Tritium retention in reduced-activation ferritic/martensitic steels

Reduced-activation ferritic/martensitic (RAFM) steels are structural material candidates for breeding blankets of future fusion reactors. Therefore, tritium (T) retention in RAFM steels is an important problem in assessing the T inventory of blankets. In this study, specimens of RAFM steels were subjected to irradiation of 20 MeV W ions to 0.54 displacements per atom (dpa), exposure to high flux D plasmas at 400 and 600 K and that to pulsed heat loads. The specimens thus prepared were exposed to DT gas at 473 K. Despite severe modification in the surface morphology, heat loads had negligible effects on T retention. Significant increase in T retention at the surface and/or subsurface was observed after D plasma exposure. However, T trapped at the surface/subsurface layer was easily removed by maintaining the specimens in the air at about 300 K. Displacement damage led to increase in T retention in the bulk due to the trapping effects of defects, and T trapped was stable at 300 K. It was therefore concluded that displacement damages had the largest influence on T retention under the present conditions.

36 MATERIALS SCIENCE↗

Evaluation of Alternate Stainless Steel Surface Treatments for Mass Spectroscopy and Other Tritium Systems

There are specific components in the SRS Tritium Facilities that are required to introduce as few chemical impurities (such as protium and methane) as possible into the process gas. Two such components are the inlet systems for the mass spectroscopy facilities and hydrogen isotope mix standard containers. Two vendors now passivate stainless steel components for these systems, and both are relatively small businesses whose future viability can be questioned, which creates the need for new sources. Stainless steel containers were designed to evaluate alternate surface treatment vendors for tritium storage and handling for these high purity tritium systems. Five vendors applied their own 'best' surface treatments to two containers each - one was a current vendor, another was a chemical vapor deposited silicon coating, and the other three were electropolishing and chemical cleaning vendors. Pure tritium gas was introduced into all ten containers and the composition was monitored over time. The only observed impurities in the gas were some HT, less CT 4 , and very small amounts of T 2 O in all cases. The currently used vendor treated containers contained the least impurities. The chemical vapor deposited silicon treatment resulted in the highest impurity levels. Sampling one set of containers after about one month of tritium exposure revealed the impurity level to be nearly the same as that after more than a year of exposure - this result suggests that cleaning new stainless steel components by tritium gas contact for about a month may be a worthy operation.

03 NATURAL GAS↗

REPORT ON THE EFFECT OF TEMPERATURE AND AMMONIA CONCENTRATION ON A515 CARBON STEEL IN TANK 241 AY 101 SIMULANT

This report documents the results from RPP-PLAN-38676, Effect of Temperature and Ammonia Concentration on A515 Carbon Steel in Tank 241-AY-101 Simulant. The purpose of this test plan was to investigate the simulant formulated for the double-shell tank (DST) 241 AY 101 (AY 101) with the addition of ammonia. The simulant was formulated from the AY-101 condensate surface layer recipe used by CC Technologies{reg_sign} in the investigation of Hanford DST chemistry, under the Expert Panel on Corrosion. AY-101 is constructed from A515 grade 60 steel. The laboratory investigation used a cylindrical corrosion coupon from this steel formulation with a surface area of 5.64 square centimeters.

36 MATERIALS SCIENCE↗

Cast CF8C-Plus Stainless Steel for Turbocharger Applications

The purpose of this Cooperative Research and Development Agreement (CRADA) project is to provide the critical test data needed to qualify CF8C-Plus cast stainless steel for commercial production and use for turbocharger housings with upgraded performance and durability relative to standard commercial cast irons or stainless steels. The turbocharger technologies include, but are not limited to, heavy-duty highway diesel engines, and passenger vehicle diesel and gasoline engines. This CRADA provides additional critical high-temperature mechanical properties testing and data analysis needed to quality the new CF8C-Plus steels for turbocharger housing applications.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Pressureless Sintering of Pre-Alloyed Nanostructured Bainitic Steel Powders

