Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid solutions”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 901 records · Page 50

Solubility and thermodynamic properties of oxygen in solid molybdenum

A formula is obtained for the solubility of oxygen in solid Mo, determined in the range from 1400 to 1900 C by equilibrating rods of zone-refined Mo with mixtures of Mo and MoO2 powders. Using the known value of the free energy of formation of MoO2, a formula is obtained for the chemical potential of oxygen in the dilute solid solution. The heat of solution of oxygen in solid Mo and the excess entropy for the interstitial solid solution are also determined, assuming that the oxygen atoms reside in the octahedral interstices of bcc Mo.

Srivastava, S. C.↗

High temperature regenerative H.sub.2 S sorbents

Efficient, regenerable sorbents for removal of H.sub.2 S from high temperature gas streams comprise porous, high surface area particles. A first class of sorbents comprise a thin film of binary oxides that form a eutectic at the temperature of the gas stream coated onto a porous, high surface area refractory support. The binary oxides are a mixture of a Group VB or VIB metal oxide with a Group IB, IIB or VIII metal oxide such as a film of V-Zn-O, V-Cu-O, Cu-Mo-O, Zn-Mo-O or Fe-Mo-O coated on an alumina support. A second class of sorbents consist of particles of unsupported mixed oxides in the form of highly dispersed solid solutions of solid compounds characterized by small crystallite size, high porosity and relatively high surface area. The mixed oxide sorbents contain one Group IB, IIB or VIIB metal oxide such as copper, zinc or manganese and one or more oxides of Groups IIIA, VIB or VII such as aluminum, iron or molybdenum. The presence of iron or aluminum maintains the Group IB, IIB or VIIB metal in its oxidized state. Presence of molybdenum results in eutectic formation at sulfidation temperature and improves the efficiency of the sorbent.

Flytani-Stephanopoulos, Maria↗

Phase equilibria and crystal chemistry of the CaO–1/2 Nd{sub 2}O{sub 3}–CoO{sub z} system at 885 °C in air

The phase diagram of the CaO–1/2 Nd{sub 2}O{sub 3}–CoO{sub z} system at 885 °C in air has been determined. The system consists of two calcium cobaltate compounds that have promising thermoelectric properties, namely, the 2D thermoelectric oxide solid solution, (Ca{sub 3−x}Nd{sub x})Co{sub 4}O{sub 9−z} (0≤x≤0.5), which has a misfit layered structure, and Ca{sub 3}Co{sub 2}O{sub 6} which consists of 1D chains of alternating CoO{sub 6} trigonal prisms and CoO{sub 6} octahedra. Ca{sub 3}Co{sub 2}O{sub 6} was found to be a point compound without the substitution of Nd on the Ca site. The reported Nd{sub 2}CoO{sub 4} phase was not observed at 885 °C. A ternary (Ca{sub 1−x}Nd{sub 1+x})CoO{sub 4−z} (x=0) phase, or (CaNdCo)O{sub 4−z}, was found to be stable at this temperature. A solid solution region of distorted perovskite (Nd{sub 1−x}Ca{sub x})CoO{sub 3−z} (0≤x≤0.25, space group Pnma) was established. In the peripheral binary systems, while a solid solution region was identified for (Nd{sub 1−x}Ca{sub x}){sub 2}O{sub 3−z} (0≤x≤0.2), Nd was not found to substitute in the Ca site of CaO. Six solid solution tie-line regions and six three-phase regions were determined in the CaO–Nd{sub 2}O{sub 3}–CoO{sub z} system in air. - Graphical abstract: Phase diagram of the 1/2 Nd{sub 2}O{sub 3}–CaO–CoO{sub x} system at 885 °C, showing the limits of various solid solutions, and the tie-line relationships of various phases. - Highlights: • Phase diagram of the CaO–1/2 Nd{sub 2}O{sub 3}–CoO{sub z} system constructed. • System consists of thermoelectric oxide (Ca{sub 3−x}Nd{sub x})Co{sub 4}O{sub 9−z} (0≤x≤0.5). • Structures of (Nd{sub 1−x}Ca{sub x})CoO{sub 3−z} and (CaNdCo)O{sub 4−z} determined.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis and Thermoelectric Properties of low-x Bi{sub 2}Se{sub 3-x}S{sub 3} Series

