At least 973 records · Page 54

Oxy-Combustion Boiler Material Development

Under U.S. Department of Energy Cooperative Agreement No. DE-NT0005262 Foster Wheeler North America Corp conducted a laboratory test program to determine the effect of oxy-combustion on boiler tube corrosion. In this program, CFD modeling was used to predict the gas compositions that will exist throughout and along the walls of air-fired and oxy-fired boilers operating with low to high sulfur coals. Test coupons of boiler tube materials were coated with deposits representative of those coals and exposed to the CFD predicted flue gases for up to 1000 hours. The tests were conducted in electric tube furnaces using oxy-combustion and air-fired flue gases synthesized from pressurized cylinders. Following exposure, the test coupons were evaluated to determine the total metal wastage experienced under air and oxy-combustions conditions and materials recommendations were made. Similar to air-fired operation, oxy-combustion corrosion rates were found to vary with the boiler material, test temperature, deposit composition, and gas composition. Despite this, comparison of air-fired and oxy-fired corrosion rates showed that oxy-firing rates were, for the most part, similar to, if not lower than those of air-firing; this finding applied to the seven furnace waterwall materials (wrought and weld overlay) and the ten superheater/reheater materials (wrought and weld overlay) that were tested. The results of the laboratory oxy-combustion tests, which are based on a maximum bulk flue gas SO 2 level of 3200 ppmv (wet) / 4050 ppmv (dry), suggest that, from a corrosion standpoint, the materials used in conventional subcritical and supercritical, air-fired boilers should also be suitable for oxy-combustion retrofits. Although the laboratory test results are encouraging, they are only the first step of a material evaluation process and it is recommended that follow-on corrosion tests be conducted in coal-fired boilers operating under oxy-combustion to provide longer term (one to two year) data. The test program details and data are presented herein.

20 FOSSIL-FUELED POWER PLANTS↗

Transformational electrode drying process (Final Report)

This report includes major findings and outlook from the transformational electrode drying project performance period from January 6, 2012 to August 1, 2012. Electrode drying before cell assembly is an operational bottleneck in battery manufacturing due to long drying times and batch processing. Water taken up during shipment and other manufacturing steps needs to be removed before final battery assembly. Conventional vacuum ovens are limited in drying speed due to a temperature threshold needed to avoid damaging polymer components in the composite electrode. Roll to roll operation and alternative treatments can increase the water desorption and removal rate without overheating and damaging other components in the composite electrode, thus considerably reducing drying time and energy use. The objective of this project was the development of an electrode drying procedure, and the demonstration of processes with no decrease in battery performance. The benchmark for all drying data was an 80°C vacuum furnace treatment with a residence time of 18 – 22 hours. This report demonstrates an alternative roll to roll drying process with a 500-fold improvement in drying time down to 2 minutes and consumption of only 30% of the energy compared to vacuum furnace treatment.

25 ENERGY STORAGE↗

Oxy-Combustion Boiler Material Development

Under U.S. Department of Energy Cooperative Agreement No. DE-NT0005262 Foster Wheeler North America Corp conducted a laboratory test program to determine the effect of oxy-combustion on boiler tube corrosion. In this program, CFD modeling was used to predict the gas compositions that will exist throughout and along the walls of air-fired and oxy-fired boilers operating with low to high sulfur coals. Test coupons of boiler tube materials were coated with deposits representative of those coals and exposed to the CFD predicted flue gases for up to 1000 hours. The tests were conducted in electric tube furnaces using oxy-combustion and air-fired flue gases synthesized from pressurized cylinders. Following exposure, the test coupons were evaluated to determine the total metal wastage experienced under air and oxy-combustions conditions and materials recommendations were made. Similar to air-fired operation, oxy-combustion corrosion rates were found to vary with the boiler material, test temperature, deposit composition, and gas composition. Despite this, comparison of air-fired and oxy-fired corrosion rates showed that oxy-firing rates were, for the most part, similar to, if not lower than those of air-firing; this finding applied to the seven furnace waterwall materials (wrought and weld overlay) and the ten superheater/reheater materials (wrought and weld overlay) that were tested. The results of the laboratory oxy-combustion tests, which are based on a maximum bulk flue gas SO2 level of 3200 ppmv (wet) / 4050 ppmv (dry), suggest that, from a corrosion standpoint, the materials used in conventional subcritical and supercritical, air-fired boilers should also be suitable for oxy-combustion retrofits. Although the laboratory test results are encouraging, they are only the first step of a material evaluation process and it is recommended that follow-on corrosion tests be conducted in coal-fired boilers operating under oxy-combustion to provide longer term (one to two year) data. The test program details and data are presented herein.