A recent study shows that powder metallurgy and pressureless sintering are a viable pathway to realize full-density bulk components of nanostructure bainitic steels. A scalable, pressureless supersolidus liquid phase sintering (SLPS) approach to process nanostructured bainitic steel is evaluated. Furthermore, to address the oxidation issues associated with the mechanical alloying of elemental powders, powder atomization is used to produce pre-alloyed nanostructured bainitic steel powders.

mechanical alloying↗

Scale formation mechanisms of martensitic steels in high CO{sub 2}/H{sub 2}O-containing gases simulating oxyfuel environments

In oxyfuel power plants, metallic components will be exposed to service environments containing high amounts of CO{sub 2} and water vapour. Therefore, the oxidation behaviour of a number of martensitic 9-12%Cr steels in a model gas mixture containing 70% CO{sub 2}-30% H{sub 2}O was studied in the temperature range 550-700{sup o}C. The results were compared with the behaviour in air, Ar-CO{sub 2} and Ar-H{sub 2}O. It was found that in the CO{sub 2}- and/or H{sub 2}O-rich gases, the mentioned steels tended to form iron-rich oxide scales with significantly higher growth rates than the Cr-rich surface scales formed during air exposure. The iron-rich scales were formed as a result of a decreased flux of chromium in the bulk alloy toward the surface because of enhanced internal oxidation of chromium in the H{sub 2}O-containing gases and carbide formation in the CO{sub 2}-rich gases. Additionally, the presence of water vapour in the exposure atmosphere led to buckling of the outer haematite layer, apparently as a result of compressive oxide growth stresses. The Fe-base oxide scales formed in CO{sub 2}(-H{sub 2}O)-rich gases appeared to be permeable to CO{sub 2} molecules resulting in substantial carburization of the steel.

20 FOSSIL-FUELED POWER PLANTS↗

Tempering and Austempering of Double Soaked Medium Manganese Steels

The addition of a tempering or austempering step to the double soaking of a 0.14C–7.17Mn (wt pct) steel was investigated in the present contribution. The double soaking heat treatment is a two-step intercritical annealing heat treatment, which generates microstructures of athermal martensite, retained austenite and ferrite when applied to medium manganese steels. Microstructures following double soaking and (aus)tempering contained a combination of retained austenite, athermal or tempered martensite, and blocky or bainitic ferrite. X-ray diffraction, dilatometry and transmission Kikuchi diffraction were utilized to investigate microstructural changes which occurred during tempering or austempering. The resulting mechanical properties were measured using uniaxial tensile testing. The double soaking plus tempering heat treatment was shown to generate an ultimate tensile strength of 1,340 MPa in combination with 28 pct total elongation while the double soaking plus austempering heat treatment resulted in an ultimate tensile strength of 1,675 MPa and total elongation of 22 pct. Overall, both novel heat treatments produced a combination of strength and ductility desired for the third generation of advanced high strength steels.

36 MATERIALS SCIENCE↗

Alloy Partitioning Effect on Strength and Toughness of κ-Carbide Strengthened Steels

Alloy partitioning during heat treatment in a lightweight precipitation hardened steel was investigated using transmission electron microscopy and atom probe tomography. The mechanical properties are discussed as a function of the effect of solution treatment temperature and aging time, giving rise to variations in chemical modulation. A wrought lightweight steel alloy with a nominal composition of Fe-30Mn-9Al-1Si-1C-0.5Mo (wt. %) was solution-treated between 1173–1273 K and aged at 773 K. Lower solution treatment temperatures retained a finer grain size and accelerated age hardening response that also produced an improved work hardening behavior with a tensile strength of -1460 MPa at 0.4 true strain. Atom probe tomography indicated these conditions also had reduced modulation in the Si and Al content due to the reduced aging time preventing silicon from diffusing out of the κ-carbide into the austenite. This work provides the framework for heat-treating lightweight, age hardenable steels with high strength and improved energy absorption.

