Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Electron Diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

Evolution of carbides in cold-work tool steels

This study aimed to present the complete history of carbide evolution in a cold-work tool steel along its full processing route for fabrication and application. A sequence of processes from cast to final hardening heat treatment was conducted on an 8% Cr-steel to reproduce a typical commercial processing route in a small scale. The carbides found at each process step were then identified by electron diffraction with energy dispersive spectroscopy in a scanning or transmission electron microscope. After solidification, MC, M{sub 7}C{sub 3} and M{sub 2}C carbides were identified and the last one dissolved during hot compression at 1180 °C. In a subsequent annealing at 870 °C followed by slow cooling, M{sub 6}C and M{sub 23}C{sub 6} were added, while they were dissolved in the following austenitization at 1030 °C. After the final tempering at 520 °C, fine M{sub 23}C{sub 6} precipitated again, thus the final microstructure was the tempered martensite with MC, M{sub 7}C{sub 3} and M{sub 23}C{sub 6} carbide. The transient M{sub 2}C and M{sub 6}C originated from the segregation of Mo and finally disappeared due to attenuated segregation and the consequent thermodynamic instability. - Highlights: • The full processing route of a cold-work tool steel was simulated in a small scale. • The carbides in the tool steel were identified by chemical–crystallographic analyses. • MC, M{sub 7}C{sub 3}, M{sub 2}C, M{sub 6}C and M{sub 23}C{sub 6} carbides were found during the processing of the steel. • M{sub 2}C and M{sub 6}C finally disappeared due to thermodynamic instability.

36 MATERIALS SCIENCE↗

Stoichiometry as key to ferroelectricity in compressively strained SrTiO{sub 3} films

While strain is a powerful tuning parameter for inducing ferroelectricity in thin film oxides, the role of stoichiometry control is critical, but far less explored. A series of compressively strained SrTiO{sub 3} films on (001) (LaAlO{sub 3}){sub 0.3}(Sr{sub 2}AlTaO{sub 6}){sub 0.35} substrates were grown by hybrid molecular beam epitaxy where the Ti cation was supplied using a metal-organic titanium tetraisopropoxide molecule that helps systematically and precisely control Sr:Ti stoichiometry in the resulting films. A stoichiometric growth window is located through X-ray diffraction and in-situ reflection high-energy electron diffraction measurements, which show a minimum out-of-plane lattice parameter as well as constant growth rate within the stoichiometric growth window range. Using temperature dependent optical second harmonic generation (SHG) characterization, a ferroelectric-to-paraelectric transition at T ∼ 180 K is observed for a stoichiometric SrTiO{sub 3} film, as well as a higher temperature structural transition at T ∼ 385 K. Using SHG polarimetry modeling, the polar point group symmetry is determined to be tetragonal 4mm with the polarization pointing out-of-plane of the film. The SHG coefficients, d{sub 31}/d{sub 15}=3 and d{sub 33}/d{sub 15}=21, were determined at 298 K. The ferroelectric transition disappears in films grown outside the growth window, thus proving the critical role of stoichiometry control in realizing strain-induced ferroelectricity.

36 MATERIALS SCIENCE↗

Molecular beam epitaxy and crystal structure of majority a -plane-oriented and substrate-strained Mn 3 Sn thin films grown directly on sapphire (0001)

The Kagome antiferromagnet Mn 3 Sn has garnered much attention due to the presence of exciting properties such as anomalous Hall and Nernst effects. This paper discusses the synthesis of crystalline Mn 3 Sn thin films, prepared on Al 2 O 3 (0001) substrates at 453 ± 5°C using molecular beam epitaxy. The growth is monitored in situ using reflection high energy electron diffraction and measured ex situ using x-ray diffraction, Rutherford back-scattering, and cross-sectional scanning transmission electron microscopy. Our analysis shows the in-plane lattice constants of a 1,M = 4.117 ± 0.027 Å and a 2,M = 4.943 ± 0.033 Å, which is a very unexpected result when compared to the bulk a-plane Mn 3 Sn. This indicates a strain in the film and makes it challenging to provide a straightforward explanation. In an effort to explain our results, we discuss two possible orientation relationships between the Mn 3 Sn films and the sapphire substrates. Samples prepared under these conditions appear to have smooth surfaces locally, but overall the film has a 3D island morphology. First-principles calculations provide atomic models of the Mn 3 Sn (112¯0) lattice on Al 2 O 3 (0001) high symmetry sites, indicating that the L3-R90° is the most stable configuration. A detailed discussion of the experimental data and theoretical results, as well as strain effects, is provided.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Physically and chemically smooth cesium-antimonide photocathodes on single crystal strontium titanate substrates

