A path-dependent fatigue crack propagation model under non-proportional modes I and III loading conditions

It has been well established that fatigue damage process is load-path dependent under non-proportional multi-axial loading conditions. Most of studies to date have been focusing on interpretation of S-N based test data by constructing a path-dependent fatigue damage model. Our paper presents a two-parameter mixed-mode fatigue crack growth model which takes into account of crack growth dependency on both load path traversed and a maximum effective stress intensity attained in a stress intensity factor plane (e.g.,KI-KIII plane). Furthermore, by taking advantage of a path-dependent maximum range (PDMR) cycle definition (Dong et al., 2010; Wei and Dong, 2010), the two parameters are formulated by introducing a moment of load path (MLP) based equivalent stress intensity factor range (ΔKNP) and a maximum effective stress intensity parameter KMax incorporating an interaction term KI·KIII. To examine the effectiveness of the proposed model, two sets of crack growth rate test data are considered. The first set is obtained as a part of this study using 304 stainless steel disk specimens subjected to three combined non-proportional modes I and III loading conditions (i.e., with a phase angle of 0°, 90°, and 180°). The second set was obtained by Feng et al. (2007) using 1070 steel disk specimens subjected to similar types of non-proportional mixed-mode conditions. Once the proposed two-parameter non-proportional mixed-mode crack growth model is used, it is shown that a good correlation can be achieved for both sets of the crack growth rate test data.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Irradiation-assisted cracking of SA508-304L weldments with 308L groove filler and 309L butter in hot water immersion constant rate extension tests

Low alloy SA508 bainitic steel is often welded to 300 series austenitic stainless steel in nuclear power plants. These dissimilar metal weldments use 309L butter applied to the low alloy steel and 308L groove filler material to join the 309L to austenite. High alloy steels (such as the 308L and 309L material used here) have been identified as having greater susceptibility to irradiation-assisted stress corrosion cracking (IASCC). Evidence is presented here of cracking under tensile loads in 309L weldment butter in LWR hydrothermal conditions that correlates irradiation induced changes at δ ferrite–γ austenite phase boundaries and γ–γ grain boundaries; specifically intergranular Cr 23 C 6 precipitates. Cracking is not observed in irradiated 308L groove filler under the same conditions. Both the 309L butter and 308L filler material have a duplex or mixed δ–γ phase microstructure due to solidification during the welding procedure. We have performed constant extension rate autoclave immersion tests in BWR normal water chemistry hot water (288 °C, 10 MPa, 2000 wt. ppb dissolved oxygen, <100 nS/cm conductivity, neutral pH) of proton irradiated (2 MeV, approximately 3 displacements per atom at a depth of 10 μm) tensile specimens. Proton irradiation to the dpa levels used here induced Cr 23 C 6 carbide precipitation at γ–γ grain boundaries and δ–γ phase boundaries in the 309L butter but not the 308L filler. Cracking was observed in the proton-irradiated volume of 309L at these interfaces in the vicinity of the Cr 23 C 6 precipitates. We hypothesis the SA508 is the source of carbon in the 309L butter. Cr depletion at γ–γ grain boundaries was also observed and may also be a root cause of cracking. Furthermore, the 309L butter is under significant tensile residual stress in the weldment that adds to applied tensile loads and this too may be a contributing factor.

309L weld butter↗

Electron backscatter diffraction characterization of fatigue crack growth in laser metal wire deposited Ti-6Al-4V

