Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PROTECTIVE COATING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

Static measurement of the thickness of the ablative coating of the solid rocket boosters

The Solid Rocket Boosters (SRB's) used to launch the Space Shuttle are coated with a layer of ablative material to prevent thermal damage when they reenter the earth's atmosphere. The coating consists of a mixture of cork, glass, and resin. A new coating (Marshall Convergent Coating, MCC-2) was recently developed that is environmentally complaint. The coating must meet certain minimum thickness standards in order to protect the SRB. The coating is applied by a robot controlled nozzle that moves from the bottom to top, as the rocket part rotates on a table. Several coats are applied, building up to the desired thickness. Inspectors do a limited amount of destructive 'wet' testing. This involves an inspector inserting a rod in the wet coating and removing the rod. This results in a hole that, of course, must be patched later. The material is cured and the thickness is measured. There is no real-time feedback as the coating is being applied. Although this might seem like the best way to control thickness, the problems with 'blowback' (reflected material covering the sensor) are formidable, and have not been solved. After the thermal coating is applied, a protective top coat is applied. The SRB part is then placed in a oven and baked to harden the surface. The operations personnel then measure the thickness of the layer using the Kaman 7200 Displacement Measuring System. The probe is placed on the surface. One person (the inspector) reads the instrument, while another(the technician) records the thickness. Measurements are taken at one foot intervals. After the measurements are taken, the number of low readings is tabulated. If more than 10 percent of the points fall below the minimum value, there is a design review, and the part may be stripped of coating, and a new coating is applied. There is no other analysis.

Harrison, Harry C.↗

Formation of Reversible Solid Electrolyte Interface on Graphite Surface from Concentrated Electrolytes

Interfacial phenomena have always been key determinants for the performance of energy storage technologies. The solid electrolyte interfacial (SEI) layer, pervasive on the surfaces of battery electrodes for numerous chemical couples, directly affects the ion transport, charge transfer and lifespan of the entire energy system. Almost all SEI layers, however, are unstable resulting in the continuous consumption of the electrolyte. Typically, this leads to the accumulation of degradation products on/restructuring of the electrode surface and thus increased cell impedance, which largely limits the long-term operation of the electrochemical reactions. Herein, a completely new SEI formation mechanism has been discovered, in which the electrolyte components reversibly self-assemble into a protective surface coating on a graphite electrode upon changing the potential. In contrast to the established wisdom regarding the necessity of employing the solvent ethylene carbonate (EC) to form a protective SEI layer on graphite, a wide range of EC-free electrolytes are demonstrated for the reversible intercalation/deintercalation of Li+ cations within a graphite lattice, thereby providing tremendous flexibility in electrolyte tailoring for battery couples. This novel finding is broadly applicable and provides guidance for how to control interfacial reactions through the relationship between ion aggregation and solvent decomposition at polarized interfaces.

Environmental Molecular Sciences Laboratory↗

Coatings degradation, section VIII

Vacuum chambers for particle irradiation of thermal control coatings, and testing of paint samples of alkali silicates and methyl silicones

SILICONE↗

Effect of Starting Microstructure on Thermal Properties forAs-Sprayed and Thermally Exposed Plasma-Sprayed YSZ Coatings

Thermal barrier coatings (TBCs) experience thermal gradients, excessive temperature, and high heat flux from hot gases in turbines during service. These extended thermal effects induce sin-tering and significant microstructure changes, which alter the resulting thermal conductivity within the TBCs. In this study plasma-sprayed Yttria Stabilized Zirconia (YSZ) TBCs using dif-ferent starting powders and process parameters were subjected to thermal aging at several tem-peratures and time intervals, after which their thermal conductivity was measured at room tem-perature. The thermal conductivity results are analyzed by introducing the Larson-Miller pa-rameter describing the creep behavior of thermal conductivity increase with annealing tempera-ture and time. One set of selected coatings was also annealed under the same conditions and the thermal conductivity was measured at elevated temperatures. The temperature-dependent ther-mal conductivity data is analyzed and used to predict long-term thermal behavior for general YSZ coating design.

36 MATERIALS SCIENCE↗

Smart Coatings for Launch Site Corrosion Protection

Smart, environmentally friendly paint system for early corrosion detection, mitigation, and healing that will enable supportability in KSC launch facilities and ground systems through their operational life cycles. KSC's Corrosion Technology Laboratory is developing a smart, self-healing coating that can detect and repair corrosion at an early stage. This coating is being developed using microcapsules specifically designed to deliver the contents of their core when corrosion starts.