Bi{sub 2}Se{sub 3}-xS{sub x} solid solutions, with low x values, were synthesized from melt. The solid solutions were studied in terms of phase purity using powder X-ray diffraction (PXRD) in order to find the maximum x value for the preservation of the single Bi2Se3-type phase. The lattice parameters were estimated and showed the reduced unit cell with the S incorporation in the lattice. SEM images confirmed the plate-like morphology of the Bi{sub 2}Se{sub 3}-xS{sub x} single-phase members. The thermoelectric properties (Seebeck coefficient and electrical conductivity) as well as IR reflectivity were also studied on members with x<0.4 that were found to form single phase Bi{sub 2}Se{sub 3}-xS{sub x} solid solutions.

36 MATERIALS SCIENCE↗

Chloride substitution in sodium borohydride

The dissolution of sodium chloride and sodium borohydride into each other resulting in formation of solid solutions of composition Na(BH{sub 4}){sub 1-x}Cl{sub x} is studied. The dissolution reaction is facilitated by two methods: ball milling or combination of ball milling and annealing at 300 deg. C for three days of NaBH{sub 4}-NaCl samples in molar ratios of 0.5:0.5 and 0.75:0.25. The degree of dissolution is studied by Rietveld refinement of synchrotron radiation powder X-ray diffraction (SR-PXD) data. The results show that dissolution of 10 mol% NaCl into NaBH{sub 4}, forming Na(BH{sub 4}){sub 0.9}Cl{sub 0.1}, takes place during ball milling. A higher degree of dissolution of NaCl in NaBH{sub 4} is obtained by annealing resulting in solid solutions containing up to 57 mol% NaCl, i.e. Na(BH{sub 4}){sub 0.43}Cl{sub 0.57}. In addition, annealing results in dissolution of 10-20 mol% NaBH{sub 4} into NaCl. The mechanism of the dissolution during annealing and the decomposition pathway of the solid solutions are studied by in situ SR-PXD. Furthermore, the stability upon hydrogen release and uptake were studied by Sieverts measurements. - Graphical Abstract: Dissolution of sodium chloride and sodium borohydride into each other resulting in formation of solid solutions of composition Na(BH{sub 4}){sub 1-x}Cl{sub x} is studied. Dissolution is facilitated by two methods: ball milling or annealing at 300 deg. C for three days of NaBH{sub 4}-NaCl samples. Sample compositions and dissolution mechanism are studied by Rietveld refinement of synchrotron radiation powder X-ray diffraction data. Highlights: > Studies of dissolution of sodium chloride and sodium borohydride into each other. > Solid state diffusion facilitated by mechanical and thermal treatments. > Dissolution is more efficiently induced by heating than by mechanical treatment. > Mechanism for dissolution studied by Rietveld refinement of in situ SR-PXD data.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural investigation of the “Tripled-Tetragonal-Tungsten-Bronze” Phases Sr 2 M 10- x O 27- y (M = Nb, Ta)

