Modeling degradation and failure of Ni-Cr-Al overlay coatings

Degradation of a Ni-16Cr-25Al-0.06Zr overlay coating on a Ni-22Cr substrate was examined after oxidation accompanied by thermal cycling. Concentration/distance profiles were measured in the coating and substrate after various one-hour cycles at 1150 C. A numerical model was developed to simulate coating degradation by simultaneous oxidation and coating/substrate interdiffusion. The validity of the model was confirmed by comparison of predicted and measured concentration/distance profiles. The ability of the model to identify critical system parameters was demonstrated for the case of initial Al and Cr content of the coating and substrate.

Nesbitt, J. A.↗

Coverage dependent effects on metal surfaces - O, S, F, and Cl on Ni

The c(2 x 2) and p(2 x 2) vibrational frequencies for a rigid Ni lattice are computed for O, S, F, and Cl on Ni(100). It is found that only O/Ni(100) shows a large difference in rigid lattice vibrational frequency. A large shift in rigid lattice vibrational frequency is also found for O/Ni(111) between 0.25 and 0.5 monolayer coverages. Also associated with the change in coverage, is a change in the height above the surface R(perpendicular). This varies from a 0.11 A reduction for O/Ni(100), to an expansion of 0.06 A for F/Ni(100).

Bauschlicher, C. W., Jr.↗

Optimization of the Ni-Cr-Al-Y/ZrO2-Y2O3 thermal barrier system

The effects of bond and thermal barrier coating compositions, thicknesses, and densities on air plasma spray deposited Ni-Cr-Al-Y/ZrO2-Y2O3 life were evaluated in cyclic furnace oxidation tests at temperatures from 1110 to 1220 C. An empirical relation was developed to give life as a function of the above parameters. The thermal barrier system tested which had the longest life consisted of Ni-35.0 wt pct Cr-5.9 wt pct Al-0.95 wt pct Y bond coating and ZrO2-6.1 wt pct Y2O3 thermal barrier coating.

Stecura, S.↗

Recent advances in Ni-H2 technology at NASA Lewis Research Center

The NASA Lewis Research Center has concentrated its efforts on advancing the Ni-H2 system technology for low Earth orbit applications. Component technology as well as the design principles were studied in an effort to understand the system behavior and failure mechanisms in order to increase performance and extend cycle life. The design principles were previously addressed. The component development is discussed, in particular the separator and nickel electrode and how these efforts will advance the Ni-H2 system technology.

Gonzalezsanabria, O. D.↗

High temperature tensile and creep behaviour of low pressure plasma-sprayed Ni-Co-Cr-Al-Y coating alloy

The high temperature tensile and creep behavior of low pressure plasma-sprayed plates of a typical Ni-Co-Cr-Al-Y alloy has been studied. From room temperature to 800 K, the Ni-Co-Cr-Al-Y alloy studied has nearly a constant low ductility and a high strength. At higher temperatures, it becomes weak and highly ductile. At and above 1123 K, the behavior is highly dependent on strain rate and exhibits classic superplastic characteristics with a high ductility at intermediate strain rates and a strain rate sensitivity of about 0.5. At either higher or lower strain rates, the ductility decreases and the strain rate sensitivities are about 0.2. In the superplastic deformation range, the activation energy for creep is 120 + or - 20 kJ/mol, suggesting a diffusion-aided grain boundary sliding mechanism. Outside the superplastic range, the activation energy for creep is calculated to be 290 + or - 20 kJ/mol.

Hebsur, M. G.↗

Test summary for advanced H2 cycle NI-CD cell

To improve operational tolerances and mass, the H2 gas recombination design provisions of the Ni-H2 system were incorporated into the sealed Ni-Cd system. Produced is a cell design capable of operating on the H2 cycle versus the normal O2 cycle. Three test cells have now completed approximately 4,330 LEO (90 minute) cycles at 20 percent depth of discharge (DOD). Performance remains stable although one cell exhibited a temporary pressure anomaly.

Miller, Lee↗

The effect of variations of cobalt content on the cyclic oxidation resistance of selected Ni-base superalloys

Cobalt levels were systematically varied in the Ni-base turbine alloys U-700 (cast), U-700m (PM/HIP), Waspaloy, Mar-M-247, In-738, Nimonic-115, U-720, and SX-R-150. the cobalt levels ranged from 0 wt pct to the nominal commercial content in each alloy. the alloys were tested in cyclic oxidation in static air at 1000, 1100 and 1150 C for 500, 200, and 100 hr, respectively. An oxidation attack parameter, Ka, derived from the specific weight change versus time data was used to evaluate the oxidation behavior of the alloys along with X-ray diffraction analysis of the surface oxides. The alloys tend to form either Cr2O3/chromite spinel or Al2O3/aluminate spinel depending on the Cr/Al ratio in the alloys. Alloys with a ratio of 3.5 or higher tend to favor the Cr oxides while those under 3.0 form mostly Al oxides. In general the Al2O3/aluminate spinel forming alloys have the better oxidation resistance. Increased cobalt content lowers the scaling resistance of the higher Cr allys while a 5.0 wt pct Co content is optimum for the Al controlling alloys. The refractory metals, particularly Ta, appear beneficial to both types of oxides, perhaps due to the formation of the omnipresent trirutile Ni(Ta, Cb, Mo, W)2O6. Both scales break down as increasing amounts of NiO are formed.

