Enhanced Stability of Lithium Metal Anode by using a 3D Porous Nickel Substrate

Lithium (Li) metal is considered the “holy grail” anode for high energy density batteries, but its applications in rechargeable Li metal batteries are still hindered by the formation of Li dendrites and low Coulombic efficiency for Li plating/stripping. An effective strategy to stabilize Li metal is by embedding Li metal anode in a three-dimensional (3D) current collector. Here, a highly porous 3D Ni substrate is reported to effectively stabilize Li metal anode. Using galvanostatic intermittent titration technique combined with scanning electron microscopy, the underlying mechanism on the improved stability of Li metal anode is revealed. It is clearly demonstrated that the use of porous 3D Ni substrate can effectively suppress the formation of “dead” Li and forms a dense surface layer, whereas a porous “dead” Li layer is accumulated on the 2D Li metal which eventually leads to mass transport limitations. X-ray photoelectron spectroscopy results further revealed the compositional differences in the solid-electrolyte interphase layer formed on the Li metal embedded in porous 3D Ni substrate and the 2D copper substrate.

Yu, Lu↗

Electrode Edge Effects and the Failure Mechanism of Lithium-Metal Batteries

Lithium (Li) metal with very high specific capacity makes it one of the ideal anode for high energy batteries. However, Li dendrite growth and the formation of isolated (or “dead”) Li during repeated Li plating/stripping processes lead to its low Coulombic efficiency (CE). In this work, we discovered for the first time that part of Li CE loss can be attributed to the edge effect of the copper (Cu) substrate electrode in a conventional Li||Cu cell configuration. The “dead” Li formed on the edge of Cu substrate was systematically investigated through scanning electron microscopy, energy dispersive X-ray spectroscopy, and two-dimensional X-ray photoelectron spectroscopy. In order to minimize the Li loss at the edge of the Cu exposed to pressure-free space, modified Li||Cu cell configuration with a Cu electrode smaller than Li metal is preferred. It was clearly demonstrated that using an electrode configuration with minimal open space or “pressure-free space” across electrodes can reduce “dead” Li accumulated during cycling and increase Li CE. This phenomena was also verified in Li metal batteries (Li||LiNi1/3Mn1/3Co1/3O2) and should be considered in the design of practical Li metal batteries.

Lee, Hongkyung↗

Ion‐Conducting, Electron‐Blocking Layer for High‐Performance Solid Electrolytes

Lithium metal batteries bring greater promise for energy density, often relying on solid‐state electrolytes to meet critical benchmarks. However, Li dendrite formation is a prevailing problem that limits the cycle life and Coulombic efficiency of solid‐state Li metal batteries. For the first time, a thin (<100 nm) layer of electronically insulating, ionically conducting lithium phosphorus oxynitride (LiPON) is applied using atomic layer deposition between a Li anode and garnet Li 7 La 3 Zr 2 O 12 (LLZO). The performance of a conformal LiPON layer as an electron barrier in symmetric Li‐LLZO cells is observed through potential step chronoamperometry, galvanostatic cycling, electron microscopy, and various spectroscopic techniques. The LiPON‐coated LLZO achieves 100 times lower electronic conductance than LLZO alone. Cycling carried out at 0.1 mA cm −2 for 100 cycles demonstrates that suppression of electron pathways into the bulk solid electrolyte improves the cycle life of a lithium metal cell. These findings suggest an electronic conductivity effect in solid‐state electrolytes. A strategy is demonstrated to design thin‐film (LiPON)‐modulated bulk solid‐state electrolytes (LLZO) capable of maintaining high ionic conductivity and electrochemical stability while reducing the effective electronic conductivity, which results in significantly decreased dendrite formation, improved cycle life, and greater interfacial integrity between the electrolyte and a Li anode.

Hitz, Emily M.↗

Enhanced Tensile and Tear Toughness Properties of Thin-Wall Vacuum-Assisted High-Pressure Die-Cast Aural-5 Alloy by Friction Stir Processing

Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.

Friction stir processing, Aural-5, Strength, Tear ↗

Microstructural refinement in ultrasonically modified A356 aluminum castings

Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.