Sr 2 Nb 10 O 27 and Sr 2 Ta 10- x O 27- y exhibit the tripled tetragonal-tungsten-bronze (TTTB)-related superstructures. In contrast to Sr 2 Ta 10- x O 27- y , where an extended solid solution was found, Sr 2 Nb 10 O 27 only forms a narrow range of solid solution, Sr 1- x Nb 10 O 27- z (0 ≤ x ≤ 0.04). Serial X-ray and neutron diffraction studies show that both compounds can be modelled in the orthorhombic Pba 2 space group. Lattice parameters obtained from powder X-ray refinements are a = 12.4269(2) Å, b = 37.194(7) Å, c = 3.87897(4) Å, for Sr 2 Ta 10- x O 27- y , and a = 12.3281(3) Å, b = 37.1561(11) Å, and c = 3.93971(7) Å for Sr 2 Nb 10 O 27 . Neutron Rietveld refinements of both structures revealed the possible reason for the differing solid solution behavior. For Sr 2 Nb 10 O 27 , all Nb sites are fully occupied, whereas in Sr 2 Ta 10- x O 27- y , three out of the nine crystallographically unique Ta sites were shown to be partially occupied. Charge adjustment is therefore possible by increasing the Sr concentration, leading to a solid solution series and smaller Ta/Sr ratio as compared to Sr 2 Nb 10 O 27 . In the TTTB-related structures, Nb and Ta ions both occupy octahedral and pentagonal bipyramidal coordination sites. Layers of interconnected corner-shared octahedra were found parallel to the ab plane, with three-, four- and five-fold tunnels found in the structure running parallel to the c-axis. Sr ions partially fill the four- and five-fold tunnels.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Morphological and Structural Changes during the Reduction and Reoxidation of CuO/CeO2 and Ce1-xCuxO2 Nanocatalysts: In Situ Studies with Environmental TEM XRD and XAS

We have studied the structural, morphological, and electronic properties of CuO/CeO{sub 2} and Ce{sub 1-x}Cu{sub x}O{sub 2} nanocatalysts during reduction/oxidation cycles using H2 and O2 as chemical probes. Time-resolved in situ characterization was performed by X-ray diffraction (XRD) and X-ray absorption spectroscopy (XAS) as well as aberration-corrected environmental transmission electron microscopy (ETEM). We have found that both types of nanocatalysts reduce to a Cu/CeO{sub 2} biphase system with significant oxygen vacancies in CeO{sub 2}. Important variations are seen in the Cu particle size and metal dispersion depending on the initial state of the copper oxide-ceria systems. During subsequent in situ oxygen annealing, the Cu precipitated from the CuO/CeO{sub 2} system reoxidized to form CuO through a Cu2O intermediate phase as expected. However, the Cu precipitated from the Ce{sub 0.8}Cu{sub 0.2}O{sub 2} solid solution behaved rather differently under oxidizing conditions, and neither oxidized to form CuO nor fully returned to a bulk Ce{sub 0.8}Cu{sub 0.2}O{sub 2} phase in solid solution. We found that 50% of the Cu returned to a Ce{sub 1-x}Cu{sub x}O{sub 2} solid solution, while the remainder was observed by in situ ETEM to form an amorphous copper oxide phase with a Cu oxidation state similar to Ce{sub 1-x}Cu{sub x}O{sub 2}, but with a local bonding environment similar to CuO. The behavior of the reduced Ce{sub 0.8}Cu{sub 0.2}O{sub 2} reflects strong interactions between Cu and the ceria matrix and illustrates the advantages of working with solid solutions of mixed oxides.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Morphological and Structural Changes During the Reduction and Reoxidation of CuO/CeO(2) and Ce(1-x)Cu(x)O(2) Nanocatalysts: In-situ Studies with Environmental TEM, XRD and XAS

