Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SCANNING ELECTRON MICROSCOPY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 955 records · Page 53

Computational thermodynamics-guided alloy design and phase stability in CoCrFeMnNi-based medium-and high-entropy alloys: An experimental-theoretical study

A computational thermodynamics approach has been employed to design CoCrFeMnNi-based medium- and high-entropy alloys (M/HEAs) with systematically varied compositions (Co(( 80-X )/ 2 )Cr(( 80-X )/ 2 )Fe X Mn 10 Ni 10 with x = 30, 40, and 50 at.%) and phase stability. Since the formation of sigma phase, usually brittle and undesirable, is a common concern, when this class of alloys is subjected to elevated temperatures (600–1000 °C), predicting its formation becomes essential. Thus, its formation and the phase equilibria were studied using the CALPHAD method, and two empirical methods, namely, valence electron concentration (VEC) and paired sigma-forming element (PSFE). Isothermal aging treatments at 900–1100 °C for 20 h were performed, since CALPHAD and VEC/PSFE predictions diverged. Both prediction methods were compared with experimental characterization by a combination of scanning electron microscopy and high-energy synchrotron X-ray diffraction. In conclusion, the predictions from the VEC/PSFE and CALPHAD calculations (depending on the database used) were shown to be quite accurate.

36 MATERIALS SCIENCE↗

Facile alignment estimation in carbon nanotube films using image processing

Whether a macroscopic assembly of carbon nanotubes can exhibit the one-dimensional properties expected from individual nanotubes critically depends on how well the nanotubes are aligned inside the assembly. Therefore, a simple and accurate method for assessing the degree of alignment is desired for the rapid characterization of carbon nanotube films and fibers. Here, we present an end-to-end solution for determining the global and local spatial orientation of carbon nanotubes in films within a short amount of time using a fast, precise, and economical approach based on an image processing method applied to scanning electron microscopy images. Further, we first use Laplacian edge enhancement filtering for improving the appearance of edge regions, which is followed by image partitioning into multiple blocks to capture the nanoscale orientation characteristics and total variation-based image decomposition of these image blocks. We then perform a 2D-fast Fourier transform on the image decomposed textural components of these edge-enhanced image blocks to determine the orientation distribution, which is utilized to estimate the 2D nematic order parameter. To show the effectiveness of our method, we corroborated our results against results obtained with other state-of-the-art image processing and experimental techniques.

2D-FFT↗

Effect of temperature on abrasion erosion in particle based concentrating solar powerplants

The use of solid particles as a heat transfer medium is being explored for concentrated solar power plants (CSP) to increase their efficiency by achieving operating temperature >700 °C. During operation, these hot particles are expected to move along the various components within the collector system, resulting in material degradation from a combination of high-temperature oxidation and erosion. In the present study, the performance of candidate materials was evaluated through a series of abrasion erosion experiments at room temperature as well as at 800 °C. Wear in metallic and refractory type materials was investigated using CarboBead® HSP 40/70 particles inside a resistance heated kiln. Furthermore, cross-sectional scanning electron microscopy (SEM) and energy dispersive x-ray spectroscopy (EDS) analysis on the specimens tested at 800 °C determined that the specific wear rate in Inconel 740H and stainless steel 316 metallic specimens was influenced by the thermally grown oxide morphology. High chromium Inconel 740H specimens exhibited greater resistance to wear with a steady state specific wear rate of 1.92E-4 mm 3 N -1 m –1 compared to 5.7E-3 mm 3 N -1 m –1 for Stainless Steel 316.

14 SOLAR ENERGY↗

Synthesis and characterization of Pt(Cu 0.67 Sn 0.33 )

Pt(Cu 0.67 Sn 0.33 ) has recently been found in a natural sample. In order to be able to characterize this new ternary compound, we synthesized it from the elements. Samples were characterized by X-ray powder diffraction, differential scanning calorimetry, thermal relaxation calorimetry, and scanning electron microscopy studies. Density functional theory-based model calculations complemented the experimental studies. Pt(Cu 0.67 Sn 0.33 )was already formed at a relatively low temperature of 773 K. Rietveld refinement of Pt(Cu 0.67 Sn 0.33 ) has been carried out in CuAu-type or L1 0 -type structure, space group P4/mmm, with Pt on 0,0,0 and disordered Cu and Sn on 1/2, 1/2, 1/2 and Z = 1. The lattice parameters are a = 2.823(1) Å, c = 3.64(1) Å, and V = 29.00(4) Å which are in good agreement with values obtained earlier on the natural sample and with the results of DFT calculations. The vibrational entropy for Pt(Cu 0.67 Sn 0.33 ) is $S_{298.15}^{vib}$ = 79.9(7) J mol -1 K -1 . The pressure dependence up to 36(2) GPa of the unit-cell volume and the lattice parameters and unit-cell volume have been obtained by synchrotron based powder diffraction using a diamond anvil cell. A fit of a 3rd-order Birch–Murnaghan equation of state to the Pt(Cu 0.67 Sn 0.33 )) (p,V)-data results in a bulk modulus of B 0 = 215(27) GPa and B' = 5(2).

