Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 973 records · Page 54

Formation of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) Nano-composites via Mechanical Alloying and Friction Stir Processing

Combination of mechanical alloying and friction stir processing was used for the fabrication of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) nano-composites. Pre-milled hematite + Al powder mixture was introduced into the stir zone generated on 1050 aluminum alloy sheet by friction stir processing. Uniform and active milled powder mixture reacted with plasticized aluminum to produced Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles. Al{sub 13}Fe{sub 4} intermetallic showed elliptical shape with a typical size of ~ 100 nm, while nano-sized Al{sub 2}O{sub 3} exhibited irregular floc-shaped particles that formed clusters with the remnant of iron oxide particles in the fine recrystallized aluminum matrix. As the milling time (1-3 h) of the introduced powder mixture increased, the volume fraction of Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles increased in the fabricated composite. The hardness and ultimate tensile strength of the fabricated nano-composites varied from 54.5 to 75 HV and 139 to 159 MPa, respectively; these are much higher than those of the friction stir processed base alloy (33 HV and 97 UTS). The highest hardness and strength were achieved for the nano-composite fabricated using the 3-h milled powder mixture; hard nano-sized reaction products and fine recrystallized grains of Al matrix had major and minor roles on enhancing these properties, respectively.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Process Derived Al-TiO{sub 2} Nanocomposite

Aluminum-based composites have many advantages over their conventional counterparts. A major problem in such composites is the clustering of particles in the matrix. Friction stir processing (FSP) can homogenize particle distribution in aluminum-based composites. In this study, unannealed TiO{sub 2} particles were used to prepare Al-TiO{sub 2} nanocomposite using FSP. The TiO{sub 2} particles, about 1 µm, were dispersed into an aluminum matrix by 6 passes of FSP. The TiO{sub 2} particles were fractured by multiple FSP passes, leading to a nano-size particle distribution in the matrix. Nanoscale dispersion was confirmed by scanning electron microscopy and transmission electron microscopy. The fractured TiO{sub 2} particles reacted with the aluminum matrix to form Al{sub 3}Ti intermetallic and Al{sub 2}O{sub 3} ceramic. The progression of the Al-TiO{sub 2} reaction from the fourth to the sixth pass of FSP was revealed by x-ray diffraction. Due to the nanoscale dispersion, the yield and ultimate tensile strength of the composite increased to 97 and 145 MPa, respectively. Ductility of the composite decreased marginally compared to the as-received aluminum. As the dispersed particles pin dislocations, the strain-hardening rate of the composite was considerably increased and the same was seen in the Kocks-Mecking plot. The TiO{sub 2} particles are mechanically activated due to their fracture during FSP, hence leading to reaction with the matrix. The particle refinement and dispersion lead to a homogeneous matrix with higher strength.

36 MATERIALS SCIENCE↗

Surface Modification of C17200 Copper-Beryllium Alloy by Plasma Nitriding of Cu-Ti Gradient Film

In the present work, a copper-titanium film of gradient composition was firstly fabricated by the dual magnetron sputtering through power control and plasma nitriding of the film was then conducted to modify C17200 Cu alloy. The results showed that the prepared gradient Cu-Ti film by magnetron sputtering was amorphous. After plasma nitriding at 650 °C, crystalline Cu-Ti intermetallics appeared in the multi-phase coating, including CuTi{sub 2}, Cu{sub 3}Ti, Cu{sub 3}Ti{sub 2} and CuTi. Moreover, even though the plasma nitriding duration of the gradient Cu-Ti film was only 0.5 h, the mechanical properties of the modified Cu surface were obviously improved, with the surface hardness enhanced to be 417 HV{sub 0.01}, the wear rate to be 0.32 × 10{sup −14} m{sup 3}/Nm and the friction coefficient to be 0.075 at the load of 10 N, which are all more excellent than the C17200 Cu alloy. In addition, the wear mechanism also changed from adhesion wear for C17200 Cu substrate to abrasive wear for the modified surface.