Highlights: • No difference in fatigue crack growth rate was confirmed within the material. • The tortuosity of the crack propagation could be related to the alpha colonies. • Large areas with similar crystallographic orientation were observed. - Abstract: By additive manufacturing (AM) there is a feasibility of producing near net shape components in basically one step from 3D CAD model to final product. The interest for AM is high and during the past decade a lot of research has been carried out in order to understand the influence from process parameters on the microstructure and furthermore on the mechanical properties. In the present study laser metal wire deposition of Ti-6Al-4V has been studied in detail with regard to its fatigue crack propagation characteristics. Two specimen orientations, parallel and perpendicular to the deposition direction, have been evaluated at room temperature and at 250 °C. No difference in the fatigue crack growth rate could be confirmed for the two specimen orientations. However, in the fractographic study it was observed that the tortuosity varied between certain regions on the fracture surface. The local crack path characteristic could be related to the alpha colony size and/or the crystallographic orientation. Moreover, large areas exhibiting similar crystallographic orientation were observed along the prior beta grain boundaries, which were attributed to the wide alpha colonies frequently observed along the prior beta grain boundaries.

36 MATERIALS SCIENCE↗

Effect of grain boundary character distribution on weld heat-affected zone liquation cracking behavior of AISI 316Ti austenitic stainless steel

Highlights: • Grain boundary engineered AISI 316 was produced through thermomechanical processing. • Grain boundary engineering resulted in random high angle boundary network disruption. • Liquation cracks are arrested at triple junctions having one or more CSL boundaries. • Grain boundary engineering resulted in improvement in liquation cracking resistance. - Abstract: In this work, the role of grain boundary engineering (GBE) on the weld heat-affected-zone (HAZ) liquation cracking resistance of austenitic stainless steel AISI 316Ti was investigated. Standard wrought-processed alloy 316Ti was cold rolled to 5% strain and subsequently annealed at 1373 K for 30 min to achieve the optimum grain boundary character distribution (GBCD). The GBE samples were found to consist of a significantly higher fraction (72%) of low Ʃ coincident site lattice (CSL) boundaries as compared to the as received (AR) samples (45%). To study the liquation cracking behavior, single-track longitudinal varestraint tests was performed on AR and GBE samples. Microstructural examination revealed that the grain coarsening and the liquation events were less prominent in the GBE samples as compared to the AR samples. It is believed that the reduced segregation of impurities to the special boundaries (coherent Ʃ3 twins, in particular) present in the GBE samples is responsible for the observed improvement in the HAZ liquation cracking resistance.

36 MATERIALS SCIENCE↗

Dislocation arrangements within slip bands during fatigue cracking

Highlights: • Dislocation cells form near early slip bands fatigue cracks in wavy-slip materials. • Lattice rotates severely and grain boundaries form between neighboring cells. • The walls of dislocation cells are preferential sites for fatigue cracking. - Abstract: Microstructures and dislocations associated with the slip band (SB) fatigue cracks were investigated in Cu single crystal and bicrystal. It is found that there are high strain localizations with abundant dislocation cells around the cracked SBs. Due to the high local strain and slip irreversibility, the lattice rotates severely leading to large misorientation and hence low- or high- angle grain boundaries could form between the neighboring cells. Moreover, the dislocation walls can serve as preferential sites for nucleation and propagation of fatigue cracks with high density of dislocations, vacancies and high strain incompatibility.

36 MATERIALS SCIENCE↗

Acoustic emission monitoring of crack propagation in additively manufactured and conventional titanium components

We report that additive manufacturing (AM) is a novel and innovative production technology that can produce complex and lightweight engineering products. In AM components, as in all engineering materials, fatigue is considered as one of the principle causes of unexpected failure. In order to detect, localise and characterise cracks in various material components and metals, acoustic emission (AE) is used as a non-destructive monitoring technique. One of the main advantages of AE is that it can be also used for dynamic damage characterisation and specifically for crack propagation monitoring. In this research, we use AE to monitor the fatigue crack growth behaviour of Ti6Al4V components under four-point bending. The samples were produced by means of AM as well as conventional material. Notched and unnotched specimens were investigated with respect to the crack severity and crack detection using AE. The main AE signal parameters –such as cumulative events, hits, duration, average frequency and rise time– were evaluated and indicate sensitivity to damage propagation in order to lead to a warning against the final fracture occurrence. Finally, this is the first time that AE is applied in AM components under fatigue.