The performance of x-ray free electron lasers and ultrafast electron diffraction experiments is largely dependent on the brightness of electron sources from photoinjectors. Here, the maximum brightness from photoinjectors at a particular accelerating gradient is limited by the mean transverse energy (MTE) of electrons emitted from photocathodes. For high quantum efficiency (QE) cathodes like alkali-antimonide thin films, which are essential to mitigate the effects of non-linear photoemission on MTE, the smallest possible MTE and, hence, the highest possible brightness are limited by the nanoscale surface roughness and chemical inhomogeneity. In this work, we show that high QE Cs 3 Sb films grown on lattice-matched strontium titanate (STO) substrates have a factor of 4 smoother, chemically uniform surfaces compared to those traditionally grown on disordered Si surfaces. We perform simulations to calculate roughness induced MTE based on measured topographical and surface-potential variations on the Cs 3 Sb films grown on STO and show that these variations are small enough to have no consequential impact on the MTE and, hence, the brightness.

43 PARTICLE ACCELERATORS↗

Low-temperature growth of low friction wear-resistant amorphous carbon nitride thin films by mid-frequency, high power impulse, and direct current magnetron sputtering

The potential of different magnetron sputtering techniques for the synthesis of low friction and wear resistant amorphous carbon nitride (a-CN{sub x}) thin films onto temperature-sensitive AISI52100 bearing steel, but also Si(001) substrates was studied. Hence, a substrate temperature of 150 °C was chosen for the film synthesis. The a-CN{sub x} films were deposited using mid-frequency magnetron sputtering (MFMS) with an MF bias voltage, high power impulse magnetron sputtering (HiPIMS) with a synchronized HiPIMS bias voltage, and direct current magnetron sputtering (DCMS) with a DC bias voltage. The films were deposited using a N{sub 2}/Ar flow ratio of 0.16 at the total pressure of 400 mPa. The negative bias voltage, V{sub s}, was varied from 20 to 120 V in each of the three deposition modes. The microstructure of the films was characterized by high-resolution transmission electron microscopy and selected area electron diffraction, while the film morphology was investigated by scanning electron microscopy. All films possessed an amorphous microstructure, while the film morphology changed with the bias voltage. Layers grown applying the lowest substrate bias of 20 V exhibited pronounced intercolumnar porosity, independent of the sputter technique. Voids closed and dense films are formed at V{sub s} ≥ 60 V, V{sub s} ≥ 100 V, and V{sub s} = 120 V for MFMS, DCMS, and HiPIMS, respectively. X-ray photoelectron spectroscopy revealed that the nitrogen-to-carbon ratio, N/C, of the films ranged between 0.2 and 0.24. Elastic recoil detection analysis showed that Ar content varied between 0 and 0.8 at. % and increased as a function of V{sub s} for all deposition techniques. All films exhibited compressive residual stress, σ, which depends on the growth method; HiPIMS produces the least stressed films with values ranging between −0.4 and −1.2 GPa for all V{sub s}, while CN{sub x} films deposited by MFMS showed residual stresses up to −4.2 GPa. Nanoindentation showed a significant increase in film hardness and reduced elastic modulus with increasing V{sub s} for all techniques. The harder films were produced by MFMS with hardness as high as 25 GPa. Low friction coefficients, between 0.05 and 0.06, were recorded for all films. Furthermore, CN{sub x} films produced by MFMS and DCMS at V{sub s} = 100 and 120 V presented a high wear resistance with wear coefficients of k ≤ 2.3 × 10{sup −5} mm{sup 3}/Nm. While all CN{sub x} films exhibit low friction, wear depends strongly on the structural and mechanical characteristics of the films. The MFMS mode is best suited for the production of hard CN{sub x} films, although high compressive stresses challenge the application on steel substrates. Films grown in HiPIMS mode provide adequate adhesion due to low residual stress values, at the expense of lower film hardness. Thus, a relatively wide mechanical property envelope is presented for CN{sub x} films, which is relevant for the optimization of CN{sub x} film properties intended to be applied as low friction and wear resistant coatings.

