Microstructure and mechanical properties of Cu x Nb 1-x alloys prepared by ball milling and high pressure torsion compacting

Here, new Cu x Nb 1-x alloys were prepared using a two-step process of ball milling and subsequent high pressure torsion compacting at ambient temperature. The alloys showed a nanocrystalline structure with grain sizes between 13–26 nm for the Cu-rich samples and 11–13 nm for the Nb-rich samples. The grain sizes decreased with the milling time and the amount of Nb in the Cu-rich and Cu in the Nb-rich samples, respectively. The distortion of the crystallographic lattice of the fcc Cu and bcc Nb suggests the formation of a solid solution. The mechanical properties studied by nanoindentation show an increase of the hardness with milling time and the amount of added element. A thermal treatment was carried out under a protective Argon atmosphere. Up to 400 °C the Cu-rich samples do not show significant signs of oxidation and in increase of hardness. The Nb-rich samples showed a continuous increase of the hardness up to 500°C, due to the precipitation of Cu, and the initial formation of NbO x .

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of titanium aluminum carbides neutron irradiated at 400–700 °C

Here, this work reports the first mechanical properties of Ti 3 AlC 2 -Ti 5 Al 2 C 3 materials neutron irradiated at ~400, 630 and 700 °C at a fluence of 2 × 10 25 n m -2 (E > 0.1 MeV) or a displacement dose of ~2 dpa. After irradiation at ~400 °C, anisotropic swelling and loss of 90% flexural strength was observed. After irradiation at ~630–700 °C, properties were unchanged. Microcracking and kinking-delamination had occurred during irradiation at ~630–700 °C. Further examination showed no cavities in Ti 3 AlC 2 after irradiation at ~630 °C, and MX and A lamellae were preserved. However, disturbance of (0004) reflections corresponding to M-A layers was observed, and the number density of line/planar defects was ~10 23 m -3 of size 5–10 nm. HAADF identified these defects as antisite Ti Al atoms. Finally, Ti 3 AlC 2 -Ti 5 Al 2 C 3 shows abrupt dynamic recovery of A-layers from ~630 °C, but a higher temperature appears necessary for full recovery.

36 MATERIALS SCIENCE↗

Influence of silicon infiltration conditions on microstructure and mechanical properties in binder jet 3D printed SiC

Atmosphere, temperature, and hold time were varied for silicon infiltrated binder jet 3D printed SiC preforms. A two-step infiltration process optimized infiltration. The first step at 1450 °C under vacuum facilitated improved wetting. The second step at elevated temperature in argon advanced infiltration while suppressing vaporization. Variation of the second-step temperature (1550–1750 °C) and hold time revealed that 1550 °C for 1 h in argon following initial vacuum treatment yielded the highest silicon uptake ratio (∼96 %) with minimal residual porosity and strengths of 150–180 MPa. Flexural strength was either stable or improved with elevated temperatures up to 1000°C. In contrast, higher temperatures or extended hold times led to increased silicon vaporization and pores. The optimized process was applied to formulations with extra carbon to enhance SiC content and interconnectedness through reaction bonding, which corresponded to increased flexural strength. These findings provide guidance for silicon infiltration in additively manufactured SiC.

Yoon, Bola [ORNL] (ORCID:0000000260875373)↗

Thermal annealing of FePt thin films by millisecond plasma arc pulses

A series of 20 and 100 nm Fe{sub 53}Pt{sub 47} thin films sputter-deposited onto Si substrates have been thermally annealed using a pulsed thermal plasma arc lamp. A series of one, three or five pulses were applied to the thin films with widths of either 50 or 100 ms. The microstructure and magnetic properties of these annealed Fe{sub 53}Pt{sub 47} films are discussed according to the various annealing conditions and A1 to L1{sub 0} phase transformation. Upon pulse annealing, the average in-plane grain size of 15 nm (nearly equivalent for both film thicknesses) was observed to increase to values near 20 nm. In general, increasing the pulse width or number of pulses increased the L1{sub 0} order parameter, tetragonality of the c/a ratio and coercivity of the specimen. The exception to this trend was for five pulses at 100 ms for both film thicknesses, which indicated a reduction of the order parameter and coercivity. This reduction is believed to be a result of the interdiffusion of Fe and Pt into the Si substrate and the formation of iron oxide clusters in the grain boundaries characterized by atom probe tomography.

36 MATERIALS SCIENCE↗