36 MATERIALS SCIENCE↗

Methods of Measuring Residual Stresses in Additively Manufactured 316L Stainless Steel

The microstructure of AM 316L stainless steel Is different from steel manufactured using conventional methods e.g. casting and forging. Data on the effects of residual stresses in the structural integrity and importance of AM parts (fatigue behavior) must be quantified. Evaluate different methods and identify a viable process for determining residual stresses in 316L stainless steel. Next step is to conduct measurements of residual stresses of samples fabricated by different manufacturers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Precipitation and mechanical properties of Nb-modified ferritic stainless steel during isothermal aging

The influence of isothermal aging on precipitation behavior and mechanical properties of Nb-modified ferritic stainless steel was investigated using Thermo-calc software, scanning electron microscopy and transmission electron microscopy. It was observed that TiN, NbC and Fe{sub 2}Nb formed in the investigated steel and the experimental results agreed well with the results calculated by Thermo-calc software. During isothermal aging at 800 deg. C, the coarsening rate of Fe{sub 2}Nb is greater than that of NbC, and the calculated average sizes of NbC and Fe{sub 2}Nb of the aged specimen agreed with the experimental results. In addition, the tensile strength and micro-hardness of the ferritic stainless steel increased with increased aging time from 24 h to 48 h. But aging at 800 deg. C for 96 h caused the coarsening of the precipitation, which led to a decrease of tensile strength and micro-hardness.

36 MATERIALS SCIENCE↗

Thermal Aging Degradation of Cast Stainless Steels in LWR Systems

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of light water reactor (LWR) power plants such as primary coolant piping and pump casing. Since a large number of massive CASS components are installed in every modern nuclear power plant, any significant degradation of CASS components will raise serious concerns on the integrity of the entire power plant. Upon the presumption that the replacement cost of such massive components is prohibitive, therefore, thorough scientific understanding and systematic monitoring the thermal aging degradation of CASS components should be essential requirements for assessing the plant safety. In the past few decades many researches have concluded that the formation of Cr-rich α-phase by Spinoidal decomposition of δ-ferrite phase, which is formed in high temperature region during cooling, is the primary mechanism for the thermal embrittlement. Cracking mechanism in the thermally-embrittled duplex stainless steels consists of cleavage initiation at ferrite and crack propagation via separation of ferrite-austenite interphase. It has been known, however, that such thermal aging embrittlement is observed only in accelerated aging conditions and the cast stainless steel grades used in nuclear plants have performed well without experiencing real embrittlement. It has been speculated that long-term thermal aging for ≥ 60 years could lead to further decomposition of designed phases and increase of precipitation. This will result in significantly increased susceptibility to embrittlement or other degradation due to thermal aging-radiation synergistic effect, irradiation-induced degradation, stress-corrosion cracking, and general corrosion. Currently, therefore, the thermal embrittlement of CASS components is one of the most serious concerns for extended operation of nuclear power plants. A scientific research is underway to address the issues related to the thermal aging degradation of CASS components. The research aims to provide knowledge-based conclusive prediction for the integrity of the CASS components of LWR power plants during extended operation up to and beyond 60 years. This presentation intends to provide an introductory overview on the thermal aging phenomena in LWR relevant conditions and discussion on the measurements of mechanical property degradation after accelerated and LWR relevant thermal aging treatments. First, the thermal aging effect on toughness is discussed in terms of the causes of embrittlement and influential parameters. Second, the talk will include a comprehensive discussion on the thermal aging effects in different CASS grades (i.e., CF3, CF3M, CF8, and CF8M), which will focus on the influence of alloying elements such as molybdenum and carbon. Third, approximate analysis on thermal reaction in CASS was carried out using Arrhenius equation to decide the effective temperature range for accelerated aging experiments to simulate 60 and 80 years of services in limited time frame. The results will provide valuable insights in the degree of thermal aging. Fourth, calculation on equilibrium precipitation was performed for model CASS alloys using the CALPHAD program, and the results will be used to describe the precipitation behaviors in association with the degradation in mechanical properties. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

