Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SINTERED MATERIALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 937 records · Page 52

Thermoelectric materials with filled skutterudite structure for thermoelectric devices

A class of thermoelectric compounds based on the skutterudite structure with heavy filling atoms in the empty octants and substituting transition metals and main-group atoms. High Seebeck coefficients and low thermal conductivities are achieved in combination with large electrical conductivities in these filled skutterudites for large ZT values. Substituting and filling methods are disclosed to synthesize skutterudite compositions with desired thermoelectric properties. A melting and/or sintering process in combination with powder metallurgy techniques is used to fabricate these new materials.

Fleurial, Jean-Pierre↗

Generation of electric-field stabilized zirconium monoxide secondary phase within cubic zirconia

Flash sintering of cubic yttria-stabilized zirconia has been studied via in situ energy dispersive diffraction. A secondary rocksalt-phase zirconium monoxide was observed emerging from the primary fluorite-phase zirconium dioxide, previously only observed as a thin interlayer at metal-oxide interfaces, upon application of a direct current electric field. The average secondary phase intensity rose over extended flow of direct current through the ceramic, faded upon removal of the field and disappeared entirely upon application of an alternating current electric field. The results indicate that the sustained application of a direct current electric field can result in significant electrochemical reduction of zirconia under high current density conditions. Poor sinterability and cracking under direct current is apparent and potential mechanisms discussed therein.

36 MATERIALS SCIENCE↗

Linking sintering stresses to nano modification in the microstructure of BaLa4Ti4O15 by transmission electron microscopy

Highlights: • by systematic HRTEM studies we link the microstructural changes in BLT ceramics to the external pressure applied during sintering; • we developed a mechanistic understanding of the role of stress in sintering; • external stresses during sintering affect the microstructural development at the nanoscale level, being responsible for the creation of higher defective bulk and grain boundary regions; • observation of high density of stacking faults (which generally arrises due to the Ti vacancy layers) indicates that the applied stress is modifying the stacking of AO{sub 3} layers of BLT which in turn creates Ti vacancy layer and stacking faults; • stress assisted sintering has, therefore, the potential to be used as a tool to design microstructures and achieve tailored properties, as suggested from our previous results in BLT and BNT. - Abstract: High quality factor and a temperature stable resonant frequency make BaLa{sub 4}Ti{sub 4}O{sub 15} (BLT) ceramics attractive materials for microwave applications. Aiming to exploit the effects of external stresses on the development of textured and anisotropic microstructures to optimise MW properties, the influence of applied external pressure during sintering of BLT ceramics is analysed. HRTEM and geometric phase analysis (GPA) showed that stresses applied during sintering, trigger the nucleation and growth of faults hypothesised to be due to the errors in the AO{sub 3} layer (basal plane) stacking sequence of the hexagonal perovskite structure. The results reveal a strong correlation between the high concentration of structural defects and the development of anisotropic microstructures, which tune the properties of BLT. Stresses applied during sintering are therefore a promising tool to design material properties.

36 MATERIALS SCIENCE↗

Effect of Strain Rate on the Plastic Deformation and Fracture of 90W-7Ni-3Fe Alloy Prepared by Liquid-Phase Sintering

In this study, the effect of the strain rates on the plastic deformation behavior and fracture mechanism of 90W-7Ni-3Fe heavy alloy prepared by liquid-phase sintering was investigated. Stress–strain tests were carried out in tensile and compression under quasi-static condition with the strain rate ranging from 10{sup −3} to 1 s{sup −1}. Dynamic test was examined using a compression split Hopkinson bar at strain rates ranging from 1000 to 1700 s{sup −1} in order to evaluate the effects of high strain rate on dynamic plastic deformation behavior. Quasi-static tests results show that the strength and hardness of this alloy increase with increasing strain rate. Results indicate that the as-sintered 90W-7Ni-3Fe heavy alloy has obvious strain-hardening characteristic under tensile or compression deformation under quasi-static condition. At this time, strain hardening is the main factor. Nevertheless, strain-hardening and strain-softening behaviors of the specimens occur simultaneously under dynamic compression condition. The effect of compressive stress on the work hardening is more obvious. A strong relevance of work-hardening effect on strain rate is also found. And the fracture mode of quasi-static and dynamic compression samples is also different.

