Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “rupture”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 973 records · Page 54

Identification of a cast iron alloy containing nonstrategic elements

A program was performed to address the mechanical and environmental needs of Stirling engine heater head and regenerator housing components, while reducing the dependence on strategic materials. An alloy was developed which contained no strategic elemental additions per se. The base is iron with additions of manganese, molybdenum, carbon, silicon, niobium, and ferro-chromium. Such an alloy should be producible on a large scale at very low cost. The resulting alloy, designated as NASAUT 4G-Al, contained 15 Mn, 15 Cr, 2 Mo, 1.5 C, 1.0 Si, 1.0 Nb (in weight percent) with a balance of Fe. This alloy was optimized for chemistry, based upon tensile strength, creep-rupture strength, fracture behavior, and fatigue resistance up to 800 C. Alloys were also tested for environmental compatibility. The microstructure and mechanic properties (including hardness) were assessed in the as-cast condition and following several heat treatments, including one designed to simulate a required braze cycle. The alloy was fabricated and characterized in the form of both equiaxed and columnar-grained castings. The columnar grains were produced by directional solidification, and the properties were characterized in both the longitudinal and transverse orientations. The NASAUT 4G-Al alloy was found to be good in cyclic-oxidation resistance and excellent in both hydrogen and hot-corrosion resistance, especially in comparison to the baseline XF-818 alloy. The mechanical properties of yield strength, stress-rupture life, high-cycle-fatigue resistance, and low-cycle-fatigue resistance were good to excellent in comparison to the current alloy for this application, HS-31 (X-40), with precise results depending in a complex manner on grain orientation and temperature. If required, the ductility could be improved by lowering the carbon content.

Cooper, C. V.↗

Elevated temperature crack growth in aluminum alloys: Tensile deformation of 2618 and FVS0812 aluminum alloys

Understanding the damage tolerance of aluminum alloys at elevated temperatures is essential for safe applications of advanced materials. The objective of this project is to investigate the time dependent subcritical cracking behavior of powder metallurgy FVS0812 and ingot metallurgy 2618 aluminum alloys at elevated temperatures. The fracture mechanics approach was applied. Sidegrooved compact tension specimens were tested at 175, 250, and 316 C under constant load. Subcritical crack growth occurred in each alloy at applied stress intensity levels (K) of between about 14 and 25 MPa/m, well below K (sub IC). Measured load, crack opening displacement and displacement rate, and crack length and growth rate (da/dt) were analyzed with several continuum fracture parameters including, the C-integral, C (sub t), and K. Elevated temperature growth rate data suggest that K is a controlling parameter during time dependent cracking. For FVS0812, da/dt is highest at 175 C when rates are expressed as a function of K. While crack growth rate is not controlled by C (sub t) at 175 C, da/dt appears to better correlate with C (sub t) at higher temperatures. Creep brittle cracking at intermediate temperatures, and perhaps related to strain aging, is augmented by time dependent transient creep plasticity at higher temperatures. The C (sub t) analysis is, however, complicated by the necessity to measure small differences in the elastic crack growth and creep contributions to the crack opening displacement rate. A microstructural study indicates that 2618 and FVS0812 are likely to be creep brittle materials, consistent with the results obtained from the fracture mechanics study. Time dependent crack growth of 2618 at 175 C is characterized by mixed transgranular and intergranular fracture. Delamination along the ribbon powder particle boundaries occurs in FVS0812 at all temperatures. The fracture mode of FVS0812 changes with temperature. At 175 C, it is characterized as dimpled rupture, and at 316 C as mixed matrix superplastic rupture and matrix-dipersoid debonding.

Leng, Yang↗

Deformation and fracture of aluminum-lithium alloys: The effect of dissolved hydrogen

The effects of dissolved hydrogen on the mechanical properties of 2090 and 2219 alloys are studied. The work done during this semi-annual period consists of the hydrogen charging study and some preliminary mechanical tests. Prior to SIMS analysis, several potentiostatic and galvanostatic experiments were performed for various times (going from 10 minutes to several hours) in the cathodic zone, and for the two aqueous solutions: 0.04N of HCl and 0.1N NaOH both combined with a small amount of As2O3. A study of the surface damage was conducted in parallel with the charging experiments. Those tests were performed to choose the best charging conditions without surface damage. Disk rupture tests and tensile tests are part of the study designed to investigate the effect of temperature, surface roughness, strain rate, and environment on the fracture behavior. The importance of the roughness and environment were shown using the disk rupture test as well as the importance of the strain rate under hydrogen environment. The tensile tests, without hydrogen effects, have not shown significant differences between low and room temperature.