36 MATERIALS SCIENCE↗

Semi-transparent p-type barium copper sulfide as a back contact interface layer for cadmium telluride solar cells

Optically transparent p-type materials play a critical role in transparent electronics including photovoltaic (PV) devices. P-type sulfide materials offer an alternative to oxides for PV application due to improved hole transport properties. Here, we report the solution-based synthesis of earth-abundant p-type transparent conducting barium copper sulfide (α-BaCu 4 S 3 , BCS) thin films. These films were characterized using scanning electron microscopy, X-ray diffraction, UV–Vis–NIR spectrophotometry, Raman spectroscopy, and spectroscopic ellipsometry. BCS films of ~100 nm thickness transmit >70% of visible light. We report on tests of the hole transport properties of these BCS films for cadmium telluride (CdTe) photovoltaics, finding that the BCS deposition process forms a beneficial tellurium (Te) rich surface on CdTe by selectively removing Cd from the surface. Based on our study, the BCS interface layer plays dual functions for CdTe PV devices as a hole transport material and as an etchant, enhancing the resulting device performance. We observed a significant increase in open-circuit voltage of CdTe solar cells with the BCS buffer layer. Furthermore, we discuss semitransparent CdTe solar cells with BCS as a hole transport layer and indium tin oxide as a finishing electrode. Semitransparent CdTe solar cells shows 13.3% conversion efficiency for the front side illumination and 1.2% efficiency for back side illumination, indicating high recombination of charge carriers generated close to the rear CdTe/BCS/ITO contact.

36 MATERIALS SCIENCE↗

Corrosion of novel reactive silver ink and commercial silver-based metallizations in diluted acetic acid

Silver-based metallizations in photovoltaic modules are susceptible to corrosion by acetic acid generated in ethylene vinyl acetate encapsulated modules, resulting in power losses over time. Here, three silver-based metallizations are exposed to diluted acetic acid, in concentrations representative of that found in field-exposed modules. Compositional, morphological, and structural changes of the metallizations are studied over 3000 h of exposure to diluted acetic acid using Raman spectroscopy mapping, X-ray diffraction, and scanning electron microscopy. The three metallizations studied are: 1) a commercial high-temperature fire-through Ag paste, commonly used for Si diffused junction solar cells; 2) a commercial low-temperature paste normally used for silicon heterojunction cells; and 3) a novel low-temperature reactive silver ink shown to be suitable for photovoltaic applications. We find distinct corrosion rates for the high-temperature silver paste and reactive silver ink in the presence of diluted acetic acid. However, the low-temperature silver paste appears to be more corrosion resistant, likely due to a polymer layer that protects the silver particles.

36 MATERIALS SCIENCE↗

Characterization of front contact degradation in monocrystalline and multicrystalline silicon photovoltaic modules following damp heat exposure

Reliability and durability tests play a key role in the photovoltaic (PV) industry by minimizing potential failure risks for both existing and new cell and module technologies. In this work, a detailed study of contact degradation in monocrystalline and multicrystalline PV modules is performed. The modules are subjected to a sequence of damp heat (DH) exposures followed by electrical characterization after each step. Electroluminescence (EL) imaging shows different darkening patterns for monocrystalline modules compared to multicrystalline modules; the former shows darkening near the busbars and the latter shows it across virtually the entire cell surface. The primary loss mechanism is confirmed to be resistive after comparing the current-voltage (I–V) characteristics at each DH exposure step. Representative samples have been cored out from both the degraded modules and controls for materials characterization to gain further insights into the degradation mechanism. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and top-down high-resolution X-ray photoelectron spectroscopy (XPS) analysis performed on the cored samples confirm the degradation is due to metallization corrosion. Our study suggests that the difference in the darkening pattern can most likely be attributed to the different silver paste composition used for contacting each cell technology, particularly the composition of the glass frit.