36 MATERIALS SCIENCE↗

Diffusion Bonding of TiAl to Ti6Al4V Using Nanolayers

Microstructural characterization of TiAl to Ti6Al4V dissimilar diffusion bonds assisted by reactive Ni/Al nanolayers was performed in this study. The nanolayers (alternated Al and Ni) were deposited onto the base material surfaces. Diffusion bonding was performed at 700 and 800 °C under pressures from 5 to 40 MPa and dwell times between 60 and 180 min. Microstructural characterization was performed using high-resolution transmission and scanning electron microscopies. The observations revealed that dissimilar TiAl to Ti6Al4V joints assisted by Ni/Al reactive nanolayers can be obtained successfully at 800 °C during 60 min using a pressure of 20 MPa. The bond interface is thin (less than 10 µm) and is mainly composed of NiAl grains. Thin layers of Al-Ni-Ti intermetallic compounds were formed adjacent to the base materials.

36 MATERIALS SCIENCE↗

Microstructures, Martensitic Transformation, and Mechanical Behavior of Rapidly Solidified Ti-Ni-Hf and Ti-Ni-Si Shape Memory Alloys

In this work, the microstructure and mechanical properties of rapidly solidified Ti{sub 50−x/2}Ni{sub 50−x/2}Hf{sub x} (x = 0, 2, 4, 6, 8, 10, and 12 at.%) and Ti{sub 50−y/2}Ni{sub 50−y/2}Si{sub y} (y = 1, 2, 3, 5, 7, and 10 at.%) shape memory alloys (SMAs) were investigated. The sequence of the phase formation and transformations in dependence on the chemical composition is established. Rapidly solidified Ti-Ni-Hf or Ti-Ni-Si SMAs are found to show relatively high yield strength and large ductility for specific Hf or Si concentrations, which is due to the gradual disappearance of the phase transformation from austenite to twinned martensite and the predominance of the phase transformation from twinned martensite to detwinned martensite during deformation as well as to the refinement of dendrites and the precipitation of brittle intermetallic compounds.

36 MATERIALS SCIENCE↗

Improving Joint Formation and Tensile Properties of Dissimilar Friction Stir Welding of Aluminum and Magnesium Alloys by Solving the Pin Adhesion Problem

Friction stir welding (FSW), as a solid-state welding technology invented by TWI in 1991, has potential to join dissimilar Al/Mg alloys. In this study, the pin adhesion phenomenon affecting joint quality during FSW of 6061-T6 aluminum and AZ31B magnesium alloys was investigated. The adhesion phenomenon induced by higher heat input easily transformed the tapered-and-screwed pin into a tapered pin, which greatly reduced the tool’s ability to drive the plasticized materials and further deteriorated joint formation. Under the condition without the pin adhesion, the complex intercalated interlayer at the bottom of stir zone was beneficial to mechanical interlocking of Al/Mg alloys, improving tensile properties. However, the formation of intermetallic compounds was still the main reason of the joint fracture, significantly deteriorating tensile properties. Under the welding speed of 60 mm/min without the pin adhesion phenomenon, the maximum tensile strength of 107 MPa and elongation of 1.2% were achieved.

36 MATERIALS SCIENCE↗

In Situ SEM Observations of Fracture Behavior of Laser Welded–Brazed Al/Steel Dissimilar Joint

Laser welding–brazing of 6061-T6 aluminum alloy to DP590 dual-phase steel with Al-Si12 flux-cored filler wire was performed. The microstructure at the brazing interface was characterized. Fracture behavior was observed and analyzed by in situ scanning electron microscope. The microstructure of the brazing interface showed that inhomogeneous intermetallic compounds formed along the thickness direction, which had a great influence on the crack initiation and propagation. In the top region, the reaction layer at the interface consisted of scattered needle-like Fe(Al,Si){sub 3} and serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the middle region, the compound at the interface was only serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the bottom region, the interface was composed of lamellar-shaped Fe{sub 1.8}Al{sub 7.2}Si. The cracks were first detected in the bottom region and propagated from bottom to top along the interface. At the bottom region, the crack initiated and propagated along the Fe{sub 1.8}Al{sub 7.2}Si/weld seam interface during the in situ tensile test. When the crack propagated into the middle region, a deflection of crack propagation appeared. The crack first propagated along the steel/Fe{sub 1.8}Al{sub 7.2}Si interface and then moved along the weld seam until the failure of the joint. The tensile strength of the joint was 146.5 MPa. Some micro-cracks were detected at Fe(Al,Si){sub 3} and the interface between the steel substrate and Fe(Al,Si){sub 3} in the top region while the interface was still connected.

