At least 919 records · Page 51

An investigation of the optical properties and water splitting potential of the coloured metallic perovskites Sr{sub 1−x}Ba{sub x}MoO{sub 3}

The solid solution Sr{sub 1−x}Ba{sub x}MoO{sub 3} (x=0.00, 0.025, 0.050, 0.075, 0.100 and 1.00) has been synthesised. Rietveld refinement of X-ray diffraction data shows that all materials crystallise with cubic (Pm-3m) symmetry and that a miscibility gap exists from x=0.1–1.0. The optical properties of the metallic perovskites Sr{sub 1−x}Ba{sub x}MoO{sub 3} have been investigated by a combination of UV–vis spectroscopy and density functional theory (DFT). Upon increasing x from 0 to 1 in Sr{sub 1−x}Ba{sub x}MoO{sub 3} there is a reduction in the measured band gap from 2.20 eV to 2.07 eV. The measured band gap is attributed to the electronic transition from the Mo 4d t{sub 2g} band to the e{sub g} band. The potential of SrMoO{sub 3} and BaMoO{sub 3} as water-splitting photocatalysts was explored but there was no evidence of hydrogen or oxygen evolution, even with the presence of a Pt co-catalyst. - Graphical abstract: Ultraviolet–visible absorbance spectra (converted from diffuse reflectance spectra) for SrMoO{sub 3} and BaMoO{sub 3}. - Highlights: • The solid solution Sr{sub 1-x}Ba{sub x}MoO{sub 3} has been synthesised. • A miscibility gap exists from x=0.1–1.0 in Sr{sub 1−x}Ba{sub x}MoO{sub 3.} • Upon increasing x from 0 to 1 in Sr{sub 1−x}Ba{sub x}MoO{sub 3} there is a reduction in the measured band gap from 2.20 eV to 2.07 eV. • The potential of SrMoO{sub 3} and BaMoO{sub 3} as water-splitting photocatalysts was explored but there was no evidence of hydrogen or oxygen evolution, even with the presence of a Pt co-catalyst.

36 MATERIALS SCIENCE↗

Equilibrium relations in the system TiO{sub 2}/V{sub 2}O{sub 5}/P{sub 2}O{sub 5} and crystal structure of a NASICON-related vanadyl(V) titanium(IV) phosphate

Vanadyl(V)-titanium-orthophosphate (V{sup V}O)Ti{sup IV}{sub 6}(PO{sub 4}){sub 9} is formed by solid state reactions in the temperature range 525{<=}{theta}{<=}780 Degree-Sign C. At higher temperature decomposition into V{sub 2}O{sub 5} and the hitherto unknown solid solution Ti(P{sub 1-x}V{sub x}){sub 2}O{sub 7} (0{<=}x{<=}0.23; 0.30{<=}x{<=}0.43) is observed. The process of phase formation has been monitored by MAS-NMR ({sup 31}P, {sup 51}V) spectroscopy. Equilibrium phase relations in the quaternary system TiO{sub 2}/VO{sub 2.5}/PO{sub 2.5} have been determined. A structure analysis from X-ray single-crystal data (P6{sub 3}/m (No. 176), Z=2; a=8.4438(3) A, c=22.215(1) A, 14 independent atoms, 87 variables, 2066 unique reflections, R1=0.032, wR2=0.084) shows the relationship of (V{sup V}O)Ti{sup IV}{sub 6}(PO{sub 4}){sub 9} to the NASICON structure family. In marked contrast to the other members of this family [Ti{sup IV}{sub 2}O{sub 9}] double-octahedra and strongly distorted tetrahedral [(V{sup V}=O)O{sub 3}] groups are observed besides isolated [Ti{sup IV}O{sub 6}] octahedra and phosphate tetrahedra. The structure model is in agreement with the results from MAS-NMR ({sup 31}P, {sup 51}V) spectroscopy. - Graphical abstract: (V{sup V}O)Ti{sup IV}{sub 6}(PO{sub 4}){sub 9} belongs to the NASICON structure family. Its structure contains [Ti{sup IV}{sub 2}O{sub 9}] double-octahedra and unprecedented, strongly distorted tetrahedral [(V{sup V}=O)O{sub 3}] groups, in stark contrast to other members of this family. The structure model is in agreement with the results from MAS-NMR ({sup 31}P, {sup 51}V) spectroscopy. Highlights: Black-Right-Pointing-Pointer Equilibrium relations for the subsolidus have been established for the system TiO{sub 2}/V{sub 2}O{sub 5}/P{sub 2}O{sub 5}. Black-Right-Pointing-Pointer Phase formation has been monitored by XRPD as well as by {sup 31}P- and {sup 51}-MAS-NMR. Black-Right-Pointing-Pointer A solid solution Ti(P{sub 1-x}V{sub x}){sub 2}O{sub 7} exists up to x=0.43 with a miscibility gap at 0.23{<=}x{<=}0.30. Black-Right-Pointing-Pointer The crystal structure of the new NASICON-related phosphate (V{sup V}O)Ti{sup IV}{sub 6}(PO{sub 4}){sub 9} is reported. Black-Right-Pointing-Pointer The crystal structure contains the unprecedented [(V=O)O{sub 3}] group.

