Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STEELS, STAINLESS - WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 973 records · Page 54

Micro- and macro-structural heterogeneities in 316L stainless steel prepared by electron-beam melting

Highlights: • Electron beam melting manufactured parts has a complicated thermal history. • The microstructure varies with the position in the sample. • Pronounced molybdenum segregation at the top disappears at the bottom. • Fast molybdenum diffusion in cell boundaries as well as grain boundaries. - Abstract: This is a study of the micro- and macrostructural variations in samples of stainless steel with the overall composition of the grade 316L, produced using electron beam melting. Electron beam melting is one of the processing methods under consideration for manufacturing some of the International Thermo- Nuclear Experimental Reactor In-Vessel components. Therefore further studies of the homogeneity of the material were conducted. Electron beam melting results in a complicated thermal history of the manufactured part giving a significant impact on the microstructure. A cellular structure that is often observed in samples prepared by selective laser melting was found in the top layers of the specimens. Further down, the structure changed until the cellular structure was almost non-existing, and the grain boundaries had become more pronounced. This revelation of a heterogeneous structure throughout the entire part is crucial for large-scale industrial applications like the Thermo- Nuclear Experimental Reactor to make sure that it is understood that the properties of the material might not be the same at every point, as well as to assure that the correct post-treatment is done. It is also exposed that a significant part of this change is due to molybdenum redistribution inside the sample when it diffuses from the cell boundaries into the cells, and into bigger agglomerates in the grain boundaries. This diffusion seems not to affect the microhardness of the samples.

36 MATERIALS SCIENCE↗

Extended continuous cooling transformation diagram for 410 stainless steel encompassing δ → γ and γ → αʹ transformations determined by dilatometry

In this study, we use dilatometry to construct an extended Continuous Cooling Transformation (CCT) diagram for 410 stainless steel, capturing both δ → γ and γ → αʹ transformations specifically for directed energy deposition (DED) additive manufacturing (AM) applications. To ensure that the findings are representative of AM specific microstructures and compositions, dilatometry coupons were extracted from a wire arc DED wall, thereby preserving the inherent microstructural and compositional variability within the material. The on-heating phase transformations, including A c1 , A c3 , and γ → δ, were found to be essentially location independent, despite the typical heterogeneity associated with AM. Conversely, increasing cooling rates were observed to shift the start and finish temperatures of both δ → γ and γ → αʹ transformations to lower values. The resulting extended CCT diagram offers a more complete depiction of phase transformation behavior in the system, enabling accurate microstructure evolution modeling and residual stress predictions specifically for directed energy deposition additive manufacturing applications.

Additive manufacturing↗

Irradiation effects on Al 0.3 CoCrFeNi and CoCrMnFeNi high-entropy alloys, and 316H stainless steel at 500 °C

To evaluate the potential of high entropy alloys (HEAs) for nuclear applications, two HEAs, Al 0.3 CoCrFeNi and CoCrFeMnNi, and a conventional Type 316H stainless steel (SS) were irradiated with 1 MeV krypton ions at 500 degrees C up to 1 dpa, and examined in-situ with a transmission electron microscope (TEM). After irradiation, a high density of ordered L1 2 nanoparticles was observed in Al 0.3 CoCrFeNi. In contrast, no phase transformation was observed in CoCrFeMnNi and 316H SS. In the thin foil regions of TEM samples, stacking-fault tetrahedra were observed in the HEAs. In the thick foil regions, interstitial dislocation loops were observed for all alloys, and the areal loop density increased linearly with foil thickness. The Al 0.3 CoCrFeNi had the largest loop size (the lowest density), followed by the CoCrFeMnNi and then the 316H SS. The higher loop nucleation rate in the 316H SS was attributed to carbon content. Finally, the degree of irradiation hardening was slightly lower for the HEAs than for the 316H SS, which is a promising sign for the nuclear application of HEAs at high temperatures.

