Effects of heat treating PM Rene' 95 slightly below the gamma-prime solvus

An investigation was performed on As-HIP Rene' 95 to obtain additional information on the variation of the amount of gamma-prime with solutioning temperatures near the gamma-prime solvus temperature and the resulting effects on tensile and stress rupture strengths of As-HIP Rene' 95. The amount of gamma-prime phase was found to increase at a rate of about 0.5% per degree Celsius as the temperature decreased from the solvus temperature to about 50 C below the gamma-prime solvus temperature. The change in the amount of gamma-prime phase with decreasing solutioning temperature was observed to be primarily associated with decreasing solubilities of Al+Ti+Nb and increasing solubility of Cr in the gamma phase. For As-HIP Rene' 95 solutioned at either 1107 or 1135 C and subsequently water-quenched and double aged for 4 hours at 815 C followed by 24 hours at 650 C, the higher solution temperature resulted in significantly greater yield strengths at room temperature and 650 C as well as a greater room-temperature ultimate strength. Also, longer stress rupture lives at 650 C were associated with the higher solution temperature.

Dreshfield, R. L.↗

Flexibilized copolyimide adhesives

Two copolyimides, LARC-STPI and STPI-LARC-2, with flexible backbones were processed and characterized as adhesives. The processability and adhesive properties were compared to those of a commercially available form of LARC-TPI. Lap shear specimens were fabricated using adhesive tape prepared from each of the three polymers. Lap shear tests were performed at room temperature, 177 C, and 204 C before and after exposure to water-boil and to thermal aging at 204 C for up to 1000 hours. The three adhesive systems possess exceptional lap shear strengths at room temperature and elevated temperatures both before and after thermal exposure. LARC-STPI, because of its high glass transition temperature provided high lap shear strengths up to 260 C. After water-boil, LARC-TPI exhibited the highest lap shear strengths at room temperature and 177 C, whereas the LARC-STPI retained a higher percentage of its original strength when tested at 204 C. These flexible thermoplastic copolyimides show considerable potential as adhesives based on this study and because of the ease of preparation with low cost, commercially available materials.

Progar, Donald J.↗

Electrical de-poling and re-poling of relaxor-PbTiO 3 piezoelectric single crystals without heat treatment

Re-poling of unexpected partially depoled piezoelectric materials conventionally needs to be first fully depoled through annealing above their Curie temperature to revive piezoelectric performances. Here, we investigated de-poling and re-poling of Pb(In 1/2 Nb 1/2 )O 3 -Pb(Mg 1/3 Nb 2/3 )O 3 -PbTiO 3 single crystals under electric fields at room temperature. We found that alternating current electric fields with amplitudes near the coercive field at low frequencies (<10 Hz) can be employed to successfully depolarize poled crystals at room temperature. We also demonstrated a reversible polarization switching process with a relaxor-PbTiO 3 single crystal ultrasound transducer without device performance degradations. This experimental observation is supported by phase-field simulation, showing that alternating current electric fields can readily induce de-poling at room temperature, while direct current electric fields induce a transient depoled state only within an uncontrollable short period of time. The findings suggest new strategies for unprecedented in-device tailoring of the polarization states of ferroelectric materials.

36 MATERIALS SCIENCE↗

High Temperature Resistant Organopolysiloxane Coating for Protecting and Repairing Rigid Thermal Insulation

Ceramics are protected from high temperature degradation, including high temperature, oxidative, aeroconvective degradation by a high temperature and oxidation resistant coating of a room temperature curing, hydrolyzed and partially condensed liquid polyorganosiloxane to the surface of the ceramic. The liquid polyorganosiloxane is formed by the hydrolysis and partial condensation of an alkyltrialkoxysilane with water or a mixture of an alkyltrialkoxysilane and a dialkyldialkoxysilane with water. The liquid polyorganosiloxane cures at room temperature on the surface of the ceramic to form a hard, protective, solid coating which forms a high temperature environment, and is also used as an adhesive for adhering a repair plug in major damage to the ceramic. This has been found useful for protecting and repairing porous, rigid ceramics of a type used on reentry space vehicles.