36 MATERIALS SCIENCE↗

Surface Phase Diagram and Alloy Formation for Antimony on Au(110)

The authors have evaporated submonolayer to monolayer Sb films on the clean Au(110) surface and investigated the resultant Sb-induced reconstructions using low energy electron diffraction, x-ray photoelectron spectroscopy, Auger electron spectroscopy, and surface x-ray diffraction. They discovered a sequence of reconstructions, namely, c(2x2), (sqrt(3)xsqrt(3))R54.7 , (((2 - 1)/(1 2))), and p(5x6), with increasing coverage of Sb. The well-known (2x1) reconstruction of the clean Au(110) surface changes to c(2x2) at an Sb coverage of theta[approximate]0.5 ML. At higher Sb coverages, there is a phase transition from c(2x2) to (sqrt(3)xsqrt(3))R54.7 , with the (sqrt(3)xsqrt(3))R54.7 pattern emerging at an Sb coverage of theta[approximate]0.7 ML. Upon further deposition, the superstructure spots of the (sqrt(3)xsqrt(3))R54.7 reconstruction each split into two, resulting in the (((2 - 1)/(1 2))) pattern at a coverage of theta[approximate]0.8 ML. Finally, an Sb/Au(110)-p(5x6) reconstruction emerges at coverages in excess of 1 ML. They have also studied the temperature dependence of the c(2x2) surface phase.

36 MATERIALS SCIENCE↗

Optical information transfer through random unknown diffusers using electronic encoding and diffractive decoding

Free-space optical information transfer through diffusive media is critical in many applications, such as biomedical devices and optical communication, but remains challenging due to random, unknown perturbations in the optical path. We demonstrate an optical diffractive decoder with electronic encoding to accurately transfer the optical information of interest, corresponding to, e.g., any arbitrary input object or message, through unknown random phase diffusers along the optical path. This hybrid electronic-optical model, trained using supervised learning, comprises a convolutional neural network-based electronic encoder and successive passive diffractive layers that are jointly optimized. After their joint training using deep learning, our hybrid model can transfer optical information through unknown phase diffusers, demonstrating generalization to new random diffusers never seen before. The resulting electronic-encoder and optical-decoder model was experimentally validated using a 3D-printed diffractive network that axially spans <70λ, where λ = 0.75 mm is the illumination wavelength in the terahertz spectrum, carrying the desired optical information through random unknown diffusers. The presented framework can be physically scaled to operate at different parts of the electromagnetic spectrum, without retraining its components, and would offer low-power and compact solutions for optical information transfer in free space through unknown random diffusive media.

36 MATERIALS SCIENCE↗

Physical properties of epitaxial ZrN/MgO(001) layers grown by reactive magnetron sputtering