LIFE ESTIMATION OF HIGH LEVEL WASTE TANK STEEL FOR F-TANK FARM CLOSURE PERFORMANCE ASSESSMENT - 9310

High level radioactive waste (HLW) is stored in underground carbon steel storage tanks at the Savannah River Site. The underground tanks will be closed by removing the bulk of the waste, chemical cleaning, heel removal, stabilizing remaining residuals with tailored grout formulations, and severing/sealing external penetrations. The life of the carbon steel materials of construction in support of the performance assessment has been completed. The estimation considered general and localized corrosion mechanisms of the tank steel exposed to grouted conditions. A stochastic approach was followed to estimate the distributions of failures based upon mechanisms of corrosion accounting for variances in each of the independent variables. The methodology and results used for one-type of tank is presented.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

HYDROGEN EFFECTS ON FRACTURE TOUGHNESS OF TYPE 316L STAINLESS STEEL FROM 175 K TO 425 K

The effects of hydrogen on the fracture-toughness properties of Type 316L stainless steel from 175 K to 425 K were measured. Fracture-toughness samples were fabricated from Type 316L stainless steel forgings and hydrogen-charged with hydrogen at 34 MPa and 623 K for two weeks prior to testing. The effect of hydrogen on the J-Integral vs. crack extension behavior was measured at various temperatures by fracturing non-charged and hydrogen-charged samples in an environmental chamber. Hydrogen-charged steels had lower toughness values than non-charged ones, but still retained good toughness properties. The fracture-toughness values of hydrogen-charged samples tested near ambient temperature were about 70% of non-charged values. For hydrogen-charged samples tested at 225 K and 425 K, the fracture-toughness values were 50% of the non-charged values. In all cases, fracture occurred by microvoid nucleation and coalescence, although the hydrogen-charged samples had smaller and more closely spaced microvoids. The results suggest that hydrogen effects on toughness are greater at 225 K than they are at ambient temperature because of strain-induced martensite formation. At 425 K, the hydrogen effects on toughness are greater than they are at ambient temperature because of the higher mobility of hydrogen.

08 HYDROGEN↗

THE SENSITIVITY OF CARBON STEELS' SUSCEPTIBILITY TO LOCALIZED CORROSION TO THE PH OF NITRATE BASED NUCLEAR WASTES

The Hanford tank reservation contains approximately 50 million gallons of liquid legacy radioactive waste from cold war weapons production, which is stored in 177 underground storage tanks. The tanks will be in use until waste processing operations are completed. The wastes tend to be high pH (over 10) and nitrate based. Under these alkaline conditions carbon steels tend to be passive and undergo relatively slow uniform corrosion. However, the presence of nitrate and other aggressive species, can lead to pitting and stress corrosion cracking. This work is a continuation of previous work that investigated the propensity of steels to suffer pitting and stress corrosion cracking in various waste simulants. The focus of this work is an investigation of the sensitivity of the steels' pitting and stress corrosion cracking susceptibility tosimulant pH. Previous work demonstrated that wastes that are high in aggressive nitrate and low in inhibitory nitrite are susceptible to localized corrosion. However, the previous work involved wastes with pH 12 or higher. The current work involves wastes with lower pH of 10 or 11. It is expected that at these lower pHs that a higher nitrite-to-nitrate ratio will be necessary to ensure tank integrity. This experimental work involved both electrochemical testing, and slow strain rate testing at either the free corrosion potential or under anodic polarization. The results of the current work will be discussed, and compared to work previously presented.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Laser Welding Characterization of Kovar and Stainless Steel Alloys as Suitable Materials for Components of Photonic Devices Packaging

