At least 937 records · Page 52

Precipitation under cyclic strain in solution-treated Al4wt%Cu I: mechanical behavior

Solution-treated AL-4wt%Cu was strain-cycled at ambient temperature and above, and the precipitation and deformation behaviors investigated by TEM. Anomalously rapid growth of precipitates appears to have been facilitated by a vacancy super-saturation generated by cyclic strain and the presence of a continually refreshed dislocation density to provide heterogeneous nucleation sites. Texture effects as characterized by Orientation Imaging Microscopy appear to be responsible for latent hardening in specimens tested at room temperature, with increasing temperatures leading to a gradual hardening throughout life due to precipitation. Specimens exhibiting rapid precipitation hardening appear to show a greater effect of texture due to the increased stress required to cut precipitates in specimens machined from rolled plate at an angle corresponding to a lower average Schmid factor. The accelerated formation of grain boundary precipitates appears to be partially responsible for rapid inter-granular fatigue failure at elevated temperatures, producing fatigue striations and ductile dimples coexistent on the fracture surface.

36 MATERIALS SCIENCE↗

Wear Behavior of an Ultra-High-Strength Eutectoid Steel

Wear behavior of an ultra-high-strength AISI 1080 steel developed through incomplete austenitization-based combined cyclic heat treatment is investigated in comparison with annealed and conventional hardened and tempered conditions against an alumina disk (sliding speed = 1 m s{sup −1}) using a pin-on-disk tribometer at a load range of 7.35-14.7 N. On a gross scale, the mechanism of surface damage involves adhesive wear coupled with abrasive wear (microcutting effects in particular) at lower loads. At higher loads, mainly the abrasive wear (both microcutting and microploughing mechanisms) and evolution of adherent oxide are observed. Besides, microhardness of matrix increases with load indicating substantial strain hardening during wear test. The rate of overall wear is found to increase with load. As-received annealed steel with the lowest initial hardness suffers from severe abrasive wear, thereby exhibiting the highest wear loss. Such a severe wear loss is not observed in conventional hardened and tempered and combined cyclic heat treatment conditions. Combined cyclic heat-treated steel exhibits the greatest wear resistance (lowest wear loss) due to its initial high hardness and evolution of hard abrasion-resistant tribolayer during wear test at higher load.

36 MATERIALS SCIENCE↗

Effects of Heating and Quenching Processing Parameters on Phase Transformation of 55CrMo Steel

Microstructure and mechanical properties after induction hardening have a significant effect on the wear resistance performance and lifetime of 55CrMo steel ball screw. In the paper, the dilatometric curves were recorded at the different heating rate by a Gleeble-1500D thermo-mechanical simulator to determine the effect of heating rate on the austenitizing temperature of 55CrMo steel. Heat treatment of some specimens was performed by the Gleeble-1500D thermal simulator at the different heating temperature, holding time and cooling rate to investigate the effect of induction hardening parameters on the phase transformation, microstructure and microhardness of 55CrMo steel. Microstructure of specimen was analyzed using an optical microscope and a scanning electron microscope. Volume fraction of retained austenite was measured using an x-ray diffractometer. The mechanical properties were evaluated by a microhardness tester. The results show that the austenitizing temperature of 55CrMo steel increases with the increasing heating rate. Increasing the heating temperature, holding time and cooling rate of specimen is helpful in obtaining a uniform cryptocrystalline martensite. Volume fraction of retained austenite is less as the heating temperature is in the range of 900-950 °C. In the induction hardening of 55CrMo steel, the heating temperature should be in the range of 900-1000 °C.