36 MATERIALS SCIENCE↗

Effect of Localized Corrosion on Fatigue–Crack Growth in 2524-T3 and 2198-T851 Aluminum Alloys Used as Aircraft Materials

Corrosion and fatigue of aluminum alloys are major issues for the in-service life assessment of aircraft structures and for the management of aging air fleets. The aim of this work was to evaluate the effect of localized corrosion on fatigue crack growth (FCG) resistance of the AA2198-T851 Al-Li alloy (Solution Heat Treated, Cold Worked, and Artificially Aged), comparing it with the FCG resistance of AA2524-T3 (Solution Heat Treated and Cold Worked), considering the effect of seawater fog environment. Before fatigue tests, the corrosion behavior of 2198-T851 and 2524-T3 aluminum alloys was verified using open circuit potential and potentiodynamic polarization techniques. Fatigue in air and corrosion fatigue tests were performed applying a stress ratio (R) of 0.1, 15 Hz (air) and 0.1 Hz (seawater fog) frequencies, using a sinusoidal waveform in all cases. The results showed that the localized characteristics of the 2198-T851 and 2524-T3 aluminum alloys are essentially related to the existence of intermetallic compounds, which, due to their different nature, may be cathodic or anodic in relation to the aluminum matrix. The corrosive medium has affected the FCG rate of both aluminum alloys, in a quite similar way. Graphical Abstract: .

36 MATERIALS SCIENCE↗

Effect of the Combined Addition of Y and Ti on the Second Phase and Mechanical Properties of China Low-Activation Martensitic Steel

In this study, approximately 0.35% Ti and two different Y contents were added to China low-activation martensitic (CLAM) steel during melting in a vacuum induction melting furnace. Scanning electron microscopy, transmission electron microscopy, x-ray diffraction, tensile tests, and Charpy impact tests were used to investigate the effects of the combined addition of Y and Ti on the second phase and mechanical properties. The results indicated that Y and Fe formed the large intermetallic compound Fe-Y; the compound easily aggregated in the grain boundaries and exhibited the strength of CLAM steel. Ti did not combine with Y to form the Y-Ti-O phase; however, it could combine with Ta and W to form MC precipitates, which were generally in the 20-50 nm size range. The CLAM steel with a higher Y content exhibited lower yield and tensile strengths at room temperature, with both steels yielding almost identical strengths at 600 °C.

36 MATERIALS SCIENCE↗

The Effect of Mo Particles Addition in Ag-Cu-Ti Filler Alloy on Ti(C,N)-Based Cermet/45 Steel-Brazed Joints

Reliable brazing of Ti(C,N)-based cermet and 45 steel was successfully achieved by using the Mo-particle-reinforced Ag-Cu-Ti composite filler. The effects of Mo content on the interfacial microstructure and mechanical properties of Ti(C,N)-based cermet/45 steel joints were analyzed. The results showed that the joint microstructure was primarily composed of Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2}, Ag(s,s)+Cu(s.s), CuTi+Mo, Ti-based solid solution, and FeTi+Fe{sub 2}Ti. With the increase in Mo content in filler, the thickness of the Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2} layer adjacent to the Ti(C,N)-based cermet decreases, while more blocky Ti-Cu intermetallic were observed in the brazing seam. The shear strength of the joint could be significantly improved by adding suitable amounts of Mo into the Ag-Cu-Ti filler, and the peak value of 263 MPa was achieved when the alloys were brazed with Ag-Cu-Ti+8wt.%Mo composite filler at 920 °C for 20 min.

