Optical Characterization of Defects in High-Efficiency (Ag,Cu)(In,Ga)Se2

We applied time-resolved photoluminescence (TRPL) spectroscopy to study optimized chalcopyrite (Ag,Cu)(In,Ga)Se2 thin films. The device shows power conversion efficiency of 18.7%. The metastable defect VSe-VCu within ACIGS at EV+0.98 eV is detected in sub-bandgap TRPL excitation spectra. TRPL lifetime of 50 ns is limited by the density of mid-gap defects such as CuGa or CuIn. The similarity of TRPL dynamics before and after light soaking indicates the optimized ACIGS thin film is less metastable because the density of VCu-VSe defect is reduced to below 10^15 cm^-3. This study indicates that ACIGS has improved cell efficiency and reliability characteristics.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Pinhole Formation in Poly-Si/SiOx Passivating Contacts on Si(111)-Oriented Textures

Poly-Si/SiOx passivating contacts were grown on inverted pyramid and random pyramid textured wafers to investigate the hypothesis that pinhole formation is most susceptible at the valleys and edges of a textured surface. Tetramethylammonium hydroxide (TMAH) etching and electron beam induced current (EBIC) were used to assess pinhole formation and charge-carrier transport. Scanning electron microscopy revealed that TMAH etching can expose pinhole locations on textured surfaces. We show that pinholes may preferentially form at the vertices of inverted pyramids. Our TMAH and EBIC analyses on random pyramids show no preferential oxide breakup at the pyramid valleys.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Voltage-Matched Strings using 3-Terminal Tandems: Fundamentals and End Losses

Strings constructed from 3-terminal tandem (3TT) cells can provide some of the performance benefits of voltage-matching with less cell complexity than strings based on 4-terminal tandem cells. However, the circuitry for a 3TT string can become more complex, making circuit analysis more challenging. Here we illustrate the essential features of single-polarity voltage-matched (VM) 3TT strings using representative examples. End losses are intrinsic to this type of string, but can be reduced by minimizing m and n in the Vtop/Vbot VM ratio m/n, and further mitigated by increasing the string length. This analysis agrees with preliminary experimental results.

3TT↗

Ultraviolet Fluorescence Bleaching Rates for New Cell Cracks

Ultraviolet Fluorescence (UVF) is an inspection tool that can be used to identify cell cracks in some photovoltaic (PV) modules. Cell cracks can also be identified with electroluminescence (EL) and similar techniques, but it is generally not possible to differentiate new cracks from old ones with EL. UVF has a unique property of taking time for the cracks to show up, which could be used to differentiate new cracks (e.g., from a recent storm) from old ones (e.g., from installation damage). We perform tests on several different modules, some the same make and model but with different bill of materials (BOMs), to characterize the amount of time that it takes for crack signatures to progress in UVF.

41 EE - Solar Energy Technologies Office (EE-4S)↗

PV Fleet Performance Data Initiative Program and Methodology

The US Department of Energy’s PV Fleet Performance Data Initiative has been launched in order to collect and evaluate production data across multiple PV fleet partners. Performance statistics are anonymized, aggregated and shared to represent a snapshot of the US commercial and utility-scale fleet. Production data have been collected from over 1500 systems representing more than 1.3 GWdc capacity. Preliminary analysis indicates median performance loss rates are in line with previous publications of system degradation, on the order of –0.6%/yr to –0.9%/yr (preliminary numbers subject to change). These values are higher than module-only degradation rates which are often used in pro-forma estimates of project performance and economics, potentially exposing owner/operators to increased risk if systems under-perform over time.

41 EE - Solar Energy Technologies Office (EE-4S)↗

GaAs Solar Cells Grown on Intentionally-Contaminated GaAs Substrates

III-V solar cells have the best performance of any semiconductor materials, but deposition of these materials relies on high-quality single crystal GaAs wafers for their superior performance. Unfortunately, the cost of these wafers makes these high-efficiency devices only accessible in high-value or niche markets. Here, we explored the effect of growing bulk GaAs crystals with lower purity input materials in order to reduce their cost. We observe that intentional impurities added to the melt before the crystal growth occurs segregate to the top of the boule. Single junction GaAs solar cells grown on wafers made from contaminated boules showed no performance degradation compared to a high-purity control wafer. These results suggest that lower purity Ga and As source materials can be used during crystal growth to reduce the cost of wafers.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Overcoming Communications Outages in Inverter Downtime Analysis