The weldability of Kovar and stainless steel alloys by Nd:YAG laser beam is studied through changing of some laser beam parameters. It has been found that there is a suitable interaction of the pulsed laser beam of low power laser pulse with both the two alloys. The change of thermophysical properties with absorbed energy from the laser pulse is discussed in this paper which reports the suitability of both Kovar and stainless steel 304 as the base materials for photonic devices packaging. We used laser weld system (LW4000S from Newport) which employs Nd:YAG laser system with two simultaneous beams output for packaging 980 nm high power laser module. Results of changing both laser spot weld width and penetration depth with changing both the pulse peak power density, pulse energy and pulse duration show that there are good linear relationships between laser pulse energy or peak power density and pulse duration with laser spot weld dimensions( both laser spot weld width and penetration depth). Therefore we concluded that there should be an optimization for both the pulse peak power and pulse duration to give a suitable aspect ratio (laser spot width to penetration depth) for achieving the desired welds with suitable penetration depth and small spot width. This is to reduce the heat affected zone (HAZ) which affects the sensitive optical components. An optimum value of the power density in the order of 10{sup 5} w/cm{sup 2} found to be suitable to induce melting in the welded joints without vaporization. The desired ratio can also be optimized by changing the focus position on the target material as illustrated from our measurements. A theoretical model is developed to simulate the temperature distribution during the laser pulse heating and predict the penetration depth inside the material. Samples have been investigated using SEM with EDS. The metallographic measurements on the weld spot show a suitable weld yield with reasonable weld width to depth ratio.

36 MATERIALS SCIENCE↗

Armor for Steel: Facile Synthesis of Hexagonal Boron Nitride Films on Various Substrates

Abstract While hexagonal boron nitride (hBN) has been widely used as a buffer or encapsulation layer for emerging electronic devices, interest in utilizing it for large‐area chemical barrier coating has somewhat faded. A chemical vapor deposition process is reported here for the conformal growth of hBN on large surfaces of various alloys and steels, regardless of their complex shapes. In contrast to the previously reported very limited protection by hBN against corrosion and oxidation, protection of steels against 10% HCl and oxidation resistance at 850 °C in air is demonstrated. Furthermore, an order of magnitude reduction in the friction coefficient of the hBN coated steels is shown. The growth mechanism is revealed in experiments on thin metal films, where the tunable growth of single‐crystal hBN with a selected number of layers is demonstrated. The key distinction of the process is the use of N 2 gas, which gets activated exclusively on the catalyst's surface and eliminates adverse gas‐phase reactions. This rate‐limiting step allowed independent control of activated nitrogen along with boron coming from a solid source (like elemental boron). Using abundant and benign precursors, this approach can be readily adopted for large‐scale hBN synthesis in applications where cost, production volume, and process safety are essential.

2D materials↗

Amphilic Water-Lean Carbon Capture Solvent Wetting Behavior through Decomposition by Stainless-Steel Interfaces

In this work, we report on a combined experimental and theoretical study of the wetting and reactivity of water-lean carbon capture solvents on the surface of common column packing materials. Paradoxically, we find that these solvents are equally able to wet hydrophobic and hydrophilic surfaces. The solvents are amphiphilic and are able to adapt to any interfacial environment due to their inherent heterogeneous molecular structure. Ab initio molecular dynamics indicates that these structures enable the formation of a strong adlayer on the surface of hydrophilic surfaces like oxidized steel which promotes solvent decomposition akin to hydrolysis from surface oxides and hydroxides. This decomposition passivates the surface, making it effectively hydrophobic, and the decomposed solvent promotes leaching of the iron into the bulk fluid. This study links the wetting behavior to the observed corrosion of the steels via decomposition of solvent at steel interfaces. The overall affect is strongly dependent on the chemical composition of the solvent, in that amines are stable, whereas imines and alcohols are not. We also observed that plastic packing shows little to no solvent degradation, but an equal degree of wetting.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