At least 973 records · Page 54

Electrolyte design for Li metal-free Li batteries

Li metal, with the lowest thermodynamically achievable negative electrochemical potential and the highest specific capacity (3860 mAh g -1 ), is the ultimate anode choice for Li batteries. However, the highest reported Li plating/stripping Coulombic efficiency (CE) of 99.5% after extensive efforts is still too low for the Li metal-free (all the Li metal in cycling comes from cathode, without anode pre-lithiation) Li metal batteries. The low CE is attributed to both non-uniform Li plating/stripping on the lithiophobic Cu current collector and Li dendrite growth through lithiophilic organic–inorganic solid electrolyte interphase (SEI) formed in carbonate electrolytes. Here, we use a lithiophilic Bismuth graphite blend (Bi–Gr) substrate to replace lithiophobic Cu current collector to seed a uniform Li nucleation, and form a lithiophobic LiF-rich SEI rather than lithiophilic organic-rich SEI to suppress Li dendrite growth. Molecular dynamics simulations reveal the preferential reduction of anions in 2.0 M LiPF 6 in tetrahydrofuran/2-methyl tetrahydrofuran (2.0 M LiPF 6 –mixTHF) electrolyte to generate LiF-rich SEI on plated Li. Bi–Gr substrate and 2.0 M LiPF 6 –mixTHF electrolyte enable the Li anodes to achieve a record high CE of 99.83% at a high capacity of 1.0 mAh cm -2 and current of 0.5 mA cm -2 . The Bi particles serve as dispersed nucleation centers that promote uniform Li deposition with strong adhesion to the substrate to avoid dead Li, while the lithiophobic LiF-rich SEI promotes lateral Li growth and suppresses the vertical Li dendrite growth even at a high current density of 3.0 mA cm -2 and high areal capacities of 3.0 mAh cm -2 . The regulation of Li nucleation and growth enables the Li metal-free LiFePO 4 full cells to achieve 100 cycles at a practical areal capacity of >2.0 mAh cm -2 . This article highlights the benefits of simultaneous substrate design to improve Li nucleation and electrolyte design to promote lithiophobic SEI growth, enabling a promising and practical route Li metal-free Li metal batteries.

36 MATERIALS SCIENCE↗

Aliovalent Anion Incorporation in Halide Na-ion Conductors for Enhanced Ionic Conductivity

Halide-based solid electrolytes (SEs), particularly zirconium (Zr)-centered halides, are attractive from a material cost perspective. Nevertheless, Zr-centered halide SEs are hindered by their low ionic conductivity. Here, in this study, we report on the cubic Na 3 ZrCl 5 S superionic conductor through strategic sulfur anion incorporation, achieving 10 times higher ionic conductivity than that of Na 2 ZrCl 6 . With the optimal composition, the highest ionic conductivity of 0.753 mS cm –1 is obtained for the 0.6Na 2 S–1.4NaCl–ZrCl 4 compound. When paired with a NaCrO 2 cathode, the assembled all-solid-state batteries (ASSBs) achieve a specific discharge capacity of 110 mA h g –1 at 0.1C and exhibit long-term cycling stability at 0.3C at room temperature over 1000 cycles (with 83% capacity retention). Moreover, in situ electrochemical impedance spectroscopy combined with distribution of relaxation times analysis reveal the dynamically interfacial stability between Na halide with electrodes. In conclusion, this work highlights the design and synthesis of advanced halide electrolytes through anion incorporation, paving the way for the development of next-generation ASSBs.

Guo, Xiaolin [Univ. of Louisville, KY (United Stat↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Enable High-Energy LiNi0.5Co0.2Mn0.3O2 by Ultra-Thin Coating through Wet Impregnation

A high cut-off voltage is required for nickel-rich layered oxide LiNixCoyMnzO2 (NCM) to meet the high energy density requirement of lithium-ion batteries in electric vehicles. However, such a high voltage application leads to an unstable interface between NCM and liquid electrolytes. To stabilize the interface, the facile wet impregnation method has been developed to apply an ultra-thin Al2O3 coating layer on the NCM particles. This coating layer was found to have a strong interaction with the NCM and resulted in Al-doped NCM at the surface structure of NCM. The change of surface structure can not only reduce the surface resistance of lithium diffusion of LiNi0.5Co0.2Mn0.3O2 (NCM523), but also stabilize the solid electrolyte interface between NCM523 and the electrolyte with the cut-off voltage of 4.5 V vs. Li/Li+. Compared to other coating methods, wet impregnation coating can provide an ultra-thin and uniform coating with surface doping on NCM particles. Furthermore, this scalable coating method can be applied to various electrode materials without adding much additional cost.

