Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNESIUM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

Grain size dependence of dynamic mechanical behavior of AZ31B magnesium alloy sheet under compressive shock loading

The effects of grain size on the dynamic deformation behavior of rolled AZ31B alloy at high strain rates were investigated. Rolled AZ31B alloy samples with grain sizes of 6, 18 and 37 μm, were subjected to shock loading tests using Split Hopkinson Pressure Bar at room temperature and at a strain rate of 1100 s{sup −} {sup 1}. It was found that a double-peak basal texture formed in the shock loaded samples. The strength and ductility of the alloy under the high strain-rate compressive loading increased with decreasing grain size. However, twinning fraction and strain hardening rate were found to decrease with decreasing grain size. In addition, orientation imaging microscopy showed a higher contribution of double and contraction twins in the deformation process of the coarse-grained samples. Using transmission electron microscopy, pyramidal dislocations were detected in the shock loaded sample, proving the activation of pyramidal slip system under dynamic impact loading. - Highlights: • A double-peak basal texture developed in all shock loaded samples. • Both strength and ductility increased with decreasing grain size. • Twinning fraction and strain hardening rate decreased with decreasing grain size. • ‘g.b’ analysis confirmed the presence of dislocations in shock loaded alloy.

36 MATERIALS SCIENCE↗

Effect of high content of manganese on microstructure, texture and mechanical properties of magnesium alloy

Highlights: • Extremely refined Mg-3.0Mn alloys are prepared by conventional extrusion process. • Mn addition can effectively weaken the basal texture of the alloys. • Strength, yield anisotropy and ductility have been obviously improved. - Abstract: In the present investigation, microstructure, texture and mechanical properties of Mg-3Mn alloys fabricated by hot extrusion process with the extrusion temperatures of 250 °C and 300 °C were investigated. The results revealed that the samples exhibited the refined microstructure and weakened basal texture. Refined microstructure of the samples was attributed to the dynamic precipitates suppressing the recrystallization grain growth during extrusion process. Weakened basal texture of the samples was explained as a result of particle stimulated nucleation (PSN) promoted by coarsened Mn precipitates altering the texture of extruded profiles during recrystallization by orienting the c-axis of grains at an angle that favors basal slip activity. As a result, the samples exhibited the high tensile elongation and good yield strength at room temperature.

36 MATERIALS SCIENCE↗

Evaluation of Zn-rich coatings for IMC reaction control in aluminum-magnesium dissimilar welds

Highlights: • Thermodynamic and diffusion simulations have estimated the Zn conc. required to change the IMC reaction in Al-Mg dissimilar welding. • The selected coating alloy was effective in changing the Al-Mg reaction path by forming τ-(Al,Zn){sub 49}Mg{sub 32} as a substitute for β-Al{sub 3}Mg{sub 2}. • Refill™ friction stir spot welds produced with the coating alloy exhibited a thinner reaction layer and an increase in lap shear strength. - Abstract: The dissimilar welding of Al to Mg is very challenging owing to the rapid formation of an intermetallic (IMC) reaction layer at the joint interface, typically comprised of the binary phases γ-Al{sub 12}Mg{sub 17} and β-Al{sub 3}Mg{sub 2}. A potential metallurgical solution has been explored that aimed to change the reaction path by using Al-Zn alloy coatings to promote alternative IMCs with a slower growth rate. To determine the optimum composition for the coating, combined CALPHAD thermodynamic calculations and diffusion simulations were used to estimate the minimum Zn concentration (20 at.%) required to suppress the formation of the faster growing Al{sub 3}Mg{sub 2} phase. This prediction was verified by both static diffusion and Refill™ friction stir spot welding (FSSW) experiments. In each case the selected coating alloy was effective in changing the Al-Mg reaction path by forming the τ-(Al,Zn){sub 49}Mg{sub 32} phase as a substitute for β-Al{sub 3}Mg{sub 2}. However, in static heat treatments there was no reduction in the IMC reaction layer thickness due to the new phase having similar growth kinetics to the β-Al{sub 3}Mg{sub 2} phase it replaced. Nevertheless, Refill™ friction stir spot welds prepared with the new AL-Zn coating alloy exhibited a thinner reaction layer and an increase in lap shear strength. This benefit was attributed to the Zn addition reducing the joint interface liquation temperature, which resulted in a lower peak weld temperature and less IMC reaction; although an increase in local eutectic melting limited the improvement observed.

