Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 937 records · Page 52

Dynamic Recrystallization Behavior of AISI 422 Stainless Steel During Hot Deformation Processes

In this work, hot compression tests were performed to investigate the dynamic recrystallization (DRX) process of a martensitic stainless steel (AISI 422) at temperatures of 950, 1000, 1050, 1100 and 1150 °C and strain rates of 0.01, 0.1 and 1 s{sup −1}. The dependency of strain-hardening rate on flow stress was used to estimate the critical stress for the onset of DRX. Accordingly, the critical stress to peak stress ratio was calculated as 0.84. Moreover, the effect of true strain was examined by fitting stress values to an Arrhenius type constitutive equation, and then considering material constants as a function of strain by using a third-order polynomial equation. Finally, two constitutive models were used to investigate the competency of the strain-dependent constitutive equations to predict the flow stress curves of the studied steel. It was concluded that one model offers better precision on the flow stress values after the peak stress, while the other model gives more accurate results before the peak stress.

36 MATERIALS SCIENCE↗

Effect of Quenching Process on Microstructures and Mechanical Properties of Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C Steel

To develop an appropriate quenching process to produce Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, the microstructures and mechanical properties of this steel were investigated under the direct quenching and tempering (DQT) and the direct quenching, reheated quenching and tempering (DQQT) heat treatment processes. The microstructure of the DQQT specimen was basically tempered sorbite with spherical precipitates, while quite a bit of tempered martensite was in the DQT specimen with dispersive nanoscaled precipitates. The yield strengths of the DQT and DQQT specimens were 1154 and 955 MPa, respectively. The yield strength of the DQT specimen was higher than that of the DQQT specimen because of its finer grain size, higher density of dislocations and dispersed precipitates. The DQQT specimen had spherical precipitates, which hindered the propagation of the crack. Moreover, the high-angle grain boundaries in the DQQT specimen took a higher proportion. Therefore, the Charpy impact values of DQT and DQQT specimens at − 60 °C were 38 and 75 J, respectively. Consequently, the mechanical properties of the Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, which met the standard of 1000 MPa grade steel plate for hydropower station, were acquired by the DQQT process.

36 MATERIALS SCIENCE↗

Processing and Characterization of Fe-Mn-Cu-Sn-C Alloys Prepared by Ball Milling and Spark Plasma Sintering

In this work, Fe-Mn-Cu-Sn-C alloys were prepared by means of powder metallurgy (PM). Powder mixtures were ball-milled for 8, 30 and 120 h and densified to < 1% porosity using spark plasma sintering (SPS) at 900 °C and 35 MPa. After consolidation, all samples of the Fe alloys were characterized by x-ray diffraction (XRD), scanning electron microscopy (SEM), hardness and flexural strength tests. Resistance to abrasive wear was evaluated in both three-body abrasion and two-body abrasion tests. The SEM observations revealed an evident dependence of grain size and microstructural homogeneity on milling time. The XRD analysis showed a marked increase in austenite content in the as-sintered specimens with milling time. Although the proportion of deformation-induced martensite was small, the strengthening effect of abrasion on the subsurface layer of the investigated alloys was clearly indicated by Knoop hardness measurements.

36 MATERIALS SCIENCE↗

Microstructural Evolution and the Precipitation Behavior in X90 Linepipe Steel During Isothermal Processing

Thermomechanical controlled processing of 560-MPa (X90) linepipe steel was simulated in the laboratory using a thermomechanical simulator to study the microstructural evolution and precipitation behavior during isothermal holding. The results indicated that martensite was obtained when the steels were isothermally held for 5 s at 700 °C. Subsequently, granular bainite and acicular ferrite transformation occurred with increased holding time. Different amount of polygonal ferrite formed after isothermally holding for 600-3600 s. Pearlite nucleated after isothermally holding for 3600 s. Precipitation occurred after isothermal holding for 5 s and continuous precipitation occurred at grain boundaries after isothermally holding for 600 s. After isothermally holding for 3600 s, large Nb/Ti carbide precipitated. The presence of MX-type precipitates was confirmed by diffraction pattern. The interphase precipitation (IP) occurred between 5 and 30 s. Maximum hardness was obtained after isothermally holding for 600 s when IP occurred and rapidly decreased to a low value, mainly because polygonal ferrite dominated the microstructure after isothermally holding for 3600 s.