Leiser, Daniel B.↗

Fabrication and evaluation of cold/formed/weldbrazed beta-titanium skin-stiffened compression panels

The room temperature and elevated temperature buckling behavior of cold formed beta titanium hat shaped stiffeners joined by weld brazing to alpha-beta titanium skins was determined. A preliminary set of single stiffener compression panels were used to develop a data base for material and panel properties. These panels were tested at room temperature and 316 C (600 F). A final set of multistiffener compression panels were fabricated for room temperature tests by the process developed in making the single stiffener panels. The overall geometrical dimensions for the multistiffener panels were determined by the structural sizing computer code PASCO. The data presented from the panel tests include load shortening curves, local buckling strengths, and failure loads. Experimental buckling loads are compared with the buckling loads predicted by the PASCO code. Material property data obtained from tests of ASTM standard dogbone specimens are also presented.

Royster, D. M.↗

Magnetic flux trapping in hydrogen-rich high-temperature superconductors

Recent discoveries of superconductivity in various hydrides at high pressures have shown that a critical temperature of superconductivity can reach near-room-temperature values. However, experimental studies are limited by high-pressure conditions, and electrical transport measurements have been the primary technique for detecting superconductivity in hydrides. Here we implement a non-conventional protocol for the magnetic measurements of superconductors in a SQUID magnetometer and probe the trapped magnetic flux in two near-room-temperature superconductors H 3 S and LaH 10 at high pressures. Contrary to traditional magnetic susceptibility measurements, the magnetic response from the trapped flux is almost unaffected by the background signal of the diamond anvil cell due to the absence of external magnetic fields. The behaviour of the trapped flux generated under zero-field-cooled and field-cooled conditions proves the existence of superconductivity in these materials. We reveal that the absence of a pronounced Meissner effect is associated with the very strong pinning of vortices inside the samples. This approach can also be a tool for studying multiphase samples or samples that have a low superconducting fraction at ambient pressure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Temperature on Thrombogenicity Testing of Biomaterials in an In Vitro Dynamic Flow Loop System

To develop and standardize a reliable in vitro dynamic thrombogenicity test protocol, the key test parameters that could impact thrombus formation need to be investigated and understood. In this study, we evaluated the effect of temperature on the thrombogenic responses (thrombus surface coverage, thrombus weight, and platelet count reduction) of various materials using an in vitro blood flow loop test system. Whole blood from live sheep and cow donors was used to assess four materials with varying thrombogenic potentials: negative-control polytetrafluoroethylene (PTFE), positive-control latex, silicone, and high-density polyethylene (HDPE). Blood, heparinized to a donor-specific concentration, was recirculated through a polyvinyl chloride tubing loop containing the test material at room temperature (22–24°C) for 1 hour, or at 37°C for 1 or 2 hours. The flow loop system could effectively differentiate a thrombogenic material (latex) from the other materials for both test temperatures and blood species ( p < 0.05). However, compared with 37°C, testing at room temperature appeared to have slightly better sensitivity in differentiating silicone (intermediate thrombogenic potential) from the relatively thromboresistant materials (PTFE and HDPE, p < 0.05). These data suggest that testing at room temperature may be a viable option for dynamic thrombogenicity assessment of biomaterials and medical devices.

Engineering↗

Thermal expansion of 4H and 6H SiC from 5 K to 340 K

The first thermal expansion measurements of the 4H and 6H polytypes of SiC below room temperature are reported. The measurements were carried out on single-crystal specimens using high-resolution capacitive-based dilatometry. For both polytypes, the thermal expansion coefficient is below 2.4 × 10 -6 1/K near room temperature. No phase transitions are observed over the 5 K to 340 K temperature range of the measurements. The thermal expansion coefficient α of 4H SiC is slightly anisotropic for measurements parallel and perpendicular to the crystallographic c axis with α ∥ about 2.2 × 10 -7 1/K larger than α ⟂ near room temperature. For 6H SiC no discernible anisotropy is observed. The differences in anisotropy can be understood by considering the ratio of hexagonal to cubic bonds of each polytype. Narrow regions with negative thermal expansion that are within the limits of our resolution (~ 1 x 10 -8 ) are observed in the vicinity of 30 K for both specimens. In conclusion, tabulated data, polynomial fits, fit parameters, and comparison to data based on lattice-parameter measurements are provided.