25 ENERGY STORAGE↗

Combined, time-resolved, in situ neutron reflectometry and X-ray diffraction analysis of dynamic SEI formation during electrochemical N 2 reduction

One means of improving performance for electrochemical ammonia production through the Li-mediated N 2 reduction reaction (Li-NRR) is by cycling the current driving the reaction between open-circuit conditions and periods of applied current density. Herein, we have investigated the dynamics of the electrode–electrolyte interface under Li-NRR conditions during current cycling using in situ time-resolved neutron reflectometry and grazing-incidence synchrotron X-ray diffraction. During cycling, measured neutron reflectivity curves indicated bilayer formation in which Li-containing species such as LiOH, Li 2 O, and small quantities of Li 3 N and metallic Li primarily appeared in a thin layer at the cathode surface, above which formed a much larger, porous, ‘solid–electrolyte interface’ (SEI) layer. Upon return to open-circuit conditions, Li-containing species quickly moved out of the thin layer, leaving a compact, stable layer of decomposition products underneath the SEI layer. This SEI layer concomitantly filled with electrolyte or dissolved, becoming indistinguishable from the electrolyte via contrast in scattering-length density (SLD). During the second current cycle, Li-containing species again preferentially deposited directly atop the cathode, with the thick SEI-like layer again appearing within a minute. This SEI layer exhibited a lower SLD more quickly than in the first cycle, which might suggest that Li-containing species become distributed within the porous SEI layer. Furthermore, these time-resolved observations of SEI and plated layers during current cycling suggest that benefits associated with return to open-circuit conditions between periods of applied current density may be related to the concomitant loss of Li-containing species from a thin layer at the cathode surface into a porous SEI layer that becomes filled with electrolyte or dissolves.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High Sulfur Loading and Capacity Retention in Bilayer Garnet Sulfurized‐Polyacrylonitrile/Lithium‐Metal Batteries with Gel Polymer Electrolytes

The cubic‐garnet (Li 7 La 3 Zr 2 O 12 , LLZO) lithium–sulfur battery shows great promise in the pursuit of achieving high energy densities. The sulfur used in the cathodes is abundant, inexpensive, and possesses high specific capacity. In addition, LLZO displays excellent chemical stability with Li metal; however, the instabilities in the sulfur cathode/LLZO interface can lead to performance degradation that limits the development of these batteries. Therefore, it is critical to resolve these interfacial challenges to achieve stable cycling. Here, an innovative gel polymer buffer layer to stabilize the sulfur cathode/LLZO interface is created. Employing a thin bilayer LLZO (dense/porous) architecture as a solid electrolyte and significantly high sulfur loading of 5.2 mg cm −2 , stable cycling is achieved with a high initial discharge capacity of 1542 mAh g −1 (discharge current density of 0.87 mA cm −2 ) and an average discharge capacity of 1218 mAh g −1 (discharge current density of 1.74 mA cm −2 ) with 80% capacity retention over 265 cycles, at room temperature (22 °C) and without applied pressure. Achieving such stability with high sulfur loading is a major step in the development of potentially commercial garnet lithium–sulfur batteries.

