At least 991 records · Page 55

Experimental Study of the Mold Flow Induced by a Swirling Flow Nozzle and Electromagnetic Stirring for Continuous Casting of Round Blooms

This study focuses on an experimental investigation of the fluid flow in round bloom continuous casting using a 1:3 model of the industrial casting process. A swirling flow nozzle, represented by the specific design of the RHI Magnesita GYRONOZZLE, is used to produce a swirling motion in the cylindrical mold. The test section is integrated into the Mini-LIMMCAST facility at HZDR, which is operated at room temperature using the ternary alloy GaInSn. Systematic measurements of horizontal and vertical velocity profiles are performed by means of the Ultrasound Doppler Velocimetry. The second part of the study focuses on the interaction between the flow driven by the GYRONOZZLE and concurrent electromagnetic stirring in the mold (M-EMS) by applying rotating magnetic fields (RMFs) at different magnetic flux densities. The effect of the GYRONOZZLE on the flow pattern inside the mold is examined with and without superimposed RMFs and compared to those of a standard single-port nozzle. The measurements reveal that the GYRONOZZLE induces a swirling flow in the whole mold. It is further shown that the influence of a simultaneously applied RMF is mainly restricted to the lower part of the mold since the transport of angular momentum to the top is suppressed by the jets pouring out from the GYRONOZZLE.

36 MATERIALS SCIENCE↗

Effect of Aging Treatment on the Precipitation Behavior and Mechanical Properties of Mg-9Gd-3Y-1.5Zn-0.5Zr Alloy

Aging heat treatments of an extruded Mg-9Gd-3Y-1.5Zn-0.5Zr (wt.%) alloy at 200, 225, and 250 °C for various times were studied. The results show that dynamic recrystallization (DRX) occurred during the extrusion process and the alloy exhibited a significant aging hardening response at temperatures ranging from 200 to 225 °C. The precipitation sequence of the alloy at 225 °C was supersaturated solid solution (SSSS) → β″ (D0{sub 19}, Mg{sub 3}RE) → β′ (bco, Mg{sub 15}RE{sub 3}), where the β′ phase was the primary precipitated phase. A large amount of discontinuous lamellar-shaped 14H-structure long period stacking ordered (LPSO) phase was also observed in the α-Mg matrix before and after aging treatments. Owing to the combined strengthening effect of fine DRXed grains, β′ nanoparticles, and widespread LPSO phases, the ultimate tensile strength and tensile yield strength of the peak-aged extruded alloy reached 409 and 303 MPa, respectively. The elongation in this circumstance was ~7.1%, which was slightly lower than that of the alloy before aging treatment.

36 MATERIALS SCIENCE↗

Effect of Tempering Temperature on the Microstructure and Properties of Fe-2Cr-Mo-0.12C Pressure Vessel Steel

To obtain the high-temperature strength and toughness of the medium–high-temperature–pressure steel, the microstructure evolution and mechanical properties of Fe-2Cr-Mo-0.12C steel subjected to three different tempering temperatures after being normalized were investigated. The results show that the microstructure of the sample, tempered in the range 675-725 °C for 50 min, did not change dramatically, yet the martensite/austenite constituents decomposed, and the bainite lath merged together and transformed into polygonal ferrite. At the same time, the precipitate size increased with an increase in tempering temperature. With the increase in the tempering temperature from 675 to 725 °C, the impact absorbed energy of the Fe-2Cr-Mo-0.12C steel at −40 °C increased from 257 to 325 J, and the high-temperature yield strength decreased; however, the high-temperature ultimate tensile strength tempered at 700 °C was outstanding (422-571 MPa) at different tested temperatures. The variations of the properties were attributed to the decomposition of M/A constituents and the coarsening of the precipitates. Fe-2Cr-Mo-0.12C steel normalized at 930 °C and tempered at 700 °C was found to have the best combination of ductility and strength.

