Inhibit the strain accumulation for 5V spinel cathode by mitigating the phase separation during high voltage stage
LiNi 0.5 Mn 1.5 O 4 (LNMO) spinel cathode is a potential cathode material for high-power, low-cost lithium-ion batteries (LIBs) due to its low raw material cost, high operating voltage and efficient lithium-ion transport channel. However, LNMO suffers from structural stability due to the two-phase-transformation during charge/discharge process, leading to poor cycling performance. Here, to address the issues, we have constructed a homogeneous aggregated LNMO cathode with a multifaceted primary particle, namely the LNMO with single-crystal secondary particles (SSP LNMO). Ex situ and in situ characterizations including the synchrotron X-ray diffraction, the neutron diffraction and full pouch cell validated that the SSP LNMO exhibit a single solid-solution reactions with a restrained lattice evolution during the delithiation/lithiation process. This is in contrast to the normal LNMO cathode, which demonstrates a significant two-phase transition from spinel Li 1-x Ni 0.5 Mn 1.5 O 4 to rock-salt MnO 2 at high voltage. Therefore, the SSP LNMO has greatly improved cycle life compared to the normal LNMO cathode. Overall, this study demonstrates the possibility of constructing LNMO based on primary-grain morphology modulation to improve the intrinsic stability of LIBs.