36 MATERIALS SCIENCE↗

Effects of mechanically alloying Al 2 O 3 and Y 2 O 3 additives on the liquid phase sintering behavior and properties of SiC

In order to improve the sintering of SiC, mixtures of Al 2 O 3 and Y 2 O 3 powders are commonly included as sintering additives. The aim of this work was to use mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures as sintering additives to promote liquid phase sintering of SiC using spark plasma sintering. The results showed that milling reduced the particle size of the powders and led to the formation of complex oxide phases (YAP, YAM, and YAG) at low temperatures. As the ball milling time increased, the mass loss of specimens sintered with mechanically alloyed Al 2 O 3 –Y 2 O 3 mixtures decreased, and accordingly the relative density increased. However, the hardness and flexural strength of sintered SiC specimens first increased and then decreased. Because the specimens prepared with oxides milled for a long time contained too much YAG/YAP and accordingly too much liquid at sintering temperature. This negatively affected the mechanical properties of the SiC specimens because of the increased volume of the complex oxide phases, which have inferior mechanical properties to SiC, in the sintered specimens. In conclusion, when the ball milling time was 6h, the hardness (24.02 GPa) and flexural strength (655.61 MPa) of the SiC specimens reached maximum values.

36 MATERIALS SCIENCE↗

Low temperature sintering of PNSZT.

Pb-based ferroelectrics are useful because of their large dielectric constants, high polarization values, and strong piezoelectric coefficients, but typically require sintering temperatures >1200 C, which leads to loss of the volatile Pb cation and necessitates the use of Pt electrodes for cofired parts. Reduced sintering temperatures can minimize lead loss and enable the use of cheaper electrodes, but must not sacrifice electrical performance. A systematic study of dopants to lower the sintering temperature of PNSZT (Pb0.992 (Zr0.815 Ti0.05 Sn0.135)0.9845 Nb0.155 O3) led to densities greater than 98.5% of theoretical at temperatures as low as 1100 C with as little as 0.2 wt% of a Pb glass additive or as high as 98% at 900 C with Cu2O additions with equivalent electrical properties to undoped materials.

36 MATERIALS SCIENCE↗

Effect of TiO{sub 2} additives to the sintering of Y{sub 2}O{sub 3}

The effect of sintering additive on the microstructure development of yttrium oxide was investigated. Different combinations of yttrium oxide with TiO{sub 2} were used as x-ray diffraction, differential thermal analysis (DTA) were sintering additive. The investigated and microstructure of resulting compacts were characterized by, using scanning electron microscopy, porosity and sintering density for all compacting samples sintered at different sintering temperature under static air.

36 MATERIALS SCIENCE↗

ZrB{sub 2}-SiC-Ta{sub 4}HfC{sub 5}/Ta{sub 4}HfC{sub 5} Oxidation-Resistant Dual-Layer Coating Fabricated by Spark Plasma Sintering for C/C Composites

In this work, a ZrB{sub 2}-SiC-Ta{sub 4}HfC{sub 5}/Ta{sub 4}HfC{sub 5} oxidation-resistant dual-layer coating was fabricated to improve the oxidation resistance of carbon–carbon (C/C) composites. The coating was prepared by pack cementation combined with the slurry paste method. Spark plasma sintering was used in the procedure. The as-prepared dual-layer coating was approximately 110 μm, and no distinct interface was observed between the coating and the matrix. The isothermal oxidation test results showed that the dual coating effectively prevented C/C composites from oxidizing. The weight loss of the coated samples was only 3.3 and 9.5% after oxidation at 1773 K for 20 h and ten thermal shock cycles between 1773 K and room temperature in air, respectively. The pores and microcracks were the main reason for the failure of the coating.