Rivet, F. C.↗

The influence of advanced processing on PWA 1480

High thermal gradient casting of PWA 1480 was evaluated as an avenue for reducing the size of casting porosity. Hot isostatic pressing (HIP) was also employed for the elimination of casting pores. An alternate to the standard PWA 1480 coating plus diffusion bonding aging heat treatment cycle was also evaluated for potential improvements in the properties of interest to the Space Shuttle Main Engine (SSME) application. Microstructural changes associated with the high thermal gradient casting process were quantified by measurement of the size and density of the casting porosity, the amount of retained casting eutectic, and dendrite arm spacings. The results of the advanced processing have shown an improvement in material microstructure due to high thermal gradient casting. Improved homogeneity of PWA 1480 is advantageous in providing an improved solution heat treatment window and, potentially, easier HIP. High thermal gradient casting improves fatigue life by reducing casting pore size. The alternate heat treatment improves the balance of strength and ductility which appears to improve low cycle fatigue life, but with a reduction in short time stress rupture life. Based upon these tests, hot isostatic pressing appears to afford further improvements in cyclic life, though additional evaluation is suggested. Development of the alternate heat treatment is not recommended due to the reduced stress rupture capability and the need to develop a new properties data base. High thermal gradient casting and HIP are recommended for application to single crystal castings.

Fritzemeier, L. G.↗

Materials for a Stirling engine heater head

Work done on the 25-kW advanced Stirling conversion system (ASCS) terrestrial solar program in establishing criteria and selecting materials for the engine heater head and heater tubes is described. Various mechanisms contributing to incompatibility between materials are identified and discussed. Large thermal gradients, coupled with requirements for long life (60,000 h at temperature) and a large number of heatup and cooldown cycles (20,000) drive the design from a structural standpoint. The pressurized cylinder is checked for creep rupture, localized yielding, reverse plasticity, creep and fatigue damage, and creep ratcheting, in addition to the basic requirements for bust and proof pressure. In general, creep rupture and creep and fatigue interaction are the dominant factors in the design. A wide range of materials for the heater head and tubes was evaluated. Factors involved in the assessment were strength and effect on engine efficiency, reliability, and cost. A preliminary selection of Inconel 713LC for the heater head is based on acceptable structural properties but driven mainly by low cost. The criteria for failure, the structural analysis, and the material characteristics with basis for selection are discussed.

Noble, J. E.↗

Apparatus For Tests Of Embrittlement By Hydrogen

Test apparatus exposes disk specimens to hydrogen in controlled, repeatable way simulating conditions in use. Disk specimen constitutes thin wall between pressure and vacuum chambers. Test proceeds until hydrogen weakens disk enough that it ruptures. Aluminum impact plate absorbs debris from ruptured disk. Apparatus replicates aspects of service environments relevant to embrittlement by hydrogen in such equipment as storage tanks, valves, and fluid-handling components containing hydrogen at high absolute or gauge pressure. Hydrogen inside permeates stressed material and produces gradient of concentration as hydrogen diffuses through material to low-pressure side.

Christianson, Rollin C.↗

Blow-down analysis of helium from a cryogenic dewar

NASA is currently developing Space Shuttle-based refilling of helium using superfluid helium on-orbit transfer (SHOOT). All the critical components of SHOOT need to be developed through ground-based tests. The helium dewar is one of these components. The Dewar consists of a vacuum vessel enclosing a superinsulated tank. The space between the vacuum vessel and the liquid tank is considered a common vacuum space. In the event that the vacuum is lost, the heat transfers to the dewar and the pressure inside the dewar increases rapidly, resulting in rupture of the dewar due to excessive pressure. Therefore, an emergency vent line is required for release of helium to prevent the dewar from rupturing. The study describes a numerical model for blow-down analysis in an emergency. This qualifies the design of the emergency vent line to be adequate for the assumed heat loads to the helium dewar.

