Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SILICONES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 955 records · Page 53

Enhancing the Electrochemical Performance of Aqueous Processed Li-Ion Cathodes with Silicon Oxide Coatings

Lithium-ion battery cathode materials suffer from bulk and interfacial degradation issues, which negatively affect their electrochemical performance. Oxide coatings can mitigate some of these problems and improve electrochemical performance. However, current coating strategies have low throughput, are expensive, and have limited applicability. In this article, we describe a low-cost and scalable strategy for applying oxide coatings on cathode materials. Here, we report synergistic effects of these oxide coatings on the performance of aqueously processed cathodes in cells. The SiO 2 coating strategy developed herein improved mechanical, chemical, and electrochemical performance of aqueously processed Ni-, Mn- and Co-based cathodes. This strategy can be used on a variety of cathodes to improve the performance of aqueously processed Li-ion cells.

25 ENERGY STORAGE↗

Dynamic Material Flow Analysis of Silicon Photovoltaic Modules to Support a Circular Economy Transition

Solar photovoltaics (PV) are the fastest growing renewable energy technologies for clean, cheap, and sustainable electricity generation. To prepare for rapid scale-up, the PV industry needs to project material requirements to build out all aspects of the supply chain appropriately and plan to handle large volumes of module waste. Impacts of deploying different material circularity strategies to reduce waste and conserve primary resources need to be quantified to inform sustainable material management. Here, we introduce the photovoltaic dynamic material flow analysis (PV DMFA) model based on PV electricity generation. The model quantifies material flows and stocks in the cradle-to-cradle life cycles of utility-scale c-Si PV systems in the United States through 2100. We present case studies for solar flat glass and aluminum frame materials under various scenarios to project the impacts of PV performance, reliability, and processing parameters, material circularity strategies, and module design shifts. In the absence of circularity measures, ~100 million MT of flat glass and ~12 million MT of aluminum would be needed for PV installations by 2100 to meet projected growth in domestic utility PV demand to nearly 1000 TWh in 2100. With optimistic but feasible improvements in efficiency, reliability, and circularity, material intensity and waste could be reduced by nearly 50%. Efficient module collection, minimally intrusive recycling, and careful scrap handling and cleaning could improve material circularity in the PV value chain. This model serves as a sustainability data support tool that may aid in the circular economy transition for PV systems.

circular economy↗

Spatial Atomic Layer Deposition of Aluminum Oxide as a Passivating Hole Contact for Silicon Solar Cells

In this work, tunneling aluminum oxide (Al 2 O 3 ) passivation layers are demonstrated to be a candidate for hole collecting, passivating contacts when coupled with a boron-doped surface. Here, these very thin Al 2 O 3 films (1.5-3 nm) are deposited using spatial atomic layer deposition (ALD) on boron diffused (110-115 Ω –1 ) hydrophilic surfaces operating as metal-insulator-semiconductor (MIS) contacts. Emitter saturation current density values of approximately ≈57 fA cm 2 are achieved for Al 2 O 3 film thicknesses of 2 nm before metallization. At this same thickness, contact resistivity values of 33 mΩ cm 2 are obtained after metallization. Most importantly, the boron diffusion, wet chemical surface preparation, and spatial ALD of Al 2 O 3 used to create these MIS structures were all performed with industrially relevant equipment on Cz wafers.

14 SOLAR ENERGY↗

Degradation and Accelerated Recovery of Surface Passivation in n+, p+, and Intrinsic Poly-Si/SiOx Passivating Contacts for Silicon Solar Cells

We report on the degradation and recovery of surface passivation of fired poly-Si/SiOx passivating contacts with hydrogen containing Al2O3 during annealing in the dark and under illumination. Upon firing to a peak temperature of 670 degrees C, the iVoc for symmetric test structures with n+, p+, and intrinsic poly-Si/SiOx contacts decreases due to a loss of surface passivation. Upon further annealing over the temperature range of 200-350 degrees C in the dark, depending on the type of doping, the surface passivation either shows further degradation followed by recovery, or direct recovery to the initial iVoc. Annealing at higher temperatures and/or higher illumination intensities accelerates the kinetics for both degradation and recovery processes. We show that the degradation and recovery processes are thermally activated and proceed identically in subsequent firing and annealing steps showing their cyclic nature. We present a series reaction model to explain the kinetics of degradation and recovery processes for n+ and intrinsic poly-Si/SiOx contacts. By fitting the model's rate expressions to the data, the determined effective activation energy barriers for degradation and recovery for n+ poly-Si/SiOx contacts in the dark are 1.24 and 1.51 eV, which are lowered under 7.5 Suns illumination to 0.76 and 1.15 eV, respectively.