36 MATERIALS SCIENCE↗

Cracking of simulated oil refinery off-gas over a coal char, petroleum coke, and quartz

The cracking of oil refinery off-gas, simulated with a gas mixture containing methane (51%), ethylene (21.4%), ethane (21.1%), and propane (6.5%), over a coal char, petroleum coke, and quartz, respectively, has been studied in a fixed bed reactor. The experiments were performed at temperatures between 850 and 1000{sup o}C and at atmospheric pressure. The results show that the conversions of all species considered increased with increasing temperature. Ethane and propane completely decomposed over all three bed materials in the temperature range investigated. However, the higher initial conversion rates of methane and ethylene cracking at all temperatures were observed only over the coal char and not on the petroleum coke and quartz, indicating a significant catalytic effect of the coal char on methane and ethylene cracking. Methane and ethylene conversions decreased with reaction time due to deactivation of the coal char by carbon deposition on the char surface and, in the later stage of a cracking experiment, became negative, suggesting that methane and ethylene had been formed during the cracking of ethane and propane. 16 refs., 13 figs., 2 tabs.

01 COAL, LIGNITE, AND PEAT↗

Self-healing of cracks in Ag joining layer for die-attachment in power devices

Sintered silver (Ag) joining has attracted significant interest in power devices modules for its ability to form stable joints with a porous interconnection layer. A function for the self-healing of cracks in sintered porous Ag interlayers at high temperatures is discovered and reported here. A crack which was prepared on a Ag joining layer was closed after heating at 200 °C in air. The tensile strength of pre-cracked Ag joining layer specimens recovers to the value of non-cracked specimens after heating treatment. Transmission electron microscopy (TEM) was used to probe the self-healing mechanism. TEM images and electron diffraction patterns show that a large quantity of Ag nanoparticles formed at the gap with the size less than 10 nm, which bridges the crack in the self-healing process. This discovery provides additional motivation for the application of Ag as an interconnection material for power devices at high temperature.

36 MATERIALS SCIENCE↗

Heat affected zone liquation cracking evaluation on FeMnAl alloys

FeMnAl steels are currently generating a lot of interest with potential applications for structural parts in armored vehicles due to their lower density and outstanding mechanical properties. Despite the extensive mechanical performance and heat treatment exploration of this alloy class, further weldability investigation is required for future large-scale deployment. In the present study, the liquation cracking of four heats of cast FeMnAl alloys was investigated by the spot-Varestraint technique. The study focuses primarily on the effect of the major elements of the FeMnAl system: C, Mn and Al. Optical and electron microscopy were employed to investigate the microstructural features, and CALPHAD was employed to aid the discussion regarding the alloy’s composition differences and their effect on the liquation cracking susceptibility. The study was able to identify that compositions with the higher Mn, C, and lower Al presented the highest liquation cracking susceptibility. Conversely, composition presenting lower Mn, C, and Al showed the most resistant behavior. Furthermore, lower Al content promoted a fully-γ microstructure at low temperatures, which encouraged the appearance of longer cracks as a γ-matrix is more susceptible to HAZ cracking than a fully ferritic (α) or duplex (α + γ) microstructure.

36 MATERIALS SCIENCE↗

Phase field modeling of crack propagation

Fracture is a fundamental mechanism of materials failure. Propagating cracks can exhibit a rich dynamical behavior controlled by a subtle interplay between microscopic failure processes in the crack tip region and macroscopic elasticity. We review recent approaches to understand crack dynamics using the phase field method. This method, developed originally for phase transformations, has the well-known advantage of avoiding explicit front tracking by making material interfaces spatially diffuse. In a fracture context, this method is able to capture both the short-scale physics of failure and macroscopic linear elasticity within a self-consistent set of equations that can be simulated on experimentally relevant length and time scales. Here, we discuss the relevance of different models, which stem from continuum field descriptions of brittle materials and crystals, to address questions concerning crack path selection and branching instabilities, as well as models that are based on mesoscale concepts for crack tip scale selection. Open questions which may be addressed using phase field models of fracture are summarized.