36 MATERIALS SCIENCE↗

Processing and Mechanical Properties of NiAl-Based In-Situ Composites

In-situ composites based on the NiAl-Cr eutectic system were successfully produced by containerless processing and evaluated. The NiAl-Cr alloys had a fibrous microstructure while the NiAl-(Cr,Mo) alloys containing 1 at. percent or more molybdenum exhibited a lamellar structure. The NiAl-28Cr-6Mo eutectic displays promising high temperature strength while still maintaining a reasonable room temperature fracture toughness when compared to other NiAl-based materials. The Laves phase NiAlTa was used to strengthen NiAl and very promising creep strengths were found for the directionally solidified NiAl-NiAlTa eutectic. The eutectic composition was found to be near NiAl-15.5Ta (at. percent) and well aligned microstructures were produced at this composition. An off-eutectic composition of NiAl-14.5Ta was also processed, consisting of NiAl dendrites surrounded by aligned eutectic regions. The room temperature toughness of these two phase alloys was similar to that of polycrystalline NiAl even with the presence of the brittle Laves phase NiAlTa. Polyphase in-situ composites were generated by directional solidification of ternary eutectics. The systems investigated were the Ni-Al-Ta-X (X=Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and both the eutectic composition and temperature were determined. Of these ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr,Al)NiTa-Cr eutectic was intermediate between those of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, David Ray↗

Structural Phase Transitions in the van der Waals Ferromagnets Fe x Pd y Te 2

Two-dimensional van der Waals (vdW) magnets are attracting significant attention, both as platforms for studying fundamental magnetic interactions and for the exciting possibility of utilizing them as building blocks in devices and heterostructures, which may lead to new physical phenomena and functionalities. Here, we provide a detailed study of the crystal structure and physical properties of the recently discovered vdW ferromagnet FePd 2 Te 2 . We find this compound has a relatively wide width of formation, and grow single crystals with compositions Fe x Pd y Te 2 where x ranges from 0.9 to 1.1 and y from 1.8 to 2.5, respectively. Temperature-dependent X-ray diffraction and transport measurements reveal that a first-order structural transition occurs in the range of T = 360–420 K, where the critical temperature, modulation wave vector, and corresponding room-temperature crystal structures all depend on chemical composition. Above the transition, the compounds with Pd fraction y > 2 adopt a disordered derivative of the tetragonal FeTe structure, with the Fe layer showing mixed Fe/Pd occupancy and the extra Pd atoms partially occupying interstitial sites. Below 370 K, the structure is incommensurately modulated, likely associated with the complex ordering of Pd/Fe atoms in the metal layers or the interstitial Pd in the vdW gaps. For y < 2, the composition Fe 1.1 Pd 1.8 Te 2 has monoclinic symmetry at room temperature that is consistent with the reported structure of FePd 2 Te 2 . This phase undergoes a structural transition at 420 K for which the high temperature structure is yet to be determined; however, based on the similarities with the y > 2 compounds, we speculate that its T > 420 K structure is also tetragonal. Importantly, the high temperature, symmetry-breaking structural transition observed here provides a likely explanation for the origin of the structural domains previously observed in FePd 2 Te 2 . All compounds investigated in the Fe x Pd y Te 2 series show metallic behavior, with magnetic characterization indicating that they are easy-plane, hard, ferromagnets with T C spanning 98–180 K. Both the critical temperature for the structural transition and the Curie temperature are moderately suppressed with increasing Pd fraction y and corresponding decreasing Fe fraction x, indicating that synthetic control over x and y paves way for the further exploration of these compounds.