36 MATERIALS SCIENCE↗

Effects of Mg-Al-O-Mn-S inclusion on the nucleation of acicular ferrite in magnesium-containing low-carbon steel

Highlights: • We redefine the mechanism of AF nucleation from Gibbs free energy of nucleation. • Complex inclusions present a better ability of inducing AF formation due to the Mn-depleted zone. • The lattice misfit and the thermal strain are calculated in this study. - Abstract: The effects of inclusion size and chemical composition on acicular ferrite (AF) nucleation and possible nucleation mechanisms were discussed. With the use of low-carbon structure steel containing 13 ppm Mg, the chemical composition and size of inclusions were quantified by scanning electron microscopy combined with an energy dispersive spectroscopy system. Results showed that the complex inclusions MgO-MnS and MgO-Al{sub 2}O{sub 3}-MnS are the most effective inclusions for inducing AF nucleation in Mg-containing A36, and their probabilities of AF nucleation are 35.8% and 41.4%, respectively. Moreover, the inclusion size in the range of 1–2 μm exhibits the most remarkable ability to induce AF formation. AF nucleates at the interface of MgO and MgO-Al{sub 2}O{sub 3} because of the low lattice misfit with AF. Complex inclusions, such as MgO-MnS and MgO-Al{sub 2}O{sub 3}-MnS, present a better ability of inducing AF formation than that of MnS due to the Mn-depleted zone.

36 MATERIALS SCIENCE↗

Strengthening mechanisms, hardening/softening behavior, and microstructure evolution in an LPSO magnesium alloy at elevated temperatures

Here, rapid degradation of the mechanical properties of conventional Mg alloys with temperature precludes their wide application in industry. The LPSO (long period stacking ordered) Mg alloys, on the other hand, show considerable potential to achieve excellent high-temperature mechanical performance. In this study, a Mg-5.1Y-2.4Zn (wt.%) extrusion alloy with the microstructure comprising of α-Mg matrix and LPSO phase was prepared. It is shown that the yield strength of the alloy at 200 °C retained ~83% of the yield strength of 198 MPa at room temperature (RT). Importantly, the ductility also improved, owing to the increased non-basal slip activities at elevated temperatures. In contrast to RT and 200 °C, the alloy exhibited softening tensile behavior with an apparent loss of yield strength at 300 °C. In-situ lattice strain analysis revealed that load transfer from α-Mg to LPSO remains effective at temperatures up to 200 °C, governing the high yield strength of the alloy. The post-mortem analysis by means of electron microscopy confirmed that the LPSO phase is structurally stable at 200 °C. In particular, the high strain hardenability is rationalized by the sandwiched LPSO structures together with stacking faults serving as effective obstacles to the motion of non-basal dislocations. The load transfer effect disappears at the temperature of 300 °C, resulting in the fast deterioration of strength of the alloy. The cracking of the LPSO phase along with the recrystallizing of α-Mg grains were found to be the main causes for the softening behavior of the alloy at 300 °C.

36 MATERIALS SCIENCE↗

Dynamic recrystallization of a wrought magnesium alloy: Grain size and texture maps and their application for mechanical behavior predictions

Effect of dynamic recrystallization (DRX) on the grain refinement and texture modification was studied by conducting a series of hot compression on AZ31B Mg alloy. Processing-grain size-texture maps were established as a function of temperature, strain rate, strain, and the Zener-Hollomon parameter (Z). Moreover, influence of simultaneous changes in the grain size and texture on tensile yield strength and ductility of the hot-worked Mg alloy was studied using the grain size and texture maps established. The processing-grain size map showed that the DRX grain size decreased with the increase in Z, also revealing various characteristics ranging from a grain growth, grain refinement, to a bimodal distribution of ultrafine grains and partially recrystallized grains. The effect of twinning on the grain refinement was also evident at high Z conditions. The processing-texture map revealed that the initial fiber texture was altered significantly to a shear, off-normal, or extension-twin texture with the increase in Z. The Schmid-factor maps were calculated to identify a dominant deformation mode during a subsequent tensile deformation of the hot-worked samples. Finally, a corresponding Hall-Petch relationship for each dominant deformation mode was used to establish tensile yield-strength maps, which agree well with the measured data.

36 MATERIALS SCIENCE↗

Sonochemical synthesis and photocatalytic property of zinc oxide nanoparticles doped with magnesium(II)

Highlights: {yields} Mg-doped ZnO nanoparticles were synthesized by sonochemical strategy. {yields} Mg-doped ZnO nanoparticles present good photocatalytic properties. {yields} The change of band gap contributes to their high efficiency in photocatalyst. -- Abstract: Mg-doped ZnO nanoparticles were successfully synthesized by sonochemical method. The products were characterized by scan electron microscopy (SEM) and X-ray powder diffraction (XRD). SEM images revealed that ZnO doped with Mg(II) nanoparticles and ZnO nanoparticles synthesized by the same strategy all had spherical topography. XRD patterns showed that the doped nanoparticles had the same crystals structures as the pure ZnO nanoparticles. The Mg-doped ZnO nanoparticles had larger lattice volume than the un-doped nanoparticles. X-ray photoelectron spectroscopy (XPS) not only demonstrated the moral ratio of Mg and Zn element on the surface of nanoparticles, but their valence in nanoparticles as well. The Mg-doped ZnO nanoparticles presented good properties in photocatalyst compared with pure ZnO nanoparticles.

