Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

The Sliding Wear and Frictional Behavior of M50-10 wt.%(Sn-Ag-Cu) Self-Lubricating Materials at Elevated Temperatures

As the main steel used in the aero-engine main shaft bearings, the tribological properties of M50 can directly affect the performance of aero-engine. The purpose of this study is to design the reasonable composition of Sn-Ag-Cu alloy and investigate the wear mechanisms of M50-10 wt.%(Sn-Ag-Cu) composites (MSACC) prepared by SPS sliding against Si{sub 3}N{sub 4} ball from 25 to 550 °C at 12 N-0.25 m/s. XRD, EPMA, FESEM and EDS mappings are conducted to understand the major mechanisms leading to the improvement in the sliding behavior of MSACC. The results indicate that MSACC with different specifications of Sn-Ag-Cu alloy shows excellent friction and wear properties from 25 to 550 °C compared to M50. M50-10 wt.%(50Sn40Ag10Cu) (MSACC-2) shows the distinguished tribological performance for the lower friction coefficients of 0.22-0.61 and less wear rates of 1.7-4.1 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1}, which is attributed to the formed excellent lubricating structure consisting of the lubricating film with massive Sn-Ag-Cu alloy and intermetallic compounds formed during the friction process, as well as the underneath mixed layer who can well support the lubricating film due to the good intersolubility between the designed Sn-Ag-Cu alloy and M50 (Fe).

36 MATERIALS SCIENCE↗

Role of Centrifugal Casting on Electrochemical Corrosion Behavior of A356-SiCp Composite in 3.5 wt.% NaCl

Role of graded microstructure in a centrifugally cast A356-SiC particle (SiCp) composite alloy disk on passivity and localized corrosion behavior in 3.5 wt.% NaCl environment has been investigated. The area fraction of SiCp has been found to decrease from the outer periphery to the core of the disk, while the apparent size and area fraction of the intermetallics and Mg-rich phase increase from the periphery to the core. As a consequence, the corrosion resistance of the as-cast disk varies with the distance from the periphery in the order 45 < 65 < 25 < 5 mm. The corrosion resistance of the centrifugally cast disk can be significantly improved through solution annealing at 540 °C for 2 h and solution annealing + aging at 175 °C for 2 h. However, between the two, the former has shown a better corrosion resistance and passivity than the latter. In the latter case, the aging treatment resulted in the precipitation of Mg{sub 2}Si phase which is prone to the corrosion attack.

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Influence of Oxygen Partial Pressure Variation on Oxidation Resistance of Ti-46.7Al-1.9W-0.5Si at 750, 850 and 950 °C

γ-TiAl intermetallic alloys can be potentially employed as structural materials for many industries where high temperature and access of atmosphere with variable oxygen partial pressures are often met. Different partial pressures of oxygen may influence oxidation behavior and induce different oxide scale phase constitutes. This study investigated the influences of oxygen partial pressures on the oxidation resistance of a γ-TiAl alloy, Ti-46.7Al-1.9W-0.5Si (at.%), in Ar-O{sub 2} environments (5%O{sub 2}, 20%O{sub 2} and 80%O{sub 2}) at 750, 850 and 950 °C, respectively. The oxidation products were characterized using scanning electron microscopy, energy-dispersive x-ray analysis, x-ray diffraction and transmission electron microscopy. The oxidation kinetic results achieved by a discontinuous gravimetric method revealed that the alloy oxidized following a parabolic rate law. The oxidation resistance of the alloy was enhanced with increasing the oxygen partial pressures at all three experimental temperatures. Multilayered oxide scales of TiO{sub 2}/Al{sub 2}O{sub 3} were developed during the oxidation process. The enhancement of oxidation resistance was resulted from preferential generation of Al{sub 2}O{sub 3} and the reduction in defects in TiO{sub 2} with increasing the oxygen partials pressures.