36 MATERIALS SCIENCE↗

Controlled Fabrication of Nanoporous Anodic Titania Films on Ti-6Al-4V Alloy for Enhanced Self-Lubricating Properties by Combining Spark Anodization and Electropulse-Assisted Ultrasonic Rolling

We report the fabrication of self-lubricating nanoporous anodic titania films through spark anodization in an aqueous ammonia sulfate electrolyte on a hardened nanocrystalline layer of Ti-6Al-4V rods after electropulse-assisted ultrasonic surface rolling process (EP-USRP). The spark anodization with an optimum anodizing voltage of 130 V produced sponge-like nanoporous anodic titania films with stable crystalline structure of rutile-phase TiO{sub 2}, and the EP-USRP resulted in a nanocrystalline layer with a higher surface hardening depth (> 220 µm) through severe plastic deformation. The combinatorial technique resulted in excellent tribological properties, with lower friction coefficient of ~ 0.72 (compared to EP-USRP of ~ 0.80), smoother wear scar with less adhesion and less wear loss (maximum depth of 12 nm, 33.3% lower than the EP-USRP sample). These enhancements are attributed to the synergetic effect of the self-lubricating nanoporous anodic titania films formed by spark anodization (which acted as transition layer and prevented direct contact between the counter materials and the substrate) and the hardened nanocrystalline layer formed by EP-USRP (which slowed down the consumption of the anodic powder).

36 MATERIALS SCIENCE↗

Hot Deformation Mechanisms of Ti22Al25Nb Orthorhombic Alloy

In this paper, the hot deformation behavior of Ti22Al25Nb was investigated by hot compression over a range of temperatures (950-1050 °C) and strain rates (0.001-1 s{sup −1}). Considering the adiabatic heating and friction, the original curves were corrected. The friction-corrected data were lower than the measured flow stress data. The flow stress data increased after the temperature correction owing to the elimination of the softening effect. In addition, the work hardening effects on the hot deformation of the normal and multi-peak flow stress curves were compared. A critical dislocation density was proposed to analyze the multi-peak phenomenon. When the dislocation density decreased to a critical value, the work hardening and dynamic recrystallization mechanisms reached a balance. Then, a new work hardening mechanism became dominant, and the flow stress increased. The effect of second-phase particles on the hot deformation mechanisms was investigated. The result showed that second-phase particles led to a high nucleation rate and a low growth rate of new recrystallization grains during the rapid hot deformation.

36 MATERIALS SCIENCE↗

Grain-Refined Microstructure and Hard Surface Layer Produced by SMRGT Process for Improved Corrosion Behavior of Mg-3Al-1Zn Alloy

To improve the surface properties and performance, a grain-refined surface layer was produced on AZ31B Mg alloy by a newly developed surface nano-crystallization and hardening process called surface mechanical rolling grinding treatment (SMRGT). The grain size refinement and minimal surface hardening were confirmed by the microstructure observations, XRD results and microhardness tests and were attributed to the multipass small strain-induced plastic deformation of the material during the SMRGT process. A nano-grain surface layer (average grain size of ~ 100 nm) and a graded microhardness variation (average ~ 113 HV adjacent to surface) along the thickness direction were generated. The E{sub corr} values of the as-SMRGTed samples were − 1.43 ± 0.03 and − 1.42 ± 0.02 V, increasing by ~ 30-40 mV compared with the values of the as-received (AR) sample (− 1.46 ± 0.02 V), corresponding to i{sub corr} ranging from 3.0 × 10{sup −5} to 1.0 × 10{sup −5} and 5.0 × 10{sup −6} A/cm{sup 2}, respectively. Charge transfer resistance (R{sub ct}) increased from 93.4 to 292.4 and 578.3 Ω (~ 3-6 times) with the increasing number of SMRGT passes. The corrosion resistance improvement was attributed mainly to the dramatic strain-induced surface grain refinement and minimal surface hardening that give rise to a more smooth and densely packed surface state.

36 MATERIALS SCIENCE↗

In situ high-energy X-ray diffraction study of tensile deformation of neutron-irradiated polycrystalline Fe-9%Cr alloy