36 MATERIALS SCIENCE↗

Processing and Characterization of Ag-Cu-Sn Brazing Alloy Prepared by a Mechanical Alloying Method

Mechanical alloying was used to prepare an Ag-Cu-Sn brazing alloy with the low amounts of intermetallic compounds. X-ray diffraction and differential scanning calorimetry were carried out to investigate the phase transformation of the as-milled samples. It seemed that the intermetallic compounds experienced the stage of synthesis-decomposition-resynthesis in the ball milling process. By controlling the ball milling time and tin contents, the solid solution phases of Ag (Cu, Sn) and Ag (Cu) were achieved in the 60Ag30Cu10Sn sample after milling for 40 h. Although the intermetallic compound will be generated during the brazing process, the improvement of their distributed morphology is beneficial for the good bonding interface of the joint with stainless steel substrate.

36 MATERIALS SCIENCE↗

High Damping of Lightweight TiNi-Ti{sub 2}Ni Shape Memory Composites for Wide Temperature Range Usage

A bimodal porous TiNi-Ti{sub 2}Ni shape memory alloy composite (SMAC) with 59% porosity was fabricated by sintering Ti-46at.%Ni elemental powders with pore-forming agent. The porous TiNi-Ti{sub 2}Ni SMAC contains two irregular pores of about 400 and 120 μm. We investigated the microstructure and pore morphology correlated with the mechanical properties and damping capacities of the SMAC. Ti{sub 2}Ni intermetallic phases with size of 1-3 μm were homogeneously distributed in the TiNi matrix. The porous TiNi-Ti{sub 2}Ni SMAC exhibits exceptionally high inverse mechanical quality factor (Q{sup −1}) of ~0.25 at < 40 °C, which is among the highest value reported for porous/dense shape memory alloys or composites to best of our knowledge, and it shows very high compressive fracture strain of about 25%. Moreover, the fabricated porous SMAC at relatively low strain amplitude can exhibit considerable high Q{sup −1} of 0.06 ~ 0.11 for a wide range of temperature between − 90 and 200 °C, which is attributed to the stress concentration distribution provided by the bimodal structure of pores and the massive interfaces between pore/matrix and TiNi/Ti{sub 2}Ni. These porous SMACs can be an ideal candidate for using as a lightweight damping material in the energy-saving applications.

36 MATERIALS SCIENCE↗

Analysis of Plastic Flow Instability During Superplastic Deformation of the Zn-Al Eutectoid Alloy Modified with 2 wt.% Cu

The aim of this work is to analyze the plastic flow instability in Zn-21Al-2Cu alloy deformed under 10{sup −3} s{sup −1} and 513 K, which are optimum conditions for inducing superplastic behavior in this alloy. An evaluation using the Hart and Wilkinson–Caceres criteria showed that the limited stability of plastic flow observed in this alloy is related to low values of the strain-rate sensitivity index (m) and the strain-hardening coefficient (γ), combined with the tendency of these parameters to decrease depending on true strain (ε). The reduction in m and γ values could be associated with the early onset of plastic instability and with microstructural changes observed as function of the strain. Grain growth induced by deformation seems to be important during the first stage of deformation of this alloy. However, when ε > 0.4 this growth is accompanied by other microstructural rearrangements. These results suggest that in this alloy, a grain boundary sliding mechanism acts to allow a steady superplastic flow only for ε < 0.4. For ε values between 0.4 and 0.7, observed occurrences of microstructural changes and severe neck formation lead to the supposition that there is a transition in the deformation mechanism. These changes are more evident when ε > 0.7 as another mechanism is thought to take over.

36 MATERIALS SCIENCE↗

Application of Al-2La-1B Grain Refiner to Al-10Si-0.3Mg Casting Alloy

This paper reports the application and microstructure refining effect of an Al-2La-1B grain refiner in Al-10Si-0.3Mg casting alloy. Compared with the traditional Al-5Ti-1B refiner, Al-2La-1B refiner shows better performances on the grain refinement of Al-10Si-0.3Mg alloy. Transmission electron microscopy analysis suggests that the crystallite structure features of LaB6 are beneficial to the heterogeneous nucleation of α-Al grains. Regarding the mechanical performances, tensile properties of Al-10Si-0.3Mg casting alloy are prominently improved, due to the refined microstructures.