36 MATERIALS SCIENCE↗

Thermophysical properties of laser-sintered Zr-ZrB2 cermets

Thermophysical properties between 293 and 1863 K were investigated for laser-sintered Zr-ZrB{sub 2} cermets containing 30, 50, and 70 wt% Zr. The measured values of coefficient of thermal expansion of Zr-ZrB{sub 2} cermets were larger than the predicted values due to the effect of Zr-O solid solution, which was formed during laser sintering. The order-disorder phase transition of Zr-O solid solution resulted in the sharp increase in heat capacity between 625 and 675 K. Thermal conductivities were calculated from measured densities, heat capacities, and thermal diffusivities. Thermal diffusivities at 473 K were 14.0, 12.2, and 8.0 mm{sup 2}/s for 30Zr-ZrB{sub 2}, 50Zr-ZrB{sub 2}, and 70Zr-ZrB{sub 2}, respectively. Thermal conductivities at 473 K were 38, 31, and 20 W {center_dot} (m {center_dot} K){sup -1} for 30Zr-ZrB{sub 2}, 50Zr-ZrB{sub 2}, and 70Zr-ZrB{sub 2}, respectively. Electron contribution to thermal conductivity of the 70Zr-ZrB{sub 2} cermet was determined using electrical resistivity measurements, which shows that total thermal conductivity mostly came from the electron contribution at high temperatures (1073-1473 K) while the phonon contribution was very small.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