crystal structure↗

Wear Potential Due to Low EHD Films During Elevated Temperatures

An earlier study showed that EHD films could be accurately measured in a running bearing and that the EHD film eventually runs-in to a steady state value [1]. In the present paper, we report on additional tests conducted on bearings with more lubricants, wider speeds, and higher temperatures. The new results consistently show that all lubricants tested, including MAC-based lubricants have EHD film levels that are lower than model predictions in some situations. In addition, the MAC lubricants studied have lower film thickness than traditional hydrocarbons. Figure 1 is taken from [1] and shows room temperature data of MAC oil and Corey 100 oil, illustrating the smaller EHD film results when using this MAC oil. Since higher temperatures produce lower films by changing the viscosity, the concern we have is that the EHD films may be too small to prevent ball/race metal contact and resulting wear at lower speeds. Best bearing practices would have the EHD film thickness be at least three (3) times the composite surface roughness. In this paper, we will present measured EHD thicknesses of lubricant films at speeds up to several thousand RPM for bearing bore sizes from as low as 6 mm (0.2 in) to as large as 35 mm (1.4 in) using MAC, Corey and KG-80. Ambient temperatures from room temperature to 52C (125F) are used. Testing was done with the base oils as well as formulated greases. Greases eventually ran in to the same EHD values as the base oil but took longer times to get there. The results clearly indicate that wear is very possible in all steel bearings when using MAC lubricants and that this condition worsens with higher temperatures and smaller bearing size.

Leville, Alan↗

A turnkey gaseous helium-cooled superconducting CORC ® dc power cable with integrated current leads

Abstract High-temperature superconducting (HTS) direct current (dc) power cable systems, capable of delivering power exceeding 10 MW while being cooled with cryogenic helium gas, have been developed for applications on naval electric ships, electric aircraft and in data centers. Current injection from room temperature into the superconducting power cable causes by far the greatest heat load to the cryogenic system. Efficient current leads with integrated helium gas heat exchangers were developed to inject a current exceeding 1 kA from room temperature into a superconducting Conductor on Round Core (CORC ® ) power cable, without the need for liquid nitrogen pre-cooling. A 2 m long single-pole CORC ® power cable system that included current leads was cooled using a Stirling cryocooler with a closed-loop helium gas circulation system. The turnkey power cable system allowed cool down from room temperature to its operating temperature of 60 K–70 K within 5 h, after which continuous operation at 1.2 kA was demonstrated. The successful development and demonstration of a CORC ® power cable with current leads containing integrated helium gas heat exchangers enables widespread implementation of HTS MW-class, high current density superconducting dc power cables in many applications with constrained space that require a power dense solution.

Physics↗

Performance and Stability Characterization of the ICARUS Light Detection System

The ICARUS detector, a key component of the Short Baseline Neutrino (SBN) Program at Fermilab, consists of two identical T300 modules filled with liquid argon. It is equipped with a Light Detection System (LDS) based on 360 8-inch Hamamatsu R5912-MOD photomultiplier tubes (PMTs) arranged behind the wire planes to collect Vacuum Ultraviolet (VUV, $\sim$ 128 nm) scintillation light. Operating under cryogenic conditions ( $\sim$ 87 K), the LDS is essential for determining the event start time (t0) with nanosecond precision for beam spill synchronization, improving longitudinal spatial resolution, and contributing to the event trigger and cosmic-ray mitigation. The performance of the LDS was investigated addressing both hardware and data analysis aspects. Following a progressive degradation in PMT gain observed during operations at FNAL, systematic gain measurements were first carried out from room temperature down to low temperatures. The results show stable performance at room temperature but a significant, irreversible reduction in gain at low temperatures. Based on these findings, a series of mitigation strategies were implemented in the ICARUS detector to preserve PMT performance and ensure reliable cryogenic operation. Currently, ongoing waveform analysis of the PMT signals is being performed to characterize signal shape, charge integration, and timing properties, aiming to refine and improve the agreement between experimental data and Monte Carlo simulations.