Barrett, Charles A.↗

Crystallization behavior of a melt-spun Fe-Ni based steel

Whether Fe-Ni-based alloys solidify with a bcc or fcc structure has been observed by many investigators to be a stronger function of kinetics and undercooling than strictly free-energy minimization. Such behavior has been observed in an Fe(52.8)Ni(28.7)Al(3.4)Ti(6.1)B(9.0) alloy. The alloy was cast as ribbons about 45 microns thick using a dual free-jet variation of chillbock melt spinning against a Cu wheel. Optical, X-ray, and electron analyses of the as-cast and annealed ribbons were performed. A microstructure of at least four layers containing combinations of ecc, bcc, and amorphous phases in differing proportions was observed in the as-cast ribbon. The midthickness layer had the most unusual features, containing fcc grains about 75 nm in size encompassing spherulitic regions as large as 15 microns comprised of fcc grains about 25 nm in size. The crystallization sequence responsible for the as-cast microstructure is discussed in terms of the competition between the formation of bcc and fcc phases as influenced by undercooling, recalescence, and variations in cooling rate experienced by the as-cast ribbon.

Michal, G. M.↗

Predicting diffusion paths and interface motion in gamma/gamma + beta, Ni-Cr-Al diffusion couples

A simplified model has been developed to predict Beta recession and diffusion paths in ternary gamma/gamma + beta diffusion couples (gamma:fcc, beta: NiAl structure). The model was tested by predicting beta recession and diffusion paths for four gamma/gamma + beta, Ni-Cr-Al couples annealed for 100 hours at 1200 C. The model predicted beta recession within 20 percent of that measured for each of the couples. The model also predicted shifts in the concentration of the gamma phase at the gamma/gamma + beta interface within 2 at. pct Al and 6 at. pct Cr of that measured in each of the couples. A qualitative explanation based on simple kinetic and mass balance arguments has been given which demonstrates the necessity for diffusion in the two-phase region of certain gamma/gamma + beta, Ni-Cr-Al couples.

Nesbitt, J. A.↗

Cosmic-ray energy spectra between 10 and several hundred GeV per atomic mass unit for elements from Ar-18 to Ni-28 - Results from HEAO 3

Results from the Heavy Nuclei experiment on HEAO 3 are used to determine the primary abundances of Ni and Fe. Ni and Fe are found to have nearly constant relative abundances over the interval of 10 to about 500 GeV per amu. Individual secondary elements derived principally from interactions of primary Fe nuclei are shown to display a power-law decrease in relative abundance up to about 150 GeV per amu. Ar/Fe and Ca/Fe ratios of 2.6 + or - 0.7 percent and 8.8 + or - 0.7 percent, respectively, are found, confirming a fractionation of source abundances in which elements with high values of the first ionization potential are depleted relative to those with low first ionization potential.

Binns, W. R.↗

The application of electrochemical impedance spectroscopy for characterizing the degradation of Ni(OH)2/NiOOH electrodes

The use of wide-band electrochemical impedance spectroscopy is described for characterizing the degradation of porous Ni(OH)2/NiOOH electrodes in concentrated KOH electrolyte solutions. The impedance spectra are interpreted in terms of a finite electrical transmission line and the changes in the components of the electrical analog are followed as a function of cycle number. The degradation of the capacity of rolled and bonded Ni(OH)2/NiOOH electrodes is caused by rupture of ohmic contacts within the active mass and by restructuring which results in a decrease in the number of active pores.

Macdonald, Digby D.↗

Ordering in the Fe-Ni system under electron irradiation

The disorder-order transformation was generated in a range of Fe-Ni alloys using 1 MeV electrons in a high voltage electron microscope. The experimental factors that influence the occurrence of the transformation were determined, and the critical disordering temperature, Tc, was determined as a function of composition. It was demonstrated that the irradiation enhanced the ordering reaction kinetics. A metastable, ordered phase transformation was not induced. From the results, it is possible to deduce new information about the Fe-Ni phase diagram below 350 C.