Single-crystal ZrN films, 830 nm thick, are grown on MgO(001) at 450 °C by magnetically unbalanced reactive magnetron sputtering. The combination of high-resolution x-ray diffraction reciprocal lattice maps, high-resolution cross-sectional transmission electron microscopy, and selected-area electron diffraction shows that ZrN grows epitaxially on MgO(001) with a cube-on-cube orientational relationship, (001){sub ZrN}‖(001){sub MgO} and [100]{sub ZrN}‖[100]{sub MgO}. The layers are essentially fully relaxed with a lattice parameter of 0.4575 nm, in good agreement with reported results for bulk ZrN crystals. X-ray reflectivity results reveal that the films are completely dense with smooth surfaces (roughness = 1.3 nm, consistent with atomic-force microscopy analyses). Based on temperature-dependent electronic transport measurements, epitaxial ZrN/MgO(001) layers have a room-temperature resistivity ρ{sub 300K} of 12.0 μΩ-cm, a temperature coefficient of resistivity between 100 and 300 K of 5.6 × 10{sup −8}Ω-cm K{sup −1}, a residual resistivity ρ{sub o} below 30 K of 0.78 μΩ-cm (corresponding to a residual resistivity ratio ρ{sub 300Κ}/ρ{sub 15K} = 15), and the layers exhibit a superconducting transition temperature of 10.4 K. The relatively high residual resistivity ratio, combined with long in-plane and out-of-plane x-ray coherence lengths, ξ{sub ‖} = 18 nm and ξ{sub ⊥} = 161 nm, indicates high crystalline quality with low mosaicity. The reflectance of ZrN(001), as determined by variable-angle spectroscopic ellipsometry, decreases slowly from 95% at 1 eV to 90% at 2 eV with a reflectance edge at 3.04 eV. Interband transitions dominate the dielectric response above 2 eV. The ZrN(001) nanoindentation hardness and modulus are 22.7 ± 1.7 and 450 ± 25 GPa.

36 MATERIALS SCIENCE↗

Growth modes in metal-organic molecular beam epitaxy of TiO{sub 2} on r-plane sapphire

Phase pure, epitaxial (101) rutile TiO{sub 2} films were grown on (012) sapphire substrates at temperatures between 485 and 725 deg. C using metal-organic molecular beam epitaxy with titanium tetraisopropoxide as the Ti source. Growth modes and rates were investigated as a function of substrate temperature using reflection high-energy electron diffraction, x-ray reflectivity, atomic force microscopy, and transmission electron microscopy. Growth rates were as high as 125 nm/h. The influence of additional oxygen supplied from a rf plasma source was investigated. Without oxygen plasma, the growth rate exhibited reaction and flux-limited regimes and layer-by-layer growth was observed in the initial stages of film growth. With oxygen plasma the growth rate became independent of temperature; films grew initially in step-flow mode and were insulating. The mechanisms for the different growth modes as a function of film thickness, temperature, and presence of oxygen are discussed.

36 MATERIALS SCIENCE↗

Experimental confirmation of Zener-polaron-type charge and orbital ordering in Pr{sub 1-x}Ca{sub x}MnO{sub 3}

Pr{sub 1-x}Ca{sub x}MnO{sub 3} in the doping range between 0.3<x<0.5 represent an extremely interesting manganite system for the study of the interplay of different kinds of ordering (charge, orbital, lattice, and spin). While there is consensus that a charge- and orbital-ordered state develops below a transition temperature T{sub co}{approx_equal}230 K, recent controversial structural refinements resulting from neutron and x-ray diffraction studies challenged our understanding of the particular type of charge ordering (CO) and orbital ordering (OO), and consequently, the underlying mechanism of the colossal resistance effects. Here, we present a detailed high-resolution transmission electron microscopy and electron-diffraction study that, based on extinction rules, resolves the current controversy and confirms the existence of the Zener-polaron (ZP)-type CO and/or OO in Pr{sub 1-x}Ca{sub x}MnO{sub 3}. The ZP-type ordering is further verified by atomic-column-resolved electron energy-loss spectroscopy revealing strong charge ordering of the in-plane oxygen-Mn bonds, while valence disproportionation at the Mn sites is less than expected. Over wide doping and temperature ranges, we observed structural phase coexistence between the ZP-CO/OO P2{sub 1}nm and the disordered Pbnm structure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis, structural and optical properties of BaMoO{sub 4}:Eu{sup 3+} shuttle like phosphors