36 MATERIALS SCIENCE↗

LANL Response to SRS Requirement G-ESR-G-00035 Item 11 Bed Temperature Requirements, For the Addition of Direct Metal Oxidation Unit 3, Revision 0

Los Alamos National Laboratory has identified a number of plutonium-bearing materials that will be placed in storage in 3013 containers per requirements of DOE-STD-3013-2004, or DOE-STD-3013-2012 when it is implemented in the LANL contract. Before these items can be considered for storage at Savannah River Site, 20 points of agreement, described in Savannah River Site (SRS) document G-ESR-G-00035, Revision 1, must be documented and provided to SRS for review. These agreements include documentation that the requirements of the 3013 Standard are met and the storage facility’s safety envelope is not compromised. Point 11 of the 20 points is the requirement that material be stabilized at 950°C for a minimum of two hours prior to packaging. This report addresses the Point 11 requirement, describing the controls used during stabilization to ensure that the material is properly stabilized using a continuous process (Advanced Recovery and Integrated Extraction System [ARIES] direct metal oxidation [DMO] and recycle oxide calcination). These controls include verification of the furnace controller thermocouple profile and verification of the profiles for the calciner tube hot zone. This report is specific to Direct Metal Oxidation Unit 3 (DMO-3). The point 11 requirements for DMO-2 and muffle furnace oxidation are covered in reference. This report does not replace reference. The process and methodology used in this report are similar to that used for Direct Metal Oxidation Unit 2, or DMO-2, as documented in reference. This report documents the performance for ARIES DMO-3. The temperature on the outside of the calciner tube must be at least 1,032°C. The auger rotation rate set point will be dependent on the pitch of the installed auger. For an auger pitch of 1.297 in/rev the auger set point will be 0.0777 rpm or less, which allows for at least 132 minutes calcination time based on worst case conditions (i.e., lowest possible powder density at the lowest initial powder temperature, and under the least favorable heat transfer conditions, and with the least favorable auger pitch of the currently installed auger.) A new auger design may be used in future modifications of DMO-3 that has an auger pitch of 1.400 ± 0.025 inches which would change the required auger set point to 0.0707 rpm or less.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Recovery Act: Waste Energy Project at AK Steel Corp. Middletown Works

In 2008, Air Products and Chemicals, Inc. (“Air Products”) began development of a project to beneficially utilize waste blast furnace “topgas” generated in the course of the iron-making process at AK Steel Corporation’s Middletown, Ohio works. In early 2010, Air Products was awarded DOE Assistance Agreement DE-EE002736 to further develop and build the combined-cycle power generation facility. In June 2012, Air Products and AK Steel Corporation terminated work when it was determined that the project would not be economically viable at that time nor in the foreseeable future. The project would have achieved the FOA-0000044 Statement of Project Objectives by demonstrating, at a commercial scale, the technology to capture, treat, and convert blast furnace topgas into electric power and thermal energy.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leach indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leach indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Assessment of Testing Options for the NTR at the INL (Final Report)