36 MATERIALS SCIENCE↗

Effect of Al on Grain Refinement and Mechanical Properties of Mg-3Nd Casting Alloy

The effect of Al on the grain refinement and mechanical properties of as-cast Mg-3Nd alloy was investigated systematically by a series of microstructural analysis, solidification analysis and tensile tests. The results show that Al has an obvious refining effect on the as-cast Mg-3Nd alloy. With increasing Al content, the grain size of the as-cast Mg-3Nd alloy decreases firstly, then increases slightly after the Al content reaching 3 wt.%, and the minimum grain size of the Mg-3Nd alloy is 48 ± 4.0 μm. The refining mechanism can be attributed to the formation of Al{sub 2}Nd particles, which play an important role in the heterogeneous nucleation. The strength and elongation of the Mg-3Nd alloy refined by Al also increase with increasing Al content and slightly decrease when the Al content is more than 3 wt.%, and the strengthening mechanism is attributed to the grain refinement as well as dispersed intermetallic particles. Furthermore, the microstructural thermal stability of the Mg-3Nd-3Al alloy is higher than that of the Mg-3Nd-0.5Zr alloy. Overall, the Mg-3Nd alloy with Al addition is a novel alloy with wide and potential application prospects.

36 MATERIALS SCIENCE↗

Effect of Sm-Rich Phase on Corrosion Behavior of Hot-Extruded AZ31-1.5Sm Magnesium Alloy

The effects of Sm on the corrosion and microstructure behavior of hot-extruded AZ31 magnesium alloy were investigated by SEM, TEM, weight loss analysis, and electrochemical measurements. The results indicated that granular Al{sub 2}Sm phase ~ 4 μm in size in the hot-extruded AZ31 magnesium alloy modified with 1.5 wt.% Sm leads to significant grain refinement. The corrosion rate decreased from 15.98 × 10{sup −4} to 11.19 × 10{sup −4} g cm{sup −2} h{sup −1} in the transverse section and from 8.57 × 10{sup −4} to 6.20 × 10{sup −4} g cm{sup −2} h{sup −1} in the longitudinal section. Compared to the unmodified alloy, the corrosion potential of the Sm-modified alloy in the transverse and longitudinal sections increased by 98 and 62 mV, respectively, and the R{sub ct} value (charge transfer resistance) in the transverse and longitudinal sections of the modified alloy increased from 1764 and 1756 to 2928 and 2408 Ω cm{sup 2}, respectively. The results showed that the corrosion resistance of hot-extruded AZ31 magnesium alloy was significantly improved by Sm addition due to the grain refinement, the decreased dislocation density, and the suppression of micro-galvanic corrosion caused by Al-Sm-(Mn) intermetallic compounds.

36 MATERIALS SCIENCE↗

The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B{sub 4}C and (Cr, Fe, Mo, Ni, Ti){sub 3}B{sub 2} phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

36 MATERIALS SCIENCE↗

Analysis of Microstructure and Sliding Wear Behavior of Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} High-Entropy Alloy

Α Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} high-entropy alloy (HEA) of the well-known family of CoCrFeNiTi has been designed using empirical parameters. The aim of this design was the production of a HEA with fcc structure that gives ductile behavior and also high strength because of the solid solution effect. The VEC calculations (8.1) supported the fcc structure while the δ factor calculations (4.97) not being out of the limit values, advised a significant lattice distortion. From the other hand, the ΔΗ{sub mix} calculations (− 9.64 kJ/mol) gave strong indications that no intermetallic would be formed. In order to investigate its potential application, the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was prepared by vacuum arc melting and a primary assessment of its surface degradation response was conducted by means of sliding wear testing using different counterbody systems for a total sliding distance of 1000 m. An effort to correlate the alloy’s wear response with the microstructural characteristics was attempted. Finally, the wear behavior of the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was compared with that of two commercially used wear-resistant alloys. The results obtained provided some first signs of the high-entropy alloys’ better wear performance when tested under sliding conditions against a steel ball.