TechPort Portfolio System↗

Thermal Testing Quality Assurance of 24LCC & 3LCC Electronic Packages

The purpose of this project is to experimentally validate the thermal fatigue life of solder interconnects for a variety of surface mount electronic packages. Over the years, there has been a significant amount of research and analysis in the fracture of solder joints on printed circuit boards. Solder is important in the mechanical and electronic functionality of the component. It is important throughout the life of the product that the solder remains crack and fracture free. The specific type of solder used in this experiment is a 63Sn37Pb eutectic alloy. Each package was manufactured with conformal coating along with and without an underfill material below the device. Conformal coating helps protect the board from environments such as electrostatic discharge and humidity. It is commonly used in broad types of engineering disciplines such as commercial, military, research and development, etc. Conformal coating can also pose a risk for the life of the board because of its high thermal expansion coefficient. This can greatly decrease the life of the product if it regularly sees high temperature variations. This leads to a shorter fatigue life of the solder. The fatigue life is a common mechanical problem in the field of electronic devices. Adding underfill can help increase the fatigue life of the solder. However, applying underfill adds time to manufacturing and production. This ultimately increases the cost per unit. The study of conformal coated printed circuit boards with and without underfill was done on two different surface mount electronic packages. The electronic packages studied were 24 and 3 contact Leadless Ceramic Chips packages. When the package was not underfilled, the coating was allowed to flow underneath. The assembly was analyzed and tested to obtain the best available combination of conformal coating, underfill, and potting to design the most robust and reliable circuit board while keeping in mind certain factors such as cost, manufacturing time, and need. Different types of conformal coatings were considered with and without underfill for each device. 29 of each component were manufactured to have a large sample size and for the sake of individual defects and imperfections. Finite Element Analysis (FEA) was performed by an engineer at Sandia National Laboratories for both Leadless Ceramic Chips. From the FEA results, a test acceleration profile was derived and the number of temperature cycles to fail the solder interconnects were found for three different cases. Experimentation was done as a secondary measure to validate this data to show confidence in the theoretical analysis. Accelerated testing functions as a quality check for the product. Accelerated testing is extremely useful in the research and development phase of engineering. It can save money from the potential of early life defects and the costs that come along with warranties. Accelerated testing makes a weaker design more robust and checks the reliability of a strong design in a shorter period of time. It is extremely helpful in a world where deliverables are in high demand and scheduling is tight. Accelerated testing helps the engineer gain an understanding of what needs to be improved and what works well. There are many different types of accelerated tests. Our circuit boards were accelerated inside a closed thermal chamber because of the high number of use cycles. The ultimate goal of this experimentation is to help identify what will prevent any premature cracking or fracturing in the solder alloy. It is important to understand that underfilling each component may or may not be needed. If underfill is not needed, there are several production benefits.

42 ENGINEERING↗

Radiometry Research

Vortex arc studies, solar flux and spectral measurements, spacecraft coatings, solar simulation studies, and solar cell radiation effects testing

TEMPERATURE CONTROL↗

Testing of Environmentally Preferable Aluminum Pretreatments and Coating Systems for Use on Space Shuttle Solid Rocket Boosters (SRB)

The solid rocket booster (SRB) has historically used a chromate conversion coating prior to protective finish application. After conversion coating, an organic paint system consisting of a chromated epoxy primer and polyurethane topcoat is applied. An overall systems approach was selected to reduce waste generation from the coatings application and removal processes. While the most obvious waste reduction opportunity involved elimination of the chromate conversion coating, several other coating system configurations were explored in an attempt to reduce the total waste. This paper will briefly discuss the use of a systems view to reduce waste generation from the coating process and present the results of the qualification testing of nonchromated aluminum pretreatments and alternate coating systems configurations.

Clayton, C.↗

A View of Compatible Heat-Resistant Alloy and Coating Systems at High-Temperatures

Conventional and advanced coatings were reviewed, and it was pointed out that the coated Ni-base superalloys decreased their creep rupture life significantly at higher temperatures, and the advanced high strength superalloy became more remarkably. Concept of diffusion barrier coating system (DBC system) and their formation process was introduced, and the results obtained for several heat-resistant alloys, stainless steel (SUS310S), Ni-Mo base alloy (Hastelloy-X), and 4{sup th} generation single crystal superalloy (TMS-138) were given. It was noted that creep-rupture life of the SUS310S and Hastelloy-X with the DBC system became longer than those of the bare alloys with or without conventional {beta}-NiAl coatings. This is due to slow creep-deformation of the Re-base alloy layer as the diffusion barrier. A novel concept based on combination of superalloys and coatings was proposed, by taking both the materials science and corrosion science into consideration.

36 MATERIALS SCIENCE↗