One of the main technologies that can be developed to dramatically enhance the human exploration of space is the nuclear thermal rocket (NTR). Several studies over the past thirty years have shown that the NTR can reduce the cost of a lunar outpost, reduce the risk of a human mission to Mars, enable fast transits for most missions throughout the solar system, and reduce the cost and time for robotic probes to deep space. Three separate committees of the National Research Council of the National Academy of Sciences have recommended that NASA develop the NTR. One of the primary issues in development of the NTR is the ability to verify a flight ready unit. Three main methods can be used to validate safe operation of a NTR: 1) Full power, full duration test in an above ground facility that scrubs the rocket exhaust clean of any fission products; 2) Full power , full duration test using the Subsurface Active Filtering of Exhaust (SAFE) technique to capture the exhaust in subsurface strata; 3) Test of the reactor fuel at temperature and power density in a driver reactor with subsequent first test of the fully integrated NTR in space. The first method, the above ground facility, has been studied in the past. The second method, SAFE, has been examined for application at the Nevada Test Site. The third method relies on the fact that the Nuclear Furnace series of tests in 1971 showed that the radioactive exhaust coming from graphite based fuel for the NTR could be completely scrubbed of fission products and the clean hydrogen flared into the atmosphere. Under funding from the MSFC, the Center for Space Nuclear Research (CSNR) at the Idaho National laboratory (INL) has completed a reexamination of Methods 2 and 3 for implementation at the INL site. In short, the effort performed the following: 1) Assess the geology of the INL site and determine a location suitable SAFE testing; 2) Perform calculations of gas transport throughout the geology; 3) Produce a cost estimate of a non-nuclear , sub-scale test using gas injection to validate the computational models; 4) Produce a preliminary cost estimate to build a nuclear furnace equivalent facility to test NTR fuel on a green field location on the INL site. The results show that the INL geology is substantially better suited to the SAFE testing method than the NTS site. The existence of impermeable interbeds just above the sub-surface aquifer ensure that no material from the test, radioactive or not, can enter the water table. Similar beds located just below the surface will prevent any gaseous products from reaching the surface for dispersion. The extremely high permeability of the strata between the interbeds allows rapid dispersion of the rocket exhaust. In addition, the high permeability suggests that a lower back-pressure may develop in the hole against the rocket thrust, which increases safety of operations. Finally, the cost of performing a sub-scale, non-nuclear verification experiment was determined to be $\$$3M. The third method was assessed through discussions with INL staff resident at the site. In essence, any new Category I facility on any DOE site will cost in excess of $\$$250M. Based on the results of this study, a cost estimate for testing a nuclear rocket at the INL site appears to be warranted. Given the fact that a new nuclear fuel may be possible that does not release any fission products, the SAFE testing option appears to be the most affordable.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Thermal and Physical Properties of Plutonium Dioxide Produced from the Oxidation of Metal: a Data Summary

The ARIES Program at the Los Alamos National Laboratory removes plutonium metal from decommissioned nuclear weapons, and converts it to plutonium dioxide in a specially-designed Direct Metal Oxidation furnace. The plutonium dioxide is analyzed for specific surface area, particle size distribution, and moisture content. The purpose of these analyses is to certify that the plutonium dioxide powder meets or exceeds the specifications of the end-user, and the specifications for the packaging and transport of nuclear materials. Analytical results from plutonium dioxide from ARIES development activities, from ARIES production activities, from muffle furnace oxidation of metal, and from metal that was oxidized over a lengthy time interval in air at room temperature, are presented. The processes studied produce plutonium dioxide powder with distinct differences in measured properties, indicating the significant influence of oxidation conditions on physical properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Estimate of Evaporation of Uranium in Vacuum Melt Casting Systems

In this document we make estimates of Uranium vapor production rates and the mass of Uranium in the vapor state during operation of a casting furnace. The information provided here is based upon the reference document: Basic Physics of Vacuum Evaporation of Uranium with a Conventional or Advanced Melt Heating System, T. A. Shepp, LLNL Document CODT – 2011-xxxx We assume that the melting furnace designs may include heated melts in a container with walls at a lower temperature than the melt surface and other systems with melts contained within a container at the same temperature as the melt. We assume that both systems operate in a vacuum environment. In the first case the Uranium vapor produced at the melt surface flows from the melt to the walls where it is collected as a solid or liquid depending upon the wall temperature, In this case the Uranium vapor exists in a non-equilibrium condition. The vapor expands from the melt surface and changes in pressure, density, temperature as well as atomic excitation. Under these circumstances an ideal gas law does not provide a complete picture. For the uniform temperature case the ideal gas law can give good information on the state of the vapor. For both cases we would like to determine an upper limit estimate of the amount of Uranium in the vapor state at any time. In the event of a breach of the containment it may also be of interest to determine the production of vapor as the melt system cools. Other vapor interactions involving a breach such as limited leaking and chemical reactions with the atmosphere all tend to limit the propagation of the vapor to occupied areas.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leachability indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Retrofit Integrated Space & Water Heating: Field Assessment: Minneapolis, Minnesota (Fact Sheet)

This project analyzed combined condensing water heaters or boilers and hydronic air coils to provide high efficiency domestic hot water and forced air space heating. Called 'Combi' systems, they provided similar space and water heating performance less expensively than installing two condensing appliances. The system's installed costs were cheaper than installing a condensing furnace and either a condensing tankless or condensing storage water heater. However, combi costs must mature and be reduced before they are competitive with a condensing furnace and power vented water heater (EF of 0.60). Better insulation and tighter envelopes are reducing space heating loads for new and existing homes. For many homes, decreased space heating loads make it possible for both space and domestic water heating loads to be provided with a single heating plant. These systems can also eliminate safety issues associated with natural draft appliances through the use of one common sealed combustion vent.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Recycling of spent batteries from electric drive vehicles (BNL-GIPP-372)

This project seeks to develop unique, energy efficient high temperature furnace technology and auxiliary equipment (e.g. material handling, cooling and electrical circuits, etc.). The furnace technology would become a critical element of the technology for recycling and reuse of high value materials from spent lithium-ion batteries for electric vehicles.