36 MATERIALS SCIENCE↗

Meta-equilibrium transition microstructure for maximum austenite stability and minimum hardness in a Ti-stabilized supermartensitic stainless steel

We report that the maximization of stable reverted austenite at room temperature through inter-critical tempering is a widely used method to reduce hardness in supermartensitic stainless steels. Nevertheless, partial martensitic transformation might occur due to insufficient compositional stabilization. In this work, we conducted a time-resolved triple-step inter-critical tempering, specially designed to obtain maximum austenite stability and minimum hardness through the progressive suppression of the martensitic transformation. The mechanism behind the progressive increase in stable reverted austenite was the generation of a meta-equilibrium state, which imposed a limit in both high temperature austenite reversion and room temperature austenite stabilization. Such limit corresponded to the high temperature volume fraction of austenite, obtained right before cooling from the first cycle. Additionally, this effect was associated to the Ni-rich fresh martensite laths acting as local Ni compositional pockets, providing site-specific austenite reversion; and to the suppression of any additional nucleation at the Ni-poor matrix as the T0 temperature for austenite reversion was strongly increased. The softening mechanism was mainly controlled by the carbon arrest effect by the precipitation of Ti (C, N), which was completed after the first tempering cycle. Nevertheless, maximizing reverted austenite and suppressing fresh martensite at room temperature did not result in additional hardness reductions.

36 MATERIALS SCIENCE↗

Mechanical Properties, Microstructural Evolution, and the Effect of Friction on the Plastic Flow of the AISI 321 Austenitic Stainless Steel Tube During Cold Pilgering: An Experimental and Simulation Analysis

The mechanical properties, microstructural evolution, and the effect of friction on the plastic flow of the AISI 321 austenitic stainless steel (ASS) tube were investigated during the cold pilger process. The elastic–plastic behavior of as-received tube was simulated by the Johnson-cook model. The model parameters were obtained by the compression and tensile tests. The mechanical properties of the material were examined by the tensile and microhardness tests. Based on the ring compression test results, three different situations for friction conditions were considered. The stress and strain states at these conditions were examined for the outer and inner surfaces of the tube. Numerical evaluation of plastic shearing due to the cold pilgering of the AISI321 tube was performed. The X-ray diffraction, ferrite scope tests, and optical microscope were also used for the microstructure evaluation and verification of the simulation results, respectively. The Latham-Cockcraft damage was calculated for different conditions by introducing the new subroutine, showing that it was strongly dependent on the friction conditions and the shear strain, ε{sub zr}, respectively. It was shown that the friction coefficient of 0.3 resulted in the minimum damage of the tube and the different friction conditions between the two surfaces of the tube enhanced the damage function. Also, the strain induced ά-martensite increased the work-hardening capacity and affected the ductility of the tube.

36 MATERIALS SCIENCE↗

Characterization of phase properties and deformation in ferritic-austenitic duplex stainless steels by nanoindentation and finite element method

The phase properties and deformation behavior of the δ–ferrite and γ–austenite phases of CF–3 and CF–8 cast duplex stainless steels were characterized by nanoindentation and microstructure-based finite element method (FEM) models. We evaluated the elastic modulus of each phase and the results indicate that the mean elastic modulus of the δ–ferrite phase is greater than that of the γ–austenite phase, and the mean nanoindentation hardness values of each phase are approximately the same. Furthermore, the elastic FEM model results illustrate that greater von Mises stresses are located within the δ–ferrite phase, while greater von Mises strains are located in the γ–austenite phase in response to elastic deformation. The elastic moduli calculated by FEM agree closely with those measured by tensile testing. Finally, the plastically deformed specimens exhibit an increase in misorientation, deformed grains, and subgrain structure formation as measured by electron backscatter diffraction (EBSD).

36 MATERIALS SCIENCE↗

Critical role of slags in pitting corrosion of additively manufactured stainless steel in simulated seawater

Abstract Pitting corrosion in seawater is one of the most difficult forms of corrosion to identify and control. A workhorse material for marine applications, 316L stainless steel (316L SS) is known to balance resistance to pitting with good mechanical properties. The advent of additive manufacturing (AM), particularly laser powder bed fusion (LPBF), has prompted numerous microstructural and mechanical investigations of LPBF 316L SS; however, the origins of pitting corrosion on as-built surfaces is unknown, despite their utmost importance for certification of LPBF 316L SS prior to fielding. Here, we show that Mn-rich silicate slags are responsible for pitting of the as-built LPBF material in sodium chloride due to their introduction of deleterious defects such as cracks or surface oxide heterogeneities. In addition, we explain how slags are formed in the liquid metal and deposited at the as-built surfaces using high-fidelity melt pool simulations. Our work uncovers how LPBF changes surface oxides due to rapid solidification and high-temperature oxidation, leading to fundamentally different pitting corrosion mechanisms.