Khan, H. J.↗

Absolute far-field displacements from the 28 June 1992 Landers earthquake sequence

Displacements observed for the Landers earthquake indicate that the depth of the bottom of the rupture is shallower towards the northern end. Displacements were dominantly symmetric and the rupture extended farther south on the Johnson Valley fault than has been mapped on the basis of surface ground offsets. The combined geodetic moment for the Landers and Big Bear earthquakes agrees well with teleseismic estimates.

Blewitt, Geoffrey↗

Mechanical behavior of high strength ceramic fibers at high temperatures

The mechanical behavior of commercially available and developmental ceramic fibers, both oxide and nonoxide, has been experimentally studied at expected use temperatures. In addition, these properties have been compared to results from the literature. Tensile strengths were measured for three SiC-based and three oxide ceramic fibers for temperatures from 25 C to 1400 C. The SiC-based fibers were stronger but less stiff than the oxide fibers at room temperature and retained more of both strength and stiffness to high temperatures. Extensive creep and creep-rupture experiments have been performed on those fibers from this group which had the best strengths above 1200 C in both single filament tests and tests of fiber bundles. The creep rates for the oxides are on the order of two orders of magnitude faster than the polymer derived nonoxide fibers. The most creep resistant filaments available are single crystal c-axis sapphire filaments. Large diameter CVD fabricated SiC fibers are the most creep and rupture resistant nonoxide polycrystalline fibers tested to date.

Tressler, R. E.↗

Teleseismic detection of a slow precursor to the great 1989 Macquarie Ridge earthquake

Low-frequency spectra for the 1989 Macquarie Ridge earthquake (magnitude 8.2) show an amplitude increase and a phase-delay decrease below 6 millihertz that require a short-term slow precursor. This earthquake can be modeled as a compound event in which a fast-rupturing, ordinary earthquake was initiated by an episode of slow, smooth deformation that began more than 100 seconds before the main shock. The moment released in the slow precursor was large, about 3 x 10 exp 20 newton-meters, equivalent to an event of magnitude 7.6. The data are consistent with the precursor being generated in a region of the oceanic upper mantle below the main rupture.

Ihmle, Pierre F.↗

Tensile properties of HK31XA-H24 magnesium-alloy sheet under rapid-heating conditions and constant elevated temperatures

Specimens of HK31XA-H24 magnesium-alloy sheet from an experimental batch were heated to failure at nominal temperature rates from 0.2 F to 100 F per second under constant-load conditions. Rapid-heating yield and rupture stresses are presented and compared with the yield and ultimate stresses from elevated-temperature tensile stress-strain tests for 1/2-hour exposure. Linear temperature-rate parameters were used to correlate rapid-heating results by constructing master curves which can be used for predicting yield stresses and temperatures and for estimating rupture stresses and temperatures.

MATERIALS, PROPERTIES - THERMAL↗

Tensile properties of AZ11A-0 magnesium-alloy sheet under rapid-heating and constant temperature

Specimens of AZ31A-0 magnesium alloy sheet were heated to rupture at nominal rates of 0.2 F to 100 F per second under constant tensile load conditions. The data are presented and compared with the results of conventional tensile stress-strain tests at elevated temperatures after 1.2-hour exposure. A temperature-rate parameter was used to construct master curves from which stresses and temperatures for yield and rupture can be predicted under rapid-heating conditions. A comparison of the elevated-temperature tensile properties of AZ31A-0 and HK31XA-H24 magnesium-alloy sheet under both constant-temperature and rapid-heating conditions is included.

MATERIALS, PROPERTIES - THERMAL↗

Investigation of Mechanisms of Blade Failure of Forged Hastalloy B and Cast Stellite 21 Turbine Blades in Turbojet Engine

An investigation was conducted to study the mechanisms of blade failure of forged Hastelloy B and cast Stellite 21. The blades were mounted in a 16-25-6 alloy rotor and subjected to 20-minute cycles consisting of 15 minutes at rated speed and approximately 5 minutes at idle. The first failures of the Hastelloy B and Stellite 21 blades were probably the result of excessive vibratory stresses and occurred after 14.25 and 16.75 hours, respectively. After 28.75 hours of operation, all but 3 of the original 25 Hastelloy B blades had either failed or contained stress-rupture-type cracks and four of the original 27 Stellite 21 blades contained stress-rupture-type cracks.