Graphical abstract: - Highlights: • BaMoO{sub 4}:Eu{sup 3+} phosphors were synthesized by a facile synthesis route. • PL and CL spectra showed dominant emissions due to ({sup 5}D{sub 0} → {sup 7}F{sub 2}) hypersensitive transitions. • The excitation wavelengths in the UV-B region make BaMoO{sub 4}:Eu{sup 3+} phosphors as a good candidate in the red region for the development of UV-based white LEDs. • PL and CL spectra showed similar CIE values close to the commercially available Y{sub 2}O{sub 3}:Eu{sup 3+} phosphors. - Abstract: Eu{sup 3+} ions doped BaMoO{sub 4} phosphor samples were synthesized by a facile synthesis process. The tetragonal phase of the host lattice was substantiated by the X-ray diffraction patterns. The morphological studies were carried out by taking the scanning electron microscope and transmission electron microscope images and confirmed the formation of shuttle like particles with perpendicular protrusions in the middle of the particle. The single crystalline nature of the phosphors was confirmed by the selected area electron diffraction pattern. The photoluminescence (PL) properties of the Eu{sup 3+} ions doped samples revealed good emission with a high asymmetry ratio when excited with ultraviolet B wavelengths (between 280 and 315 nm). The cathodoluminescence (CL) spectra showed similar results to the PL spectra. The calculated CIE values based on the PL and CL spectra were almost similar and confirmed the rich red emission.

36 MATERIALS SCIENCE↗

Role of Dysprosium Doping on Structural, Optical, Magnetic and Electrical Properties of ZnO Nanorods

Well-defined Dy-doped ZnO rods were synthesized by hydrothermal route. Various studies were carried out on the synthesized rods like x-ray diffraction to confirm their hexagonal wurtzite structure; TEM, HRTEM and selected area electron diffraction to establish their rodlike structure; energy-dispersive x-ray spectroscopy analysis confirming appropriate substitution of dopant; UV-Vis spectra, which showed decrease in band gap with dopant concentration and photoluminescence study furnishing information regarding the presence of various types of defects. Further, magnetic studies were done using VSM to confirm roomtemperature ferromagnetic behaviour of both for undoped and doped ZnO rods and, the electrical studies were performed using four probe method, which confirmed that the ‘variation in resistivity with dopant concentration’ was related to crystallinity of the samples. UV-Vis spectra showed effect of dopant concentration on band gap and photoluminescence study confirms induced ferromagnetic behaviour due to Dy doping.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Reordering between tetrahedral and octahedral sites in ultrathin magnetite films grown on MgO(001)

Magnetite ultrathin films were grown using different deposition rates and substrate temperatures. The structure of these films was studied using (grazing incidence) x-ray diffraction, while their surface structure was characterized by low energy electron diffraction. In addition to that, we performed x-ray photoelectron spectroscopy and magneto optic Kerr effect measurements to probe the stoichiometry of the films as well as their magnetic properties. The diffraction peaks of the inverse spinel structure, which originate exclusively from Fe ions on tetrahedral sites are strongly affected by the preparation conditions, while the octahedral sites remain almost unchanged. With both decreasing deposition rate as well as decreasing substrate temperature, the integrated intensity of the diffraction peaks originating exclusively from Fe on tetrahedral sites is decreasing. We propose that the ions usually occupying tetrahedral sites in magnetite are relocated to octahedral vacancies. Ferrimagnetic behaviour is only observed for well ordered magnetite films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ordered structures based on self-organized Au and CdSe nanoparticles

Methods for obtaining cadmium selenide and gold nanoparticles have been developed. The sizes of the nanoparticles are determined and the morphology, structure, and chemical composition of these nanoparticles and their ensembles are studied by a complex of structural methods: electron diffraction, X-ray diffraction, energy-dispersive X-ray analysis, high-resolution transmission electron microscopy, and small-angle X-ray scattering. Gold nanoparticles are mainly spherical and have an average size of 10 nm. They are single-phase and have an fcc crystal structure. Samples of synthesized CdSe nanoparticles contain monodisperse spherical particles 12 nm in size with a wurtzite structure. The deposition of nanoparticles on a carbon substrate is accompanied by their self-organization into a closely packed two-dimensional structure with a pronounced texture in which all nanoparticles are oriented in the [001] direction perpendicularly to the carbon substrate plane.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Capturing Structural Dynamics in Crystalline Silicon Using Chirped Electrons from a Laser Wakefield Accelerator