36 MATERIALS SCIENCE↗

Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies

Degradation due to acetic acid in photovoltaic (PV) modules has been a commonly observed phenomenon for both damp-heat exposure and outdoor operations. Acetic acid is a degradation byproduct of ethylene-vinyl acetate (EVA), a common module encapsulant. To address this issue, robust metallization pastes and cell technologies are being developed. However, it is important to assess how these technologies perform in an acetic acid environment and withstand degradation before they are implemented in the solar market. In this work, we investigate the impact of acetic acid exposure on four different cell groups: monofacial passivated emitter and rear contact (PERC) cells with advanced telluride-based front contact pastes, bifacial PERC cells with novel aluminum rear contact pastes, bifacial tunnel oxide passivated contacts (TOPCon) cells, and silicon heterojunction (SHJ) cells. These cells were exposed to acetic acid for different time increments. The recombination losses were characterized by Suns-VOC, and multi-variate regression analysis of intensity-dependent photoluminescence (PL) images with Griddler AI. Resistive losses were tracked with the transmission line method (TLM). Samples showing severe performance degradation were selected for further materials characterization to understand the root cause. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and X-ray photoelectron spectroscopy (XPS) were performed to investigate the change in materials properties. Our study shows that the front contacts of the bifacial TOPCon cells and monofacial PERC cells were significantly affected by acetic acid exposure. Here, the SHJ cells were found to be the most stable.

14 SOLAR ENERGY↗

Innovative recycling of high purity silver from silicon solar cells by acid leaching and ultrasonication

Precious and scarce silver (Ag) is used as a front electrical contact in silicon solar panels. With massive amounts of solar panel waste coming to end-of-life, it is imperative to recover all the Ag from these modules. In this paper, we propose a novel method to easily reclaim Ag from end-of-life silicon solar cells using low concentration sulfuric acid (H 2 SO 4 ) leaching followed by ultrasonication. Our process simplifies the Ag recycling procedure by directly recovering the Ag contacts from solar cells, eliminating the need for secondary precipitation/electrodeposition. First, scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDX) and X-ray photoelectron spectroscopy (XPS) was used to study the leaching and ultrasonication process on rejected solar wafers. Next, a solar panel from landfill was heated in a furnace to burn off the polymer encapsulant. The silicon wafers were then collected from the burning process and leached in 2 M H 2 SO 4 at two different shaking speeds for 48 hours at room temperature. Finally, the end-of-life silicon wafer pieces were collected, sonicated in water, and then the sonication water was centrifuged to show a proof-of-concept to recover the Ag contacts. Inductively coupled plasma optical emission spectroscopy (ICPOES) is used to monitor dissolved elements in the leachate as a function of time and shaking speed. XPS is used to evaluate the composition of the silicon cell wafer surface before and after H 2 SO 4 leaching. SEM is used to image the recovered Ag contacts morphology and EDX confirms the recovered particles contain high amounts of Ag. Furthermore, a proposed schematic illustrates the authors’ hypothesis for the peeling mechanism.

14 SOLAR ENERGY↗

High temperature fracture toughness of single-layer CrAlN and CrAlSiN hard coatings

Hardness and toughness are among of the most important physical properties of hard coatings and it is important to analyze them at temperatures present during coating applications. CrAlN and CrAlSiN are hard coating materials frequently used in high temperature applications. Here, while both possess high oxidation resistance and thermal stability, they differ in their microstructure. In this work, the fracture toughness of magnetron-sputtered single-layer CrAlN and CrAlSiN hard coatings was determined up to 700 °C by in-situ scanning electron microscopy micro-cantilever deflection tests. The results show a decreasing trend of the fracture toughness with increasing temperature. While both coatings' fracture toughness trends are similar up to 400 °C, they diverge at higher temperatures. In general, the evolution of the fracture toughness with increasing temperature shows similarities to the observed changes in hardness in the same temperature range.