25 ENERGY STORAGE↗

Improving Cycling Performance of Anode-Free Lithium Batteries by Pressure and Voltage Control

The anode-free lithium (Li) batteries (AFLBs) have great potential to provide higher energy density than most other batteries. However, the performance of AFLBs is very sensitive to pressure and other operating parameters, especially for coin cells widely used in AFLB investigations. Therefore, optimizing cell assembly parameters and test protocol is critical to get reliable and comparable results in this field. In this work, the operating voltage range of AFLBs using a localized high concentration electrolyte has been optimized. The morphology of the deposited Li in AFLBs is much more indicting to the pressure than other type of batteries due to the absence of anode active material (i.e. Li) as a pressure cushion layer in the as prepared cells. With an optimized cycling protocol, a thin layer of uniform nucleation sites can be formed in the initial cycle which will facilitate smooth Li desposition/stripping in the subsequent cycles of AFLBs. The solid electrolyte interphase layer formed under optimized pressure and uniform pressure distribution exhibits a good mechanical stability even after long-term cycling. In conclusion, with an optimized cell configuration, the internal pressure in the coin cells has been optimized to improve the cycling performance of AFLBs (Cu||NMC811) with 72% of capacity retention in 100 cycles.

25 ENERGY STORAGE↗

Discharge Rate‐Driven Li 2 O 2 Growth Exhibits Unconventional Morphology Trends in Solid‐State Li‐O 2 Batteries

Solid-state lithium oxygen batteries (LOBs) are known for their enhanced safety, higher electrochemical stability, and improved energy density compared to liquid-state LOBs. However, the investigation of solid-state LOBs is limited with little understanding of their discharge and charge processes. In this work, a polymer-based solid-state LOB is used to investigate the effect of discharge rate on lithium peroxide (Li 2 O 2 ) formation, the oxygen evolution reaction (OER), and cycle performance. Notably, we observe a counterintuitive trend: Li 2 O 2 particle size increases with increasing discharge current density, in contrast to liquid systems. This behavior arises from inherent space charge layers that restrict Li⁺ transport under high current, and spatially heterogeneous active sites at the solid electrolyte–cathode interface, directly evidenced by small angle X-ray scattering (SAXS), which govern nucleation accessibility and promote site-selective Li 2 O 2 growth. Furthermore, higher current densities improve ORR and OER efficiency but accelerate anode degradation, while lower currents promote side reactions. These opposing effects result in a trade-off that defines an optimal discharge rate (0.1 mA cm -2 ) for maximizing cycle life. This study provides a new mechanistic perspective on discharge-driven processes in solid-state LOBs and offers practical guidelines for performance optimization in future high-energy battery systems.

Discharge current density↗

Co-solvents with high coulombic efficiency in propylene carbonate based electrolytes

A homologous series of cyclic carbonate or propylene carbonate (PC) analog solvents with increasing length of linear alkyl substitutes were synthesized and used as co-solvents with PC for graphite based lithium ion half cells. A graphite anode reaches a capacity around 310 mAh/g in PC and its analog co-solvents with 99.95% Coulombic efficiency. Cyclic carbonate co-solvents with longer alkyl chains are able to prevent exfoliation of graphite when used as co-solvents with PC. The cyclic carbonate co-solvents of PC compete for solvation of Li ion with PC solvent, delaying PC co-intercalation. Reduction products of PC on graphite surfaces via single-electron path form a stable Solid Electrolyte Interphase (SEI), which allows the reversible cycling of graphite.

25 ENERGY STORAGE↗

Exploring the Ion Solvation Environments in Solid-State Polymer Electrolytes through Free-Energy Sampling

The success of poly(ethylene oxide) (PEO) in solid-state polymer electrolytes for lithium-ion batteries is well established. Recently, in order to understand this success and to explore possible alternatives, we studied polyacetal electrolytes to deepen the understanding of the effect of the local chemical structure on ion transport. Advanced molecular dynamics techniques using newly developed, tailored interaction potentials have helped elucidate the various coordination environments of ions in these systems. In particular, the competition between cation-Anion pairing and coordination by the polymer has been explored using free-energy sampling (metadynamics). At equivalent reduced temperatures, with respect to the polymer-specific glass-Transition temperature, two-dimensional free-energy plots reveal the existence of multiple coordination environments for the lithium (Li) ions in these systems and their relative stabilities. Furthermore, we observe that the Li-ion movement in PEO follows a serial, stepwise pathway when moving from one coordination state to another, whereas this happens in a more continuous and concerted fashion in a polyacetal such as poly(1,3-dioxalane) [P(EO-MO)]. The implication is that interconversion between coordination states of the Li ions may be easier in P(EO-MO). However, the overarching observation from our free-energy analysis is that Li-ion coordination is dominated by the polymer (in either case) and contact-ion pairs are rare. We rationalize the observed higher increase in glass-Transition temperature (Tg) with salt loading in polyacetals as due to intermolecular Li-ion coordination involving multiple polymer chains, rather than just one chain for PEO-based electrolytes. This interchain coupling in the polyacetals, resulting in the higher Tg, works against any gains due to variations in Li-ion coordination that might enhance transport processes over PEO. Further research is required to overcome the interdependence between local coordination and macroscopic properties to compete with PEO electrolytes at the same absolute working temperature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrolytes Containing Triethyl Phosphate Solubilized Lithium Nitrate for Improved Silicon Anode Performance

