Pitting Corrosion of Supermartensitic Stainless Steel in Chloride Solutions Containing Thiosulfate or H{sub 2}S

Deepwater oil and gas extraction environment have high salinity, low oxygen content, and the presence of carbon dioxide and hydrogen sulfide (H{sub 2}S). Handling of H{sub 2}S-containing gaseous mixtures should be carried out in laboratories with special installations, owing to the high toxicity of this gas. An alternative is the use of non-toxic substances that can generate H{sub 2}S in the medium, such as sodium thiosulfate. The objective of this work is to study the viability of substituting H{sub 2}S by thiosulfate for the evaluation of the susceptibility to pitting corrosion in sour environments of the supermartensitic stainless steel (SMSS). The electrochemical behavior of SMSS in NACE TM0177-2016 solution C solution containing different concentrations of H{sub 2}S or thiosulfate ions at 10{sup −3} mol/L was performed by using cyclic potentiodynamic polarization (CPP). The condition of shorter OCP time (300 s) prevents the formation of a passive layer and allows the generation of H{sub 2}S due to the reaction of the solution with the metal surface. The CPP curves of SMSS in the media containing 3% H{sub 2}S/Ar (2.96 kPa) and 10{sup −3} M of thiosulfate ions (OCP 300 s) were similar, the pitting potential was about − 322.5 ± 8.7 and − 338.8 ± 11.4 mV{sub Ag/AgCl}, respectively, and the pit morphology showed several small pits on the steel surface in both conditions, suggesting the viability of the use of thiosulfate-containing brines to simulate H{sub 2}S solutions.

36 MATERIALS SCIENCE↗

Corrosion Fatigue Behaviors of Type 316 LN Cold-Worked Stainless Steels in Acidified Chloride Environment

The effect of cold work (CW) on the microstructure and corrosion fatigue (CF) resistance of 316 LN stainless steel (SS) using microscopic, electrochemical and surface analytical methods was investigated. The CF resistance increases with CW. The fractographs revealed that the crack growth zone was minimum for the base metal as compared to CW SS. Fatigue-tested sample revealed a slip offset was high for as-received, while not much significant difference for 5 and 20% CW SS at low mean stress levels. The presence of NH{sub 4} improved passivity by the formation of nitrate ions that inhibits anodic dissolution.

36 MATERIALS SCIENCE↗

Investigation of Corrosion of 304 Stainless, Inconel 625, and Haynes 230 in a Chloride-Salt-Based Thermal Storage Medium

One of the critical challenges for latent heat thermal energy storage systems in concentrating solar power applications is corrosion of metallic alloys as containment and heat transfer fluid tube materials in corrosive salts at high temperatures. In this study, the effects of MgCl 2 on the corrosion of stainless steel 304, Inconel 625, and Haynes 230 alloys were investigated through embedded metal samples in the graphite foam/MgCl 2 storage medium. Four experimental testing modules were fabricated, and experimental tests were conducted under controlled environment by heating the testing modules to and keeping them at 750 °C for 100, 200, 500, and 1000 h. The estimated corrosion rates based on the weight losses for stainless steel 304, Inconel 625, and Haynes 230 were 94, 9, and 8 μm/year, respectively. The fitted equations for the loss of the thickness as functions of the exposure time show that the corrosion rates decrease with the exposure time. Additionally, the results on the corrosion zones or depths and chromium segregation ranges of the experimental samples are also presented.

36 MATERIALS SCIENCE↗

Zirconium chloride molecular species: combining electron impact mass spectrometry and first principles calculations

Zirconium tetrachloride was synthesized from the reaction between zirconium metal and chlorine gas at 300 °C and was analyzed by electron impact mass spectrometry (EI-MS). Substantial fragmentation products of ZrCl 4 were observed in the mass spectra, with ZrCl 3 being the most abundant species, followed by ZrCl 2 , ZrCl, and Zr. The predicted geometry and kinetic stability of the fragments previously mentioned were investigated by density functional theory (DFT) calculations. Here, energetics of the dissociation processes support the most stable fragment to be ZrCl 3 while the least abundant are ZrCl and ZrCl 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solubility of U(VI) in chloride solutions. II. The stable oxides/hydroxides in alkaline KCl solutions: Thermodynamic description and relevance in cementitious systems

In this study, the solubility of U(VI) is investigated from undersaturation conditions in 0.1, 0.51, 1.03, 3.31 and 4.58 m KCl–KOH solutions at pHm = 7.5–14.6 (with pH m = –log [H + ] in molal units). All experiments were performed under Ar atmosphere at T = (22 ± 2)°C. XRD, quantitative chemical analysis, SEM–EDS and TG–DTA confirm that K 2 U 2 O 7 ·1.5H 2 O(cr) is the solid phase controlling the solubility in all evaluated systems at pH m ≥ 9.5. Below this pH m and with decreasing KCl concentration, the formation of sub-stoichiometric phases with K:U < 1 is indicated by XRD and solubility data. The concentration of uranium in equilibrium with K 2 U 2 O 7 ·1.5H 2 O(cr) shows a pH-independent behaviour up to pH m ≈ 11 regardless of ionic strength, whereas an increase of the solubility with a well–defined slope of +1 (log [U] vs. pH m ) is observed at pH m ≥11. These results are consistent with the predominance of UO 2 (OH) 3 – and UO 2 (OH) 4 2- species as previously reported in the literature. The combination of solubility data obtained in the present study with K 2 U 2 O 7 ·1.5H 2 O(cr) and the U(VI) hydrolysis scheme reported in Altmaier et al. (2017) yields a solubility product of log *K° s ,0{0.5K 2 U 2 O 7 ·1.5H 2 O(cr)} = (12.0 ± 0.2). SIT ion interaction coefficients for UO 2 (OH) 3 – and UO 2 (OH) 4 2- with K + are derived based on the newly generated experimental data in dilute to concentrated KCl systems and analogy with NaCl systems. This work extends the thermodynamic database available for U(VI) and allows more accurate source term calculations in the context of nuclear waste disposal under boundary conditions where significant K concentrations may be present and redox conditions lie in the stability field of U(VI). Finally, the K 2 U 2 O 7 ·1.5H 2 O(cr) solid phase can be considered to control the solubility of U(VI) in the degradation phase I of cement and cementitious materials.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