14 SOLAR ENERGY↗

High-temperature active oxidation of nanocrystalline silicon-carbide: A reactive force-field molecular dynamics study

Flexible woven SiC ceramics are prone to accelerated fiber embrittlement under high temperature oxidation in dynamic oxygen environments. The nanocrystalline structure of the constituent fibers impacts the reaction kinetics and phase transformations during active oxidation. However, fundamental understanding and quantification of grain boundary effects on oxidation behavior in nanocrystalline SiC remain elusive when temperatures exceed 1500 K. This study deploys large-scale molecular dynamics simulations with a reactive force-field to elucidate the complex roles of atomic oxygen reservoir conditions and grain size on oxidation kinetics and the nature of oxides produced in both monocrystalline and nanocrystalline 3C-SiC between 1100 K and 2000 K. The simulations with dynamically replenished oxygen provide good agreement with oxidation kinetics and activation energies for the monocrystalline Si(100) and C(100) orientations published in the available literature. This study reveals that, by contrast, nanocrystalline SiC samples exhibit two distinct oxidation kinetics with a transition point at 1500 K due to surface melting, which is supported by experimental evidence. The introduction of a grain-boundary network produces a two-fold decrease in oxidation activation energies compared to monocrystalline SiC below 1500 K. Above 1500 K, however, the activation energies rise substantially due to the formation of a liquid Si phase at the SiC/Si oxide interface. Further, it is shown that the stability of the interfacial liquid phase is promoted by incoherent grain boundaries in the crystalline SiC. These findings are important for the deployment of nanocrystalline SiC fibers in advanced thermal protection systems for high-temperature applications.

36 MATERIALS SCIENCE↗

Transient testing of uranium silicide fuel in zircaloy and silicon carbide cladding

Using the newly restarted Transient Reactor Test (TREAT) facility at Idaho National Laboratories, fresh (unirradiated) U 3 Si 2 fuel pellets were tested under reactivity-initiated accident conditions in dry helium capsules. These tests were performed with total energy depositions sufficient to induce melting of the U 3 Si 2 fuel pellets based on available thermophysical property data. The instrumented experiments utilized in-pile thermocouples and infrared pyrometers to measure the cladding temperature during the transient, which are in reasonable agreement with predicted peak cladding temperatures using a simple BISON fuel performance model. This same model is then used to predict expected cladding stresses during the transients in areas where pellet cladding interaction is expected. It was shown that for transient energy depositions up to 528J/g rod like geometry of the test articles was maintained. While it is acknowledged that more confirmatory testing is required in more prototypic environments, these first of their kind experiments have demonstrated that unirradiated U 3 Si 2 fuel and unirradiated SiC-SiC claddings can likely retain a “rod like” geometry for transient energy depositions up to 528J/g.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Optical measure of disorder: Why Urbach analysis works for amorphous silicon but fails for amorphous carbon