The isothermal section of Gd–Ni–Si system at 1070 K

The Gd–Ni–Si system has been investigated at 1070 K by X-ray and microprobe analyses. The existence of the known compounds, i.e.: GdNi{sub 10}Si{sub 2}, GdNi{sub 8}Si{sub 3}, GdNi{sub 5}Si{sub 3}, GdNi{sub 7}Si{sub 6}, GdNi{sub 6}Si{sub 6}, GdNi{sub 4}Si, GdNi{sub 2}Si{sub 2}, GdNiSi{sub 3}, Gd{sub 3}Ni{sub 6}Si{sub 2}, GdNiSi, GdNiSi{sub 2}, GdNi{sub 0.4}Si{sub 1.6}, Gd{sub 2}Ni{sub 2.35}Si{sub 0.65}, Gd{sub 3}NiSi{sub 2}, Gd{sub 3}NiSi{sub 3} and Gd{sub 6}Ni{sub 1.67}Si{sub 3}, has been confirmed. Moreover, five new phases have been identified in this system. The crystal structure for four of them has been determined: Gd{sub 2}Ni{sub 16−12.8}Si{sub 1−4.2} (Th{sub 2}Zn{sub 17}-type), GdNi{sub 6.6}Si{sub 6} (GdNi{sub 7}Si{sub 6}-type), Gd{sub 3}Ni{sub 8}Si (Y{sub 3}Co{sub 8}Si-type) and Gd{sub 3}Ni{sub 11.5}Si{sub 4.2}(Gd{sub 3}Ru{sub 4}Ga{sub 12}-type). The compound with composition ~Gd{sub 2}Ni{sub 4}Si{sub 3} still remains with unknown structure. Quasi-binary phases, solid solutions, were detected at 1070 K to be formed by the binaries GdNi{sub 5}, GdNi{sub 3}, GdNi{sub 2}, GdNi, GdSi{sub 2} and GdSi{sub 1.67}; while no appreciable solubility was observed for the other binary compounds of the Gd–Ni–Si system. Magnetic properties of the GdNi{sub 6}Si{sub 6}, GdNi{sub 6.6}Si{sub 6} and Gd{sub 3}Ni{sub 11.5}Si{sub 4.2} compounds have also been investigated and are here reported. - Graphical abstract: The Gd–Ni–Si system has been investigated at 1070 K by X-ray and microprobe analyses. The known GdNi{sub 10}Si{sub 2}, GdNi{sub 8}Si{sub 3}, GdNi{sub 5}Si{sub 3}, GdNi{sub 7}Si{sub 6}, GdNi{sub 6}Si{sub 6}, GdNi{sub 4}Si, GdNi{sub 2}Si{sub 2}, GdNiSi{sub 3}, Gd{sub 3}Ni{sub 6}Si{sub 2}, GdNiSi, GdNiSi{sub 2}, GdNi{sub 0.4}Si{sub 1.6}, Gd{sub 2}Ni{sub 2.35}Si{sub 0.65}, Gd{sub 3}NiSi{sub 2}, Gd{sub 3}NiSi{sub 3} and Gd{sub 6}Ni{sub 1.67}Si{sub 3} compounds have been confirmed and five new ~Gd{sub 2}Ni{sub 4}Si{sub 3} (unknown type), Gd{sub 2}Ni{sub 16−12.8}Si{sub 1−4.2} (Th{sub 2}Zn{sub 17}-type), GdNi{sub 6.6}Si{sub 6} (GdNi{sub 7}Si{sub 6}-type), Gd{sub 3}Ni{sub 8}Si (Y{sub 3}Co{sub 8}Si-type) and Gd{sub 3}Ni{sub 11.5}Si{sub 4.2} (Gd{sub 3}Ru{sub 4}Ga{sub 12}-type) compounds have been detected in Gd–Ni–Si system at 1070 K. Quasi-binary phases, solid solutions, were detected at 1070 K to be formed by the binaries GdNi{sub 5}, GdNi{sub 3}, GdNi{sub 2}, GdNi, GdSi{sub 2} and GdSi{sub 1.67}; while no detectable solubility was observed for the other binary compounds of the Gd–Ni–Si system. Magnetic properties of the GdNi{sub 6}Si{sub 6}, GdNi{sub 6.6}Si{sub 6} and Gd{sub 3}Ni{sub 11.5}Si{sub 4.2} compounds have also been investigated and are here reported. - Highlights: • Gd–Ni–Si isothermal section was obtained at 1070 K. • Sixteen known ternary gadolinium nickel silicides were confirmed in Gd–Ni–Si. • Five new gadolinium nickel silicides were detected in Gd–Ni–Si. • GdNi{sub 6}Si{sub 6}, GdNi{sub 6.6}Si{sub 6} and Gd{sub 3}Ni{sub 11.5}Si{sub 4.2} show ferromagnetic-type ordering.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In Situ TEM for Structural and Chemical Evolutions of Bimetallic Pt–Ni Nanoparticles at Elevated Temperatures: Implications for Heterogeneous Catalysis

Platinum-based bimetallic nanoparticles (NPs) are of great interest for their applications in catalysis. The catalytic properties of these NPs are significantly dependent on their morphology, structure, and composition, whose response to thermal input remains challenging to be fully understood. This study investigates the thermally induced structural and chemical evolutions of single-crystalline Pt-Ni NPs using in situ transmission electron microscopy. The observed morphological evolution includes the facet development from a truncated octahedron to a spherical-like isotropic shape, followed by the formation of pancake-like ellipsoid shape at high temperatures due to surface atom migration and interfacial wetting enabled by the particle-substrate interaction. Comparative investigations by in situ scanning transmission electron microscopy with energy dispersive X-ray spectroscopy mapping elucidate that the solid-solution compositional configuration can be retained over a large temperature range, while core-shell NPs undergo irreversible solid-solution transitions through chemical homogenization at elevated temperatures. Finally, these findings elucidate the effect of thermal input on structural evolution and compositional redistribution of Pt-Ni bimetallic NPs, offering valuable insights into the design of heterogeneous catalysts.

25 ENERGY STORAGE↗

Structural evolution, sintering behavior and microwave dielectric properties of (1−x)Li{sub 2}TiO{sub 3} + xLiF ceramics

