Effect of alloying elements, cold work, and hydrogen on the irradiation-induced growth behavior of zirconium alloy variants - 2016-0040
In-reactor dimensional changes in zirconium-based alloys result from a complex interplay of many factors, such as (1) alloy type and composition, including the addition of elements such as niobium, iron, and tin; (2) fabrication process, including cold work, texture, and residual stresses; (3) irradiation temperature; and (4) hydrogen levels. In many cases, the observed dimensional changes in light water reactor fuel-assembly components-especially at high exposures-cannot be fully explained based on current growth and creep models. Therefore, a systematic approach was taken in this multi-year (2005-2011) Nuclear Fuel Industry Research Program investigation. The objective was to measure stress-free irradiation-induced growth (IIG) of specially fabricated alloys through irradiation under controlled conditions in the BOR-60 fast-flux test reactor up to a high fluence of approximately 2X10{sup 26} m{sup -2} (E>1 MeV)-equivalent to maximum of approximately 37 dpa exposure-followed by postirradiation examinations (PIEs). Irradiation temperature was within a narrow temperature range (320±10 deg. C). The PIEs included dimensional-change and microhardness measurements, metallography and hydride etching, and scanning transmission electron microscopy (STEM) or transmission electron microscopy (TEM). All irradiation samples (typically flat rectangular coupons or curvilinear cutouts of cladding tubes sized 35 by 6.5 by 0.8 mm) were pre-filmed to avoid the uptake of impurity hydrogen from sodium-cooled BOR-60. A wide variety of samples representing standard LWR cladding alloys with and without pre-hydriding (approximately 116 to approximately 718 ppm) as well as special compositions with iron contents (100 to 4,000 ppm) were irradiated. The irradiation in BOR-60 was done in five different stages (eight micro-cycles) and lasted approximately 18 months with interim and final growth measurements made using a high precision-length measurement device. Results of the extensive investigation include: significant effects of Fe, Nb, and hydrogen additions; quantification of growth rates from low to very high fluences (dpas); measurement of volume changes; and correlation of growth with -component dislocation densities. (authors)