36 MATERIALS SCIENCE↗

Influence of Ni-Cr substitution on the magnetic and electric properties of magnesium ferrite nanomaterials

Graphical abstract: Variation of saturation magnetization (M{sub S}) and magnetocrystalline anisotropy coefficient (K{sub 1}) with Ni-Cr content for Mg{sub 1-x}Ni{sub x}Cr{sub x}Fe{sub 2-x}O{sub 4} (x = 0.0-0.5). Highlights: Black-Right-Pointing-Pointer Mg{sub 1-x}Ni{sub x}Cr{sub x}Fe{sub 2-x}O{sub 4} are synthesized by novel PEG assisted microemulsion method. Black-Right-Pointing-Pointer High field regime of M-H loops are modeled using Law of Approach to saturation. Black-Right-Pointing-Pointer A considerable increase in the value of M{sub S} from 148 kA/m to 206 kA/m is achieved Black-Right-Pointing-Pointer {rho}{sup RT} enhanced to the order of 10{sup 9} {Omega}cm at potential operational range around 300 K. -- Abstract: The effect of variation of composition on the structural, morphological, magnetic and electric properties of Mg{sub 1-x}Ni{sub x}Cr{sub x}Fe{sub 2-x}O{sub 4} (x = 0.0-0.5) nanocrystallites is presented. The samples were prepared by novel polyethylene glycol (PEG) assisted microemulsion method with average crystallite size of 15-47 nm. The microstructure, chemical, and phase analyses of the samples were studied by the scanning electron microscopy (SEM), atomic force microscopy (AFM), energy dispersive X-ray fluorescence (ED-XRF), and X-ray diffraction (XRD). Compositional variation greatly affected the magnetic and structural properties. The high-field regimes of the magnetic loops are modelled using the Law of Approach (LOA) to saturation in order to extract information about their anisotropy and the saturation magnetization. Thermal demagnetization measurements are carried out using VSM and significant enhancement of the Curie temperature from 681 K to 832 K has been achieved by substitution of different contents of Ni-Cr. The dc-electrical resistivity ({rho}{sup RT}) at potential operational range around 300 K is increased from 7.5 Multiplication-Sign 10{sup 8} to 4.85 Multiplication-Sign 10{sup 9} {Omega}cm with the increase in Ni-Cr contents. Moreover, the results of the present study provide sufficient evidence to show that the electric and magnetic properties of Mg-ferrite have been improved significantly by substituting low contents of Ni-Cr.

36 MATERIALS SCIENCE↗

Temperature dependence of the luminescence of calcium-magnesium phosphate Ca{sub 3}Mg{sub 3}(PO{sub 4}){sub 4}:Eu{sup 2+}, a blue-emitting material for white light-emitting diodes

Graphical abstract: - Highlights: • Emission spectrum at 20 K confirms that Eu{sup 2+} ions occupy three sites. • Decay curves of three types of Eu{sup 2+} reflect the characteristics of energy transfer. • The Eu(I) emission is thermally quenched at 323 K. • Ca{sub 3}Mg{sub 3}(PO{sub 4}){sub 4}:Eu{sup 2+} has good thermal stability. • Ca{sub 3}Mg{sub 3}(PO{sub 4}){sub 4}:Eu{sup 2+} is a promising phosphor for near UV excited white LEDs. - Abstract: A blue-emitting phosphor Ca{sub 3}Mg{sub 3}(PO{sub 4}){sub 4}:Eu{sup 2+} peaking at 450 nm was synthesized by a solid state reaction. The XRD patterns, luminescence properties, decay curves of samples as well as their thermal quenching and comparing the luminescence properties with that of commercial material were investigated. At 20 K, the emission spectrum exhibiting two distinct bands peaking at 437 and 473 nm with a shoulder peak at 510 nm can be attributed to the overlap of Eu(I), Eu(II) and Eu(III) emission bands. At 423 K the PL intensity decreases to 80% of the value at room temperature, and the emission wavelength shifts toward high energy. The derived activation energy indicates that the lowest energy level of the Eu{sup 2+} 4f{sup 6}5d{sup 1} state is well isolated from the host lattice conduction band. The PL spectra and chromaticity coordinates are close to those of BAM. Ca{sub 3}Mg{sub 3}(PO{sub 4}){sub 4}:Eu{sup 2+} could be a potential candidate for near-UV excited white LEDs.