36 MATERIALS SCIENCE↗

The Influence of Galvanizing Parameters on the Structural Development of Zn-Al-Based Coatings

The evolution of some layers’ characteristics, deposited by galvanization, was monitored according to the technological parameters of the process. Two types of alloys from the Zn-Al and Zn-Al-Ti-B systems were used for deposition. The structure of the deposited layers was analyzed by optical and electron microscopy. The chemical composition, phases and compounds in the structures were identified. The mechanical properties of the structural constituents of the layers were determined by nanoindentation. These techniques highlighted the typical non-uniformities in terms of composition and properties in the layers, mainly due to the diffusion and distribution of iron from the steel substrate in the deposited layers. The evaluation of iron diffusion in the deposited layer was done by differential thermal analysis. The values of the critical temperatures (melting temperature, eutectic temperature and solidification temperature) were correlated with the parameters used during deposition. It was observed that the structure of the coatings is layered, with a specific order from the steel substrate to the edge. In these layers, the constituents are mixtures of soft solid solutions of Al in Zn (η and β) and hard intermetallic compounds. Moreover, increasing the immersion time in the galvanizing bath and the bath temperature leads to an increase in iron diffusion in the coating layer, which contributes to lower coating thickness, thus reducing its durability in operation.

36 MATERIALS SCIENCE↗

Wetting and Brazing of Chromium Film-Deposited Alumina Using AgCu Filler Metal

Wetting behavior of AgCu filler on chromium film-deposited Al{sub 2}O{sub 3} ceramics was studied by sessile drop method under vacuum, and brazing of chromium-deposited alumina using AgCu was carried out. Cr film can improve the wettability of AgCu filler on alumina ceramics, and the contact angle decreased dramatically. However, with further increase in temperature and extension of wetting time, Cr atom might diffuse excessively to molten alloy or substrate leading to thinned or disappeared Cr film on alumina; thus, the contact angle of AgCu on alumina increased. The reliable alumina joint was obtained via chromium deposition using AgCu filler brazed at 900 °C for 10 min, and no hard or brittle intermetallic compounds formed in the brazed joint. The maximum shear strength of 16.8 MPa was achieved when the thickness of deposited chromium film was 2 μm.

36 MATERIALS SCIENCE↗

Microstructures and Mechanical Properties of Resistance Spot-Welded Steel/Aluminum Alloy Joints with Process Tapes

The microstructure and mechanical property of resistance spot-welded joints of steel and aluminum were studied by using process tapes. The steel/aluminum joint consists mainly of aluminum nugget and interface zone. The liquid nugget solidification has an epitaxial growth characteristic, and the interface zone displays a double-layer structure, Fe{sub 2}Al{sub 5} layer at steel side and Fe{sub 4}Al{sub 13} layer at aluminum nugget side. Compared with joints without process tape, the joint nugget diameter and tensile shear load increased by 35.45 and 10.98%, respectively, and its indentation ratio decreased by 56.25% due to the process tapes increasing heat input, producing larger nugget diameter and continuous interface layer, and protecting against deep indentation. The joining area of intermetallic layer and aluminum nugget is weak link in the joint. It is favorable to use the process tapes for improving welding quality, raising joint strength, and energy saving.

36 MATERIALS SCIENCE↗

Study on Microstructure and Properties of AZ31/6061 GTAW Butt Joints According to Mg-Cd-Al Ternary System

AZ31 Mg and 6061 Al were successfully joined by GTAW method with Cd as filler metal. The tensile strength of the joints reached 170 MPa through this alloying method according to Mg-Cd-Al ternary system. The microstructure, phases, element distribution and fracture mechanism of alloyed joints were studied. The results suggest that the fusion zone is mainly composed of CdMg compounds and Al-based solid solution. A transitional zone thickness of 40-80 μm with few primary Al{sub 12}Mg{sub 17} and fine Al{sub 12}Mg{sub 17}-MCMS (MCMS represents a mixture of CdMg and CdMg{sub 3} compounds) eutectic is formed between the AZ31 base metal and fusion zone. The fracture surface presents three distinct regions because of the different distribution of Al{sub 12}Mg{sub 17} compounds in the transitional zone. The alloying with Cd filler metal can disperse Al{sub 12}Mg{sub 17} intermetallic compounds and form CdMg ordered compounds with excellent plasticity. Thus, the mechanical properties of alloyed joints have been significantly enhanced.