Graphical abstract: - Highlights: • Structure, sinterability and dielectric properties of LiF-doped Li{sub 2}TiO{sub 3} were studied. • Li{sub 2}TiO{sub 3} can be densitied (TD 98%) at lower sintering temperature by LiF additions. • Excellent microwave dielectric properties could be obtained. - Abstract: Structural evolution, sintering behavior, and microwave dielectric properties of (1−x)Li{sub 2}TiO{sub 3} + xLiF (0.05 ≤ x ≤ 0.70) ceramics have been studied by X-ray diffraction (XRD), Scanning Electron Microscopy (SEM), Raman spectra, thermal dilatometry and microwave resonant measurement at the frequency of about 7–11 GHz. The results show that Li{sub 2}TiO{sub 3} can form limited solid solution with LiF (x ≤ 0.4) and LiF second phase appeared when x{sup 3}0.5. The structure of the solid solution transformed from ordered monoclinic phase (β-Li{sub 2}TiO{sub 3} (ss)) to disordered cubic rock salt (α-Li{sub 2}TiO{sub 3} (ss)) when x{sup 3}0.15. The presence of short range ordering was confirmed for the cubic phase. The sinterability was considerably improved by doping with LiF. Densified ceramics with about 95–98% theoretical density could be obtained for the doped compositions after sintering at 900–1150 °C/2 h. An optimized microwave dielectric properties with ε{sub r} of ∼23.6, Q × f of ∼108,000 GHz and τ{sub f} of ∼4.2 ppm/°C could be obtained for the x = 0.1 composition after sintering at 1100 °C/2 h.

36 MATERIALS SCIENCE↗

Study of the intermediate layer at the n{sup +}-CdS/p-CdTe interface

The effect of production conditions and subsequent stimulation by ultrasonic irradiation on the formation of a solid solution at the n-CdS/p-CdTe interface in solar cells has been investigated. The phase composition of the solid-solution transient layer was investigated by a nondestructive photoelectric method (measurement of the spectral distribution of photosensitivity in the gate and photodiode modes). It is shown that the phase composition and thickness of the intermediate CdTe{sub 1-x}S{sub x} layer depend strongly on the heterostructure formation conditions.

36 MATERIALS SCIENCE↗

Nucleation of Pre-precipitates in Structural Materials under Cascade-Forming Irradiation

A model is proposed to calculate pre-precipitate nucleation rate in supersaturated solid solutions under cascade-forming irradiation. Estimates of the rate of nucleation of copper-enriched clusters in Fe–Cu solid solutions with a copper concentration of 0.05–0.18 at. % due to reactor irradiation are carried out. A comparison with the experimental data on irradiation of structural materials shows that the formation of precipitate nuclei takes place in the cascade region involved at the final stages of cascade relaxation, whose volume is about two times higher than the cascade volume at the dynamic stage.

36 MATERIALS SCIENCE↗

Aluminum doped zirconia nanopowders: Wet-chemical synthesis and structural analysis by Rietveld refinement

Alumina/zirconia nanopowders, with up to 20 mol% Al{sub 2}O{sub 3}, were prepared by wet-chemical synthesis technique, using controlled hydrolysis of alkoxides. The as-synthesized powders are amorphous, have very high specific surface area and the corresponding particle size smaller than 4 nm. Amorphous powders with 0, 10 and 20 mol% Al{sub 2}O{sub 3} crystallize at 460, 692 and 749 deg. C, respectively, as a single-phase tetragonal zirconia, without any traces of alumina phases. Rietvled refinement of X-ray diffraction data, used for the detailed structural analysis of annealed nanopowders, showed that the high-temperature zirconia phase is stabilized due to the formation of ZrO{sub 2}/Al{sub 2}O{sub 3} solid solutions. High solubility of alumina in the tetragonal zirconia (up to 28.6 at% Al{sup 3+}) and stabilization of tetragonal zirconia solid solution up to high temperature (as high as 1150 deg. C) were also confirmed.

36 MATERIALS SCIENCE↗

Co-precipitation of yttrium and barium fluorides from aqueous solutions

Highlights: ► BaF{sub 2}–YF{sub 3} system has been studied under the non-equilibrium ambient conditions. ► Ba{sub 1−x}Y{sub x}F{sub 2+x} (x = 0.35–0.75) solid solution phase has cubic fluorite-type structure. ► Ba{sub 1−x}Y{sub x}F{sub 2+x} cubic crystal lattice parameter a{sub 0} does not change monotonously. ► Different types of lattice defects determine a dependency from sample composition. ► (H{sub 3}O{sup +})Y{sub 3}F{sub 10}{sup −}·nH{sub 2}O phase precipitates from HF aqueous solutions instead of YF{sub 3}·nH{sub 2}O. -- Abstract: Co-precipitation of barium and yttrium fluorides from aqueous solutions at room temperature produced non-equilibrium Ba{sub 1−x}Y{sub x}F{sub 2+x} nanofluoride phase with face-centered cubic crystal lattice of fluorite-type with the composition interval of the homogeneity for x = 0.35–0.75. Lattice parameter a of this solid solution nanophase varied as a function of the sample chemical composition in a complex manner with two areas of linear dependency, from x = 0.35 to 0.45 and from x = 0.50 to 0.75. A plausible explanation of this phenomenon included a change of the type of crystal lattice defects and the manner of their population with the corresponding ions. An increase of the relative amount of yttrium in the HF reaction system led to the formation of hydroxonium salt of decafluorotriyttrium acid, (H{sub 3}O{sup +})Y{sub 3}F{sub 10}{sup −}·nH{sub 2}O, instead of expected YF{sub 3} hydrate. No formation of oxyfluoride phases under acidic conditions has been observed.