We have studied the structural, morphological, and electronic properties of CuO/CeO{sub 2} and Ce{sub 1-x}Cu{sub x}O{sub 2} nanocatalysts during reduction/oxidation cycles using H{sub 2} and O{sub 2} as chemical probes. Time-resolved in situ characterization was performed by X-ray diffraction (XRD) and X-ray absorption spectroscopy (XAS) as well as aberration-corrected environmental transmission electron microscopy (ETEM). We have found that both types of nanocatalysts reduce to a Cu/CeO{sub 2} biphase system with significant oxygen vacancies in CeO{sub 2}. Important variations are seen in the Cu particle size and metal dispersion depending on the initial state of the copper oxide-ceria systems. During subsequent in situ oxygen annealing, the Cu precipitated from the CuO/CeO{sub 2} system reoxidized to form CuO through a Cu{sub 2}O intermediate phase as expected. However, the Cu precipitated from the Ce{sub 0.8}Cu{sub 0.2}O{sub 2} solid solution behaved rather differently under oxidizing conditions, and neither oxidized to form CuO nor fully returned to a bulk Ce{sub 0.8}Cu{sub 0.2}O{sub 2} phase in solid solution. We found that {approx} 50% of the Cu returned to a Ce{sub 1-x}Cu{sub x}O{sub 2} solid solution, while the remainder was observed by in situ ETEM to form an amorphous copper oxide phase with a Cu oxidation state similar to Ce{sub 1-x}Cu{sub x}O{sub 2}, but with a local bonding environment similar to CuO. The behavior of the reduced Ce{sub 0.8}Cu{sub 0.2}O{sub 2} reflects strong interactions between Cu and the ceria matrix and illustrates the advantages of working with solid solutions of mixed oxides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A low-temperature synthetic route to ternary iron-manganese metal fluorides nanoparticles

Ternary metal fluoride Fe{sub x}Mn{sub 1−x}F{sub 2} (x = 0.00, 0.25, 0.50, 0.75, and 1.00), which is a potential cathode material for next-generation Li-ion batteries, were synthesized via a convenient, low-temperature, bottom-up solution-phase method. The lattice dimensions deduced from X-ray diffraction suggested formation of homogeneous solid solutions. With increasing Fe content, the morphology of the solid changed from cubic particles to dendritic, with an average particle size of 20–40 nm. The results suggested that this synthetic method constitutes a translatable route to large-scale production of ternary metal fluoride nanoparticles. - Graphical abstract: Homogeneous random solid solutions of ternary metal fluoride Fe{sub x}Mn{sub 1−x}F{sub 2} can be prepared by room temperature coprecipitation of precursors followed by drying and calcination at 350 °C. Display Omitted - Highlights: • Homogeneous ternary mixed metal iron-manganese fluoride Fe{sub x}Mn{sub 1−x}F{sub 2} nanoparticles prepared by room temperature coprecipitation and calcination. • Fe{sub x}Mn{sub 1−x}F{sub 2} nanoparticles form different morphology aggregates depending on the composition. • Lattice dimensions from X-ray diffraction suggested formation of homogeneous solid solutions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystal chemistry of Co-doped Zn{sub 7}Sb{sub 2}O{sub 12}

Zn{sub 7}Sb{sub 2}O{sub 12} forms a full range of Co-containing {alpha} solid solutions, Zn{sub 7-x}Co{sub x}Sb{sub 2}O{sub 12}, with an inverse-spinel structure at high temperature. At low temperatures for x<2, the solid solutions transform into the low temperature {beta}-polymorph. For x=0, the {beta}{yields}{alpha} transition occurs at 1225{+-}25 deg. C; the transition temperature decreases with increasing x. At high x and low temperatures, {alpha} solid solutions are formed but are non-stoichiometric; the (Zn+Co):Sb ratio is >7:2 and the compensation for the deficiency in Sb is attributed to the partial oxidation of Co{sup 2+} to Co{sup 3+}. From Rietveld refinements using ND data, Co occupies both octahedral and tetrahedral sites at intermediate values of x, but an octahedral preference attributed to crystal field stabilisation, causes the lattice parameter plot to deviate negatively from the Vegard's law. Sub-solidus compatibility relations in the ternary system ZnO-Sb{sub 2}O{sub 5}-CoO have been determined at 1100 deg. C for the compositions containing {<=}50% Sb{sub 2}O{sub 5}. - Graphical abstract: Zn{sub 7}Sb{sub 2}O{sub 12} forms a full range of Co-containing {alpha} solid solutions, Zn{sub 7-x}Co{sub x}Sb{sub 2}O{sub 12}, with an inverse-spinel structure at high temperature. From the Rietveld refinement using ND data, Co occupies both octahedral and tetrahedral sites at intermediate values of x, but an octahedral preference attributed to crystal field stabilisation, causes the lattice parameter plot to deviate negatively from the Vegard's law.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Spectral and Structural Characteristics of (Lu{sub 1 –} {sub x}Eu{sub x}){sub 2}(WO{sub 4}){sub 3} Tungstates