36 MATERIALS SCIENCE↗

Elevated Temperature Corrosion Studies of AlCrN and TiAlN Coatings by PAPVD on T91 Boiler Steel

The present investigation discusses the hot corrosion behavior of AlCrN and TiAlN nano-coatings on T91 boiler steel by PAPVD process subjected to molten salt of Na{sub 2}SO{sub 4}-60%V{sub 2}O{sub 5} at 900 °C for 50 cycles. Surface and cross-sectional studies were performed by AFM, SEM/EDS and XRD techniques to understand the corrosion kinetics and mechanism. T91 bare boiler steel as well as TiAlN-coated specimen has shown higher internal oxidation as well as weight gain. The better corrosion resistance of AlCrN-coated specimen has been observed by virtue of higher availability of Cr and Al in the oxide scale as well as adherent and dense coating. The betterment of AlCrN coating can be attributed to low internal oxidation as well as movement of Cr and Al toward oxide scale to form protective corrosion barriers.

36 MATERIALS SCIENCE↗

Elevated Temperature Solid Particle Erosion Performance of Plasma-Sprayed Co-based Composite Coatings with Additions of Al{sub 2}O{sub 3} and CeO{sub 2}

In this paper, investigation into solid particle erosion behavior of atmospheric plasma-sprayed composite coating of CoCrAlY reinforced with Al{sub 2}O{sub 3} and CeO{sub 2} oxides on Superni 76 at elevated temperature of 600 °C is presented. Alumina particles are used as erodent at two impact angles of 30° and 90°. The microstructure, porosity, hardness, toughness and adhesion properties of the as-sprayed coatings are studied. The effects of temperature and phase transformation in the coatings during erosion process are analyzed using XRD and EDS techniques. Optical profilometer is used for accurate elucidation of erosion volume loss. CoCrAlY/CeO{sub 2} coating showed better erosion resistance with a volume loss of about 50% of what was observed in case of CoCrAlY/Al{sub 2}O{sub 3}/YSZ coating. Lower erosion loss is observed at 90° as compared to 30° impact angle. The erosion mechanism evaluated using SEM micrograph revealed that the coatings experienced ductile fracture exhibiting severe deformation with unusual oxide cracks. Reinforced metal oxides provide shielding effect for erodent impact, enabling better erosion resistance. The oxidation of the coating due to high-temperature exposure reforms erosion process into oxidation-modified erosion process.

36 MATERIALS SCIENCE↗

On the Influence of the Heat Treatment Temperature on the Superelastic Compressive Behavior of the Ni-Rich NiTi Shape Memory Alloy

In this paper, the relationship between the heat treatment temperature and the thermomechanical behavior of the Ni-rich NiTi shape memory alloy was experimentally investigated. Thermal analysis was performed through a differential scanning calorimetry experiments, and the NiTi superelastic effect was exhibited through loading/unloading compression cycle. It was found that the transformation temperatures and the compressive mechanical response are strongly affected by the heat treatment temperatures. The stress-induced phase transformation was characterized through the relationship between the heat treatment temperature and transformation stresses, elastic moduli and the deformation level upon loading. Subsequently, the evolution of the mechanical hysteresis loops and the mechanical dissipated energy was discussed. The obtained findings are supported by hardness measurements. To better understand the global tendency of the various phase transformation stages, the critical stress-temperature diagram was provided for different proposed heat treatment temperatures.

36 MATERIALS SCIENCE↗

Effects of Heat Treatment on Corrosion and Wear Behaviors of Mg-6Gd-2Zn-0.4Zr Alloy in Simulated Body Fluid

Mg-6Gd-2Zn-0.4Zr (wt.%, GZ62K) alloy was processed by solution treatment under different temperatures. The microstructure, hardness, corrosion and wear behaviors in simulated body fluid (SBF) have been studied. The results indicate that the (Mg, Zn){sub 3}Gd phase decreases, the precipitated phases gradually increase, and the long-period stacking ordered structure disappears with the increase of solution temperature. The alloy has better corrosion resistance after solution treatment, and that solution treated at 490 °C for 12 h shows the best corrosion resistance. The friction coefficient of the alloy under dry sliding condition decreases slightly, but the mass loss increases with increasing the solution temperature. The alloy solution treated at 460 °C for 12 h exhibits the lowest friction coefficient and mass loss in SBF, and it also has the best wear resistance under dry sliding condition.