36 MATERIALS SCIENCE↗

Multi-scale experimental study of creep-fatigue failure initiation in a 709 Stainless Steel alloy using high resolution digital image correlation. Final report

This report discusses the efforts made towards the multi-scale study of the creep-fatigue response of stainless steel 709. Multiple experimental techniques, including digital image correlation (DIC) and electron backscatter diffraction (EBSD), were used in assessing the evolution of damage accumulation during fatigue, creep-fatigue, and thermomechanical fatigue of alloy 709. The role of microstructural features, hold times, temperature, and loading profiles were quantified and the interchangeability of temperature and time was investigated. Finally, a thermomechanical fatigue model was shown to predict well the failure of samples with varying loading profiles. Results indicate that strain accumulation in 709 steel happens primarily near grain boundaries (GBs) with the strains around GBs being inversely proportional to their measured residual burgers vector. Furthermore, hot-spots for strain accumulation were shown to be the locations of eventual microcrack nucleation. The introduction of hold times to the periodic loading cycle increases the damage accumulation rate and thus shortens the fatigue life of samples–this was true for both room temperature and high temperature. Thermomechanical cycling was shown to have little effect on the end life of samples, with the damage accumulation rate for in-phase and out-of-phase cycling being similar to isothermal fatigue. The interchangeability of time and temperature was shown to be possible within the studied load, time, and temperature ranges, since deformation mechanisms driving strain accumulation did not change with temperature (up to 650°C). The Neu-Sehitoglu thermomechanical fatigue model, with constants obtained from the literature and in part from our experimental results, was applied to predict failure of isothermal creep-fatigue samples. The main objectives of this work were to:(a) Perform high-resolution digital image correlation measurements (HiDIC) for alloy 709; (b) Quantify and assess damage accumulation at the microstructure under fatigue, TMF, and creep-fatigue conditions of 709; (c) Study of the role of hold times, i.e., adding a creep component, to: Room temperature cycling, High temperature cycling, Failure; (d) Study the mechanisms of thermomechanical fatigue in this alloy; (e) Investigate the existence of a time-temperature interchangeability criterion to aid in accelerated creep-fatigue testing; (f) Establish the validity of a combined creep-fatigue model for life prediction for 709. This report is structured with each subsequent section detailing the efforts, results, and conclusions related to each of the objectives described, mostly in chronological order.

36 MATERIALS SCIENCE↗

Simulations of crack extensions in arc-shaped tension specimens of uncharged and hydrogen-charged 21-6-9 austenitic stainless steels using cohesive zone modeling with varying cohesive parameters

Crack extensions in uncharged and hydrogen-charged side-grooved A(T) specimens of conventionally forged 21-6-9 austenitic stainless steels are simulated using the cohesive zone modeling approach. Two-dimensional plane strain finite element analyses with fixed cohesive parameters are first conducted to fit the experimental load-displacement curves. Similar analyses using varying cohesive parameters as functions of the crack extension are then conducted to fit the experimental load-crack extension and crack extension-displacement curves. The computational results with varying cohesive parameters can fit very well the experimental data. The computational results also indicate that the average cohesive energy for the hydrogen-charged A(T) specimen is lower than that for the uncharged A(T) specimen.

42 ENGINEERING↗

Cathodic Kinetics on Platinum and Stainless Steel in NaOH Environments

During typical atmospheric conditions, cathodic reduction reactions produce hydroxyl ions increasing the pH in the cathodic region. Therefore, cathodic reduction reactions are investigated on platinum and stainless steel 304 L (SS304L) in NaOH solutions ranging in pH from 13.6 to 16.5. It was found that in solution pHs less than 16.5 the cathodic reduction reaction on Pt and SS304L was ORR with an electron transfer number less than two due to superoxide formation as an intermediate. Increasing pH decreased the number of electrons transferred. At a pH of 16.5, the cathodic reduction reaction on SS304L is no longer ORR and the cathodic current on the surface of the alloy is due to oxide reduction occurring on the surface as indicated by the creation of multi-component Pourbaix diagrams. The results of this study have important implications for predicting corrosion in atmospheric environments.

25 ENERGY STORAGE↗

In Situ Measurement of Stress Corrosion Crack Tip Properties During Environmentally Induced Cracking in Stainless Steel 304L

The influence of the external cathodic area, stress intensity, and electrochemical polarization level on the resultant crack growth rate and crack tip pH and potential was studied for stainless steel 304L in a sodium chloride environment. Before testing, the validity of in situ crack tip property measurements using microprobes and drilled holes was supported through modeling efforts and confirmed with experimental observations. Here, it was found that increasing the R-ratio during corrosion fatigue increased the crack growth rate and decreased the measured crack tip pH of the 304L sample. Decreasing the electrochemical potential (i.e., cathodic polarization) of the bulk sample increased the crack tip pH and stopped measured crack extension under constant K conditions. Conversely, increasing the potential of the bulk sample decreased the crack tip pH and induced cracking under constant K conditions. Decreasing the cathodic area external to the crack increased the measured pH at the crack tip and decreased the crack growth rate under fatigue conditions. For the given configuration, environment, and alloy studied, fatigue crack growth is not sustained by cathodic reactions solely occurring in the crack wake and notch. These results have implications for the ability to predict atmospheric crack growth rates from laboratory, full immersion experiments.