We investigate the basis for the Paradox where the Urbach-slope disorder parameter disagrees with the Raman width in amorphous diamond-like carbon (DLC) materials (lower Urbach-Eo yet greater Raman width). We examined the bandgap and Urbach-slope measurement issues. While significant errors are identified, ultimately these cannot resolve the Paradox. This resolution involves large changes in shape of DLC's absorption band resulting from large energy shifts. To solidify the understanding of band energy shifts, we examined their properties using a-Si:H, well known for its agreement between Raman and Urbach-slope disorder parameters. Using Tauc-Lorentz (T-L) dispersion functions, the Urbach method works for a-Si:H because small changes in shape occur, as measured by (i) peak position, (ii) peak width, (iii) peak amplitude, and (iv) and gap energies. Moreover, for a-Si:H, a 5th condition (v) there is no other feature below the principal band to interfere with its fall. All 5 of these conditions fail for DLCs. Because T-L dispersions accommodate asymmetry, we traced the Paradox to a steepening of the band shape as it pushes toward lower energy. This steepening is unrelated to disorder, but to a boundary value problem where energy cannot be negative. We conclude that Urbach analysis is invalid for DLC materials, but the T-L width is a good measure instead. We also examined another disorder measure, where π bonds should be considered as disorder relative to the σ bonds in an idealized “amorphous diamond” sp 3 network: superconvergence can be used to quantify these π transitions. Finally, further molecular orbital calculations are needed to properly interpret the changes in T-L widths.

36 MATERIALS SCIENCE↗

Embodied energy and carbon from the manufacture of cadmium telluride and silicon photovoltaics

Here, looking beyond the traditional cost and efficiency metrics of photovoltaics (PV), this work evaluates the impact of embodied energy, embodied carbon, and energy payback time of two dominant technologies (CdTe and Si) on global decarbonization goals. The relative effects of PV technology type, technological advances, energy grid mix, and recycling are evaluated in terms of fostering decarbonization goals. If the highest carbon-intensity scenarios are realized, 2%-14% of the remaining estimated global carbon budget might be consumed to manufacture modules without including their balance of systems. Applying a carbon cost indicates that CdTe might have an additional value of $\$$0.02-$\$$0.04/W relative to Si PV manufactured with the same energy mix. Due to the scale of the challenge, any actions leading to an increased deployment of thin-film PV and/or a significant decrease in the deployed PV's embodied carbon through changing the manufacturing grid mix have demonstrable value in helping the world stay within its remaining estimated carbon budget.

14 SOLAR ENERGY↗

Operando NMR characterization of cycled and calendar aged nanoparticulate silicon anodes for Li-ion batteries

Replacing graphite anodes with Si anodes can greatly increase the energy of current Li-ion batteries. Detailed characterization of Si lithiation reactions, SEI formation, and reversibility are therefore active areas of research. Solid-state 7 Li nuclear magnetic resonance (NMR) spectroscopy is useful for characterizing different lithium local environments within Si anodes. Here, we developed an operando NMR methodology to characterize aging of carbon-coated nanoparticulate Si anodes in pouch cells paired with Ni-rich cathodes. We observed a new lithiation mechanism in the Si nanoparticles: direct formation of over-lithiated Li 15+x Si 4 (x<0.6) phase. Furthermore, our novel operando cells maintained good performance with long-term cycle and calendar aging. Here we identified trapped lithium silicides as a major contributor to capacity fade with aging. Finally, we determined that the addition of Mg (TFSI) 2 to the electrolyte decreased the amount of trapped lithium silicides and therefore increased the capacity and capacity retention for the nanoparticulate Si used.

25 ENERGY STORAGE↗

Mechanisms of stored energy release in silicon carbide materials neutron-irradiated at elevated temperatures

Understanding the stored energy release behavior of SiC is crucial for the design of SiC-based fuel cladding for light water reactors because stored energy release affects response during accident conditions. Differential scanning calorimetry was used to evaluate the stored energy of monolithic SiC and SiC fiber–reinforced SiC matrix composite variants following neutron irradiation under light water reactor–relevant dose and temperature conditions. The tests were performed at heating rates of 0.5, 3, and 20 K/min up to 1,273 K. The onset temperature of the energy release roughly corresponded to the irradiation temperature, and energy release was delayed as the heating rate increased. The monolithic and composite specimens exhibited similar stored energy release behavior up to ~1,000 K, and above that temperature, the energy release depended more on material type. The energy release measured in this study is below the material-specific heat capacity at temperatures below ~1,000 K but exceeds it under certain material and annealing conditions at temperatures above ~1,000 K. The amount of irradiation-induced volumetric swelling of the specimens was an indication of the total stored energy. Based on this observation, the energy release behavior was described by a swelling recovery model.