36 MATERIALS SCIENCE↗

Lateral cracks during sliding indentation on various optical materials

A series of static and sliding indentation (ie, scratching) was performed and characterized on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 –Al 2 O 3 –K 2 O–BaO (Phosphate)] at various applied loads using various indenters (Vickers, 10 µm conical, and 200 µm conical). Despite having different load dependencies, the lateral crack depth formed during sliding indentation quantitatively scales with that formed during static indentation, explaining why static indentation has been historically effective in describing various grinding parameters. Depending on the indenter geometry, the amount of residual trench damage (plastic deformation and local fracturing) during sliding indentation was often enhanced by more than an order of magnitude compared with static indentation. A simple ploughing scratch model, which considers both tangential and normal stresses (where the tangential stress is amplified by relatively small tangential contact area), explains this enhancement and other observed trends. Accounting for the high correlation between residual trench depth and volumetric fracturing, the model is extended to estimate the amount of fracture damage as a function of the material properties of the workpiece, indenter geometry, and applied load. Such a model has utility in the design of optimized grinding processes, particularly the abrasive geometry. Finally, at higher loads (>1 N), lateral cracks were often observed to preferentially propagate in the forward scratching direction, as opposed to perpendicular to the scratch as typically observed. High-speed imaging of the scratch process confirms that these cracks propagate ahead of the sliding indenter during the scratching event. Finite element stress analysis suggests the ploughing frictional forces increase the mode I tensile stresses at the leading edge of the sliding indenter explaining the direction of crack propagation of such cracks.

36 MATERIALS SCIENCE↗

Acoustic Emission and Guided Wave Monitoring of Fatigue Crack Growth on a Full Pipe Specimen

Continuous on-line monitoring of active and passive systems, structures and components in nuclear power plants will be critical to extending the lifetimes of nuclear power plants in the US beyond 60 years. Acoustic emission and guided ultrasonic waves are two tools for continuously monitoring passive systems, structures and components within nuclear power plants and are the focus of this study. These tools are used to monitor fatigue damage induced in a SA 312 TP304 stainless steel pipe specimen. The results of acoustic emission monitoring indicate that crack propagation signals were not directly detected. However, acoustic emission monitoring exposed crack formation prior to visual confirmation through the detection of signals caused by crack closure friction. The results of guided ultrasonic wave monitoring indicate that this technology is sensitive to the presence and size of cracks. The sensitivity and complexity of GUW signals is observed to vary with respect to signal frequency and path traveled by the guided ultrasonic wave relative to the crack orientation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Mitigating Crack Formation When Using High Oxygen Permeability Ionomer in PEMFC Catalyst Layers

High oxygen permeability ionomers (HOPIs) are being developed as an alternative to conventional perfluorosulfonic (PFSA) ionomers for cathodes in proton exchange membrane fuel cells (PEMFCs). HOPIs aim to reduce local oxygen transport resistance, improving performance and reducing degradation as the catalyst loses surface area. However, HOPIs' more rigid, 3D backbone leads to increased crack density in the cathode, potentially causing accelerated degradation. This study investigates crack formation in HOPI-based and PFSA-bound catalyst layers (CLs). We conducted a comprehensive parametric study to identify conditions and catalyst slurry components that minimize cracking. CLs were fabricated with various ionomer and catalyst types, under different relative humidity (RH) levels, solids weight percentages, solvent ratios, and ionomer-to-carbon ratios (I/C). Results show that HOPI-based CLs exhibit less cracking when fabricated under low RH conditions, with lower solids weight percentage, higher alcohol content, and lower I/C. Additionally, catalysts with low/medium surface area carbon supports show less cracking than those with high surface area carbon supports.