36 MATERIALS SCIENCE↗

Determination of Phase Composition of Cobalt Nanoparticles Using {sup 59}Co Internal Field Nuclear Magnetic Resonance

It is well known that cobalt exhibits polymorphism, i.e., the co-existence of both the hcp and fcc phases. In particular, the method of synthesis and other thermodynamic conditions is known to play a crucial role in determining the particular phase of cobalt. In this work, we have compared the phase composition of the cobalt nanoparticles synthesized using two different solvents (water) and ethanol (Co@C). XRD measurements confirm the existence of fcc phase in commercial cobalt nanoparticles (Co@A), co-existence of fcc and hcp phases in Co@B, while the existence of the hcp phase in Co@C. We have studied these cobalt nanoparticles using {sup 59}Co internal field nuclear magnetic resonance (IFNMR) for verification of phase composition. Our studies reveal that the Co@A has fcc as a major phase with minor quantity hcp phase. Co@B exhibits approximately equal amount of fcc and hcp phase while Co@C exhibits hcp as a major phase with minor fcc phase. Our SEM micrograph studies confirm that the cobalt particles have spherical shape in the fcc phase. The cobalt particles exhibit both spherical and dendrite morphology confirming the co-existence of fcc and hcp phases, while the sample with pure hcp phase exhibits the dendrite morphology. Our studies also throw light on understanding the effect of solvent in the phase formation of the cobalt nanoparticles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Automated Tracing of Horizontal Neuron Processes During Retinal Development

In the developing mammalian retina, horizontal neurons undergo a dramatic reorganization oftheir processes shortly after they migrate to their appropriate laminar position. This is an importantprocess because it is now understood that the apical processes are important for establishing theregular mosaic of horizontal cells in the retina and proper reorganization during lamination isrequired for synaptogenesis with photoreceptors and bipolar neurons. However, this process isdifficult to study because the analysis of horizontal neuron anatomy is labor intensive and time-consuming. In this paper, we present a computational method for automatically tracing the three-dimensional (3-D) dendritic structure of horizontal retinal neurons in two-photon laser scanningmicroscope (TPLSM) imagery. Our method is based on 3-D skeletonization and is thus able topreserve the complex structure of the dendritic arbor of these cells. We demonstrate theeffectiveness of our approach by comparing our tracing results against two sets of semi-automatedtraces over a set of 10 horizontal neurons ranging in age from P1 to P5. We observe an averageagreement level of 81% between our automated trace and the manual traces. This automatedmethod will serve as an important starting point for further refinement and optimization.

59 BASIC BIOLOGICAL SCIENCES↗

In Situ Synchrotron X-ray Study of Ultrasound Cavitation and Its Effect on Solidification Microstructures

Considerable progress has been made in studying the mechanism and effectiveness of using ultrasound waves to manipulate the solidification microstructures of metallic alloys. However, uncertainties remain in both the underlying physics of how microstructures evolve under ultrasonic waves, and the best technological approach to control the final microstructures and properties. We used the ultrafast synchrotron X-ray phase contrast imaging facility housed at the Advanced Photon Source, Argonne National Laboratory, US to study in situ the highly transient and dynamic interactions between the liquid metal and ultrasonic waves/bubbles. The dynamics of ultrasonic bubbles in liquid metal and their interactions with the solidifying phases in a transparent alloy were captured in situ. The experiments were complemented by the simulations of the acoustic pressure field, the pulsing of the bubbles, and the associated forces acting onto the solidifying dendrites. The study provides more quantitative understanding on how ultrasonic waves/bubbles influence the growth of dendritic grains and promote the grain multiplication effect for grain refinement.

36 MATERIALS SCIENCE↗

Effects of Undercooling and Cooling Rate on Peritectic Phase Crystallization Within Ni-Zr Alloy Melt