The effect of neutron irradiation on tensile deformation of a Fe-9wt.%Cr alloy was investigated using in situ high-energy synchrotron X-ray diffraction during room-temperature uniaxial tensile tests. New insights into the deformation mechanisms were obtained through the measurements of lattice strain evolution and the analysis of diffraction peak broadening using the modified Williamson-Hall method. Two neutron-irradiated specimens, one irradiated at 300 °C to 0.01 dpa and the other at 450 °C to 0.01dpa, were tested along with an unirradiated specimen. The macroscopic stress–strain curves of the irradiated specimens showed increased strength, reduced ductility and work-hardening exponent compared to the unirradiated specimen. The evolutions of the lattice strain, the dislocation density and the coherent scattering domain size in the deformation process revealed different roles of the submicroscopic defects in the 300°C/0.01 dpa specimen and the TEM-visible nanometer-sized dislocation loops in the 450°C/0.01 dpa specimen: submicroscopic defects extended the linear work hardening stage (stage II) to a higher strain, while irradiation-induced dislocation loops were more effective in dislocation pinning. Lastly, while the work hardening rate of stage II was unaffected by irradiation, significant dynamic recovery in stage III in the irradiated specimens led to the early onset of necking without stage IV as observed in the unirradiated specimen.

36 MATERIALS SCIENCE↗

The effect of carbon on the microstructures, mechanical properties, and deformation mechanisms of thermo-mechanically treated Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 high entropy alloys

We investigated the effects of cold rolling followed by annealing on the mechanical properties and dislocation substructure evolution of undoped and 1.1 at. % carbon-doped Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 high entropy alloys (HEAs). X-ray diffraction, scanning electron microscopy (SEM), transmission electron microscopy (TEM) and atom probe tomography (APT) were employed to characterize the microstructures. The as-cast HEAs were coarse-grained and single phase f.c.c., whereas the thermo-mechanical treatment caused recrystallization (to fine grain sizes) and precipitation (a B2 phase for the undoped HEA; and a B2 phase, and M 23 C 6 and M 7 C 3 carbides for the C-doped HEA). Carbon, which was found to have segregated to the grain boundaries using APT, retarded recrystallization. The reduction in grain size resulted in a sharp increase in strength, while the precipitation, which produced only a small increase in strength, probably accounted for the small decrease in ductility for both undoped and C-doped HEAs. For both undoped and C-doped HEAs, the smaller grain-sized material initially exhibited higher strain hardening than the coarse-grained material but showed a much lower strain hardening at large tensile strains. Wavy slip in the undoped HEAs and planar slip in C-doped HEAs were found at the early stages of deformation irrespective of grain size. At higher strains, dislocation cell structures formed in the 19 μm grain-sized undoped HEA, while microbands formed in the 23 μm grain-sized C-doped HEA. Conversely, localized dislocation clusters were found in both HEAs at the finest grain sizes (5 μm). The inhibition of grain subdivision by the grain boundaries and precipitates lead to the transformation from regular dislocation configurations consisting of dislocation-cells and microbands to irregular dislocation configurations consisting of localized dislocation clusters, which further account for the decrease in ductility. Our investigation of the formation mechanism and strain hardening of dislocation cells and microbands could benefit future structural material design.

36 MATERIALS SCIENCE↗

Response of 14YWT alloys under neutron irradiation: A complementary study on microstructure and mechanical properties

Nanostructured ferritic alloys (NFAs) having sub-micron grain size with a high density of nano-oxides (NOs) (size of ~2-3 nm) are one of the best candidates for structural components in Generation IV nuclear systems. In this study, 14YWT NFA cladding tubes were irradiated in BOR60 reactor up to 7 dpa at 360-370 °C. Detailed microstructural analysis has been conducted using bright field transmission electron microscopy, bright field scanning transmission electron microscopy, energy filtered transmission electron microscopy, energy dispersive X-ray spectroscopy, electron energy loss spectroscopy and transmission Kikuchi diffraction techniques. This revealed cavities, <100> and <111> type dislocation loops, and α' precipitates forming after irradiation with relationships between cavities and NOs, and α' precipitates and NOs. Cavities mostly form on the NOs; whereas, α' precipitates form between the NOs where the point defect concentration is high. Moreover, α' precipitates are distributed homogenously on and around the dislocation loops which is consistent with the observation that there is no Cr segregation on dislocation loops. Grain boundaries were found to be mostly depleted in Cr; however, the characteristics of each grain boundary determines the Cr behavior and the α' denuded zone around the grain boundaries. Mechanical properties of the irradiated tubes have been determined by using both low force and high force nanoindentation techniques, resulting in 1.03±0.33 GPa and 0.82±0.20 GPa hardening, respectively. Dispersed barrier hardening calculations and nanoindentation measurements are in good agreement. In this paper, 14YWT NFA has been systematically studied after neutron irradiation to better understand its superior performance: low α' concentration, low swelling and low radiation-induced hardening.