25 ENERGY STORAGE↗

1366 Project Silicon: Reclaiming US Silicon PV Leadership

1366 Technologies’ Project Silicon addresses two of the major goals of the DOE’s PV Manufacturing Initiative Part 2 program: 1) How to reclaim a strong silicon PV manufacturing presence and; 2) How to lower the levelized cost of electricity (“LCOE”) for solar to $0.05-$0.07/kWh, enabling wide-scale U.S. market adoption. To achieve these two goals, US companies must commercialize disruptive, high-value technologies that are capable of rapid scaling, defensible from foreign competition, and suited for US manufacturing. These are the aims of 1366 Technologies Direct Wafer ™ process. The research conducted during Project Silicon led to the first industrial scaling of 1366’s Direct Wafer™ process – an innovative, US-friendly (efficient, low-labor content) manufacturing process that destroys the main cost barrier limiting silicon PV cost-reductions: the 35-year-old grand challenge of making quality wafers (40% of the cost of modules) without the cost and waste of sawing. The SunPath program made it possible for 1366 Technologies to build its demonstration factory, a key and critical step in the Company’s evolution. The demonstration factory allowed 1366 to build every step of the process flow at production size, eliminating potential risk and ensuring the success of the Company’s subsequent scaling for a 1 GW factory to be constructed in Western New York in 2016 and 2017. Moreover, the commercial viability of the Direct Wafer process and its resulting wafers were established as 1366 formed key strategic partnerships, gained entry into the $8B/year multi-Si wafer market, and installed modules featuring Direct Wafer products – the veritable proving grounds for the technology. The program also contributed to the development of three Generation 3 Direct Wafer furnaces. These furnaces are the platform for copying intelligently and preparing our supply chain – large-scale expansion will not require a bigger machine but more machines. SunPath filled the crucial development step between the original research effort in Lexington and the GW factory scheduled to be online before the end of the decade. At the conclusion of the project, it is clear that the Direct Wafer™ technology will have a dramatic impact on the entire silicon photovoltaic supply chain by effectively doubling existing silicon capacity (by reducing silicon usage by 50%) and reducing supply chain capital costs by 35%. The technology, when fully-scaled in the US, will also lead to significant job growth, with the eventual creation of 1,000 jobs in Western New York.

14 SOLAR ENERGY↗

Silicon Carbide Temperature Monitor Processing Improvements. Status Report

Silicon carbide (SiC) temperature monitors are used as temperature sensors in Advanced Test Reactor (ATR) irradiations at the Idaho National Laboratory (INL). Although thermocouples are typically used to provide real-time temperature indication in instrumented lead tests, other indicators, such as melt wires, are also often included in such tests as an independent technique of detecting peak temperatures incurred during irradiation. In addition, less expensive static capsule tests, which have no leads attached for real-time data transmission, often rely on melt wires as a post-irradiation technique for peak temperature indication. Melt wires are limited in that they can only detect whether a single temperature is or is not exceeded. SiC monitors are advantageous because a single monitor can be used to detect for a range of temperatures that occurred during irradiation. As part of the process initiated to make SiC temperature monitors available at the ATR, post-irradiation evaluations of these monitors have been previously completed at the High Temperature Test Laboratory (HTTL). INL selected the resistance measurement approach for determining irradiation temperature from SiC temperature monitors because it is considered to be the most accurate measurement. The current process involves the repeated annealing of the SiC monitors at incrementally increasing temperature, with resistivity measurements made between annealing steps. The process is time consuming and requires the nearly constant attention of a trained staff member. In addition to the expensive and lengthy post analysis required, the current process adds many potential sources of error in the measurement, as the sensor must be repeatedly moved from furnace to test fixture. This time-consuming post irradiation analysis is a significant portion of the total cost of using these otherwise inexpensive sensors. An additional consideration of this research is that, if the SiC post processing can be automated, it could be performed in an MFC hot cell, further reducing the time and expense of lengthy decontaminations prior to processing. Sections of this report provide a general description of resistivity techniques currently used to infer peak irradiation temperature from silicon carbide temperature monitors along with some representative data, the proposed concepts to improve the process of analyzing irradiated SiC temperature monitors, the completed efforts to prove the proposed concepts, and future activities. The efforts detailed here succeeded in designing and developing a real-time automated SiC resistivity measurement system, and performed two initial test runs. Activities carried out include the assembly and integration of the system hardware; the design and development of a preliminary monitor fixture; the design of a technique to automate the data analysis and processing; the development of the communication, coordination, and user software; and the execution and troubleshooting of test run experiments using the box furnace. Although the automation system performed as required, the designed fixture did not succeed in establishing the needed electrical contacts with the SiC monitor.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Incorporation of the Joule Heating of highly conducting materials into the Truchas code via an asymptotic approach