The liquid Ni-16.75 at. pct Zr peritectic alloy was substantially undercooled and containerlessly solidified by an electromagnetic levitator and a drop tube. The dependence of the peritectic solidification mode on undercooling was established based on the results of the solidified microstructures, crystal growth velocity, as well as X-ray diffraction patterns. Below a critical undercooling of 124 K, the primary Ni{sub 7}Zr{sub 2} phase preferentially nucleates and grows from the undercooled liquid, which is followed by a peritectic reaction of Ni{sub 7}Zr{sub 2}+L → Ni{sub 5}Zr. The corresponding microstructure is composed of the Ni{sub 7}Zr{sub 2} dendrites, peritectic Ni{sub 5}Zr phase, and inter-dendritic eutectic. Nevertheless, once the liquid undercooling exceeds the critical undercooling, the peritectic Ni{sub 5}Zr phase directly precipitates from this undercooled liquid. However, a negligible amount of residual Ni{sub 7}Zr{sub 2} phase still appears in the microstructure, indicating that nucleation and growth of the Ni{sub 7}Zr{sub 2} phase are not completely suppressed. The micromechanical property of the peritectic Ni{sub 5}Zr phase in terms of the Vickers microhardness is enhanced, which is ascribed to the transition of the peritectic solidification mode. To suppress the formation of the primary phase completely, this alloy was also containerlessly solidified in free fall experiments. Typical peritectic solidified microstructure forms in large droplets, while only the peritectic Ni{sub 5}Zr phase appears in smaller droplets, which gives an indication that the peritectic Ni{sub 5}Zr phase directly precipitates from the undercooled liquid by completely suppressing the growth of the primary Ni{sub 7}Zr{sub 2} phase and the peritectic reaction due to the combined effects of the large undercooling and high cooling rate.

36 MATERIALS SCIENCE↗

Influence of Electropulsing Treatment on the Initial Solidification of Molten Steel During Continuous Casting

An electropulsing-assisted mold simulator (EPMS) technique was developed to investigate the effect of pulsed electric current on the initial solidification behavior of molten steel during the process of continuous casting. The results indicated that the variation of mold hot surface temperatures in the meniscus area decreased from 375.8 K to 394 K for the case without electropulsing treatment (EPT) to 363.5 K to 377.3 K for the one with EPT. The mold surface heat fluxes fluctuated around the baseline of 0.83 and 2.42 MW/m{sup 2} in the cases with and without EPT, respectively, which indicated that a higher thermal resistance between the initial shell and copper mold was introduced by employing the EPT. The crystal fraction of slag films increased from 69.8 to 77.9 pct, whereas the grain size of mold flux film decreased, when compared the case of EPT treatment with the benchmark one, which suggested that the pulsed electric current promotes the movement of molten clusters and particles, leading to the enhancement of mold flux crystallization and the improvement of thermal resistance. Moreover, the solidification structure of steel along the direction of solidification (from the mold to melt) includes a fine chilled grain layer close to the mold, a columnar dendrite layer in the middle, and equiaxed grains next to the melt core, in which a compacted microstructure with smaller secondary dendrite arm spacing was observed in the case of the EPT. The results demonstrate that the EPT could refine the as-cast solidification microstructure.

36 MATERIALS SCIENCE↗

Surface Modification of High-Carbon Steel Using Fiber Laser and Its Thermal, Microstructural and Tribological Analysis

In this study, surface modification of high-carbon steel was carried out using 2 kW fiber laser and thermal, microstructural and tribological characterizations were performed. The process parameters selected for laser surface treatment were laser power (600-1500 W) and scan speed (3000-4500 mm/min). Infrared pyrometer was used to record the surface temperature during the process. The metallographic analysis was carried out using an optical microscope to find the depth and width of the laser-treated zone. Scanning electron microscopy and energy-dispersive spectroscopy were performed to reveal the microstructure and compositional changes taking place in the laser-treated zone. It was observed that the dendritic growth took place from the top surface toward the center of the laser-treated zone. The amount of dendritic growth can be related to the maximum surface temperature generated during the process. XRD analysis indicated the formation of some intermetallic compounds and phase shifts taking place in the laser-treated zone. Residual stress analysis was performed to analyze the amount of stress accumulation in the laser-treated zone. When the temperature cycle was analyzed, it was found that the melting of the steel resulted in the formation of a surface under compressive stress while the non-melt hardened zone developed a surface under tensile stress. The maximum Vickers microhardness value achieved was about 958.8 HV{sub 0.5} for 1500 W power and 3000 mm/min scan speed. Scratch test was performed on the laser-treated track, and it was found that the hardened zone showed better tribological properties with respect to the parent material. Finally, it was observed that the surface roughness value increased with higher heat input probably due to high rate of oxide formation as well as due to the presence of martensite in the laser-treated zone.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a Multiphase FeCrCuMnNi High-Entropy Alloy