36 MATERIALS SCIENCE↗

Fine structure of Fe-Co-Ga and Fe-Cr-Ga alloys with low Ga content

Investigation of Ga influence on the structure of Fe-Cr and Fe-Co alloys was performed with the use of {sup 57}Fe Mössbauer spectroscopy and X-ray diffraction methods. In the alloys of the Fe-Cr system, doping with Ga handicaps the decomposition of solid solutions, observed in the binary alloys, and increases its stability. In the alloys with Co, Ga also favors the uniformity of solid solutions. The analysis of Mössbauer experiments gives some grounds to conclude that if, owing to liquation, clusterization, or initial stages of phase separation, there exist regions enriched in iron, some amount of Ga atoms prefer to enter the nearest surroundings of iron atoms, thus forming binary Fe-Ga regions (or phases)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tunable Magnetic Transition to a Singlet Ground State in a 2D van der Waals Layered Trimerized Kagomé Magnet

Incorporating magnetism into two-dimensional (2D) van der Waals (vdW) heterostructures is crucial for the development of functional electronic and magnetic devices. Here, we show that Nb 3 X 8 (X = Cl, Br) is a family of 2D layered trimerized kagomé magnets that are paramagnetic at high temperatures and undergo a first-order phase transition on cooling to a singlet magnetic state. X-ray diffraction shows that a rearrangement of the vdW stacking accompanies the magnetic transition, with high- and low-temperature phases consistent with scanning transmission electron microscopy images of the end members α-Nb 3 Cl 8 and β-Nb 3 Br 8 . The temperature of this transition is systematically varied across the solid solution Nb 3 Cl 8–x Br x (x = 0–8), with x = 6 having transitions near room temperature. Furthermore, the solid solution also varies the optical properties, which are further modulated by the phase transition. As such, they provide a platform on which to understand and exploit the interplay between dimensionality, magnetism, and optoelectronic behavior in vdW materials.

2D materials↗

Temperature dependence, 0 to 40 deg. C, of the mineralogy of Portland cement paste in the presence of calcium carbonate

Thermodynamic calculations disclose that significant changes of the AFm and AFt phases and amount of Ca(OH){sub 2} occur between 0 and 40 deg. C; the changes are affected by added calcite. Hydrogarnet, C{sub 3}AH{sub 6}, is destabilised at low carbonate contents and/or low temperatures < 8 deg. C and is unlikely to form in calcite-saturated Portland cement compositions cured at < 40 deg. C. The AFm phase actually consists of several structurally-related compositions which form incomplete solid solutions. The AFt phase is close to its ideal stoichiometry at 25 deg. C but at low temperatures, < 20 deg. C, extensive solid solutions occur with CO{sub 3}-ettringite. A nomenclature scheme is proposed and AFm-AFt phase relations are presented in isothermal sections at 5, 25 and 40 deg. C. The AFt and AFm phase relations are depicted in terms of competition between OH, CO{sub 3} and SO{sub 4} for anion sites. Diagrams are presented showing how changing temperatures affect the volume of the solid phases with implications for space filling by the paste. Specimen calculations are related to regimes likely to occur in commercial cements and suggestions are made for testing thermal impacts on cement properties by defining four regimes. It is concluded that calculation provides a rapid and effective tool for exploring the response of cement systems to changing composition and temperature and to optimise cement performance.