36 MATERIALS SCIENCE↗

Electrodeposition Process and Performance of CuIn(Se{sub x}S{sub 1−x}){sub 2} Film for Absorption Layer of Thin-Film Solar Cells

CuIn(Se{sub x}S{sub 1−x}){sub 2} thin film is prepared by the electrodeposition method for the absorption layer of the solar cell. The CuIn(Se{sub x}S{sub 1−x}){sub 2} films are characterized by cyclic voltammetry measurement for the reduction of copper, indium, selenium and sulfur in selenium and sulfur in aqueous solutions with sodium citrate and without sodium citrate. In the four cases, the defined reduction process for every single element is obtained and it is observed that sodium citrate changes the reduction potentials. A linear relationship between the current density of the reduction peak and (scan rate v){sup 1/2} for copper and indium is achieved, indicating that the process is diffusion controlled. The diffusion coefficients of copper and indium ions are calculated. The diffusional coefficient D value of copper is higher than that of indium, and this is the reason why the deposition rate of copper is higher. When four elements are co-deposited in the aqueous solution with sodium citrate, the quaternary compound of CuIn(Se{sub x}S{sub 1−x}){sub 2} is deposited together with Cu{sub 3}Se{sub 2} impure phases after annealing, as found by XRD spectra. Morphology is observed by SEM and AFM. The chemical state of the films components is analyzed by XPS. The UV-Visible spectrophotometer and electrochemistry workstation are employed to measure the photoelectric properties. The results show that the smooth, uniform and compact CuIn(Se{sub x}S{sub 1−x}){sub 2} film is a semiconductor with a band gap of 1.49 eV and a photovoltaic conversion efficiency of 0.45%.

36 MATERIALS SCIENCE↗

Surface Layers of Zr-18%Nb Alloy Modified by Ultrasonic Impact Treatment: Microstructure, Hardness and Corrosion

Near-surface layers in Zr-18%Nb alloy were modified using ultrasonic impact treatment (UIT). The effects of the UIT processing time on a microstructural formation, omega/alpha precipitations, microhardness and corrosion are analyzed. XRD analysis, TEM and SEM observations and EDX characterization allow establishing the links between the microstructure, microhardness and corrosion behavior of the surface layers formed. At the strain extent up to e ≈ 0.3, structural formation occurs under influence of deformation induced heating, which facilitates omega precipitation in beta phase and mechanically induced oxygen transport and oxide formation. XRD analysis reveals moderate compressive residual stresses (− 160 MPa) and pronounced {110} texture after the UIT process. Generation of dislocations and hindering of their movement by nanoscale omega precipitates manifest themselves as the broadening of diffraction peaks occurred mainly owing to the lattice microstrains, and they provide marked strain hardening. The enhanced anticorrosion properties of Zr-18%Nb alloy in saline solution were concluded to be a result of the formation of a protective oxide film, {110} texture and compressive stresses.

36 MATERIALS SCIENCE↗

Influence of Asymmetric Cyclic Loading on Structural Evolution and Deformation Behavior of Cu-5 at.% Zr Alloy: An Atomistic Simulation-Based Study

Molecular dynamics (MD) simulation-based studies of tensile test and structural evolution of Cu-5 at.% Zr alloy under asymmetric cyclic loading (i.e., ratcheting behavior) considering various stress ratios such as − 0.2, − 0.4 and − 0.6 for different temperatures, viz.≈ 100, 300 and 500 K have been performed using embedded atom model Finnis–Sinclair potential. According to obtained stress–strain response from MD calculation, Cu-5 at.% Zr alloy specimen is pristine in nature as sudden drop in stress just after yield stress and subsequent elastic type deformation are observed for this alloy. Predicted ratcheting strain by MD simulation for Cu-5 at.% Zr alloy varies from 4.5 to 5%. Significant increase in ratcheting strain has been observed with the increase in temperature. Slight reduction in crystallinity is identified at the middle of the each loading cycle from the performed radial distribution function analysis and cluster analysis.