36 MATERIALS SCIENCE↗

Unveiling damage mechanisms of chromium-coated zirconium-based fuel claddings at LWR operating temperature by in-situ digital image correlation

Here, we investigate the coupled thermomechanical fracture mechanisms of coated nuclear fuel claddings at Light Water Reactor (LWR) operating temperatures. These coated claddings are a highly attractive, near-term solution, which addresses the demands for accident-tolerant fuel systems and provide greater oxidation resistance. However, the fracture mechanisms of these coatings, which may create channels for oxidation ingression, must be fully understood prior to implementation. Thus, high-temperature expanding plug experiments were conducted on coated cladding specimens at a temperature of 315 °C, consistent with the operating environment of LWRs. Furthermore, in-situ thermomechanical deformation was measured with stereo digital image correlation during heating and mechanical testing to separately resolve contributions of thermal and mechanical strain. Digital image correlation, supported by acoustic emissions (AE) detection, was also leveraged to track cracking activity during loading. Coating fracture was found to initiate at total hoop strains of 0.34%. The thermal deformation of the coated claddings was investigated via finite element simulations, revealing a bidirectional stress-state within the coating with axial and circumferential strains of 0.026 and 0.031%. This bidirectional stress-state was attributed with the generation of off-axis fracture pattern within the coating as identified via post-experiment scanning electron microscopy. Thus, this study unveiled critical, coupled thermomechanical mechanisms governing the coating fracture of coated claddings at LWR temperatures.

36 MATERIALS SCIENCE↗

Effect of CMAS viscosity on the infiltration depth in thermal barrier coatings of different microstructures

Calcium magnesium aluminum silicate (CMAS) is one of the leading concerns for the gas turbine industry. The effects of CMAS viscosity and the coating microstructure on CMAS infiltration depth were explored by conducting a time dependent interaction study. Three CMAS compositions were used from literature, and their viscosities predicted through FactSage viscosity module were drastically different. The interaction was carried out on three different TBCs synthesized using the solution precursor plasma spray process (SPPS): two of the TBCs were made of yttrium aluminum garnet (YAG) having different microstructures that promote different modes of CMAS infiltration, and one TBC was made of gadolinium zirconate (GZO). All samples had stress relieving vertical cracks and different intensities of horizontally banded porosity, (inter pass boundaries IPBs). A concentration of 100 mg/cm 2 of CMAS was applied on the TBCs which were then subjected to a 5-minute interaction at 1300 °C. Samples were analyzed using scanning electron microscopy (SEM), electron dispersive X-ray spectroscopy (EDXS), and transmission electron microscopy (TEM). Low viscosity CMAS readily penetrated the TBCs while more viscous CMAS showed less penetration. The depth of CMAS infiltration depended on the coating microstructure. In the YAG with IPBs, the CMAS spread horizontally in the IPBs before infiltrating deeper, resulting in reduced infiltration depth compared to other samples in spite of having wider vertical cracks. TEM and EDXS analysis were performed to investigate the phases present in the CMAS-TBC interaction region in YAG. Two regions were chosen, the top TBC surface in direct contact with the sea of CMAS, and the region at the CMAS penetration ended within the coating. Finally, the results showed that no secondary phases like apatite were observed in YAG, thus it can be concluded that the arrest of CMAS happened solely because of CMAS viscosity and the short infiltration time.

36 MATERIALS SCIENCE↗

Corrosion protection of mild steel by superhydrophobic magnetite coating

Corrosion-resistant hydrophobic magnetite coatings on mild steel surfaces were developed by immersion method. The effect of steel surface roughness (R a ) on its hydrophobicity was systematically studied using contact angle measurement (CAM), scanning electron microscopy (SEM), and atomic force microscopy (AFM). The corrosion resistance of hydrophobic magnetite coatings was evaluated using a potentiodynamic polarization test. The durability of the coatings was assessed in air, tap water, and 3.5 wt% NaCl environments. Hydrophobic magnetite coating with a water contact angle of 146-152° showed excellent resistance to corrosion, longevity in atmospheric air, and significant self-cleaning properties. The primary focus of this study was to develop a quick and simple immersion technique to create hydrophobic surfaces on mild steel. Finally, results suggest that surface roughness plays a significant role in surface hydrophobicity, and enhancing the hydrophobicity of mild steel improves its corrosion resistance.