36 MATERIALS SCIENCE↗

First Materials Science Research Rack Capabilities and Design Features

The first Materials Science Research Rack (MSRR-1) will accommodate dual Experiment Modules (EM's) and provide simultaneous on-orbit processing operations capability. The first international Materials Science Experiment Module for the MSRR-1 is an international cooperative research activity between NASA's Marshall Space Flight Center (MSFC) and the European Space Agency's (ESA) European Space Research and Technology Center. (ESTEC). This International Standard Payload Rack (ISPR) will contain the Materials Science Laboratory (MSL) developed by ESA as an Experiment Module. The MSL Experiment Module will accommodate several on-orbit exchangeable experiment-specific Module Inserts. Module Inserts currently planned are a Quench Module Insert, Low Gradient Furnace, Solidification with Quench Furnace, and Diffusion Module Insert. The second Experiment Module for the MSRR-1 configuration is a commercial device supplied by MSFC's Space Products Department (SPD). It includes capabilities for vapor transport processes and liquid metal sintering. This Experiment Module will be replaced on-orbit with other NASA Materials Science EMs.

Schaefer, D.↗

Synthesis and transport property of AgSbTe{sub 2} as a promising thermoelectric compound

Polycrystalline AgSbTe{sub 2} ternary compound materials with high phase purity were fabricated using a combined process of mechanical alloying and spark plasma sintering. It was found that stoichiometric AgSbTe{sub 2} is a promising composition for low-and-mediate temperature applications, whose ZT reaches 1.59 at 673 K, benefiting from its extremely low thermal conductivity (0.30 W/mK) in addition to its low electrical resistivity (<1.1x10{sup -4} {omega} m) and large positive Seebeck coefficient (260 {mu}V/K). On the other hand, deviating from this formula would lead to unstable phase structures and higher thermal conductivity, which make the samples less attractive as thermoelectric materials or components of thermoelectric systems.

36 MATERIALS SCIENCE↗

Selective laser sintering of MA956 oxide dispersion strengthened steel

Oxide Dispersion Strengthened (ODS) steels’ qualities of radiation damage resistance and high strength at high temperature make them promising nuclear structural materials. However, the dispersed yttria that gives ODS steel its beneficial qualities are generally compromised during joining processes, making fabrication difficult and expensive. The selective laser sintering process offers a potential path through this barrier by which net-shape parts can feasibly be built via additive manufacturing without fully melting the structure. By rastering a 400 W laser over a MA956 ODS steel powder bed, here we additively built parts with varying build conditions. Although density was achieved to within 97% of the wrought MA956, ultimate tensile strengths achieved only 65% of the wrought strength. Spectroscopy analysis points to the agglomeration of the yttria nano-particles as a possible explanation for the loss in strength. Further study might benefit from exploration of other parameters such as thinner powder build layers which would require less energy input to achieve sintering while minimizing time above the melting temperature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comparative performance of geopolymers made with metakaolin and fly ash after exposure to elevated temperatures

This paper presents the results of a study on the effect of elevated temperatures on geopolymers manufactured using metakaolin and fly ash of various mixture proportions. Both types of geopolymers (metakaolin and fly ash) were synthesized with sodium silicate and potassium hydroxide solutions. The strength of the fly ash-based geopolymer increased after exposure to elevated temperatures (800 deg. C). However, the strength of the corresponding metakaolin-based geopolymer decreased after similar exposure. Both types of geopolymers were subjected to thermogravimetric, scanning electron microscopy and mercury intrusion porosimetry tests. The paper concludes that the fly ash-based geopolymers have large numbers of small pores which facilitate the escape of moisture when heated, thus causing minimal damage to the geopolymer matrix. On the other hand, metakaolin geopolymers do not possess such pore distribution structures. The strength increase in fly ash geopolymers is also partly attributed to the sintering reactions of un-reacted fly ash particles.