Saia, Clara [U. Catania (main); INAF, Catania; Cat↗

Influences of chemical and thermal environments on delay in a Ti-6Al-4V alloy

Experiments were conducted within the framework of linear fracture mechanics to study the effects of chemical and thermal environments on crack-growth retardation (delay) in mill-annealed Ti-6Al-4V alloy under elemental load spectra. Attention is focused on the influence of hold time at high load on delay in a 3.5 percent NaCl solution at room temperature. It is shown that delay is strongly affected by hold time at high load, where delay is longest if the high-load excursion occurs at high temperature and the subsequent fatigue is at room temperature, and shortest if the temperature profile is reversed. The results suggest that residual stresses ahead of the advancing crack play an important role in delay. The significance of combined load and environment (chemical and thermal) effects in terms of modeling and life prediction procedures is discussed.

Shih, T. T.↗

Lamination residual strains and stresses in hybrid laminates

An investigation is conducted of the effects of hybridization on the magnitude of lamination residual stresses. Eight-ply graphite/Kevlar 49/epoxy and graphite/S-glass/epoxy laminates were studied. The same matrix resin was selected for all basic materials to ensure compatibility and uniform curing of the various plies. The specimens, with inserted strain gages and thermocouples, were subjected to curing and postcuring cycles in an autoclave. Subsequently, the specimens were subjected to a thermal cycle from room temperature to 444 K and down to room temperature. It was found that hydridizing reduces apparently residual strains and stresses in the graphite plies. However, these strains were not affected much by the type and degree of hybridization.

Daniel, I. M.↗

RF Sputtering of Gold Contacts On Niobium

Reliable gold contacts are deposited on niobium by combination of RF sputtering and photolithography. Process results in structures having gold only where desired for electrical contact. Contacts are stable under repeated cycling from room temperature to 4.2 K and show room-temperature contact resistance as much as 40 percent below indium contacts made by thermalcompression bonding.

Barr, D. W.↗

Subpicosecond time-resolved studies of coherent phonon oscillations in thin-film YBa2Cu3O(6+x) (x less than 0.4)

The results are reported of the first time-resolved observation of impulsively generated coherent optical phonon oscillations in the semiconducting cuprate compound YBa2Cu3O(6+x ) (x less than 0.4). The oscillations, which were probed through time-resolved transmissivity modulation, had a period of 237 fsec at room temperature, corresponding to a Raman active mode at A(1g) symmetry at 142/cm. No oscillations were observed in the superconducting form of Y-Ba-Cu-O either above or below Tc. The amplitude, frequency, and linewidth of this mode were measured over a temperature range from about 7 K to room temperature.

Chwalek, J. M.↗

SiC (SCS-6) Fiber Reinforced-Reaction Formed SiC Matrix Composites: Microstructure and Interfacial Properties

Microstructural and interfacial characterization of unidirectional SiC (SCS-6) fiber reinforced-reaction formed SiC (RFSC) composites has been carried out. Silicon-1.7 at.% molybdenum alloy was used as the melt infiltrant, instead of pure silicon, to reduce the activity of silicon in the melt as well as to reduce the amount of free silicon in the matrix. Electron microprobe analysis was used to evaluate the microstructure and phase distribution in these composites. The matrix is SiC with a bi-modal grain-size distribution and small amounts of MoSi2, silicon, and carbon. Fiber push-outs tests on these composites showed that a desirably low interfacial shear strength was achieved. The average debond shear stress at room temperature varied with specimen thickness from 29 to 64 MPa, with higher values observed for thinner specimens. Initial frictional sliding stresses showed little thickness dependence with values generally close to 30 MPa. Push-out test results showed very little change when the test temperature was increased to 800 C from room temperature, indicating an absence of significant residual stresses in the composite.

Singh, M.↗