The EM module of the Truchas code currently lacks the capability to model the Joule (Ohmic) heating of highly conducting materials that are inserted into induction furnaces from time to time to change the heating profile. This effect is difficult to simulate directly because of the requirement to resolve the extremely thin skin depth of good conductors, which is computationally costly. For example, copper has a skin depth, δ ~ 1 mm, for an oscillation frequency of tens of kHz. The industry is interested in determining what fraction of the heating power is lost to the Joule heating of these good conductors inserted inside the furnaces. The approach presented in this document is one of asymptotics where the leading order (unperturbed) solution is taken as that which emerges from solving the EM problem for a perfectly conducting insert. The conductor is treated as a boundary of the domain. The perturbative correction enters as a series expansion in terms of the dimensionless skin depth δ/L, where L is the characteristic size of the EM system. The correction at each order depends on the previous. This means that the leading order correction only depends on the unperturbed solution, in other words, it does not require Truchas to perform an additional EM field solve. Thus, the Joule heating can be captured by a clever leveraging of the existing tools in Truchas with only slight modifications.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Retrofitting Forced Air Combi Systems: A Cold Climate Field Assessment

This project analyzed combined condensing water heaters or boilers and hydronic air coils to provide high efficiency domestic hot water (DHW) and forced air space heating. Called "combi" systems, they provided similar space and water heating performance less expensively than installing two condensing appliances. The system's installed costs were cheaper than installing a condensing furnace and either a condensing tankless or condensing storage water heater. However, combi costs must mature and be reduced before they are competitive with a condensing furnace and power vented water heater (energy factor of 0.60). Better insulation and tighter envelopes are reducing space heating loads for new and existing homes. For many homes, decreased space heating loads make it possible for both space and domestic water heating loads to be provided with a single heating plant. These systems can also eliminate safety issues associated with natural draft appliances through the use of one common sealed combustion vent. The combined space and water heating approach was not a new idea. Past systems have used non-condensing heating plants, which limited their usefulness in climates with high heating loads. Previous laboratory work (Schoenbauer et al. 2012a) showed that proper installation was necessary to achieve condensing with high efficiency appliances. Careful consideration was paid to proper system sizing and minimizing the water temperature returning from the air handling unit to facilitate condensing operation.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Retrofitting Forced Air Combi Systems: A Cold Climate Field Assessment

This project analyzed combined condensing water heaters or boilers and hydronic air coils to provide high efficiency domestic hot water (DHW) and forced air space heating. Called 'combi' systems, they provided similar space and water heating performance less expensively than installing two condensing appliances. The system's installed costs were cheaper than installing a condensing furnace and either a condensing tankless or condensing storage water heater. However, combi costs must mature and be reduced before they are competitive with a condensing furnace and power vented water heater (energy factor of 0.60). Better insulation and tighter envelopes are reducing space heating loads for new and existing homes. For many homes, decreased space heating loads make it possible for both space and domestic water heating loads to be provided with a single heating plant. These systems can also eliminate safety issues associated with natural draft appliances through the use of one common sealed combustion vent. The combined space and water heating approach was not a new idea. Past systems have used non-condensing heating plants, which limited their usefulness in climates with high heating loads. Previous laboratory work (Schoenbauer et al. 2012a) showed that proper installation was necessary to achieve condensing with high efficiency appliances. Careful consideration was paid to proper system sizing and minimizing the water temperature returning from the air handling unit to facilitate condensing operation.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