At least 991 records · Page 55

Microstructure and mechanical properties of FeCrAl alloys under heavy ion irradiations

FeCrAl ferritic alloys are excellent cladding candidates for accident tolerant fuel systems due to their high resistance to oxidation as a result of formation of a protective Al 2 O 3 scale at high temperatures in steam. In this study, we report the irradiation response of the 10Cr and 13Cr FeCrAl cladding tubes under Fe 2+ ion irradiation up to ~16 dpa at 300 °C. Dislocation loop size, density and characteristics were determined using both two beam bright field transmission electron microscopy and on-zone scanning transmission electron microscopy techniques. 10Cr (C06M2) tube has a lower dislocation density, larger grain size and a slightly weaker texture compared to the 13Cr (C36M3) tube before irradiation. After irradiation to 0.7 dpa and 16 dpa, the fraction of <100> type sessile dislocations decreases with increasing Cr amount in the alloys. It has been found that there is neither void formation nor α' precipitation as a result of ion irradiations in either alloy. Therefore, dislocation loops were determined to be the only irradiation induced defects contributing to the hardening. Nanoindentation testing before the irradiation revealed that the average nanohardness of the C36M3 tube is higher than that of the C06M2 tube. The average nanohardness of irradiated tube samples saturated at 1.6-2.0 GPa hardening for both tubes between ~3.4 dpa and ~16 dpa. The hardening calculated based on transmission electron microscopy was found to be consistent with nanohardness measurements.

36 MATERIALS SCIENCE↗

Influence of mechanical alloying and extrusion conditions on the microstructure and tensile properties of Low-Cr ODS FeCrAl alloys

Low-chromium (<10%Cr) high strength oxide dispersion strengthened (ODS) FeCrAl alloys are considered promising candidates for accident tolerant fuel cladding in light water fission reactors. These alloys are designed to combine the beneficial high temperature mechanical properties of ODS materials with the exceptionally high temperature oxidation resistance of FeCrAl in comparison to conventional Zr-containing cladding materials, while also providing good mechanical and aqueous corrosion behavior under normal light water reactor operating conditions. The initial (1st generation) ODS FeCrAl alloys combined gas atomized FeCrAl powders with yttria and other oxides for alloying element additions using the mechanical alloying approach. These alloys exhibited low ductility but excellent high temperature tensile strength while maintaining good oxidation resistance at temperatures up to 1400 °C. In an attempt to improve alloy ductility for accident tolerant fuel cladding applications, new low-Cr ODS FeCrAl alloys with decreased oxygen content were developed with the Zr alloying solute already gas atomized into the powder prior to mechanical alloying. The resultant Fe-10Cr-6.1Al-0.3Zr+0.3Y 2 O 3 (106ZY) powders were ball milled for 10, 20, and 40hr followed by consolidation via hot extrusion at temperatures ranging from 900 to 1050 °C. Increasing the mechanical alloying time decreased the resultant grain size and improved high temperature tensile properties. Decreasing the extrusion temperature refined the grain size and subsequently strengthened the ODS FeCrAl 106ZY alloys while lowering the ductility. Scanning transmission electron microscopy (STEM) and energy dispersive spectroscopy (EDS) demonstrated the Zr solute addition effectively sequestered impurity C and N within the matrix. The root mean square (RMS) hardening superposition model for yield strength shows good agreement with experimental results. Errors between predicted and experimental values are discussed within the scope of processing parameters. As a result, these 2nd generation 106ZY alloys show a distinct increase in alloy ductility without sacrificing the high temperature tensile properties characteristic of legacy or 1st generation ODS FeCrAl alloys.

36 MATERIALS SCIENCE↗

The influence of co-doping Ag and Sb on microstructure and thermoelectric properties of PbTe prepared by combining hydrothermal synthesis and melting