ENGINES, TURBO-JET↗

Axial crack propagation and arrest in pressurized fuselage

The crack arrest capability of a tear strap in a pressurized precracked fuselage was studied through instrumented axial rupture tests of small scale models of an idealized fuselage. Upon pressurization, rapid crack propagation initiated at an axial through crack along the stringer and immediately kinked due to the mixed modes 1 and 2 state caused by the one-sided opening of the crack flap. The diagonally running crack further turned at the tear straps. Dynamic finite element analysis of the rupturing cylinder showed that the crack kinked and also ran straight in the presence of a mixed mode state according to a modified two-parameter crack kinking criterion.

Kosai, M.↗

Thermomechanical Behavior of Advanced SiC Fiber Multifilament Tows

In order to relate single fiber behavior to multiple fiber behavior in composites, fast-fracture tensile strength, creep, and stress-rupture studies were conducted on advanced SiC fiber multifilament tows in the temperature range from 20 to 1400 C in air as well as in inert environments. For conditions of small fiber creep (short times and low temperatures), the tow results of this study confirm the ability of limited single fiber data to model the strength behavior of multiple fibers in a bundle. For conditions of high creep (long times and high temperatures), further studies are needed to explain tow rupture behavior being better than average single fiber behavior.

Yun, Hee Mann↗

Effect of Hf-Rich Particles on the Creep Life of a High-strength Nial Single Crystal Alloy

Additions of small amounts of Hf and Si to NiAl single crystals significantly improve their high-temperature strength and creep properties. However, if large Hf-rich dendritic particles formed during casting of the alloyed single crystals are not dissolved completely during homogenization heat treatment, a large variation in creep rupture life can occur. This behavior, observed in five samples of a Hf containing NiAl single crystal alloy tested at 1144 K under an initial stress of 241.4 MPa, is described in detail highlighting the role of interdendritic Hf-rich particles in limiting creep rupture life.

Garg, A.↗

Creep of Uncoated and Cu-Cr Coated NARloy-Z

Stress rupture creep tests were performed on uncoated and Cu-30vol%Cr coated NARloy-Z copper alloy specimens exposed to air at 482 C to 704 C. The results showed that creep failure in air of unprotected NARloy-Z was precipitated by brittle intergranular surface cracking produced by strain assisted grain boundary oxidation (SAGBO) which in turn caused early onset of tertiary creep. For the protected specimens, the Cu-Cr coating remained adherent throughout the tests and was effective in slowing down the rate of oxygen absorption, particularly at the higher temperatures, by formation of a continuous chromium oxide scale. As the result of reducing oxygen ingress, the coating prevented SAGBO initiated early creep failure, extended creep deformation and increased the creep rupture life of NARloy-Z over the entire 482 C to 704 C test temperature range.

Walter, R. J.↗

Performance of Two Boron-Modified S-816 Alloys in a Turbojet Engine Operated at 1650 F

S-816+B and modified S-816+B cast cobalt-base alloys were evaluated as turbine-bucket materials at 16500 F. Stress-rupture and tensile data obtained from these alloys had indicated satisfactory strength for engine operation at 1650 F. Although both alloys exhibited a limited ductility in room-temperature laboratory impact tests, there was a significant increase in impact resistance in the 1650 F tests. Bucket failures began after 10 hours of engine testing and continued at various intervals during the 107.5-hour test. Bucket lives were short relative to the predicted lives based on stress-rupture considerations (280 hr for S-816+B and 1750 hr for modified S-816+B). No significant difference was apparent in the performance of the two alloy groups. The primary cause of bucket failures in both alloys was mechanical fatigue. Impact damage occurred as a direct result of bucket tip fatigue failures and was a secondary cause of bucket failures. The impact of small pieces of fractured bucket tips on surrounding buckets caused a relatively large amount of impact damage to buckets of both alloys. The amount of impact damage from induced fractures at the bucket midspan, which provided relatively large failed fragments, was no greater than that which occurred as a result of tip failures.

Waters, William J.↗