Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “polyimide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 901 records · Page 50

Research to Significantly Enhance Composites Survivability at 550 F in Oxidative Environments

Methylene dianiline (MDA) and its derivatives have been used in the synthesis of polyimides to yield polymers with characteristic low-density, high tensile strength, improved solubility in organic solvents, low-melt viscosities and high thermal stability (greater than 550 F) in air. Polyimides with such properties are desirable for use in aerospace systems, e.g., jet engines, airframe, missiles, and rockets where weight is critical. Recent research at Prairie View A&M University is focused on developing monomers to generate polyimides with enhanced performance over that of NASA s PMR-15. The objective of this work is to synthesize three ring aromatic diamines which are non-toxic and when reacted with the appropriate dianhydrides will yield polyimides with lower viscosity, improve processability, good retention of mechanical properties, and oxidative stability at high environmental temperatures. Modifications of the three ring aromatic diamines include replacing the methylene linkages with aromatic ethers by nucleophilic aromatic substitution reactions and incorporating mono- and di-substituents to the center aromatic ring. An update of current reactions involved in synthesis efforts to generate three ring aromatic monomers for polyimides with methylene, carbonyl, and ether linkages separating the aromatic moieties will be displayed.

Meador, Michael A.↗

Environmental Influence of Gravity and Pressure on Arc Tracking of Insulated Wires Investigated

Momentary short-circuit arcs between a defective polyimide-insulated wire and another conductor may thermally char (pyrolize) the insulating material. The charred polyimide, being conductive, can sustain the short-circuit arc, which may propagate along the wire through continuous pyrolization of the polyimide insulation (arc tracking). If the arcing wire is part of a multiple-wire bundle, the polyimide insulation of other wires within the bundle may become thermally charred and start arc tracking also (flash over). Such arc tracking can lead to complete failure of an entire wire bundle, causing other critical spacecraft or aircraft failures. Unfortunately, all tested candidate wire insulations for aerospace vehicles were susceptible to arc tracking. Therefore, a test procedure was designed at the NASA Lewis Research Center to select the insulation type least susceptible to arc tracking. This test procedure addresses the following three areas of concern: (1) probability of initiation, (2) probability of reinitiation (restrike), and (3) extent of arc tracking damage (propagation rate). Item 2 (restrike probability) is an issue if power can be terminated from and reapplied to the arcing wire (by a switch, fuse, or resettable circuit breaker). The degree of damage from an arcing event (item 3) refers to how easily the arc chars nearby insulation and propagates along the wire pair. Ease of nearby insulation charring can be determined by measuring the rate of arc propagation. Insulation that chars easily will propagate the arc faster than insulation that does not char very easily. A popular polyimide insulated wire for aerospace vehicles, MIL-W-81381, was tested to determine a degree of damage from an arcing event (item 3) in the following three environments: (1) microgravity with air at 1-atm pressure, (2) 1g with air at 1 atm, and (3) 1g within a 10^-6 Torr vacuum. The microgravity 1-atm air was the harshest environment, with respect to the rate of damage of arc tracking, for the 20 AWG (American Wiring Gauge) MIL-W-81381 wire insulation type . The vacuum environment resulted in the least damage. Further testing is planned to determine if the environmental results are consistent between insulation types and to evaluate the other two parameters associated with arc tracking susceptibility.

Source record↗

Prediction of Mechanical Properties of Polymers With Various Force Fields

The effect of force field type on the predicted elastic properties of a polyimide is examined using a multiscale modeling technique. Molecular Dynamics simulations are used to predict the atomic structure and elastic properties of the polymer by subjecting a representative volume element of the material to bulk and shear finite deformations. The elastic properties of the polyimide are determined using three force fields: AMBER, OPLS-AA, and MM3. The predicted values of Young s modulus and shear modulus of the polyimide are compared with experimental values. The results indicate that the mechanical properties of the polyimide predicted with the OPLS-AA force field most closely matched those from experiment. The results also indicate that while the complexity of the force field does not have a significant effect on the accuracy of predicted properties, small differences in the force constants and the functional form of individual terms in the force fields determine the accuracy of the force field in predicting the elastic properties of the polyimide.

Odegard, Gregory M.↗

Substituted Cyclohexene Endcaps for Polymers with Thermal-Oxidative Stability

This invention relates to polyimides having improved thermal-oxidative stability, to the process of preparing said polyimides, and the use of polyimide prepolymers in the preparation of prepregs and composites. The polyimides are particularly usefull in the preparation of fiber-reinforced, high-temperature composites for use in various engine parts including inlets, fan ducts, exit flaps and other parts of high speed aircraft. The polyimides are derived from the polymerization of effective amounts of at least one tetracarboxylic dianhydride, at least one polyamine and a novel dicarboxylic endcap having the formula presented.