This paper presents two methods of detecting inverter downtime and estimating lost production from downtime events using timeseries system production measurements. The methods focus on distinguishing communications interruptions from true production outages and are successful in most cases. To enable fleet-scale analysis of inverter availability, the methods are designed to be semi-autonomous. The first method uses only inverter and system meter AC power measurements while the second uses cumulative production and expected energy data to classify outages and estimate lost production. The methods are demonstrated using real field data and the results are discussed.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Evaluating Non-Fluoropolymer-Based Co-Extruded Backsheets Using Combined-Accelerated Stress Testing and Materials Forensics

Co-extruded, non-fluoropolymer backsheet films for photovoltaic (PV) modules have gained popularity in recent years based on their cost competitiveness. However, their viability has been thrown into question as a result of widespread, early-life field-failures of some materials, particularly the polyamide (PA)-based “AAA” backsheet product. Failure to detect weaknesses in those earlier products could be due, in part, to insufficient quality testing practices. New testing protocols have recently been developed to better evaluate such materials. Here we show the testing results for a non-fluoropolymer, co-extruded PA-based backsheet film, which demonstrates greater durability than AAA and some commercial fluoropolymers. Using material characterization techniques including Fourier-transform infrared spectroscopy (FTIR), wide-angle x-ray scattering (WAXS), differential scanning calorimetry (DSC), X-ray photoelectron spectroscopy (XPS), elongation-to-break (ETB), and optical microscopy we perform a comprehensive failure analysis to better understand the materials weaknesses. This analysis can ultimately inform how best to improve the material and extend its lifetime. This work serves as a demonstration that some materials should not be discounted due to a single poorly designed product and that more appropriate qualification testing with subsequent materials analysis can be used to develop better materials.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Modeling Spectrally-Selective Reflection for Thermal Management in Monofacial and Bifacial Modules

Parasitic absorption in photovoltaic modules is a major source of waste heat, which drives operating temperatures 20-30K above ambient. Spectrally-selective sub-bandgap reflection can reduce parasitic absorption, thereby improving module efficiency and power output. Here, we investigate the performance of 1-D spectrally-selective mirrors in monofacial Al BSF and PERC modules, and bifacial PERC modules. In monofacial modules, these mirrors offer >1.2% increase in energy yield compared to single-layer anti-reflection coatings, while cooling by over 1K on average. Mirrors reduced bifacial module parasitic absorption by up to 34 W/m2 out of 1240 W/m2 incident.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Optimization of Source Material for in-situ Arsenic Doping via Vapor Transport Deposition of CdTe Films

In-situ doping of CdTe/CdSeTe films with arsenic is performed using pre-doped source material prepared by high pressure Bridgman (HPB) melt growth. Arsenic level in the source material is varied from 1018-1020 cm-3. Correspondingly, dopant incorporation in the films prepared using vapor transport deposition (VTD) varied from 3x1017 cm-3–1x1018cm-3. In this range, dopant activation is found to inversely correlate with the dopant incorporation, suggesting compensation. The results from this study indicate film properties can be adjusted by source material.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Estimating Subhourly Inverter Clipping Loss From Satellite-Derived Irradiance Data

Photovoltaic system production simulations are conventionally run using hourly weather datasets. Hourly simulations are sufficiently accurate to predict the majority of long-term system behavior but cannot resolve high-frequency effects like inverter clipping caused by short-duration irradiance variability. Direct modeling of this subhourly clipping error is only possible for the few locations with high-resolution irradiance datasets. This paper describes a method of predicting the magnitude of this error using a machine learning regressor ensemble model, comprised of a random forest and an XGBoost model, and 30-minute satellite irradiance data. The method predicts a correction for each 30-minute interval with the potential to roll up into 60-minute corrections to match an hourly energy model. The model is trained and validated at locations where the error can be directly simulated from 1-minute ground data. The validation shows low bias at most ground station locations. The model is also applied to gridded satellite irradiance to produce a heatmap of the estimated clipping error across the United States. Finally, the relative importance of each predictor satellite variable is retrieved from the model and discussed.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Effect of Dopant Compensation on the Conductivity of the Intrinsic poly-Si Isolation Region in Passivated IBC Silicon Solar Cells

The performance of IBC solar cells depends on the ability of this region to electrically isolate the doped fingers so that shunting does not occur and reduce the cell fill factor. We report on simulations which model the region between the p- and n-type poly-Si fingers of interdigitated back contact (IBC) solar cells as a series of resistors extending from one doped finger to the other. We demonstrate that the existence of a well compensated region between the doped fingers is enough to prevent shunting and loss of cell performance, despite contamination of dopants from the opposing dopant fingers. We show through these simulations that a net doping concentration below ~1018 cm-3 will enable a high resistivity and identify the conditions under which this highly resistive region forms despite imperfect finger edges. Additionally, we apply this analysis to tails measured by time-of-flight secondary ion mass spectrometry and confirm this hypothesis for our experimentally measured tails.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Demonstration of Passivation Using a Low-Temperature-Grown, Al-Containing Window Layer by HVPE