An electrolyte consisting of lithium nitrate (LiNO3) and lithium difluoro(oxalato)borate (LiDFOB) in ethylene carbonate (EC), ethylmethyl carbonate (EMC), and triethyl phosphate (TEP) is used to improve the long-term cycling stability of silicon anodes. TEP was selected for its ability to dissolve LiNO 3 in carbonates to a concentration of ~0.2 M. The large amount of LiNO 3 combined with the LiDFOB salt leads to a capacity retention of 87.1% after one hundred cycles due to the formation of a relatively stable solid electrolyte interphase (SEI). Ex-situ surface analysis reveals that the SEI consists of oxalates, lithium alkyl carbonates, borates, and nitrate reduction products. By selecting two components which are preferentially reduced (LiNO 3 and LiDFOB), the SEI is able to inhibit continuous solvent decomposition and allows for improved electrochemical cycling for pure silicon anodes.

25 ENERGY STORAGE↗

Evaluating the Effect of Electrolyte Additive Functionalities on NMC622/Si Cell Performance

Unstable electrode/electrolyte interface is the major cause of degradation for silicon (Si)-based anodes for lithium (Li)-ion batteries. Development of functional electrolyte additives can provide a viable path toward stabilizing the dynamic Si/electrolyte interface, which will benefit the development of high energy density Li-ion batteries. Here, we evaluate polymerizable electrolyte additives with varying functional groups (fluorocarbon, thiophosphate, and fluorophosphazene). The additives are examined using LiNi 0.6 Mn 0.2 Co 0.2 O 2 /Si full cells where the cycle performance and impedance are measured. Electrochemical tests show that the fluorine-containing additives provide better passivation at the Si electrode, leading to enhanced full cell performance. Here, among the three additives examined, best electrochemical performance is observed from the fluorocarbon-containing compound, followed by fluorophosphazene- and thiophosphate-containing compounds. Characterization of the solid electrolyte interphase (SEI) on cycled electrodes using Auger electron spectroscopy (AES), X-ray photoelectron spectroscopy (XPS), and attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR) reveal that higher concentration of fluorine and lithium oxide, and lower concentration of carbonate and organic species correlate with enhanced electrochemical performance.

25 ENERGY STORAGE↗

Oxygen redox and instability in energy ceramics

Energy ceramics, including solid electrolytes and catalysts for high-temperature fuel/electrolysis cells and oxide cathodes for batteries, often experience harsh chemical and electrochemical conditions. Practical and new applications require that these devices are operated under ever more extreme redox conditions for higher energy density and power density. This challenges the stability of the energy ceramic materials and calls for a better understanding of the degradation mechanisms and innovative strategies for degradation mitigation. Here we present our analysis and perspectives on degradation phenomena in three categories of electrochemical devices of practical interest, including solid oxide fuel/electrolysis cells, protonic ceramic fuel/electrolysis cells, and lithium-ion batteries. We also discuss the stability/degradation of the key ceramic components from the view of oxygen redox and instability arising from anodic bias, transport limitation, and coupled electro-chemo-mechanics at the virtual and physical interfaces. We hope these perspectives provide design principles for electroceramic chemistry, microstructure, and processing.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of temperature on capacity fade in silicon-rich anodes