36 MATERIALS SCIENCE↗

The Effect of Multiple Shot Peening on the Corrosion Behavior of Duplex Stainless Steel

Various types of shot peening treatments were applied to duplex stainless steel. The effects of shot peening intensity and working procedures on the microstructure were investigated. The domain size and microstrain evolution in the surface layer were characterized utilizing the Rietveld method. As the shot peening intensity increased, the surface roughness increased in the surface layer; however, it decreased after multiple (dual and triple) shot peening. The mole fraction of strain-induced martensite as a function of the intensity of shot peening was evaluated by XRD measurements. Both potentiodynamic polarization curves and salt spray tests of shot-peened samples in NaCl solution were investigated. The results indicate that traditional shot peening has negative effects on corrosion resistance with increasing shot peening intensity; however, the corrosion rate can be reduced by means of multiple shot peening.

36 MATERIALS SCIENCE↗

Tensile Deformation Temperature Impact on Microstructure and Mechanical Properties of AISI 316LN Austenitic Stainless Steel

Uniaxial tensile tests were conducted on AISI 316LN austenitic stainless steel from − 40 to 300 °C at a rate of 0.5 mm/min. Microstructure and mechanical properties of the deformed steel were investigated by optical, scanning and transmission electron microscopies, x-ray diffraction, and microhardness testing. The yield strength, ultimate tensile strength, elongation, and microhardness increase with the decrease in the test temperature. The tensile fracture morphology has the dimple rupture feature after low-temperature deformations and turns to a mixture of transgranular fracture and dimple fracture after high-temperature ones. The dominating deformation microstructure evolves from dislocation tangle/slip bands to large deformation twins/slip bands with temperature decrease. The deformation-induced martensite transformation can only be realized at low temperature, and its quantity increases with the decrease in the temperature.

36 MATERIALS SCIENCE↗

Effect of Different Thermomechanical Processes on the Microstructure, Texture, and Mechanical Properties of API 5L X70 Steel

A commercial API 5L X70 steel plate was subjected to different thermomechanical processes to propose a novel thermomechanical rolling path to achieve improved mechanical properties. Scanning electron microscopy, electron backscatter diffraction, and x-ray texture analysis were employed for microstructural characterization. The results showed that strain-free recrystallized {001} ferrite grains that developed at higher rolling temperature could not meet the American Petroleum Institute (API) requirements. Also, refined and work-hardened grains that have formed in the intercritical region with high stored energy do not provide suitable tensile properties. However, fine martensite–austenite constituents dispersed in ferrite matrix with grains having predominantly {111} and {110} orientations parallel to the normal direction that developed under isothermal rolling at 850 °C provided an outstanding combination of tensile strength and ductility.

36 MATERIALS SCIENCE↗

Effect of Final Cooling Temperature on Microstructure and Mechanical Properties of a Cr-Ni-Mo-V Bainite Steel

The microstructural evolution and mechanical properties of a low-carbon high-strength bainitic steel under different final cooling temperatures were studied. The microstructures of the experimental steel at different final cooling temperatures were composed of acicular ferrite and granular bainite. A decrease in final cooling temperature resulted in an increase in volume fraction of granular bainite and a decrease in volume fraction of acicular ferrite. The specimen with the lowest final cooling temperature (459 °C) exhibited the highest yield strength, tensile strength, and yield ratio, and a lower total elongation than the specimens with the highest final cooling temperatures (501 and 535 °C) because of the higher volume fraction of granular bainite and finer bainitic ferrite lath. The specimen with the lowest final cooling temperature had a lower absorbed energy than that of the highest final cooling temperature, because the strip-like martensite–austenite (M-A) constituents that existed between the bainitic ferrite or in prior austenite grain boundaries reduced its toughness. At an intermediate final cooling temperature of 501 °C, the experimental steel exhibited excellent mechanical properties with a yield strength, tensile strength, and absorbed energy of 825 MPa, 1232 MPa, and 102 J, respectively.

36 MATERIALS SCIENCE↗

High Chromium Cast Irons: Destabilized-Subcritical Secondary Carbide Precipitation and Its Effect on Hardness and Wear Properties

This work evaluates the effect of a destabilization treatment combined with a subcritical diffusion (SCD) and a subsequent quenching (Q) steps on precipitation of secondary carbides and their influence on the wear properties of HCCI (16%Cr). The destabilization of the austenite at high temperature leads to a final microstructure composed of eutectic and secondary carbides, with an M{sub 7}C{sub 3} nature, embedded in a martensitic matrix. An improved wear resistance was observed in the SCD + Q samples in comparison with the Q one, which was attributed to the size of secondary carbides.