36 MATERIALS SCIENCE↗

Fractographical characterization of hot pressed and pressureless sintered AlN-doped ZrB{sub 2}–SiC composites

In this paper, ZrB{sub 2}–SiC composites doped with 0–5 wt.% AlN were prepared by a low pressure hot pressing as well as a pressureless sintering methods at 1900 °C for 2 h. The influence of aluminum nitride addition on the sinterability and microstructure development of such ceramic composites was studied by a fractographical approach. The results revealed that only 1 wt.% AlN can aid the densification process of the hot pressed ceramic composite via the liquid phase sintering mechanism due to the formation of nano-scale metakaolinite spinel layers. In the pressureless sintering method, adding more AlN can increase the formation of gaseous products which raised the amount of porosities in the final microstructure. The formation of nano-graphite phase in the hot pressing process, the formation of Al{sub 2}OC in the pressureless sintering process, and the formation of BN in the both processes were disclosed by X-ray diffraction, SEM and TEM analyses. - Highlights: • The effect of AlN addition on densification of ZrB{sub 2}–SiC composites was studied. • AlN promotes the densification in hot pressed samples by liquid phase formation. • A fully dense composite was obtained by adding 1 wt.% AlN in hot pressing process. • In pressureless sintering, more AlN content intensifies the formation of porosities.

36 MATERIALS SCIENCE↗

CATALYSTS NHI Thermochemical Systems FY 2009 Year-End Report

Fiscal Year 2009 work in the Catalysts project focused on advanced catalysts for the decomposition of sulfuric acid, a reaction common to both the Sulfur-Iodine (S-I) cycle and the Hybrid Sulfur cycle. Prior years’ effort in this project has found that although platinum supported on titanium oxide will be an acceptable catalyst for sulfuric acid decomposition in the integrated laboratory scale (ILS) project, the material has short comings, including significant cost and high deactivation rates due to sintering and platinum evaporation. For pilot and larger scale systems, the catalyst stability needs to be improved significantly. In Fiscal Year 2008 it was found that at atmospheric pressure, deactivation rates of a 1 wt% platinum catalyst could be reduced by 300% by adding either 0.3 wt% iridium (Ir) or 0.3 wt% ruthenium (Ru) to the catalyst. In Fiscal Year 2009, work focused on examining the platinum group metal catalysts activity and stability at elevated pressures. In addition, simple and complex metal oxides are known to catalyze the sulfuric acid decomposition reaction. These metal oxides could offer activities comparable to platinum but at significantly reduced cost. Thus a second focus for Fiscal Year 2009 was to explore metal oxide catalysts for the sulfuric acid decomposition reaction. In Fiscal Year 2007 several commercial activated carbons had been identified for the HI decomposition reaction; a reaction specific to the S-I cycle. Those materials should be acceptable for the pilot scale project. The activated carbon catalysts have some disadvantages including low activity at the lower range of reactor operating temperature (350 to 400°C) and a propensity to generate carbon monoxide in the presence of water that could contaminate the hydrogen product, but due to limited funding, this area had low priority in Fiscal Year 2009. Fiscal Year 2009 catalyst work included five tasks: development, and testing of stabilized platinum based H2SO4 catalysts, development and testing of metal oxide based H2SO4 catalysts, support of the ILS for catalyst studies, conducting a long term catalyst stability test at anticipated operating temperatures and pressures, and developing capabilities for conducting pressurized catalyst tests.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase transition and piezoelectric property of (Bi{sub 0.5}Na{sub 0.5}){sub 0.94}Ba{sub 0.06}Zr{sub y}Ti{sub 1-y}O{sub 3}(y=0-0.04) ceramics

The ceramics with the composition of (Bi{sub 0.5}Na{sub 0.5}){sub 0.94}Ba{sub 0.06}Zr{sub y}Ti{sub 1-y}O{sub 3} (BNBZ100yT, in which y=0,0.01,0.02,0.04) were prepared successfully by the solid state reaction method. X-ray diffraction studies revealed the perovskite structure in BNBZ100yT ceramics sintered at 1170 deg. C for 2 h in air. The relative densities of the sintered ceramics were around 97%-99%. The temperature dependent dielectric properties of BNB6T and BNB6Z4T ceramics showed their relaxor-like behaviors. Decreases in remnant polarization, coercive field, and disappearance of piezoelectric properties were found by the substitution of 2 and 4 mol % Zr{sup 4+} for Ti{sup 4}+ in these ceramics. Electron diffraction patterns taken in a transmission electron microscope demonstrated the existence of cubic crystalline phase in the BNB6Z4T ceramics leading to the disappearance of piezoelectric property. Decrease in grain size was also observed with the substitution of Zr{sup 4+} for Ti{sup 4+} in BNB6T ceramics.