36 MATERIALS SCIENCE↗

Investigation of the temperature-dependent failure processes in PVD Cr-coated ZIRLO nuclear fuel cladding using in situ X-ray micro-tomography imaging

In this work, an accident tolerant fuel cladding system with Cr coating deposited using physical vapour deposition (PVD) method onto commercial Optimized ZIRLO™ was studied. The cladding tubes were machined into C-rings and loaded to failure under compression with real-time synchrotron micro-X-ray computed tomography (XCT) imaging at room temperature (RT), 345 °C, 650 °C and 950 °C in argon (Ar) atmosphere. The mechanical behaviour and failure processes were found strongly temperature-dependent where the Cr coating showed brittle fracture at RT and 345 °C, ductile fracture at 650 °C and a reversion to brittle fracture at 950 °C. Nanoindentation measurements and scanning electron microscopy (SEM) imaging were conducted on the materials after high temperature testing. It was found that recrystallisation of the Cr coating occurred at elevated temperatures, which significantly affected its local properties hence the failure behaviour at different temperatures. This work represents the first in situ 3D XCT observation of progressive failure processes in PVD Cr-coated ZIRLO claddings up to 950 °C providing critical insights into its brittle-to-ductile transition (BDTT) behaviour and subsequent ductile-to-brittle reversion with the increase in temperature. Moreover, results are compared with other PVD Cr-coated Zircaloy materials from open literature; the influences of the coating microstructure and local properties on the failure stress/strain and fracture processes are discussed.

Yuan, Guanjie↗

Silicon Dioxide Deposited Using Atmospheric Pressure Plasma Chemical Vapor Deposition for Improved Adhesion and Water Intrusion Resistance for Lightweight Manufacturing

This work aims to demonstrate the barrier coating, and adhesion promoting properties of silica-based coatings deposited using an atmospheric pressure plasma torch (APPT). This is achieved by applying an industrial grade adhesive to silica thin films deposited, on the surfaces to be joined, using atmospheric pressure plasma chemical vapor deposition (APP-CVD), to make single joint lap shear samples of different metal combinations commonly found in lightweight manufacturing such as aluminum and magnesium as well as steel. To deposit these thin films, two separate silicon based organic precursors, hexamethyldisiloxane (HMDSO), and tetraehylorthosilicate (TEOS), are used. Here, samples are bonded using DuPont Betamate 1486 adhesive, and the lap shear results for these films are compared to the lap shear results of a chemically cleaned control using the same adhesive. The APPT uses a microwave power supply and gas mixtures of N 2 and Ar. The adhesion of the films are tested using lap shear, and elevated temperature water soaks are conducted on the joints as well to simulate environmental exposure. Lap shear results from samples with silica thin films max shear stress are 25%-115% increase compared to control samples depending on material. After exposure to water soak the max shear strength of the joints decreased by less than 15%, which demonstrates the films capabilities as a water barrier. Film morphology is examined using Scanning Electron Microscopy (SEM), and the film’s composition and approximate thickness are obtained using Rutherford Backscattering Spectroscopy (RBS).

36 MATERIALS SCIENCE↗

Fractal analysis on Ag 2 O thin film using a data-driven approach

The synthesis of fractal Ag oxide (Ag 2 O) on the surface of Ag thin film has been achieved at room temperature by using Synchrotron X-ray irradiation. We have performed an automated quantitative analysis of a batch of 1879 fractal Ag 2 O patterns in a scanning electron microscopy (SEM) image within a radius of 2000 mm outward from the center of the X-ray beam. The morphology is similar to that of the diffusion-limited cluster aggregation (DLCA) model. The fractal dimension (D) of Ag 2 O is between 1.7 and 1.5 from the center to the edge. The area distribution density of fractal Ag 2 O follows a quadratic function with radius R. It is found that the branches’ number of fractal Ag 2 O is a key factor affecting the fractal dimension. The more branches the fractal has, the greater the D is. This is the first time that Ag fractal has been investigated by combining automated data analysis methods with batch experimental data. This data-driven approach provides a new research perspective for rationally regulating materials’ fractal morphology and performance.

36 MATERIALS SCIENCE↗

Effect of substrate temperature on the growth of Nb 3 Sn film on Nb by multilayer sputtering

Here, we report on the fabrication of niobium tin (Nb 3 Sn) films by multilayer sequential sputtering on niobium at substrate temperatures ranging from room temperature to 250 °C. The multilayers were then annealed inside a separate vacuum furnace at 950 °C for 3 h. The material properties of the films were characterized by X-ray diffraction, scanning electron microscopy, energy-dispersive X-ray spectroscopy, atomic force microscopy, and transmission electron microscopy. The superconducting properties of the films were studied by four-point probe resistivity measurements from room temperature to below the superconducting critical temperature T c . The highest film T c was 17.76 K, obtained when the multilayers were deposited at room temperature. When the deposition temperature was raised to 250 °C, a significant reduction in voids was achieved while the film's T c was 17.58 K.

36 MATERIALS SCIENCE↗