corrosion fatigue↗

Stainless-Steel-Foam Structures Evaluated for Fan and Rotor Blades

The goal of this project is to use a sandwich structure design, consisting of two stainlesssteel face sheets and a stainless-steel-foam core, to fabricate engine fan and propeller blades. Current fan blades are constructed either of polymer matrix composites (PMCs) or hollow titanium alloys. The PMC blades are expensive and have poor impact resistance on their leading edges, thereby requiring a metallic leading edge to satisfy the Federal Aviation Administration s impact requirements relating to bird strikes. Hollow titanium blades cost more to fabricate because of the intrinsically difficult fabrication issues associated with titanium alloys. However, both these current concepts produce acceptable lightweight fan blades.

Lerch, Bradley A.↗

Effect of Hot Rolling on the Microstructure and Mechanical Properties of Nitrogen Alloyed Austenitic Stainless Steel

In the present investigation, the effect of multi-pass hot rolling in the temperature range of 700–1000 °C on the microstructure and mechanical properties of nitrogen alloyed austenitic stainless steel was studied with the aid of optical microscopy, tensile testing and x-ray diffraction measurements. The microstructural changes that occurred in the hot rolled specimens were elongation of grains in rolling direction, nucleation of new grains at the grain boundaries of elongated grains and growth of nucleated grains to form fully recrystallized grains. Elongated grains formed at lower rolling temperature (700–800 °C) due to inadequate strain/temperature for the initiation of dynamic recrystallization. At higher rolling temperature (900–1000 °C), fine grains formed due to dynamic recrystallization. Tensile properties showed strong dependency on the rolling temperature. Tensile strength increased with the decrease in the rolling temperature at the cost of ductility. Maximum strength was observed in samples hot rolled at 700 °C with yield strength of 917 MPa and ductility of 25%. This variation in the tensile properties with the rolling temperature is attributed to changes in the dislocation density and grain structure. The estimated yield strength from the dislocation density, solid solution and grain boundary strengthening closely matched with experimentally determined yield strength confirming the role of dislocation density and grain size in the strengthening.

36 MATERIALS SCIENCE↗

Extreme variation in fatigue: Fatigue life prediction and dependence on build volume location in laser powder bed fusion of 17-4 stainless steel

Laser powder bed fusion (LPBF), a metal additive manufacturing technology, is well-suited for design optimization but fatigue life is limited by manufacturing defects. In this work, 17-4 stainless steel components were manufactured in densely populated build volumes, simulating at-scale LPBF production. Tests revealed extreme variability in fatigue life data, analyzed via rigorous statistical tools. The El-Haddad model, modified for finite-life, enabled defect-based life prediction. Specimen location within the build volume correlated to life, which was heteroscedastic. Investigating defect concentration over the build volume explained typical life and scatter. Finally, these findings argue for qualification approaches which acknowledge high material lot variability.

36 MATERIALS SCIENCE↗

Tritium migration to the surfaces of Type 316 stainless steel; aluminum 6061; and oxygen-free, high-conductivity copper

The migration of tritium to the surfaces of aluminum 6061, oxygen-free, high-conductivity copper (OFHC), and stainless-steel 316 from the bulk metal was studied using low-pressure Tonks–Langmuir argon plasma. The plasma is shown to be effective at removing tritium from metal surfaces in a controlled manner. Tritium is removed in decreasing quantities with successive plasma exposures, which suggests a depletion of the surface and near-surface tritium inventories. A diffusion model was developed to predict tritium migration from the bulk and its accumulation in the water layers present on the metal surface. The model reproduces the rate of tritium re-growth on the surface for all three metals and can be used to calculate the triton solubility in the water layers present on metal surfaces. The ratio of surface-to-bulk solubilities at the water-layer/bulk-metal interface uniquely determines the concentration ratio between these two media. Removing the tritium-rich water layers induces tritium to migrate from the bulk to the surface. Furthermore, this process is driven by a concentration gradient that develops in the bulk because of the perturbation on the surface.

36 MATERIALS SCIENCE↗