08 HYDROGEN↗

Stress Relaxation Cracking of Alloys at Temperatures Higher Than 540°C

Type 347H stainless steel (347H SS), used in commercial concentrating solar power (CSP) thermal energy storage to store solar-salt at a temperature of 565°C, has been reported in the literature to be susceptible to stress-relaxation cracking (SRC). The welded heat-affected zone (HAZ) and fusion zone (FZ) of 347H SS, particularly in thick sections, are known to be susceptible to failure during post-weld heat treatment (reheat cracking). SRC could also occur after months or years under an elevated-temperature service environment. Two conditions must be present for failure to occur in the HAZ and/or FZ: 1) a modified or sensitized microstructure and 2) sufficiently high tensile residual stresses present at the elevated service temperature. The overarching goal of this project is to recommend SRC mitigation protocols to avoid susceptibility to fail through SRC at temperatures relevant for CSP. Post weld heat treatment conditions and alternative alloys are investigated as potential mitigation solutions to SRC. We used Gleeble thermomechanical simulation tests and finite element (FE) models to understand the susceptibility of 347H SS to SRC as a function of temperature, stress, and microstructure. We started with a literature review of weldability issues with 347H SS and techniques to mitigate SRC in 347H SS weldments. Next, we used Gleeble experiments to determine reheat cracking susceptibility in the simulated HAZ of 347SS weldments and an alternative alloy, 316L SS (NUCL 167 SPH) with boron added. We also performed Gleeble experiments to compare the reheat cracking susceptibility of 347H cross welded with two different fillers: E347, which is used in some commercial CSP TES tanks, and E16.8.2. We validated the experimental results with FE models of the residual stresses. We found that although the 316L (NUCL 167 SPH) is less susceptible to reheat cracking, it is slightly weaker than 347H and ASME BP&V codes limit its use to a service condition of 565°C. We also found that welds using E16.8.2 as the weld filler are less susceptible to failure than those using E347, likely due to the higher creep ductility of E16.8.2, and that it may be used as an alternative filler for repair welding of 347H welds or as the primary choice of filler for newly developed weld joints. We also found that post weld heat treatment could be a viable solution for mitigating stress in E347-347H SS thick, constrained welds, like those found in CSP tanks, and propose several options for mitigating SRC in existing and future TES tanks.

14 SOLAR ENERGY↗

Towards Commercialization of Low-Cost, Crack-Tolerant, Screen-Printable Metallization by Full-Size Module Testing and Field Characterization

This project is motivated by the need to develop a materials engineering solution to reduce solar module degradation caused by cell cracks. The cell-crack-induced power loss is a long-term degradation mechanism and one of the main causes of solar panel field failures. Cell cracks can occur during module fabrication, transportation, installation, and long-term operation due to thermomechanical stressors. Our team’s internal estimation – based on the national weather pattern, frequency of severe weather, and 39- GW asset survey by Heliolytics – reveals that the cell-crack-induced module degradation translates to lost revenues >$17B over an average 5-year period for solar farm owners and to reduced reliability (<25 years panel lifetime) for solar energy consumers. In response to this challenge, the prime recipient offers a metal matrix composite (MMC) silver paste that is tailor-engineered for screen-printing gridlines and busbars, which serve as the electrical contacts on solar cells. We formulate our MMC paste by adding low-cost (∼0.02¢/WDC for research grade), surface-engineered carbon nanotubes to commercially available silver paste. The MMC paste offers a drop-in, cost-effective solution to cell cracks for solar cell and module manufacturers. The main goal of this project was to conduct field-relevant, module-level analysis and qualification of MMC metallization.

