Furthermore, these findings provide useful information for modeling of hydraulic fracture treatments where BPVs may influence development of the stimulated fracture network, for example by limiting height growth.

58 GEOSCIENCES↗