Ag and Sb co-doped PbTe (AgPb{sub 18}SbTe{sub 20}) and pure PbTe nanopowders were hydrothermally synthesized. The synthesized nanopowders were heated at 1173-1223 K in vacuum for 5 h followed by a slow cooling. The nanopowders and the bulk samples were characterized by X-ray diffraction and electron microscopy, respectively. Electrical transport properties of the bulk samples were measured from room temperature to {approx}773 K. The results showed that co-doping Ag and Sb into PbTe has significant effects on both the nanopowders and bulk samples. Bulk AgPb{sub 18}SbTe{sub 20} sample showed n-type conduction in the whole temperature range measured, while bulk PbTe sample exhibited a transition from p- to n-type conduction at {approx}500 K. The thermoelectric properties of PbTe were markedly improved after co-doping of Ag and Sb. The AgPb{sub 18}SbTe{sub 20} sample has a dimensionless figure of merit of {approx}0.94 at 723 K. - Graphical abstract: SEM image of the fracture surface of an AgPb{sub 18}SbTe{sub 20} material prepared by combining hydrothermal synthesis and melting. The material has a ZT value of about 0.94 at 723 K.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structural, microstructural and surface properties of a specific CeO{sub 2}-Bi{sub 2}O{sub 3} multiphase system obtained at 600 {sup o}C

Polycrystalline samples of (1-x) CeO{sub 2}-x/2 Bi{sub 2}O{sub 3} phases, where x is the atom fraction of bismuth have been synthesized by the precipitation process and after the thermal treatment at 600 {sup o}C, under air. Samples are first characterized by the X-ray diffraction and scanning electron microscopy. To determine the samples specific surface areas, Brunauer-Emmett-Teller (BET) analyses have been performed. In the composition range 0{<=}x{<=}0.20, a cubic solid solution with fluorite structure is obtained. For compositions x comprised between 0.30 and 0.90, two types of T' (or {beta}') and T (or {beta}) tetragonal phases, similar to the well-known {beta}' or {beta} Bi{sub 2}O{sub 3} metastable structural varieties, are observed. However, the crystal cell volumes of these {beta}' or {beta} Bi{sub 2}O{sub 3} phases increase with the composition x in bismuth: this might be due to the presence of defects or substitution by cerium atoms, in the tetragonal lattices. Using X-ray diffraction profile analyses, correlations between bismuth composition x and crystal sizes or lattice distortions have been established. The solid-gas interactions between these polycrystalline materials and air-CH{sub 4} and air-CO flows have been studied as a function of temperature and composition x, using Fourier transform infrared (FTIR) analyses of the conversions of CH{sub 4} and CO gases into the CO{sub 2} gas. The transformations of CH{sub 4} and CO molecules as a function of time and temperature are determined through the intensities of FTIR CO{sub 2} absorption bands. Using the specific surface areas determined from BET analyses, these FTIR intensities have been normalized and compared. For all bismuth compositions, a low catalytic reactivity is observed with air-CH{sub 4} gas flows, while, for the highest bismuth compositions, a high catalytic reactivity is observed with air-CO gas flows. -- Graphical abstract: Catalytic efficiencies of CeO{sub 2}-Bi{sub 2}O{sub 3}system: catalytic actions on methane (on the left) or carbon monoxide (on the right) of (1-x)CeO{sub 2}-x/2 Bi{sub 2}O{sub 3} samples, as a function of the fraction x, and for fixed temperatures: on the vertical axis, the intensities of CO{sub 2} FTIR absorption bands are reported. Strong efficiency of bismuth rich samples for CO conversion. Display Omitted Research highlights: {yields} Stabilization of metastable polymorph Bi{sub 2}O{sub 3} phases in the mix system [(1-x)CeO{sub 2}+(x/2)Bi{sub 2}O{sub 3}] at 600 {sup o}C. {yields} Solid gas interactions between this system and air-CO or air-CH{sub 4} gas flows at various temperatures and bismuth compositions. {yields} High efficiency of bismuth rich samples to convert CO into CO{sub 2}.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of duplex stainless steel subjected to hydrostatic extrusion

The nanostructure and mechanical properties of ferritic-austenitic duplex stainless steel subjected to hydrostatic extrusion were examined. The refinement of the structure in the initial state and in the two deformation states (ε = 1.4 and ε = 3.8) was observed in an optical microscope (OM) and a transmission electron microscope (TEM). The results indicate that the structure evolved from microcrystalline with a grain size of about 4 μm to nanocrystalline with a grain size of about 150 nm in ferrite and 70 nm in austenite. The material was characterized mechanically by tensile tests performed in the two deformation states. The ultimate strength appeared to increase significantly compared to that in the initial deformation stages, which can be attributed to the grain refinement and plastic deformation. The heterogeneity observed in microregions results from the dual-phase structure of the steel. The results indicate that hydrostatic extrusion is a highly potential technology suitable for improving the properties of duplex steels. - Highlights: • Duplex stainless steel was hydro extruded to a total strain of 3.8 • After the last stage of deformation heterogeneous structure was obtained in the material • As a result of stresses non-diffusive transformation γ→α’ occurred in the material • Nanometric (sub)grains were obtained in the austenite regions.