We present hydride vapor phase epitaxy (HVPE) growth of single junction GaAs solar cells with Al0.4Ga0.6As front passivation layers at a growth temperature of 650°C. Devices achieved a short circuit current density of ~27.52 mA/cm2 after anti-reflection coating, similar to devices that used GaInP windows with the same bandgap, indicating that AlGaAs provides front-surface passivation resulting in a low interface recombination velocity. The low temperature growth of Al containing III-V materials by HVPE allows for compatibility with In-containing alloys in high-efficiency III-V device structures for various applications.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Submicron Thickness Characterization of Poly-Si Thin Films on Textured Surfaces by X-Ray Diffraction for Minimizing Parasitic Absorption in Poly-Si/SiO2 Passivating Contact Cells

Poly-Si/SiO2 passivating contacts have shown great potential for industry-relevant next-generation solar cells. Previous work has demonstrated an improved Jsc from dry reactive ion etching in an SF6 environment, using front metal grids as a self-aligned mask. Here, we show an effective method to measure the front poly-Si thickness on an alkaline textured surface using X-ray diffraction. The calculated thicknesses are compared with cross-section SEM analysis and Quokka simulation. We show that by thinning the front poly-Si from 200 nm to 60 nm, Jsc increases by 2.4 mA/cm2, leading to an absolute efficiency gain of 1.73%. Finally, we discuss possible reasons for the premature loss of passivation before the removal of all poly-Si.

41 EE - Solar Energy Technologies Office (EE-4S)↗

High Efficiency Evaporated CdSeTe/CdTe Solar Cells With and Without MgZnO Buffer Layer

High efficiencies of ~19% CdTe solar cell devices were made using a thermal evaporation technique to deposit absorber layers of CdSe and CdTe. The absorber films were very high quality for a device fabrication, and with demonstrated high efficiency, it is a viable option to employ thermal evaporation in research and manufacturing. We also investigated four different interfaces scenarios of with and without MZO and CdSe in the device near front interface. The results clearly indicate that Se plays a key role in improving device performance, but the MZO is not necessarily required unless experiment goals demanded. Removing the MZO layer from the device structure and being able to use thermal evaporator for CdTe deposition will help with cost reduction in manufacturing.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Using Spectral Measurements to Characterize Solar Reference Cells on a Two-Axis Tracker

A study is commencing relating the spectral responsivity of reference cells in the field to changing spectral distribution during the day. Initial results indicate that measurements of the incident spectral distribution can be used to match results of reference cell measurements on a two-axis tracker with a standard deviation of ±0.25% under clear-sky conditions. Initial results are provided. As more data are obtained covering a variety of field conditions and locations, the robustness of these results will be tested. The website https://midcdmz.nrel.gov/apps/sitehome.pl?site=PVRES contains the data generated by this project.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Clear Sky Irradiance Year-to-Year Variations and Trends

Solar radiation data for seven SURFRAD stations for the period 1996-2018 show an increase in irradiance under clear skies over the period, but the increase was not constant and shorter periods may have even experienced decreases in irradiance. A popular implementation of a clear sky model provided modeled irradiances for comparison with the SURFRAD data under conditions screened for clear skies. The use of the clear sky model, which did not consider year-to-year variances in atmospheric turbidity, was found problematic for resolving small changes in irradiance important for determining PV system degradation over three or five years, but less problematic for a period of ten years.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Employing Fracture Statistics to Track Cell Reliability Through Module Fabrication

In this work we demonstrate how fracture statistics may be employed to track cell reliability through module fabrication steps. We were able to detect how cell cutting equipment could reduce cell fracture strain by 25 % as well as increase its variability. A smaller reduction was found to result from the ribbon soldering operation, and all cells measured were weaker when strained in an orientation perpendicular to the gridlines. Cell fracture measurements were found to be consistent with the number of cracked cells experienced in full sized modules exposed to mechanical loading. A structural mechanics model was created to elucidate how the requisite fracture strain is developed in a cell encapsulated within a PV module and demonstrates that this strain decreases more than 50 % from its center to edge when placed within the inner loading span of four-point flexure. The associated implications on the apparent cell strength is examined with an effective volume treatment.