36 MATERIALS SCIENCE↗

Experimental Research on Selective Laser Melting AlSi10Mg Alloys: Process, Densification and Performance

In this work, a set of experiments was designed to investigate the effect of process parameters on the relative density of the AlSi10Mg parts manufactured by SLM. The influence of laser scan speed v, laser power P and hatch space H, which were considered as the dominant parameters, on the powder melting and densification behavior was also studied experimentally. In addition, the laser energy density was introduced to evaluate the combined effect of the above dominant parameters, so as to control the SLM process integrally. As a result, a high relative density (> 97%) was obtained by SLM at an optimized laser energy density of 3.5-5.5 J/mm{sup 2}. Moreover, a parameter–densification map was established to visually select the optimum process parameters for the SLM-processed AlSi10Mg parts with elevated density and required mechanical properties. The results provide an important experimental guidance for obtaining AlSi10Mg components with full density and gradient functional porosity by SLM.

36 MATERIALS SCIENCE↗

A Two-Way Shape Memory Study on Ni-Rich NiTi Shape Memory Alloy by Combination of the All-Round Treatment and the R-Phase Transformation

Ni{sub 4}Ti{sub 3} precipitates are formed in Ni-rich NiTi shape memory alloys (SMAs) after a certain heat treatment. Such a treatment then results in the changed phase transformation behavior of the alloy switching from the one-step reversible phase change B2 ↔ B19′ to the two-step, B2 ↔ R ↔ B19′, phase change. The present study reports a two-way shape memory (TWSM) due to an all-round treatment followed by an R-phase constraint aging at room temperature. The enhanced TWSM behavior was observed upon temperature cycling between 273 K (R-phase) and 77 K (B19′ phase). The effect of various constraint strains in R-phase aging by employing different diameters of the constraint ring was studied. However, the TWSM effect due to constraining the R-phase will be eliminated after a temperature rise of specimen to the fully parent phase (373 K).

36 MATERIALS SCIENCE↗

Effects of Tungsten Addition on the Microstructure and Mechanical Properties of Near-Eutectic AlCoCrFeNi{sub 2} High-Entropy Alloy

The effects of tungsten addition on the microstructure and mechanical properties of near-eutectic AlCoCrFeNi{sub 2} high-entropy alloy were investigated in this paper. The AlCoCrFeNi{sub 2}W{sub x} alloys comprised the primary BCC phase plus eutectic FCC/BCC phases. It was found that W element can both promote the formation of the primary BCC phase and act as a solid solution strengthening element. The hardness of the AlCoCrFeNi{sub 2}W{sub x} alloys increased from HV 293 to HV 356.2 with the increase in W content. The addition of W element improved the strength of alloys but reduced ductility. Thereinto, the AlCoCrFeNi{sub 2}W{sub 0.2} alloy showed the most excellent compressive properties with the fracture strength of 2785.9 MPa and the plastic strain of 0.42, respectively, which implied the potential industrial application values.

36 MATERIALS SCIENCE↗

High Strength, Utilizable Ductility and Electrical Conductivity in Cold Rolled Sheets of Cu-Cr-Zr-Ti Alloy

The microstructure and properties of Cu-0.5Cr-0.03Zr-0.04Ti (wt.%) alloy subjected to cold rolling and aging were investigated using hardness and electrical conductivity measurement, tensile testing, and transmission electron microscopy. Plates subjected to 85% reduction in thickness showed significant improvement in the strength compared to solution treated and aged condition. By proper selection of aging temperature, ductility could be significantly improved without reduction in the strength. Aging of the cold rolled sheet at 420 °C for 1 h yielded an ultimate tensile strength and yield strength of 540 and 460 MPa, respectively. On the other hand, total and uniform elongation was 16 and 12%, respectively, with an electrical conductivity of 65 %IACS. The combination of properties achieved after cold rolling and aging is attributed to the higher dislocation density, ultrafine grains and nano-sized chromium precipitates.