36 MATERIALS SCIENCE↗

Influence of Annealing on the Properties of Explosively Welded Titanium Grade 1—AW7075 Aluminum Alloy Bimetals

Explosive welding of titanium Grade 1 to AW7075 aluminum alloy arranged in parallel setup was performed. The annealing of produced bimetals at the temperatures of 450, 500 and 550 °C for times ranging from 20 to 100 h was carried out after explosive welding. The produced bimetal was characteristic by its wavy interface typical for that bonding process. Increase in the microhardness at the interface was recorded due to work hardening. Delamination of titanium Grade 1 flyer sheet was firstly observed when annealing temperature of 500 °C for 40 h was carried out. Annealing at 550 °C also resulted in delamination of upper sheet. The intermetallic compound (IMC) layer was observed at the interface after annealing of bimetals. The higher the annealing temperature and time, the higher the thickness of continuous IMC layer. The maximum measured thickness of IMC layer averaged 13 µm. Energy dispersive x-ray spectroscopy (EDS) and x-ray diffraction (XRD) analyses revealed that the interface layer is consisted of Al{sub 18}Ti{sub 2}Mg{sub 3} IMC. Microhardness at the interface increased dramatically up to 439 HV0.1 after annealing of bimetal due to the presence of above-mentioned IMC.

36 MATERIALS SCIENCE↗

A Low-Cost Lightweight Entropic Alloy with High Strength

In this study, a series of lightweight Al–Mg system entropic alloys containing Zn, Cu, and Si were designed based on the order/disorder or entropy, and eutectic concepts. The alloys of Al{sub 58.5}Mg{sub 31.5}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 63}Mg{sub 27}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 66.7}Mg{sub 23.3}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}; Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}; and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} were prepared by induction melting under a high-purity argon atmosphere and then casted into stainless steel molds. The microstructures which were tested in the as-cast state exhibited multiphases and contained apparent volume fractions of intermetallic compounds and solid solutions. Then, the compressive mechanical properties of the alloys were measured, and high fracture strengths of 577, 677, 590, 498, 814, and 794 MPa, respectively, were determined. Strong hardening phenomena were observed in the Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}, Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}, and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} alloys at room temperature, with amazing plasticity percentages of 13.8, 24.8, and 32.7%, respectively. The property differences in the lightweight alloys were analyzed using the following parameters: the critical values of the enthalpy of mixing; atomic size differences; ratio of entropy to enthalpy; valence electron concentration (VEC); and Pauling electronegativity difference. Finally, three of the aforementioned parameters (atomic size difference, enthalpy of mixing, and Pauling electronegativity difference) were regarded in this study as the crucial rules for the lightweight multicomponent alloys.

36 MATERIALS SCIENCE↗

Welding Heat Input Influence on UNS S82441 Lean Duplex Stainless Steel Corrosion Resistance Assessed by Scanning Vibrating Electrode Technique (SVET)

The precipitation of the intermetallic phases can impair mechanical and corrosion properties. In the case of lean duplex stainless steels, they present solidification mode as primary ferrite, with austenite precipitation in the solid state, during cooling. This means the heat-affected zone balanced microstructure can be changed during the welding by the cooling rate, which is associated to the welding heat input, the thickness of the plate and the physical properties of the material. This work intends to present the influence of welding heat input on the corrosion resistance of UNS S82441 lean duplex stainless steel. The gas metal arc welding process was used to make the weld beads, using ER2209 as filler metal, which characterizes a dissimilar welded joint. The corrosion resistance of these specimens was analyzed through scanning vibrating electrode technique. It was observed that welding heat input variation distinctly influences corrosion in different zones of the weld beads over the specimen exposure time. The weld bead under intermediate welding heat input showed the highest corrosion rate and the one under the highest welding heat input, the lowest corrosion rate intensity.

36 MATERIALS SCIENCE↗

Synthesis and Structural Characterization of Sb-Doped TiFe{sub 2}Sn Heusler Compounds

Ternary Heusler compounds form a numerous class of intermetallics, which include two families with general compositions ABC and AB{sub 2}C, usually referred to as half- and full-Heusler compounds, respectively. Given their tunable electronic properties, made possible by adjusting the chemical composition, these materials are currently considered for the possible use in sustainable technologies such as solar energy and thermoelectric conversion. According to theoretical predictions, Sb substitution in the TiFe{sub 2}Sn full-Heusler compound is thought to yield band structure modifications that should enhance the thermoelectric power factor. In this work, we tested the phase stability and the structural and microstructural properties of such heavily doped compounds. We synthesized polycrystalline TiFe{sub 2}Sn{sub 1−x}Sb{sub x} samples, with x = 0, 0.1, 0.2 and 1.0 by arc melting, followed by an annealing treatment. The structural characterization, performed by x-ray powder diffraction and microscopy analyses, confirmed the formation of the pseudo-ternary Heusler structure (cF16, Fm-3m, prototype: MnCu{sub 2}Al) in all samples, with only few percent amounts of secondary phases and only slight deviations from nominal stoichiometry. With increasing Sb substitution, we found a steady decrease in the lattice parameter, confirming that the replacement takes place at the Sn site. Quite unusually, the as-cast samples exhibited a higher lattice contraction than the annealed ones. The fully substituted x = 1.0 compound, again adopting the MnCu{sub 2}Al structure, does not form as stoichiometric phase and turned out to be strongly Fe deficient. The physical behavior at room temperature indicated that annealing with increasing temperature is beneficial for electrical and thermoelectrical transport. Moreover, we measured a slight improvement in electrical and thermoelectrical properties in the x = 0.1 sample and a suppression in the x = 0.2 sample, as compared to the undoped x = 0 sample.