36 MATERIALS SCIENCE↗

Multiphase Microstructure in a Metastability-Assisted Medium Carbon Alloy Steel

A medium carbon alloy steel is processed by austenizing at 900 °C for 30 min, then rapid quenching into a patented quenching liquid and holding at 170 °C for 5 min, finally isothermally holding at 250 °C for different times. The morphology and mechanical properties are performed by using optical microscopy and scanning electron microscopy. A multiphase microstructure characterized by a mixture of lenticular prior martensite (PM), fine needle bainitic ferrite and filmy retained austenite (RA) is obtained. It is found that the PM formed firstly upon quenching can accelerate the subsequent bainitic transformation and promote refinement of multiphase colonies. The results show that an optimum mechanical property of a 4000.9 MPa bending strength and a 2030 MPa tensile strength is achieved at 250 °C for 120 min, which is attributed to the multiphase microstructural characteristics and a high product of the volume fraction of RA and the carbon content of austenite.

36 MATERIALS SCIENCE↗

Effect of Multiple Local Repairs on Microstructure and Mechanical Properties of T24 Steel Welded Joint

The effect of multiple local repairs on the microstructure and mechanical properties of the T24 steel welded joints was studied. T24 steel tubes were butt-welded by the GTAW method. Peripheral welded joints were made in four locations of the tube. In order to simulate the repair procedure, the welds were cut off from the root and the first local repair was performed. Other two local repairs were carried out in the same way. After each local repair, the microstructure and mechanical properties of the joints were evaluated. The results of the mechanical tests demonstrate that only two local repairs can be performed on the T24 steel peripheral welded joint. After the third local repair, impact energy of the welded joint was lower than required value, which is attributed to the coarser martensite and the coarser carbide precipitates formed in the heat-affected zone, compared with the weld metal.

36 MATERIALS SCIENCE↗

Effect of Zener–Holloman Parameter on the Prior Austenite Grain size in a 12Cr-10Ni Precipitation-Hardenable Stainless Steel

Hot isothermal plane strain compression (PSC) tests were carried out on a 12Cr-10Ni martensitic precipitation-hardenable (PH) stainless steel, in the temperature range of 750-1050 °C, to study microstructural evolution during large strain deformation. The nature of stress–strain curves varies with Zener–Holloman parameter (Z) with specimens deformed at high Z showing steady-state behavior and those deformed at lower Z showing flow softening. Prior austenite grain size (PAGS), d, exhibited a strong correlation to Z showing a bilinear behavior represented as: d = (1803.9)Z{sup −0.094} for high Z deformation and d = (1456.2)Z{sup −0.058} for low Z deformation. Based on the above study, it is recommended to thermomechanically process 12Cr-10Ni steel at Z ≥ 10{sup 22} for obtaining products with good strength–toughness balance.

36 MATERIALS SCIENCE↗

Processing Parameter Effects on Residual Stress and Mechanical Properties of Selective Laser Melted Ti6Al4V

Selective laser melting (SLM) process is characterized by large temperature gradients resulting in high levels of residual stress within the additively manufactured metallic structure. SLM-processed Ti6Al4V yields a martensitic microstructure due to the rapid solidification and results in a ductility generally lower than a hot working equivalent. Post-process heat treatments can be applied to SLM components to remove in-built residual stress and improve ductility. Residual stress buildup and the mechanical properties of SLM parts can be controlled by varying the SLM process parameters. This investigation studies the effect of layer thickness on residual stress and mechanical properties of SLM Ti6Al4V parts. This is the first-of-its kind study on the effect of varying power and exposure in conjunction with keeping the energy density constant on residual stress and mechanical properties of SLM Ti6Al4V components. It was found that decreasing power and increasing exposure for the same energy density lowered the residual stress and improved the % elongation of SLM Ti6Al4V parts. Increasing layer thickness resulted in lowering the residual stress at the detriment of mechanical properties. The study is based on detailed experimental analysis along with finite element simulation of the process using ABAQUS to understand the underlying physics of the process.

36 MATERIALS SCIENCE↗

Study of Tribological Characteristics of Multi-pass SMAW Armox 500T Steel Joints

Study of tribological characteristics of multi-pass shielding metal arc-welded (SMAW) Armox 500T steel joints in comparison with its counterpart base metal was carried out. Series of dry sliding wear tests were carried out as a function of applied loads ranging from 30 to 120 N and sliding distances from 1000 to 6000 m at a constant sliding velocity using pin-on-disk tribometer. It was observed that specific wear rate and lost volume in SMAW joints significantly high compared to Armox 500T base metal in the range of loads and sliding distances considered in the present study. The scanning electron micrographs indicated that wear of Armox 500T base metal occurred due to micro-grooving and adhesion, on the other hand, micro-delamination was observed in SMAW joints. Microstructural investigations revealed that base metal exhibits superior tribological properties as compared to SMAW joints due to the formation of martensite lath in acicular form with coarse and fine precipitates.