Recent progress in laser wakefield acceleration has led to the emergence of a new generation of electron and X-ray sources that may have enormous benefits for ultrafast science. These novel sources promise to become indispensable tools for the investigation of structural dynamics on the femtosecond time scale, with spatial resolution on the atomic scale. Here in this paper, we demonstrate the use of laser-wakefield-accelerated electron bunches for time-resolved electron diffraction measurements of the structural dynamics of single-crystal silicon nano-membranes pumped by an ultrafast laser pulse. In our proof-of-concept study, we resolve the silicon lattice dynamics on a picosecond time scale by deflecting the momentum-time correlated electrons in the diffraction peaks with a static magnetic field to obtain the time-dependent diffraction efficiency. Further improvements may lead to femtosecond temporal resolution, with negligible pump-probe jitter being possible with future laser-wakefield-accelerator ultrafast-electron-diffraction schemes.

36 MATERIALS SCIENCE↗

Twist-Angle-Dependent Ultrafast Charge Transfer in MoS 2 -Graphene van der Waals Heterostructures

Vertically stacked transition metal dichalcogenide-graphene heterostructures provide a platform for novel optoelectronic applications with high photoresponse speeds. Photoinduced nonequilibrium carrier and lattice dynamics in such heterostructures underlie these applications but have not been understood. In particular, the dependence of these photoresponses on the twist angle, a key tuning parameter, remains elusive. Here, using ultrafast electron diffraction, we report the simultaneous visualization of charge transfer and electron–phonon coupling in MoS 2 -graphene heterostructures with different stacking configurations. We find that the charge transfer timescale from MoS 2 to graphene varies strongly with twist angle, becoming faster for smaller twist angles, and show that the relaxation timescale is significantly shorter in a heterostructure as compared to a monolayer. These findings illustrate that twist angle constitutes an additional tuning knob for interlayer charge transfer in heterobilayers and deepen our understanding of fundamental photophysical processes in heterostructures, of importance for future applications in optoelectronics and light harvesting.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Epitaxial Fe-Ge thin films on Ge(111): Morphology, structure, and magnetic properties versus stoichiometry

We have studied the growth and magnetic properties of thin Fe-Ge films synthesized (codeposited at room temperature and postannealed at 250 deg. C) on Ge(111) wafers versus stoichiometry. Morphology and crystal structure have been investigated in situ by means of scanning tunneling microscopy, low-energy electron diffraction, and x-ray photoelectron diffraction and ex situ with x-ray diffraction. The magnetic properties were characterized ex situ by conventional polar and longitudinal magneto-optical Kerr effect and transverse biased initial inverse susceptibility and torque measurements. It is found that the growth is epitaxial for Ge content up to approx48 at. % (approxFe{sub 1.1}Ge composition). In particular, the film is homogeneous and flat and adopts a crystalline structure of hexagonal symmetry derived from the B8{sub 2} (Ni{sub 2}In) structure over a wide stoichiometry range extending from Fe{sub 2}Ge to Fe{sub 1.1}Ge. The epitaxial orientation between the Ge substrate and the germanide layer is (0001)Fe-Ge||(111)Ge with [1120]Fe-Ge||110]Ge. We found however that the surface periodicity and the out-of-plane lattice parameter c evolve within this stoichiometry range and two distinct stoichiometry regimes appear on both sides of a critical stoichiometry (approxFe{sub 1.5}Ge). Indeed, from Fe{sub 2}Ge to Fe{sub 1.5}Ge the surface periodicity is p(2x2) and c continuously decreases with Fe content, whereas from Fe{sub 1.5}Ge to Fe{sub 1.1}Ge the surface periodicity is (sq root(3)xsq root(3))R30 deg. and c remains constant. These features have been interpreted as a clear fingerprint of a minor transformation of the crystalline structure but without any change in symmetry. This structural order transformation is discussed in relation to previous results reported in the case of macroscopic single-crystal Fe-Ge ingots. On both sides of the wide [Fe{sub 2}Ge,Fe{sub 1.1}Ge] composition range the layer is no more homogeneous. More precisely, for higher Fe content the film contains both the above mentioned Ni{sub 2}In-derived phase and a Fe-richer phase (probably bcc Fe) whereas for higher Ge content the layer is amorphous. Magnetic characterization showed in particular that the homogeneous Ni{sub 2}In-derived epilayers are ferromagnetic with a Curie temperature that varies drastically with the stoichiometry, rising up to a high T{sub C} value of approx450 K for the Fe-rich Fe{sub 1.9}Ge composition. Finally, whatever the stoichiometry, the magnetic easy axis of the homogeneous phase lies in the film plane and a small uniaxial anisotropy is superimposed on a sixfold order one that results from the hexagonal symmetry of the crystallographic structure.