A FeCrCuMnNi high-entropy alloy was produced using vacuum induction melting, starting from high-purity raw materials. The microstructure and mechanical properties of the as-cast FeCrCuMnNi alloy were studied, considering x-ray diffraction (XRD), scanning electron microscopy, and hardness and tensile tests. XRD results revealed the existence of two FCC phases and one BCC phase. Microstructural evaluation illustrated that the as-cast alloy has a typical cast dendritic structure, where dendrite regions (BCC) were enriched in Cr and Fe. Interdendritic regions were saturated with Cu and Ni and revealed G/B(T) {110} 〈111〉 and Brass {110} 〈112〉 as the major texture components. The produced alloy revealed an excellent compromise in mechanical properties due to the mixture of solid solution phases with different structures: 300 HV hardness, 950 MPa ultimate tensile strength and 14% elongation. Microhardness test results also revealed that the BCC phase was the hardest phase. The fracture surface evidenced a typical ductile failure. Furthermore, heat treatment results revealed that phase composition remained stable after annealing up to 650 °C. Phase transformation occurred at higher temperatures in order to form more stable phases; therefore, FCC2 phase grew at the expense of the BCC phase.

36 MATERIALS SCIENCE↗

The Effects of Sc Addition on the Microstructure and Mechanical Properties of Be-Al Alloy Fabricated by Induction Melting

This study investigated the alloying effects of 0.4 wt.% Sc on the microstructure, mechanical properties, and fracture behavior of a cast Be-Al alloy prepared by vacuum induction melting. The micromechanics of Sc-containing secondary-phase particles (SPs) were characterized by nanoindentation, and the fracture behavior of the alloy was investigated via tensile fractography and optical metallography. The addition of 0.4 wt.% Sc significantly modified the alloy microstructure by decreasing the secondary dendritic arm spacing (SDAS), weakening the dendritic structure of Be, and producing an equiaxed/cellular alloy microstructure with refined Be grains. Sc alloying increased the Vickers hardness by 36%, elastic modulus by 28%, yield strength by 35%, ultimate strength by 52%, but decreased the elongation from 3.6 to 2.9%. Sc-containing SPs had a higher elastic modulus, yield strength, microhardness, and a lower plasticity index than the Be and Al matrices, resulting in interface separation during the fracture process. SPs located at the Be/Al interfaces did not act as microcrack sources for the matrices, whereas highly faceted SPs within the Be grains induced microcrack formation and decreased the elongation. The failure mode of the cast Be-Al-0.4Sc alloy still involved the brittle cleavage failure of Be regions and ductile dimple failure of Al regions, which was not the case with the cast Be-Al alloy.

36 MATERIALS SCIENCE↗

Microstructural and Mechanical Characterization of Directionally Solidified Conventional and Nb-Modified Mar-M247 Superalloy

This study analyzes the effects of replacing Ta by Nb (at.% basis) in the phase transformation temperatures, Scheil solidification behavior, and microstructural mechanical features of a Nb-modified as well as conventional Mar-M247 superalloys. Both alloys were directionally solidified at a withdrawal rate of 18 cm/h under a thermal gradient of about 80 °C/cm. DSC results were compared to thermodynamic simulations of phase transformation temperatures and showed a good correlation. The replacement of Ta by Nb has not altered the solidification path of Mar-M247, keeping the sequence L → L + γ → L + γ + MC → L + γ + MC + γ/γ′ eutectic. Due to the segregation of Hf and Zr to the very last liquid to solidify, a low melting point γ/Ni{sub 5}(Hf,Zr) constituent was observed. The as-solidified microstructures of both Mar-M247(Nb) and Mar-M247 were constituted of columnar dendrites of gamma matrix (γ) phase with cuboidal gamma-prime (γ′) precipitates. In addition, γ/γ′-eutectic was observed in the interdendritic region along with MC carbides in blocky, script (blocky dendritic), needle-like and fine nodular morphologies. Both alloys contained about 1.5 vol.% of MC carbides. The MC carbides in Mar-M247(Nb) and Mar-M247 are, respectively, Nb-rich and Ta-rich, with only a limited amount of Hf being detected in the MC phase. The yield stress of Nb-modified Mar-M247 showed higher values up to 750 °C. For higher temperatures, above 800 °C, a conventional Mar-M247 presented a higher value of yield stress.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure Evolution and Mechanical Properties of Selective Laser Melted Inconel 718 Alloy