14 SOLAR ENERGY↗

Chloride-Induced Stress Corrosion Cracking of Friction Stir-Welded 304L Stainless Steel: Effect of Microstructure and Temperature

Dry storage canisters of used nuclear fuels are fabricated using SUS 304L stainless steel. Chloride-induced stress corrosion cracking (CISCC) is one of the major failure modes of dry storage canisters. The cracked canisters can be repaired by friction stir welding (FSW), a low-heat input ‘solid-phase’ welding process. It is important to evaluate the ClSCC resistance of the friction stir welded material. Stress corrosion cracking (SCC) studies were carried out on mill-annealed base materials and friction stir welded 304L stainless U-bend specimens in 3.5% NaCl + 5 N H2SO4 solution at room temperature and boiling MgCl2 solution at 155 °C. The engineering stress on the outer fiber of the FSW U-bend specimen was ~60% higher than that of the base metal (BM). In spite of the higher stress level of the FSW, both materials (FSW and BM) showed almost similar SCC failure times in the two different test solutions. The SCC occurred in the thermo-mechanically affected zone (TMAZ) of the FSW specimens in the 3.5% NaCl + 5 N H2SO4 solution at room temperature, while the stirred zone (SZ) was relatively crack-free. The failure occurred at the stirred zone when tested in the boiling MgCl2 solution. Hydrogen reduction was the cathodic reaction in the boiling MgCl2 solution, which promoted hydrogen-assisted cracking of the heavily deformed stirred zone. The emergence of the slip step followed by passive film rupture and dissolution of the slip step could be the SCC events in the 3.5% NaCl + 5 N H2SO4 solution at room temperature. However, the slip step height was not sufficient to cause passivity breakdown in the fine-grained SZ. Therefore, the SCC occurred in the partially recrystallized softer TMAZ. Overall, the friction-stirred 304L showed higher tolerance to ClSCC than the 304L base metal.

304L austenitic stainless steel↗

A Model to Account for the Effects of Load Ratio and Hydrogen Pressure on the Fatigue Crack Growth Behavior of Pressure Vessel Steels

A phenomenological model for estimating the effects of load ratio R and hydrogen pressure P H2 on the hydrogen-assisted fatigue crack growth rate (HA–FCGR) behavior in the transient and steady-state regimes of pressure vessel steels is described. The “transient regime” is identified with crack growth within a severely embrittled zone of intense plasticity at the crack tip. The “steady-state” behavior is associated with the crack growing into a region of comparatively lower hydrogen concentration located further away from the crack tip. The model treats the effects of R and P H2 as being functionally separable. In the transient regime, the effects of the hydrogen pressure on the HA–FCGR behavior were negligible but were significant in the steady-state regime. The hydrogen concentration in the steady-state region is modeled as being dependent on the kinetics of lattice diffusion, which is sensitive to pressure. Experimental HA–FCGR data from the literature were used to validate the model. The new model was shown to be valid over a wide range of conditions that ranged between –1 ≤ R ≤ 0.8 and 0.02 ≤ P H2 ≤ 103 MPa for pressure vessel steels.

36 MATERIALS SCIENCE↗

Fatigue Crack Growth Database for Damage Tolerance Analysis

The objective of this project was to begin the process of developing a fatigue crack growth database (FCGD) of metallic materials for use in damage tolerance analysis of aircraft structure. For this initial effort, crack growth rate data in the NASGRO (Registered trademark) database, the United States Air Force Damage Tolerant Design Handbook, and other publicly available sources were examined and used to develop a database that characterizes crack growth behavior for specific applications (materials). The focus of this effort was on materials for general commercial aircraft applications, including large transport airplanes, small transport commuter airplanes, general aviation airplanes, and rotorcraft. The end products of this project are the FCGD software and this report. The specific goal of this effort was to present fatigue crack growth data in three usable formats: (1) NASGRO equation parameters, (2) Walker equation parameters, and (3) tabular data points. The development of this FCGD will begin the process of developing a consistent set of standard fatigue crack growth material properties. It is envisioned that the end product of the process will be a general repository for credible and well-documented fracture properties that may be used as a default standard in damage tolerance analyses.

Metallic materials↗