The structure, luminescence, and IR absorption spectra of (Lu{sub 1 –} {sub x}Eu{sub x}){sub 2}(WO{sub 4}){sub 3} solid solutions are studied in a wide range of europium concentrations (0 ≤ x ≤ 1). As the europium concentration increases, two types of crystalline phases sequentially alternate. An orthorhombic phase (space group Pbcn) of tungstate solid solutions is observed at 0 ≤ x < 0.5. In the range 0.5 ≤ x ≤ 0.8, along with the orthorhombic phase, a monoclinic phase (space group C2/c) appears; at x > 0.8, the solid solution has a monoclinic structure. The correspondence between the structure and spectral characteristics of these compounds is found. A change in the structure state leads to not only changes in luminescence spectra, but also in tungstate luminescence excitation spectra. In connection with the hydrophilicity of (Lu{sub 1 –} {sub x}Eu{sub x}){sub 2}(WO{sub 4}){sub 3} solid solutions, the water adsorption isotherm for tungstate samples and its effect on their spectral and structural characteristics is studied. It is found that the luminescence maximum under resonant excitation of Eu{sup 3+} ions is observed in samples with monoclinic structure C2/c at x ~ 0.9.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis, Structure, IR-Spectroscopic Characterization, and Ionic Conductivity of Mg{sub 0.5}Zr{sub 2}(AsO{sub 4}){sub x}(PO{sub 4}){sub 3−x}

Mg{sub 0.5}Zr{sub 2}(AsO{sub 4}){sub x}(PO{sub 4}){sub 3−x} arsenate phosphates have been prepared by a sol–gel process and characterized by X-ray diffraction, IR spectroscopy, and impedance spectroscopy. The results indicate the formation of a continuous series of solid solutions with the Sc{sub 2}(WO{sub 4}){sub 3} structure (sp. gr. P2{sub 1/n}) in the composition range 0 < x < 3. The unit-cell parameters of the solid solutions increase linearly with composition, as a consequence of arsenic substitution for phosphorus, which has a smaller ionic radius. The number of observed stretching and bending bands of the AsO{sub 4}{sup 3-} and PO{sub 4}{sup 3-} ions in the IR spectra of the solid solutions agrees with that predicted by factor group analysis for space group P2{sub 1/n}. The observed gradual shift of the absorption bands of the AsO{sub 4} tetrahedra to lower frequencies with increasing arsenic content on the tetrahedral site supports the X-ray diffraction evidence of the formation of substitutional solid solutions. The cation conductivity of Mg{sub 0.5}Zr{sub 2}(AsO{sub 4}){sub x}(PO{sub 4}){sub 3−x} with 0 ≤ х ≤ 1 has been shown to exceed the conductivity of the parent magnesium zirconium arsenate.

36 MATERIALS SCIENCE↗

Laves phase in alloy 718 fusion zone — microscopic and calorimetric studies

Microstructural characterization of alloy 718 fusion zone welded with both solid solution and age hardenable filler metal has been done. The microsegregation and the aging response were studied by employing three levels of weld cooling rate. Gas Tungsten Arc welding process was used. The fusion zone of solid solution filler metal has been responding to the aging treatment due to the weld process conditions and weld metal chemistry. However the weld metal composition was modified due to the higher molybdenum (Mo) content in solid solution filler metal. The effect of this modification on the phase reaction temperatures was studied and the same was compared with the conventional filler metal. - Graphical abstract: Display Omitted - Highlights: • Interdendritic segregation has been controlled by weld cooling rate. • Laves phase formation has been studied with cooling rate and weld metal chemistry. • Aging response with solid solution filler metal has been demonstrated. • Reduction in Laves phase and alloying element segregation has been confirmed. • Reaction temperatures were found modified because of Mo addition.