36 MATERIALS SCIENCE↗

Metal thin film growth on multimetallic surfaces: From quaternary metallic glass to binary crystal

The work presented in this thesis mainly focuses on the nucleation and growth of metal thin films on multimetallic surfaces. First, we have investigated the Ag film growth on a bulk metallic glass surface. Next, we have examined the coarsening and decay of bilayer Ag islands on NiAl(110) surface. Third, we have investigated the Ag film growth on NiAl(110) surface using low-energy electron diffraction (LEED). At last, we have reported our investigation on the epitaxial growth of Ni on NiAl(110) surface. Some general conclusions can be drawn as follows. First, Ag, a bulk-crystalline material, initially forms a disordered wetting layer up to 4-5 monolayers on Zr-Ni-Cu-Al metallic glass. Above this coverage, crystalline 3D clusters grow, in parallel with the flatter regions. The cluster density increases with decreasing temperature, indicating that the conditions of island nucleation are far-from-equilibrium. Within a simple model where clusters nucleate whenever two mobile Ag adatoms meet, the temperature-dependence of cluster density yields a (reasonable) upper limit for the value of the Ag diffusion barrier on top of the Ag wetting layer of 0.32 eV. Overall, this prototypical study suggests that it is possible to grow films of a bulk-crystalline metal that adopt the amorphous character of a glassy metal substrate, if film thickness is sufficiently low. Next, the first study of coarsening and decay of bilayer islands has been presented. The system was Ag on NiAl(110) in the temperature range from 185 K to 250 K. The coarsening behavior, has some similarities to that seen in the Ag(110) homoepitaxial system studied by Morgenstern and co-workers. At 185 K and 205 K, coarsening of Ag islands follows a Smoluchowski ripening pathway. At 205 K and 250 K, the terrace diffusion limited Ostwald ripening dominants. The experimental observed temperature for the transition from SR to OR is 205 K. The SR exhibits anisotropic island diffusion and the OR exhibits 1D decay of island length while keeping the corresponding island width constant. Third, LEED indicates that, up to about 6 BL (12 ML), the Ag film adopts the (110) structure on lattice matched NiAl(110) surface, supporting the previous assignment based upon island heights measured in STM. Starting at 4.5 to 6 BL, (111) diffraction pattern is detected. This is also in agreement with previous STM study. Careful examinations of the LEED patterns reveal the slight difference in lattice constants between bulk Ag and bulk NiAl. At last, we performed STM studies of Ni deposition on NiAl(110) in the temperature range from 200 K to 400 K. Ni forms 'dense' Ni(100)-like islands on NiAl(110) with a zig-zag shaped stripe feature which is probably due to strain relief. DFT analysis provides insights into the island growth shapes, which are rationalized by the thermodynamics and kinetics of the film growth process. For thick Ni films (coverage exceeding 6 ML), a Ni(111)-like structure developed. Traditional MF theory is applied to analyze island density at 200 K. Deviation from homogeneous nucleation behavior for island size distribution and island density reveals the presence of heterogeneous nucleation mediated by the Ni antisite point defects on NiAl(110) surface.

36 MATERIALS SCIENCE↗