36 MATERIALS SCIENCE↗

Effects of mixing energy on technological properties and hydration kinetics of grouting mortars

During slurry preparation, effects of certain phenomena on fluidity and hardening characteristics of cement-based grouts have been reported. Deterioration of fluidity and hardening will affect the slurry performance, quality of workmanship and result in subsequent structural defects. There has been little research conducted on the effects of mixing energy during slurry preparation which has focused on the reasons or mechanisms for changes in characteristic properties. This work describes and measures the effects of several mixing parameters on properties of grouting materials, such as fluidity, hardening characteristics, shrinkage, heat of hydration, ion elution and crystallographic structure using X-ray diffraction and SEM. The results indicate that long mixing processes cause deterioration in fluidity and setting properties. These observations can be explained by acceleration in hydration kinetics and changes in microstructures and subsequent changes in dispersion states due to different mixing durations.

36 MATERIALS SCIENCE↗

High Temperature Irradiation Effects in Selected Generation IV Structural Alloys

In the Generation IV Materials Program cross-cutting task, irradiation and testing were carried out to address the issue of high temperature irradiation effects with selected current and potential candidate metallic alloys. The materials tested were (1) a high-nickel iron-base alloy (Alloy 800H); (2) a nickel-base alloy (Alloy 617); (3) two advanced nano-structured ferritic alloys (designated 14YWT and 14WT); and (4) a commercial ferritic-martensitic steel (annealed 9Cr-1MoV). Small tensile specimens were irradiated in rabbit capsules in the High-Flux Isotope Reactor at temperatures from about 550 to 700 C and to irradiation doses in the range 1.2 to 1.6 dpa. The Alloy 800H and Alloy 617 exhibited significant hardening after irradiation at 580 C; some hardening occurred at 660 C as well, but the 800H showed extremely low tensile elongations when tested at 700 C. Notably, the grain boundary engineered 800H exhibited even greater hardening at 580 C and retained a high amount of ductility. Irradiation effects on the two nano-structured ferritic alloys and the annealed 9Cr-1MoV were relatively slight at this low dose.

36 MATERIALS SCIENCE↗

Proton irradiation damage of an annealed Alloy 718 beam window

Mechanical testing and microstructural analysis was performed on an Alloy 718 window that was in use at the Los Alamos Neutron Science Center (LANSCE) Isotope Production Facility (IPF) for approximately 5 years. It was replaced as part of the IPF preventive maintenance program. The window was transported to the Wing 9 hot cells at the Chemical and Metallurgical Research (CMR) LANL facility, visually inspected and 3-mm diameter samples were trepanned from the window for mechanical testing and microstructural analysis. Shear punch testing and optical metallography was performed at the CMR hot cells. The 1-mm diameter shear punch disks were cut into smaller samples to further reduce radiation exposure dose rate using Focus Ion Beam (FIB) and microstructure changes were analyzed using a Transmission Electron Microscopy (TEM). Irradiation doses were determined to be ~0.2–0.7 dpa (edge) to 11.3 dpa (peak of beam intensity) using autoradiography and MCNPX calculations. The corresponding irradiation temperatures were calculated to be ~34–120 °C with short excursion to be ~47–220 °C using ANSYS. Mechanical properties and microstructure analysis results with respect to calculated dpa and temperatures show that significant work hardening occurs but useful ductility still remains. The hardening in the lowest dose region (~0.2–0.7 dpa) was the highest and attributed to the formation of γ" precipitates and irradiation defect clusters/bubbles whereas the hardening in the highest dose region (~11.3 dpa) was lower and attributed mainly to irradiation defect clusters and some thermal annealing.