36 MATERIALS SCIENCE↗

Single electron–hole pair sensitive silicon detector with surface event discrimination

Here, we demonstrate single electron-hole pair resolution in a single-sided, contact-free 1 cm$^2$ by 1 mm thick Si crystal operated at 48 mK, with a baseline energy resolution of 3 eV. This crystal can be operated at voltages in excess of $\pm50$ V, resulting in a measured charge resolution of 0.06 electron-hole pairs. The high aluminum coverage ($\sim$70%) of this device allows for the discrimination of surface events and separation of events occurring near the center of the detector from those near the edge. We use this discrimination ability to show that dark events seen in previous detectors of a similar design are likely dominated by charge leakage along the side wall of the device. We saw only a small reduction in dark event rate with this biasing scheme, further suggesting that sidewall and edge-dominated processes are responsible for the majority of these events.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Test and extraction methods for the QC parameters of silicon strip sensors for ATLAS upgrade tracker

The Quality Control (QC) of pre-production strip sensors for the Inner Tracker (ITk) of the ATLAS Inner Detector upgrade has finished, and the collaboration has embarked on the QC test programme for production sensors. This programme will last more than 3 years and comprises the evaluation of approximately 22000 sensors. 8 Types of sensors, 2 barrel and 6 endcap, will be measured at many different collaborating institutes. The sustained throughput requirement of the combined QC processes is around 500 sensors per month in total. Measurement protocols have been established and acceptance criteria have been defined in accordance with the terms agreed with the supplier. For effective monitoring of test results, common data file formats have been agreed upon across the collaboration. To enable evaluation of test results produced by many different test setups at the various collaboration institutes, common algorithms have been developed to collate, evaluate, plot and upload measurement data. This allows for objective application of pass/fail criteria and compilation of corresponding yield data. These scripts have been used to process the data of more than 3000 sensors so far, and have been instrumental for identification of faulty sensors and monitoring of QC testing progress.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Characterization of front contact degradation in monocrystalline and multicrystalline silicon photovoltaic modules following damp heat exposure

Reliability and durability tests play a key role in the photovoltaic (PV) industry by minimizing potential failure risks for both existing and new cell and module technologies. In this work, a detailed study of contact degradation in monocrystalline and multicrystalline PV modules is performed. The modules are subjected to a sequence of damp heat (DH) exposures followed by electrical characterization after each step. Electroluminescence (EL) imaging shows different darkening patterns for monocrystalline modules compared to multicrystalline modules; the former shows darkening near the busbars and the latter shows it across virtually the entire cell surface. The primary loss mechanism is confirmed to be resistive after comparing the current-voltage (I–V) characteristics at each DH exposure step. Representative samples have been cored out from both the degraded modules and controls for materials characterization to gain further insights into the degradation mechanism. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and top-down high-resolution X-ray photoelectron spectroscopy (XPS) analysis performed on the cored samples confirm the degradation is due to metallization corrosion. Our study suggests that the difference in the darkening pattern can most likely be attributed to the different silver paste composition used for contacting each cell technology, particularly the composition of the glass frit.

36 MATERIALS SCIENCE↗

Tin Metal Improves the Lithiation Kinetics of High-Capacity Silicon Anodes

Si-based anodes present a great promise for high energy density lithium-ion batteries. However, its commercialization is largely hindered by a grand challenge of a rapid capacity fade. Here, we demonstrate excellent cycling stability on a Si-Sn thin film electrode that outperforms pure Si or Sn counterpart under the similar conditions. Combined with the first-principles calculations, in situ transmission electron microscopy studies reveal a reduced volume expansion, increased conductivity, as well as dynamic rearrangement upon lithiation of the Si-Sn film. Here we attribute the improved lithiation kinetics to the formation of a conductive matrix that comprises a mosaic of nanostructured Sn, Li y Sn (specifically, Li 7 Sn 2 develops around the lithiation potential of Si), and Li x Si. This work provides an important advance in understanding the lithiation mechanism of Si-based anodes for next-generation lithium-ion batteries.

25 ENERGY STORAGE↗