36 MATERIALS SCIENCE↗

Synthesis and magnetic properties of single phase titanomagnetites

The focus of this paper is the study of cation distributions and resulting magnetizations in titanomagnetites (TMs), (1−x)Fe{sub 3}O{sub 4−x}Fe{sub 2}TiO{sub 4} solid solutions. TM remnant states are hypothesized to contribute to planetary magnetic field anomalies. This work correlates experimental data with proposed models for the TM pseudobinary. Improved synthesis procedures are reported for single phase Ulvöspinel (Fe{sub 2}TiO{sub 4}), and TM solid solutions were made using solid state synthesis techniques. X-ray diffraction and scanning electron microscopy show samples to be single phase solid solutions. M-H curves of TM75, 80, 85, 90, and 95 (TMX where X = at. % of ulvöspinel) were measured using a Physical Property Measurement System at 10 K, in fields of 0 to 8 T. The saturation magnetization was found to be close to that predicted by the Neel model for cation distribution in TMs. M-T curves of the remnant magnetization were measured from 10 K to 350 K. The remnant magnetization was acquired at 10 K by applying an 8 T field and then releasing the field. Experimental Neel temperatures are reported for samples in the Neel model ground state.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Zr on microstructures and mechanical properties of an Al-Mg-Si-Cu-Cr alloy prepared by low frequency electromagnetic casting

The Al-1.6Mg-1.2Si-1.1Cu-0.15Cr (all in wt. %) alloys with and without Zr addition prepared by low frequency electromagnetic casting process were investigated by using the optical microscope, scanning electron microscope and transmission electron microscope equipped with energy dispersive analytical X-ray. The effects of Al{sub 3}Zr phases on the microstructures and mechanical properties during solidification, homogenization, hot extrusion and solid solution were studied. The results show that Al{sub 3}Zr phases reduce the grain size by ∼ 29% and promote the formation of an equiaxed grain structure during solidification. Numerous spherical Al{sub 3}Zr dispersoids with 35–60 nm in diameters precipitate during homogenization, and these fine dispersoids change little during subsequent hot extrusion and solid solution. Adding 0.15 wt. % Zr results in no recrystallization after hot extrusion and partial recrystallization after solid solution, while the recrystallized grain size is 400–550 μm in extrusion direction in the Zr-free alloy. In addition, adding 0.15 wt. % Zr can obviously promote Q′ phase precipitation, while the β″ phases are predominant in the alloy without Zr. Adding 0.15 wt. % Zr, the ultimate tensile strength of the T6 treated alloy increases by 45 MPa, while the elongation remains about 16.7%. - Highlights: • Minor Zr can refine as-cast grains of the LFEC Al-Mg-Si-Cu-Cr alloy. • L1{sub 2} Al{sub 3}Zr phases with 35–60 nm in diameter precipitate during homogenization. • L1{sub 2} and DO{sub 22} Al{sub 3}Zr phases result in partial recrystallization after solid solution. • Minor Zr can promote the precipitation of Q′ phases. • Mechanical properties of Al-Mg-Si-Cu-Cr-Zr alloy are higher than those of AA7005.