36 MATERIALS SCIENCE↗

Effects of helium on irradiation response of reduced-activation ferritic-martensitic steels: Using nickel isotopes to simulate fusion neutron response

Understanding the effects of helium on microstructures and mechanical properties of reduced-activation ferritic-martensitic steels is important to use of these steels in fusion reactor structures. The 9Cr-2WVTa steels were doped with 58Ni and 60Ni isotopes at 2 weight percent to control the rate of transmutation helium generation. The samples were irradiated in the High Flux Isotope Reactor to ~24 displacements per atom at nominal temperatures of 300, 400, and 500°C, producing 228 and 7 atomic parts-per-million helium in the 58 Ni- and 60 Ni-doped samples, respectively. Transmission electron microscopy revealed a variety of precipitates and the radiation-induced dislocation loops and cavities (voids or helium bubbles). Tensile tests of the irradiated samples at the irradiation temperatures showed radiation-induced hardening at 300°C and radiation-induced softening at 400°C. Analysis indicates that the hardening primarily originated from the loops and cavities. The 58 Ni-doped samples had greater strengthening contributions from loops and cavities, leading to higher hardening with lower ductility than the 60 Ni-doped samples. The greater helium production of 58 Ni did not show pronounced reductions in ductility of the samples.

36 MATERIALS SCIENCE↗

The influence of nitrogen and nitrides on the structure and properties of proton irradiated ferritic/martensitic steel

The 12Cr1MoWV (wt%) ferritic/martensitic steel HT9 is a candidate material for fuel cladding in advanced nuclear reactors, such as the Versatile Test Reactor currently under development. As such, understanding the relationship between microstructure and mechanical properties in the context of irradiation environments for these steels is critical. N content, and more specifically interstitial N, has been hypothesized to be detrimental to irradiated properties at lower temperatures (less than 0.3T m ) to a total of 6 dpa; however, in this work at a dose of 1 dpa the irradiated microstructure was improved with added N, leading to less irradiation hardening. Three variants of HT9 were irradiated with 1.5 MeV protons to a dose of 1 dpa at 300°C. The HT9 variants included Low (10 ppm), Mid (190 ppm), and High (440 ppm) N alloys that were otherwise nearly identical. Changing the N content had a variety of effects on the irradiated defect structures. As N content increased, the average dislocation loop diameter decreased, while the number density of loops increased. Additionally, extensive Ni clustering was observed on dislocations and interfaces. The Mid and High N specimens exhibited significantly less hardening (ΔHV≃100) relative to the Low N specimen (ΔHV≃160). The decrease in hardening is attributed to vanadium carbonitride acting as a sink for Ni clusters that would otherwise form on dislocations. Under the irradiation conditions used, these results suggest increasing the N content in HT9 may have a desirable effect on the irradiated structure and properties at the dose studied, as well as the swelling resistance at higher doses. In other words, N content appears to be a powerful tool for tailoring the self-interstitial atom cluster mobility in F/M steels for different temperature and dose applications.

36 MATERIALS SCIENCE↗

Defect-specific strength factors and superposition model for predicting strengthening of ion irradiated Fe18Cr alloy

Here, a high-purity binary alloy Fe18Cr was subjected to heavy-ion irradiation in order to provide improved understanding of the irradiation effect on radiation hardening associated with dislocation loop and network formation, α’ precipitation. The specimens were irradiated with 8 MeV Fe ions (~2 μm ion range) to midrange doses of 0.37 and 3.7 dpa at 300, 350 and 450 °C using dose rates of ~10 –5 –10 –3 dpa/s. Nanoindentation testing was performed to extract the bulk equivalent hardness at low depth from these ion irradiated specimens. High-quality transmission electron microscopy (TEM) images were acquired by utilizing a flash electropolishing method on the Focused Ion Beam (FIB) prepared liftouts. An accurate calculation of the strength factor was provided based on detailed TEM characterization of the irradiated microstructures. A newly refined hardening superposition method was applied to combine the strengthening components from each microstructure. The good agreement between microstructure predicted strength and measured strength further demonstrated the fidelity to use hardening model to quantify the mechanical properties of ion irradiated materials.