Reuter, K. B.↗

A study of microstructural characteristics of Ni-based superalloys at high temperatures

The microstructural characteristics of the Ni-based superalloy MAR-M245(Hf) which is used in manufacturing the components of the Space Shuttle main engine are studied. These superalloys need optimum heat treatment to get the best results. To find out the optimum heat treatment, the techniques of differential thermal analysis (DTA) and the optical photomicrographs were utilized. In the first phase, the existing experimental equipment like cutting, grinding/polishing machines and metallurgical microscope were set up to cut/polish and take the photomicrographs. In the beginning of the project a Perkin Elmer differential thermal analyzer DTA1700 along with a temperature programmed and the needed computer interface was procured and made operational. In the second year a Leitz Metallux-3 hot state research microscope was also procured and installed for in-situ observation of the superalloy samples. The hot stage when tested for the first time alloyed the thermocouple with the Tantalum heating element and has now been installed. Samples of MAR-M246(Hf), MAR-M247, Waspaloy, Udimet-41, CMSX-3, and CMSX-3 (Polycrystalline and single crystals) were studied using a differential thermal analyzer and the results are reported. Photomicrographs of the Ni-based superalloy MAR-M246 (Hf) were recorded before and after heat treatment at certain temperatures. More heat treatments need to be done before a final inference can be reached.

Lal, Ravindra B.↗

Small capacity, low cost (Ni-H2) design concept for commercial, military, and higher-volume aerospace applications

Nickel-Hydrogen (Ni-H2) batteries have become the technology of choice for both commercial and defense-related satellites in geosynchronous orbits. Their use for low-earth- orbit (LEO) applications is not as advanced, but seems just as inevitable because of their inherent advantages over nickel-cadmium batteries. These include superior energy density, longer cycle life, and better tolerance to over-charge and reversal. Ni-H2 cells have the added advantage in both construction and operation of not presenting the environmental possibility of cadmium pollution. Unfortunately, but necessarily, the design of these cells has been driven to high cost by the sophistication of the satellites and their uses. Now, using most of the same concepts but less costly materials and techniques, a low-cost, small cell design has been developed. Combined with the concept of the common pressure vessel, this new design promises to be ideal for the "small-sat" and commercial markets which, increasingly, are calling for large numbers of less-expensive satellites.

James R Wheeler↗

Static compression of iron to 300 GPa and Fe(0.8)Ni(0.2) alloy to 260 GPa - Implications for composition of the core

Results are reported on a room temperature static compression study of iron and the Fe(0.8)Ni(0.2) alloy to above 260 GPa, which provide direct pressure-volume measurements on geophysically important materials at the conditions close to those at the inner core boundary. The diffraction patterns obtained by XRD indicate that pure iron remains in the hcp structure to 304 GPa and that Fe(0.8)Ni(0.2) is stable to at least 255 GPa. The results of this study, in conjunction with work at higher temperatures, will make it possible to address directly the question of the composition of the inner core with a level of certainty that were previously applicable only to the mantle.

Mao, H. K.↗

1000 to 1200 K time-dependent compressive deformation of single-crystalline and polycrystalline B2 Ni-40Al

The 1000-K and 1200-K time-dependent deformation of 100-line-oriented and non-100-line-oriented single crystals of Ni-40Al (made by a modified Bridgman technique) was examined over a large range of strain rates (from 0.1 to 10 to the -7th per sec). The results were compared with those for polycrystalline Ni-40Al made by hot pressing XD synthesized powder. The results from measurements of slow-plastic-strain-rate properties of the two materials show that single crystals offer no strength advantage over polycrystalline material. Both forms were found to deform via a dislocation climb mechanism.

Whittenberger, J. D.↗

Life evaluation of 35Ah Ni-Cd cell in Japan

The National Space Development Agency of Japan (NASDA) began developing Nickel-Cadmium (Ni-Cd) cells for space use in 1985. Sanyo Electric was responsible for the cell design, manufacturing, and initial testing. The cell life was evaluated by NASDA in the Tsukuba Space Center (TKSC). The development is presently in the qualification Test (QT) phase. Recent life-cycle data for 35 Ah Ni-Cd cells are presented.

Kuwajima, S.↗

A statistical analysis of elevated temperature gravimetric cyclic oxidation data of 36 Ni- and Co-base superalloys based on an oxidation attack parameter

A large body of high temperature cyclic oxidation data generated from tests at NASA Lewis Research Center involving gravimetric/time values for 36 Ni- and Co-base superalloys was reduced to a single attack parameter, K(sub a), for each run. This K(sub a) value was used to rank the cyclic oxidation resistance of each alloy at 1000, 1100, and 1150 C. These K(sub a) values were also used to derive an estimating equation using multiple linear regression involving log(sub 10)K(sub a) as a function of alloy chemistry and test temperature. This estimating equation has a high degree of fit and could be used to predict cyclic oxidation behavior for similar alloys and to design an optimum high strength Ni-base superalloy with maximum high temperature cyclic oxidation resistance. The critical alloy elements found to be beneficial were Al, Cr, and Ta.

Barrett, Charles A.↗