36 MATERIALS SCIENCE↗

Microstructural Properties of Heat-Treated LENS In Situ Additively Manufactured Titanium Aluminide

This study reports on the microstructure, phase identification and hardness property of the LENS-manufactured binary Ti-Al alloy which was achieved via laser in situ alloying. The in situ alloying method, using laser beam as an energy source, indicated that it is possible to achieve a binary gamma phase microstructure from elemental powders of Ti and Al. The as-produced sample, however, was characterized of having different microstructure at the top, middle and bottom regions. The middle and top layers had similar hardness which was lower than that of the bottom region. The as heat-treated sample was characterized of lamellar grain microstructure at the top and just grains at the bottom and the middle. The observed grains were different in size, phase and hardness. This study indicated that in addition to the pores and the precipitation of α{sub 2} phase or aluminum segregation on the grain boundary veins intermetallics lead to severe cracking. Overall, the hardness values of the as-produced and heat-treated samples were similar, and due to extensive cracking, it was inferred that both samples will lack ductility.

36 MATERIALS SCIENCE↗

Pulsed TIG Welding–Brazing of Aluminum–Stainless Steel with an Al-Cu Twin Hot Wire

A TIG welding–brazing process with a twin aluminum hot wire technique was utilized to control the heat input, improve the joint formation, suppress the interfacial intermetallic compounds (IMCs) and increase the joint strength, thereby creating reliable joints between an aluminum alloy and stainless steel with an ER2319 filler. Twin wires with reasonable diameters and filling modes led to a satisfactory weld of parent metals with varying thicknesses. By the hot wire technique, the reasonable range of the welding current was extended and the thickness of the interfacial IMC at the seam bottom was reduced. In addition, both the tensile strength and stability of the joints increased compared with a cold wire. The IMC consisted of θ-(Fe,Cu){sub 4}Al{sub 13} and minor Cr{sub 0.7}Fe{sub 0.3}Al{sub 6}, and the precipitated phases in the weld were Al{sub 2}Cu and Al{sub 2}CuMg. With an increasing welding current, the IMC thickness significantly increased, while the joint strength decreased. The fracture positions of the joints varied with the corresponding welding currents.

36 MATERIALS SCIENCE↗

The Effect of Brazing on Microstructure of Honeycomb Liner Material Hastelloy X

Labyrinth seals with abradable metallic honeycomb structures are common in gas turbines to ensure a tight sealing between rotor and stator. These seals have a big impact on the turbine efficiency. The honeycombs made from nickel-based superalloys are brazed onto backing segments in order to form liners. In this work, the microstructure of Hastelloy X honeycombs after brazing with a nickel-chromium-silicon braze filler alloy is investigated. It was found that the braze filler can wet the honeycomb foils over their entire height up to the contact surface with the rotor. After solidification, the braze filler alloy forms γ and silicides (NiSi and Ni{sub y}(Mo, Cr){sub x}Si). The intermetallic silicides give high hardness to the honeycomb liners. Between the braze filler alloy and the honeycomb foils, interdiffusion zones are observed. For the rub-in behavior of the honeycomb liners, not only the foil material but also the comportment of the composite made up of the foil material, the braze filler material and the interdiffusion zones has to be considered.