36 MATERIALS SCIENCE↗

Electrochemical Behavior Assessment of As-Cast Mg-Y-RE-Zr Alloy in Phosphate Buffer Solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}) Using Electrochemical Impedance Spectroscopy and Mott–Schottky Techniques

In the present study, electrochemical behavior of as-cast Mg-Y-RE-Zr alloy (RE: rare-earth alloying elements) was investigated using electrochemical tests in phosphate buffer solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}). X-ray diffraction techniques and Scanning electron microscopy equipped with energy dispersive x-ray spectroscopy were used to investigate the microstructure and phases of the experimental alloy. Different electrochemical tests such as potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS) and Mott–Schottky (M–S) analysis were carried out in order to study the electrochemical behavior of the experimental alloy in phosphate buffer solutions. The PDP curves and EIS measurements indicated that the passive behavior of the as-cast Mg-Y-RE-Zr alloy in phosphate buffer solutions was weakened by an increase in the pH, which is related to formation of an imperfect and less protective passive layer on the alloy surface. The presence of the insoluble zirconium particles along with high number of intermetallic phases of RE elements mainly Mg{sub 24}Y{sub 5} in the magnesium matrix can deteriorate the corrosion performance of the alloy by disrupting the protective passive layer that is formed at pH values over 11. These insoluble zirconium particles embedded in the matrix can detrimentally influence the passivation. The M–S analysis revealed that the formed passive layers on Mg-Y-RE-Zr alloy behaved as an n-type semiconductor. An increase in donor concentration accompanying solutions of higher alkalinity is thought to result in the formation of a less resistive passive layer.

36 MATERIALS SCIENCE↗

Investigation of the Tribological Properties of AlxSi-1.2Fe(Mn) (x = 5-13 wt.%) Alloys

The effect of Fe-impurity and Mn modification on the sliding wear behavior of Al-xSi-1.2Fe(Mn) (x = 5-13 wt.%) alloys was investigated in dry sliding against AISI 52100 steel. According to the results, in the Si range of 5-9 wt.%, Fe-impurity promotes the formation of finely distributed β-Al{sub 5}FeSi intermetallics in the matrix increasing its hardness and potential to support the tribolayer leading to the improved wear characteristics. The presence of Fe in the composition of Al-(9-13)Si alloys, however, leads to the formation of primary β-platelets that their sizes and volume fractions increase with Si concentration. The formation of primary compounds increases the hardness, but makes the alloys less ductile and more vulnerable to microcracking and wear. Manganese modification converts the β-Fe platelets to the α-Al{sub 15}(Fe,Mn){sub 3}Si{sub 2} compounds with different morphologies. The substitution of fine β-platelets by α-Chinese scripts in Al-(5-9)Si-1.2FeMn alloys reduces the wear resistance, but the formation of primary α-compounds with star-like or polyhedral morphologies in Al-(9-13)Si-1.2FeMn alloys improves their wear characteristics. Moreover, it was found that the formation of Fe(Mn)-rich compounds affects the friction coefficient which is likely due to the fracture of particles in the subsurface region, their interaction with contacting surfaces, and their effect on the stability of the tribolayer.

36 MATERIALS SCIENCE↗

Mechanical Properties and Interface Evaluation of Al/AZ31 Multilayer Composites Produced by ARB at Different Rolling Temperatures

Many researchers have studied the microstructure and mechanical properties of Al/Mg composites rolled at a unique temperature; however, the effect of rolling temperature, which is one of the more decisive accumulative roll bonding (ARB) parameters, has not been investigated. In this work, laminated Al/Mg composites were fabricated by ARB at different temperatures using AZ31 magnesium alloy and commercially pure aluminum sheets. The microstructure of the layers and the mechanical properties of the rolled Al/AZ31 composites were investigated. Tensile and bending properties of the multilayer materials were examined by tensile and three-point bending tests. The results showed that mechanical bonding of the layers was improved with increasing rolling temperature. As a result, the intermediate rolling temperature (300 °C) indicated the best mechanical properties. Moreover, hot rolling caused an accelerated formation of intermetallic compounds.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