36 MATERIALS SCIENCE↗

Finite Element Simulation and Optimization of Gas-Quenching Process for Tool Steels

Various gas-quenching processes, including marquenching, were investigated to optimize gas-quenching processes in terms of distortion and hardness by means of numerical and experimental analyses. The temperature, microstructure, hardness, and distortion during the various gas-quenching processes of a tool steel block were simulated using a finite element method based on a coupled thermo-metallurgical–mechanical model. The predicted temperature, hardness, and distortion agreed well with the experimental data. The tool steel block (200 × 150 × 70 mm{sup 3}) quenched under 10 bar pressure of nitrogen gas (Case 2) had higher hardness due to the higher martensite fraction and larger distortion owing to the higher thermal stress induced by faster cooling, compared to the block quenched under 2 bar pressure of nitrogen gas (Case 1). The tool steel block marquenched under 10 bar pressure of nitrogen gas interrupted by isothermal holding at 500 °C (Case 3) had 30% smaller distortion with a negligible loss of hardness compared to Case 2. Furthermore, the simulation results could provide an optimized process condition to minimize distortion of the gas-quenched tool steel block while satisfying the hardness requirement.

36 MATERIALS SCIENCE↗

Dissimilar Metal Weld Joints of P91/Ni Alloy: Microstructural Characterization of HAZ of P91 and Stress Analysis at the Weld Interfaces

Microstructure evolution and hardness were evaluated at the interface of two friction-welded transition joints between P91 and AISI 304 fabricated applying Inconel interlayers, viz. single-interlayer weld (P91/IN600/AISI304) and three-interlayer weld (P91/IN625/IN600/IN800H/AISI304). The welds were subjected to post-weld heat treatment at 1023 K for 1 h followed by air cooling and a long-term exposure at 973 K for 100, 250, and 500 h. A soft zone with the absence of lath martensite was noticed in both the welds which was located at the intercritical heat-affected zone of the welds. This zone was found to be extending with time toward the fine grain heat-affected zone by carbide precipitation and coarsening at the grain boundaries. Soft zone formation at the interface of the welds was found to be due to carbon diffusion. The presence of high-nickel-content alloy at the interface was proven to be beneficial in stopping carbon diffusion at the interface. Though soft zones existed in both the welds, better creep rupture life was observed for three-interlayer welds. Finite element analysis of these weld joints was performed for thermal loading followed by tensile loading. The results from this analysis indicated that thermal expansion also plays an important role in the failures of these dissimilar weld joints by creating high stress at the interface due to incompatibility.

36 MATERIALS SCIENCE↗

Effect of Rolling Temperature on Fracture Properties of INRAFMS at Different Temperatures

Two heats of Indian reduced activation ferritic / martensitic steel have been produced with similar chemical composition and identical process parameters except the start and final rolling temperature referred as P950 and P1050, respectively. Fracture behaviours of both the heats have been evaluated, and it was found that quasistatic fracture properties are better for P1050 than P950. An attempt is made to establish the reasons for the observed behaviour through optical, scanning electron microscopic, electron backscatter diffraction and transmission electron microscopic studies. These variations are attributed to the difference in rolling temperature of both heats. P1050 meets the acceptance criteria as per Indian specifications, and it compares favourably with the international grades of equivalent RAFM steels.

36 MATERIALS SCIENCE↗

Effect of Deep Cryogenic Treatment on Mechanical Properties and Microstructure of the Tool Steel CR7V for Hot Stamping

To solve the failure problem of hot stamping tool, the CR7V steel was deep cryogenically treated at different dwelling times with multiple tempering. The hardness, impact toughness and wear resistance of the CR7V steel were examined, and the effects of deep cryogenic treatment on the microstructure of the CR7V steel were studied by means of optical microscope, scanning electron microscope and energy-dispersive spectroscopy. The results show that deep cryogenic treatment has little effect on the hardness of the tempered CR7V steel, but improves its impact toughness and wear resistance. The improvement in mechanical properties is a result of the combination of dissolution of large carbide particles, formation of small-sized and uniformly distributed carbide particles and fine tempered martensite structure. The cryogenic treatment is optimized as follows: vacuum gas quenching, deep cryogenic treatment at − 196 °C for 6 h and triple tempering at 560 °C for 2 h, which improves the wear resistance by 68% and the impact toughness by 58% compared to the conventional heat treatment.

36 MATERIALS SCIENCE↗