36 MATERIALS SCIENCE↗

In Vitro Degradation, Antibacterial Activity and Cytotoxicity of Mg-3Zn-xAg Nanocomposites Synthesized by Mechanical Alloying for Implant Applications

A class of biodegradable Mg-3Zn-xAg nanocomposites was presented in the present study with the assessments for implant application. The evaluations included the effects of increasing the Ag content from 0.5 to 3 wt.% on the corrosion behavior, mechanical properties, antibacterial activity and cytotoxicity of Mg-3Zn-xAg nanocomposite. Microstructural analysis revealed the secondary phase intermetallic Mg{sub 54}Ag{sub 17} along the grain boundaries, with grain refinement as a result of increasing the Ag concentration. 0.5 wt.% Ag results in increasing the compressive strength and elongation; however, further addition decreases the compressive strength. The nanocomposite samples were verified for the improved antimicrobial activity by utilizing both E. coli and S. aureus bacteria, the growth of which was suppressed around all Ag-containing nanocomposites, whereas bacterial proliferations were detected around the Mg-3Zn nanocomposite. The escalating levels of Ag in the nanocomposite resulted in the elevated antimicrobial effect. Cell adhesion and proliferation were not significantly influenced by the inclusion of 0.5-1 wt% Ag into Mg-3Zn nanocomposite; however, cell adhesion and proliferation were lower on the surfaces of the nanocomposite containing 2-3 wt.% Ag counterparts. According to the mechanical, corrosion and biological assessments in the current research, it can be concluded that the nanocomposite containing 0.5 wt.% Ag can be properly applied as an orthopedic implant biomaterial.

36 MATERIALS SCIENCE↗

Dry Sliding Wear Behavior and Mechanism of a Hot-Dip Aluminized Steel as a Function of Sliding Velocity

Fe-Al intermetallic coatings were prepared on AISI 1045 steel by hot-dip aluminizing and subsequent high-temperature diffusion. The dry sliding wear tests were performed for the aluminized steel with various substrate hardnesses in the velocity range of 0.75-4 m/s on a pin-on-disk configuration. The dry sliding wear behavior and mechanisms of the aluminized steel under various velocities were explored. It was found that the wear rate decreased substantially with an increase in sliding velocity from 0.75 to 1.5 and then slightly varied in the velocity range of 1.5-4 m/s. The wear behavior and mechanisms of the aluminized steel were noticed to be closely related with tribo-layers. As tribo-layers contained more oxides with Fe{sub 2}O{sub 3}, the wear resistance of the aluminized steel was markedly improved because of their protective function. The substrate hardness also changed the wear behavior of the aluminized steel by affecting the stability of tribo-layers because the substrate hardness was inversely proportional to the thermal stability of the substrate structure. Under a low velocity of 0.75 m/s, adhesive wear and abrasive wear prevailed owing to the metal-on-metal contact, resulting in a higher wear rate. At 1.5-4 m/s, mild oxidative wear prevailed due to the stable existence of tribo-oxides layers. However, at 1.5 and 4 m/s for the substrate hardness of 45 HRC, the wear rate was slightly increased because the protection of tribo-layers was weakened by a double-layered structure or more cracks in tribo-layers and coatings.

36 MATERIALS SCIENCE↗

Surface Modification of High-Carbon Steel Using Fiber Laser and Its Thermal, Microstructural and Tribological Analysis

In this study, surface modification of high-carbon steel was carried out using 2 kW fiber laser and thermal, microstructural and tribological characterizations were performed. The process parameters selected for laser surface treatment were laser power (600-1500 W) and scan speed (3000-4500 mm/min). Infrared pyrometer was used to record the surface temperature during the process. The metallographic analysis was carried out using an optical microscope to find the depth and width of the laser-treated zone. Scanning electron microscopy and energy-dispersive spectroscopy were performed to reveal the microstructure and compositional changes taking place in the laser-treated zone. It was observed that the dendritic growth took place from the top surface toward the center of the laser-treated zone. The amount of dendritic growth can be related to the maximum surface temperature generated during the process. XRD analysis indicated the formation of some intermetallic compounds and phase shifts taking place in the laser-treated zone. Residual stress analysis was performed to analyze the amount of stress accumulation in the laser-treated zone. When the temperature cycle was analyzed, it was found that the melting of the steel resulted in the formation of a surface under compressive stress while the non-melt hardened zone developed a surface under tensile stress. The maximum Vickers microhardness value achieved was about 958.8 HV{sub 0.5} for 1500 W power and 3000 mm/min scan speed. Scratch test was performed on the laser-treated track, and it was found that the hardened zone showed better tribological properties with respect to the parent material. Finally, it was observed that the surface roughness value increased with higher heat input probably due to high rate of oxide formation as well as due to the presence of martensite in the laser-treated zone.

36 MATERIALS SCIENCE↗