Coin half-cells containing 80 wt% silicon electrodes are assembled and cycled at the similar to C/10 rate in the temperature range of 25-55 degrees C. To the best of our knowledge, this is the first time that the effect of temperature is reported for such high-silicon-containing cells. Two different electrolytes are used in this study, a baseline electrolyte and the baseline electrolyte +10 wt% fluoroethylene carbonate (FEC). Analysis of the capacity vs. cycle count data by curve fitting reveals that the addition of FEC markedly affects the capacity loss mechanism. Without FEC, the kinetic rate law for the capacity loss mechanism can be described as the sum of two logistic growth models. With the addition of FEC, the rate law depends on ln(t). Clearly, the addition of FEC has a profound effect on the mechanism of capacity loss. Interestingly, X-ray photoelectron spectroscopy (XPS) shows that the composition of the solid electrolyte interphase (SEI) layer changes markedly from mostly organic to mostly inorganic in the presence of FEC and how it varies at the different temperatures tested, especially in the absence of FEC.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing the Anion–Solvent Interaction for Ultralow Temperature Lithium Metal Batteries

Anion solvation in electrolytes can largely change the electrochemical performance of the electrolytes, yet has been rarely investigated. Herein, three anions of bis(trifluoromethanesulfonyl)imide (TFSI), bis(fluorosulfonyl)imide (FSI), and derived asymmetric (fluorosulfonyl)(trifluoro-methanesulfonyl)imide (FTFSI) are systematically examined in a weakly Li + cation solvating solvent of bis(3-fluoropropyl)ether (BFPE). In-situ liquid secondary ion mass spectrometry demonstrates that FTFSI - and FSI - anions are associated with BFPE solvent, while weak TFSI - /BFPE cluster signals are detected. Molecular modeling further reveals that the anion–solvent interaction is accompanied by the formation of H-bonding-like interactions. Further, anion solvation enhances the Li + cation transfer number and reduces the organic component in solid electrolyte interphase, which enhances the Li plating/stripping Coulombic efficiency at a low temperature of -30 °C from 42.4% in TFSI-based electrolytes to 98.7% in 1.5 m LiFTFSI and 97.9% in LiFSI-BFPE electrolytes. The anion–solvent interactions, especially asymmetric anion solvation also accelerate the Li + desolvation kinetics. The 1.5 m LiFTFSI-BFPE electrolyte with strong anion–solvent interaction enables LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)||Li (20 µm) full cell with stable cyclability even under -40 °C, retaining over 92% of initial capacity (115 mAh g -1 , after 100 cycles). The anion–solvent interactions insights allow to rational design the electrolyte for lithium metal batteries and beyond to achieve high performance.

25 ENERGY STORAGE↗

Stabilized Electrode/Electrolyte Interphase by a Saturated Ionic Liquid Electrolyte for High-Voltage NMC532/Si-Graphite Cells

Nonaqueous electrolyte has become one of the technical barriers in enabling Li-ion battery comprising of a high voltage cathode and high capacity anode. Here, we demonstrate a saturated piperidinum bis(fluorosulfonyl)imide ionic liquid (IL) with a LiFSI salt not only supports the redox reaction on the cathode at high voltages, but also shows exceptional kinetic stability on the lithiated anode as evidenced by its improved cycling performance in a NMC532/Si-graphite full cells cycled between 4.6 and 3.0 V. On the basis of the spectroscopic/microscopic analysis and molecular dynamics (MD) simulations, the superior performance of the cells is attributed to the formation of solid-electrolyte-interphase on both electrode as well as unique solvation structure where a deadlocked coordination network is established at the saturated state, which prevents transition metal dissolution into the electrolyte via a solvation process.

25 ENERGY STORAGE↗

Stern layers on RuO2 (100) and (110) in electrolyte: Surface X-ray scattering studies

Electrochemical Stern layers are observed on the surfaces of RuO 2 single crystals in 0.1 M CsF electrolyte. The Stern layers formed at the interfaces of RuO 2 (110) and (100) are compared to the previously reported Stern layer on Pt (111) [Liu et al., J. Phys. Chem. Lett., 9 (2018) 1265]. While the Cs + density profiles at the potentials close to hydrogen evolution reactions are similar, the hydration layers intervening the surface and the Cs + layer are significantly denser on RuO 2 surfaces than that on Pt(111) surface, reflecting the oxygen termination of RuO 2 surfaces. The overall similarities between Stern layers on ruthenium surfaces and platinum surface suggest the universal presence of Stern layers in all well-defined solid-electrolyte interfaces.