36 MATERIALS SCIENCE↗

A novel process route for the production of spherical SLS polymer powders

Currently, rapid prototyping gradually is transferred to additive manufacturing opening new applications. Especially selective laser sintering (SLS) is promising. One drawback is the limited choice of polymer materials available as optimized powders. Powders produced by cryogenic grinding show poor powder flowability resulting in poor device quality. Within this account we present a novel process route for the production of spherical polymer micron-sized particles of good flowability. The feasibility of the process chain is demonstrated for polystyrene e. In a first step polymer microparticles are produced by a wet grinding method. By this approach the mean particle size and the particle size distribution can be tuned between a few microns and several 10 microns. The applicability of this method will be discussed for different polymers and the dependencies of product particle size distribution on stressing conditions and process temperature will be outlined. The comminution products consist of microparticles of irregular shape and poor powder flowability. An improvement of flowability of the ground particles is achieved by changing their shape: they are rounded using a heated downer reactor. The influence of temperature profile and residence time on the product properties will be addressed applying a viscous-flow sintering model. To further improve the flowability of the cohesive spherical polymer particles nanoparticles are adhered onto the microparticles’ surface. The improvement of flowability is remarkable: rounded and dry-coated powders exhibit a strongly reduced tensile strength as compared to the comminution product. The improved polymer powders obtained by the process route proposed open new possibilities in SLS processing including the usage of much smaller polymer beads.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Thermal properties of field-assisted-sintered SiCN–Y 2 O 3 composites

Polymer-derived amorphous SiCN has excellent high-temperature stability and properties. To reduce the shrinkage during pyrolysis and to improve the high-temperature oxidation resistance, Y 2 O 3 was added as a filler. In this study, polymer-derived SiCN–Y 2 O 3 composites were fabricated by mixing a polymeric precursor of SiCN with Y 2 O 3 submicron powders in different ratios. The mixtures were cross-linked and pyrolyzed in argon. SiCN–Y 2 O 3 composites were processed using field-assisted sintering technology at 1350°C for 5 min under vacuum. Dense SiCN–Y 2 O 3 composite pellets were successfully made with relative density higher than 98% and homogeneous microstructure. Due to low temperature and short time of the heat-treatment, the grain growth of Y 2 O 3 was substantially inhibited. The Y 2 O 3 grain size was ~1 μm after sintering. The composites’ heat capacity, thermal diffusivity, and thermal expansion coefficients were characterized as a function of temperature. The thermal conductivity of the composites ceramics decreased as the amount of amorphous SiCN increased and the coefficient of thermal expansion (CTE) of the composites increased with Y 2 O 3 content. However, the thermal conductivity and CTE did not follow the rule of mixture. This is likely due to the partial oxidation of SiCN and the resultant impurity phases such as Y 2 SiO 5 , Y 2 Si 2 O 7 , and Y 4.67 (SiO 4 ) 3 O.

36 MATERIALS SCIENCE↗

Al{sub 2}O{sub 3}-TiC Composite Prepared by Spark Plasma Sintering Process: Evaluation of Mechanical and Tribological Properties

Al{sub 2}O{sub 3}-10TiC composites were synthesized by spark plasma sintering (SPS) process. Microstructural and mechanical properties of the composite reveal homogeneous distribution of the fine TiC particles in the matrix. The samples were produced with different sintering temperature, and it shows that the hardness and density gradually increases with increasing sintering temperature. Abrasion wear test result reveals that the composite sintered at 1500 °C shows high abrasion resistance (wt. loss ~ 0.016 g) and the lowest abrasion resistance was observed for the composite sample sintered at 1100 °C (wt. loss ~ 1.459 g). The profilometry surface roughness study shows that sample sintered at 1100 °C shows maximum roughness (R{sub a} = 6.53 µm) compared to the sample sintered at 1500 °C (R{sub a} = 0.66 µm) corroborating the abrasion wear test results.

36 MATERIALS SCIENCE↗