36 MATERIALS SCIENCE↗

Microstructure and dielectric properties of BaTiO{sub 3} ceramic doped with yttrium, magnesium, gallium and silicon for AC capacitor application

Graphical abstract: Core–shell structure can be obtained in BaTiO{sub 3} ceramics co-doped with Y–Mg-Ga-Si. Y-Mg-Ga-Si co-dopant can obviously reduce dielectric loss, improve AC breakdown voltage and flatten temperature dependence of capacitance curve. - Highlights: • Y-Mg-Ga-Si co-doped BaTiO{sub 3} ceramics with core-shell structure were prepared. • Y{sup 3+}, Mg{sup 2+}, and Ga{sup 3+} dissolved in the lattice BaTiO{sub 3} replacing Ba{sup 2+} site or Ti{sup 4+} site. • Y{sup 3+} and Ga{sup 3+} tended to remain close to the grain boundaries as a shell maker. • Y-Mg-Ga-Si co-doped BaTiO{sub 3} ceramics show high AC breakdown voltage and low tanδ. - Abstract: The microstructures and dielectric properties of Y-Mg-Ga-Si co-doped barium titanate ceramics were investigated. Y{sup 3+} dissolved in the lattice of BaTiO{sub 3} replacing both Ba{sup 2+} site and Ti{sup 4+} site, and Mg{sup 2+} replaced Ti{sup 4+} site. The replacements of Y{sup 3+} and Mg{sup 2+} inhibit the grain growth, cause tetragonal-to-pseudocubic phase transition, reduce the dielectric loss, and flatten the temperature dependence of capacitance curve. The incorporation of Ga{sup 3+} can improve sintering and increase permittivity. Y{sup 3+} and Ga{sup 3+} tended to remain close to the grain boundaries, and play an important role as a shell maker in the formation of the core–shell structure in the co-doped BaTiO{sub 3} ceramics. Excellent dielectric properties: ϵ{sub r} = ∼2487, tanδ = ∼0.7% (at 1 kHz), ΔC/C{sub 25} < ∼6.56% (from −55 °C to 125 °C) and alternating current breakdown voltage E < ∼4.02 kV/mm can be achieved in the BaTiO{sub 3}–0.02Y{sub 2}O{sub 3}–0.03MgO–0.01Ga{sub 2}O{sub 3}–0.005SiO{sub 2} ceramics sintered at 1380 °C. This material has a potential application in alternating current multilayer ceramic capacitor.

36 MATERIALS SCIENCE↗

Superconductivity of magnesium diboride

Over the past 14 years MgB 2 has gone from a startling discovery to a promising, applied superconductor. In our article we present a brief overview of the synthesis and the basic superconducting properties of this remarkable compound. Specifically, the effect of pressure, substitutions and neutron irradiation on superconducting properties are discussed.

36 MATERIALS SCIENCE↗

A new magnesium sheet alloy and its multi-stage homogenization for simultaneously improved ductility and strength at room temperature

We report that a new Mg-2Zn-0.3Ca-0.2Ce-0.1Mn (ZXEM2000) alloy and a multi-stage homogenization process have been designed and developed based on CALculation of Phase Diagram (CALPHAD) modeling results and experimental validation. The new sheet alloy offers an excellent combination of ductility (about 29% elongation) and yield strength (157 MPa), promising room-temperature forming applications. Microstructure characterization reveals that the exceptional properties of this alloy are mainly attributed to the weak basal texture, fine average grain size and high density of nano-scale Mn and Mg 6 Zn 3 Ca 2 precipitates achieved through multi-stage heat treatment and thermomechanical processing.

36 MATERIALS SCIENCE↗

Briefly Bound to Activate: Transient Binding of a Second Catalytic Magnesium Activates the Structure and Dynamics of CDK2 Kinase for Catalysis

We have determined high-resolution crystal structures of a CDK2/Cyclin A transition state complex bound to ADP, substrate peptide, and MgF{sub 3}{sup -}. Compared to previous structures of active CDK2, the catalytic subunit of the kinase adopts a more closed conformation around the active site and now allows observation of a second Mg{sup 2+} ion in the active site. Coupled with a strong [Mg{sup 2+}] effect on in vitro kinase activity, the structures suggest that the transient binding of the second Mg{sup 2+} ion is necessary to achieve maximum rate enhancement of the chemical reaction, and Mg{sup 2+} concentration could represent an important regulator of CDK2 activity in vivo. Molecular dynamics simulations illustrate how the simultaneous binding of substrate peptide, ATP, and two Mg{sup 2+} ions is able to induce a more rigid and closed organization of the active site that functions to orient the phosphates, stabilize the buildup of negative charge, and shield the subsequently activated {gamma}-phosphate from solvent.

59 BASIC BIOLOGICAL SCIENCES↗