36 MATERIALS SCIENCE↗

Defect formation and transmutation behaviors in irradiated tungsten under thermal-neutron shielded and mixed spectrum conditions

Here, this study investigates the microstructural evolution of pure tungsten irradiated under thermal-neutron shielded and mixed spectrum conditions in the High Flux Isotope Reactor (HFIR). Four samples were irradiated at temperatures from 570 °C to 1130 °C up to 0.73 dpa. Neutron spectrum significantly influenced the accumulation of transmutation products, with Re+Os content estimated at ∼0.3–0.6% under thermal-neutron shielded conditions and ∼5.2% under the mixed spectrum condition. Irradiation temperature strongly influences tungsten’s microstructure, with dislocation loops and fine voids forming at lower temperatures and only larger voids and Re/Os segregation observed at higher temperature. Under thermal-neutron shielded conditions, dislocation loops and voids were observed at 570 °C and 790 °C. At the highest irradiation temperature (1130 °C), dislocation loops were no longer observed, while larger but less dense voids remained. Re and Os segregation to void surfaces was evident at 790 °C and 1130 °C, though no precipitation was observed. In contrast, under the mixed-spectrum condition, both spherical and needle-like Re/Os-rich precipitates were observed, frequently accompanied by large voids. Dislocation loops were not observed, but loop-like contrast within the precipitates suggests they may have nucleated on pre-existing loops. Irradiation-induced hardening was assessed for the shielded samples at 570 °C and 790 °C. Dispersed barrier hardening (DBH) analysis, based on TEM-resolved defects, revealed that voids were the dominant contributors to hardening, consistent with literature results. A schematic model is proposed to describe defect and precipitate evolution in tungsten under fusion-relevant transmutation-to-dpa conditions.

Dislocation loops↗

Inorganic polymers from alkali activation of metakaolin: Effect of setting and curing on structure

Geopolymers, obtained by chemical reaction between aluminosilicate oxides and silicates under highly alkaline conditions, are studied in this paper. The proposed mechanism of geopolymer setting and hardening or curing consists of a dissolution, a transportation or an orientation, as well as a polycondensation step. The aim of this paper is to investigate the influence of the curing time and temperature, the relative humidity and the reagents temperature on the geopolymerization process in order to obtain a resistant matrix usable for inertization of hazardous wastes. The evolution of the process from the precursors dissolution to final geopolymer matrix hardening has been followed by FTIR spectroscopy, X-ray diffractometry, SEM/EDS and leaching tests. The results show the significant influence of both curing temperature in the curing stage and of the mould materials on the matrix stability. The easy-to-run preparation procedure for a chemically stable metakaolin geopolymer individuated can be summarized as reagents setting and curing at room temperature and material mould which permits moisture level around 40%. - Graphical abstract: Chemical stability as a function of curing conditions. Highlights: ► Metakaolin in highly alkaline solutions produced solid materials at room temperature. ► Curing time and temperature, relative humidity, reagents temperature were optimized. ► Leaching tests were used to confirm final hardening. ► FTIR spectroscopy, SEM analysis and X-ray diffractometry were used to interpret matrix stability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A facile electron microscopy method for measuring precipitate volume fractions in AlCuMg alloys

Precipitate volume fraction is an important parameter to estimate the strength of precipitation-hardened metals. In this study, a facile method was applied to measure the precipitate volume fractions in an age-hardened AlCuMg alloy. In this method, the precipitate volume fraction values can be obtained by multiplying the volume precipitate number densities with the averaged precipitate volumes, which can be easily measured in scanning electron microscopy and transmission electron microscopy, respectively. Compared with the conventional method, in which the specimen thickness has to be measured in transmission electron microscopy, the method proposed in this study is more facile to perform. - Highlights: Black-Right-Pointing-Pointer We have proposed a facile method to measure precipitate volume fractions for precipitation-hardened metals. Black-Right-Pointing-Pointer This technique works well for the square-shaped {theta} Prime -phase nano-precipitates in 2xxx aluminum alloys. Black-Right-Pointing-Pointer Interesting is that the proposed method is easy for materials scientists and engineers to perform.

36 MATERIALS SCIENCE↗