36 MATERIALS SCIENCE↗

Influence of annealing temperature on microstructure and tensile property of cold-rolled Fe-0.2C-11Mn-6Al steel

To fully realize the potential of austenite characterized by strip-like and equiaxed structure and enhance the comprehensive mechanical properties of medium-Mn steel, the as-hot-rolled Fe-0.2C-11Mn-6Al steel was subjected to cold roll annealing to refine the grain size. The ultimate tensile strength of the cold-rolled steel annealed at 650 °C was significantly enhanced, while the total elongation was markedly decreased. The variation in tensile properties of the annealed cold-rolled steel was due to weakening of transformation induced plasticity (TRIP) effect and enhanced twinning induced plasticity (TWIP) effect with increase in quenching temperature. Furthermore, austenite had two different morphologies, strip-like and granular. Though the grain size of granular austenite increased with increased annealing temperature, the austenite stability increased with increase in quenching temperature, which is contrary to the expectations. This is attributed to refinement of large austenite strips induced by recrystallization.

36 MATERIALS SCIENCE↗

Effect of post annealing on microstructure and mechanical properties in Ni-free N-containing ODS steel

The precipitation behaviour of Y2O3 and MnO nanoparticles after isothermal treatment, in a Ni-free N-containing oxide dispersion strengthened (ODS) steel was studied by wide-angle X-ray scattering (WAXS), ultra-small-angle and small-angle X-ray scattering (USAXS/SAXS), small angle neutron scattering (SANS) and scanning transmission electron microscopy (STEM). Mechanical properties were investigated via tensile and micro-hardness testing. Additional precipitation occurred during annealing, in addition to the precipitates formed during sintering. The highest volume distribution of Y2O3, with average size of 6 nm, was determined by alloy contrast variation (ACV) analysis of SAXS and SANS for the sample annealed at 800 °C; this sample shows the highest hardness and ultimate tensile strength. Above that temperature, coarsening of both matrix and precipitates and depletion of nitrogen from matrix degraded the mechanical properties. The very fine nanoparticles and thermally induced dissolution of nitrogen influenced mechanical properties.

alloy contrast variation (ACV)↗

Microstructure development and properties of micro-alloyed copper, Cu-0.3Zr-0.15Ag, produced by electron beam additive manufacturing

A micro-alloyed copper powder, Cu-0.3Zr-0.15Ag wt.%, was produced using gas atomization reaction synthesis. Zirconium was added to copper to sequester the oxygen present as copper oxide surface films on the powder particles. The as-received powders, as well as the intentionally oxidized powders were used to fabricate solid test articles by electron beam powder bed fusion additive manufacturing. Dense samples fabricated from as-received powder demonstrated nominal UTS, yield, and elongation values at 260 MPa, 150 MPa, and 34%, respectively. The average electrical conductivity of these samples was measured at 95% of the international annealed copper standard (IACS). Samples fabricated from the oxidized powder exhibited nominal UTS, yield, and elongation of 241 MPa, 146 MPa, and 43%, respectively, with an electrical conductivity of 95 % IACS. During characterization, it was observed that, rather than forming nano-scale dispersoids, the Zirconia (ZrO 2 ) appeared as discontinuous stringers in the metallographic cross-sections that crossed grain and melt pool boundaries. This was rationalized by tracing the presence of the micro-alloying addition of elemental zirconium, which was found to react with surface oxides dissociated in the melt pool to form ZrO 2 , which then solidified on the surface of the melt pool through an allotropic transformation to monoclinic ZrO 2 in discontinuous films and spheroids ranging in size from nanometers to microns. This was confirmed by microscopic analysis of the tops of the melt pools. On subsequent melt passes, these ZrO 2 structures were displaced and redistributed within the melt pool.

36 MATERIALS SCIENCE↗