36 MATERIALS SCIENCE↗

Structure, luminescence and thermal quenching properties of Eu doped Sr{sub 2−x}Ba{sub x}Si{sub 5}N{sub 8} red phosphors

Eu{sup 2+} doped Sr{sub 2-x}Ba{sub x}Si{sub 5}N{sub 8} phosphors were synthesized at 1610 ℃ for 4 h via the solid-state reaction method. The XRD results confirm that the complete solid solutions are formed. With the increase of x, the emission spectra show an obvious blue-shift from 610 nm to 585 nm under the excitation of 460 nm. The color tone can be tuned from yellow to red. The corresponding mechanism for the blue-shift of peak-wavelength is studied in detail. The results of decomposed Gaussian spectra and fluorescence lifetime show that the local coordination structure surrounding activator ions changes with increasing x value. It is found that the probability of Eu occupying Sr1 and Sr2 site is dependent on Ba/Sr ratio. The variation of thermal quenching properties and the corresponding mechanism is discussed in detail. The results indicate that Eu{sup 2+} doped Sr{sub 2-x}Ba{sub x}Si{sub 5}N{sub 8} is a promising orange red-emitting phosphor for near UV or blue light-pumped white light-emitting-diodes (wLEDs). - Graphical abstract: Eu{sup 2+} doped Sr{sub 2-x}Ba{sub x}Si{sub 5}N{sub 8} solid solutions were prepared by the solid-state reaction method. The structure, luminescence and thermal quenching properties with varying Ba/Sr ratio were investigated in detail. - Highlights: • The stucture and luminescence properties of Eu doped Sr{sub 2-x}Ba{sub x}Si{sub 5}N{sub 8} phosphors were investigated. • The samples with the intermediate compositions(x=1.0,1.5) show better stability than the end members of both Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+} and Ba{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+}. • The possible mechanism for the improvement of thermal quenching properties was proposed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fabrication and microstructural characterization of Al/Zn-enriched layers on pure magnesium

Al/Zn-enriched surface layers were fabricated by heating Mg specimens in contact with Al–Zn powder mixtures in a vacuum furnace at 445 °C. The layer formation process took place through partial melting at the Mg-substrate/powder-mixture interface. Heating times ranged from 20 to 80 min. The layer microstructure and composition were analyzed by optical microscopy (OM), scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). The layers were 100–900 μm in thickness, depending on the treatment time. The examination results revealed that the layers consisted of Mg{sub 17}(Al,Zn){sub 12} and Mg{sub 5}Al{sub 2}Zn{sub 2} intermetallic phases and a solid solution of Al and Zn in Mg. Between the Al/Zn-enriched layer and the Mg substrate, there was a transition zone of a solid solution of Al and Zn in Mg with a thickness of 20–30 μm. The layers had much higher microhardness than the Mg substrate. - Highlights: ► The layers were produced by heating Mg in contact with an Al–Zn powder mixture. ► The layer formation process at 445 °C proceeded with the liquid phase contribution. ► The Al/Zn-enriched layers were thick, dense, uniform and continuous. ► The layers contained Mg–Al–Zn intermetallic phases. ► The hardness of the layers was much higher than that of the Mg substrate.

36 MATERIALS SCIENCE↗

Investigation of surface potential in the V-defect region of MBE Cd{sub x}Hg{sub 1−x}Te film

Atomic-force microscopy is used to investigate the distribution of the contact-potential difference (surface potential) in Cd{sub x}Hg{sub 1−x}Te epitaxial films grown by molecular-beam epitaxy. Modification of the solid-solution composition near the V-defect results in a variation in the contact-potential difference. It is shown that the solid-solution composition varies by ∼0.05 (2.5 at %) towards increasing mercury content in the V-defect region, and a region of mercury depletion by 0.36 at % is observed at the V-defect periphery. From analysis of the surface-potential distribution, it is shown that the Cd{sub x}Hg{sub 1−x}Te epitaxial film contains unform V-defects with a diameter less than 1 μm in addition to macroscopic V-defects.

36 MATERIALS SCIENCE↗

Thermal Properties in the MgAl2O4-Al2O3 System

Compositional effects on the thermal diffusivity in the MgAl2O4-Al2O3 system were studied. The lowest thermal diffusivity, 0.0258 +/-5% cm/s, was measured between 79.8 and 83.9 wt% Al2O3 quenched from various temperatures between 1500 and 1700C. All of the chemistries in this range extend past the solvus, but still form a singe super-saturated spinel solid solution, regardless of quenching tempeature. A super-saturated metastable solid solution region was observed at 1500, 1600, and 1700C extending to 83.9, 85.2, and 87.1 wt% Al2O3, respectively. Beyond 83.9% Al2O3 a significant increase in thermal diffusivity, 11.7%, was observed and its attributed to precipiation of Al2O3 through spinodal decomposition.

Wilkerson, Dr. Kelley R.↗