The microstructure characteristics of the selective laser melted Inconel 718 alloy under as-deposited, homogenization + solution + aging (HSA) and solution + aging (SA) conditions were studied. The anisotropy and heterogeneity of mechanical properties under different conditions were also investigated. Under the as-deposited condition, the morphology and size of the grains are heterogeneous. The dendrite structures which grow nearly perpendicular to the molten pool traces, accompanying interdendritic Laves phase, can be observed within the grains. The dendrite structure completely disappeared, and the Laves phases embedded in the interdendritic regions also dissolved into the matrix to precipitate γ′ and γ″ phases after heat treatments. Fully recrystallized grains were obtained under the HSA condition, while only incomplete recrystallized grains were obtained under the SA condition. However, the characteristics of γ′ and γ″ phases are very similar under the HSA and SA conditions. Significant improvement in strength after heat treatments was due to the dissolution of undesirable Laves phase and the precipitation of γ′ and γ″ phases. For all the three conditions, different tensile properties were observed depending on the orientation of the specimens. The scatter of mechanical properties is notable, and heat treatments increased the scatter of mechanical properties.

36 MATERIALS SCIENCE↗

The Effect of Weld Metal Composition on Microstructural and Mechanical Properties of Dissimilar Welds Between Monel 400 and Inconel 600

The current work was carried out to characterize welding of Inconel 600 superalloy and Monel 400. In the present study, gas tungsten arc welding (GTAW) with four types of filler metals (ENiCu, ENiCu-7, ENiCr-3 and ENiCrFe-3) was utilized. The filler metals were categorized into two groups based on the presence of Cr and Nb in their chemical composition. This paper describes the selection and application of welding consumables in manufacturing dissimilar metal combinations. It was found that (Nb/Cr) ratio and Fe content can affect on the size and amount of carbides. During solidification of ENiCr-3 and ENiCrFe-3 filler metals, Nb leaves dendritic cores and is rejected to inter-dendritic regions because of its high tendency for segregation. However, No brittle Laves phase was detected in the welds. The interface between weld metal and base metal and gradual changes in alloying elements were also investigated by scanning electron microscopy. EDX analysis was also applied for different samples. Microhardness measurements and tensile test were performed on the joints. The average hardness value in the weld metal obtained from ENiCrFe-3 is higher than the other welds. ENiCu-7 weld exhibited the highest tensile strength of 540 MPa and percent elongation of 53% in contrast to ENiCrFe-3 weld with the lowest tensile strength (518 MPa) and percent elongation (39%).

36 MATERIALS SCIENCE↗

Multiscale Modeling of Microstructural Evolution in Fused-Coating Additive Manufacturing

A quantitative phase field model with adaptive-computational-domain-expansion (ACDE) method was developed to simulate the microstructural evolution in fused-coating additive manufacturing process. A heat transfer and fluid flow model was established to investigate the solidification behavior of the molten pool in a single deposited layer. The solidification parameters such as temperature gradient and solidification rate were calculated from the macroscopic model and then fed into the phase field model to get the microstructure at different positions within a single deposited layer. Columnar dendrites were formed at the bottom of the deposited layer, and equiaxed dendrites appeared in the upper part of the layer. The ACDE method is used to improve the simulation efficiency. The metallographic experiments and energy-dispersive spectrometer analysis for composition were conducted on the fused-coating specimen, and the results were in good accordance with the simulations.

36 MATERIALS SCIENCE↗

A Successful Synthesis of the CoCrFeNiAl0.3 Single-Crystal, High-Entropy Alloy by Bridgman Solidification

For the first time, a face-centered-cubic, single-crystal CoCrFeNiAl{sub 0.3} (designated as Al0.3), high-entropy alloy (HEA) was successfully synthesized by the Bridgman solidification (BS) method, at an extremely low withdrawal velocity through a constant temperature gradient, for which it underwent two BS steps. Specially, at the first BS step, the alloy sample underwent several morphological transitions accompanying the crystal growth from the melt. This microstructure evolves from as-cast dendrites, to equiaxed grains, and then to columnar crystals, and last to the single crystal. In particular, at the equiaxed-grain region, some visible annealing twins were observed, which indicates a low stacking fault energy of the Al0.3 alloy. Although a body-centered- cubic CoCrFeNiAl (Al1) HEA was also prepared under the same conditions, only a single columnar-crystal structure with instinctively preferential crystallographic orientations was obtained by the same procedure. A similar morphological transition from dendrites to equiaxed grains occurred at the equiaxed-grain region in Al1 alloy, but the annealing twins were not observed probably because a higher Al addition leads to a higher stacking fault energy for this alloy.

36 MATERIALS SCIENCE↗