36 MATERIALS SCIENCE↗

Thermoelectric materials development

A systematic search for advanced thermoelectric materials was initiated at JPL several years ago to evaluate candidate materials which includes consideration of the following property attributes: (1) semiconducting properties; (2) large Seebeck coefficient; (3) high carrier mobility and high electrical conductivity; (4) low lattice thermal conductivity; and (5) chemical stability and low vapor pressure. Through this candidate screening process, JPL identified several families of materials as promising candidates for improved thermoelectric materials including the skutterudite family. As part of an ongoing effort to develop skutterudite materials with lower thermal conductivity values, several solid solutions and filled skutterudite materials were investigated under the effort sponsored by DOE. The efforts have primarily focused on: (1) study of existence and properties of solid solutions between the binary compounds CoSb3 and IrSb3, and RuSb2Te, and (2) CeFe(4-x)Sb12 based filled compositions. For the solid solutions, the lattice thermal conductivity reduction was expected to be reduced by the introduction of the Te and Ru atoms while in the case of CeFe(4-x)Ru(x)Sb12 based filled compositions. For the solid solutions, the lattice thermal conductivity reduction was expected to be reduced by the introduction of the Te and Ru atoms while in the case of CeFe(4-x)Ru(x)Sb12 filled compositions, the reduction would be caused by the rattling of Ce atoms located in the empty voids of the skutterudite structure and the substitution of Fe for Ru. The details of the sample preparation and characterization of their thermoelectric properties are reported in this report.

Fleurial, J. P.↗

Perfect short-range ordered alloy with line-compound-like properties in the ZnSnN 2 :ZnO system

We present a new solid-state material phase which is a disordered solid solution but offers many ordered line-compound features. The emergent physical phenomena are rooted in the perfect short-range order which conserves the local octet rule. We model the dual-sublattice-mixed semiconductor alloy (ZnSnN 2 ) 1-x (ZnO) 2x using first-principles calculations, Monte-Carlo simulations with a model Hamiltonian, and an extension of the regular solution model by incorporating short-range order. We demonstrate that this unique solid solution, occurring at a “magic” composition, can provide an electronically pristine character without disorder-induced charge localization and, therefore, a superior carrier transport similar to ordered phases. Interestingly, this phase shows singularities that are absent in the conventional solid-solution models, such as the regular solution and band-gap bowing model. Thermodynamically, this alloy phase has a sharply reduced enthalpy at its composition (like a line compound), but it still requires the entropy from long-range disorder to be stabilized at experimentally accessible temperatures.

36 MATERIALS SCIENCE↗

Preparation and structure of carbonated calcium hydroxyapatite substituted with heavy rare earth ions

Highlights: Black-Right-Pointing-Pointer LnCaHap solid solution particles were prepared using five types of heavy rare earth ions by a precipitation method. Black-Right-Pointing-Pointer The length and the crystallinity of the LnCaHap particles first increased and then decreased with increasing Ln{sup 3+} contents. Black-Right-Pointing-Pointer A series of YCaHap solid solution particles formed with Y/(Y + Ca) = 0-0.10 were investigated using various methods in detail. -- Abstract: Calcium hydroxyapatite (CaHap) particles substituted five types of heavy rare earth ions (Ln: Y{sup 3+}, Gd{sup 3+}, Dy{sup 3+}, Er{sup 3+} and Yb{sup 3+}) were synthesized using a precipitation method and characterized using various means. These Ln ions strongly affected the crystal phases and the structures of the products. With increasing Ln/(Ln + Ca) in the starting solution ([X{sub Ln}]), the length and the crystallinity of the particles first increased and then decreased. The rare earth metal-calcium hydroxyapatite (LnCaHap) solid solution particles were obtained at [X{sub Y}] {<=} 0.10 for substituting Y system and at [X{sub Ln}] {<=} 0.01-0.03 for substituting the other Ln systems. LnPO{sub 4} was mixed with LnCaHap at higher [X{sub Ln}] for all Ln systems. A series of yttrium-calcium hydroxyapatite (YCaHap) solid solutions with [X{sub Y}] = 0-0.10 were investigated using XRD, TEM, ICP-AES, IR and TG-DTA in detail.

36 MATERIALS SCIENCE↗