Source record↗

Fiber reinforced thermoplastic resin matrix composites

Polyimide polymer composites having a combination of enhanced thermal and mechanical properties even when subjected to service temperatures as high as 700.degree. F. are described. They comprise (a) from 10 to 50 parts by weight of a thermoplastic polyimide resin prepared from 2,2-bis[4-(4-aminophenoxy)phenyl]hexafluoropropane and (b) from 90 to 50 parts by weight of continuous reinforcing fibers, the total of (a) and (b) being 100 parts by weight. Composites based on polyimide resin formed from 2,2-bis[4-(4-aminophenoxy)phenyl]hexafluoropropane and pyromellitic dianhydride and continuous carbon fibers retained at least about 50% of their room temperature shear strength after exposure to 700.degree. F. for a period of 16 hours in flowing air. Preferably, the thermoplastic polyimide resin is formed in situ in the composite material by thermal imidization of a corresponding amide-acid polymer prepared from 2,2-bis[4-(4-aminophenoxy)phenyl]hexafluoropropane. It is also preferred to initially size the continuous reinforcing fibers with up to about one percent by weight of an amide-acid polymer prepared from 2,2-bis[4-(4-aminophenoxy)phenyl]hexafluoropropane. In this way imidization at a suitable elevated temperature results in the in-situ formation of a substantially homogeneous thermoplastic matrix of the polyimide resin tightly and intimately bonded to the continuous fibers. The resultant composites tend to have optimum thermo-mechanical properties.

Jones, Robert J.↗

Tribological Evaluation of Candidate Gear Materials Operating Under Light Loads in Highly Humid Conditions

A series of pin-on-disk sliding wear tests were undertaken to identify candidate materials for a pair of lightly loaded timing gears operating under highly humid conditions. The target application involves water purification and thus precludes the use of oil, grease and potentially toxic solid lubricants. The baseline sliding pair is austenitic stainless steel operating against a carbon filled polyimide. The test load and sliding speed (4.9N, 2.7ms) were chosen to represent average contact conditions of the meshing gear teeth. In addition to the baseline materials, the hard superelastic NiTiNOL 60 (60NiTi) was slid against itself, against the baseline polyimide, and against 60NiTi onto which a commercially deposited dry film lubricant (DFL) was applied. The alternate materials were evaluated as potential replacements to achieve a longer wear life and improved dimensional stability for the timing gear application. An attempt was also made to provide solid lubrication to self-mated 60NiTi by rubbing the polyimide against the disk wear track outside the primary 60NiTi-60NiTi contact, a method named stick or transfer-film lubrication. The selected test conditions gave repeatable friction and wear data and smooth sliding surfaces for the baseline materials similar to those in the target application. Friction and wear for self-mated stainless steel were high and erratic. Self-mated 60NiTi gave acceptably low friction (0.2) and modest wear but the sliding surfaces were rough and potentially unsuitable for the gear application. Tests in which 60NiTi pins were slid against DFL coated 60NiTi and DFL coated stainless steel gave low friction and long wear life. The use of stick lubrication via a secondary polyimide pin provided effective transfer film lubrication to self-mated 60NiTi tribological specimens. Using this approach, friction levels were equal or lower than the baseline polyimide-stainless combination and wear was higher but within data scatter observed in these preliminary tests. Based upon these results, self-mated 60NiTi gear teeth utilizing solid lubrication, is a reasonable approach for the target application.

tribology↗

Tribological Evaluation of Candidate Gear Materials Operating Under Light Loads in Highly Humid Conditions

A series of pin-on-disk sliding wear tests were undertaken to identify candidate materials for a pair of lightly loaded timing gears operating under highly humid conditions. The target application involves water purification and thus precludes the use of oil, grease and potentially toxic solid lubricants. The baseline sliding pair is austenitic stainless steel operating against a carbon filled polyimide. The test load and sliding speed (4.9 N, 2.7 m/s) were chosen to represent average contact conditions of the meshing gear teeth. In addition to the baseline materials, the hard superelastic NiTiNOL 60 (60NiTi) was slid against itself, against the baseline polyimide, and against 60NiTi onto which a commercially deposited dry film lubricant (DFL) was applied. The alternate materials were evaluated as potential replacements to achieve a longer wear life and improved dimensional stability for the timing gear application. An attempt was also made to provide solid lubrication to self-mated 60NiTi by rubbing the polyimide against the disk wear track outside the primary 60NiTi-60NiTi contact, a method named stick or transfer-film lubrication. The selected test conditions gave repeatable friction and wear data and smooth sliding surfaces for the baseline materials similar to those in the target application. Friction and wear for self-mated stainless steel were high and erratic. Self-mated 60NiTi gave acceptably low friction (approx. 0.2) and modest wear but the sliding surfaces were rough and potentially unsuitable for the gear application. Tests in which 60NiTi pins were slid against DFL coated 60NiTi and DFL coated stainless steel gave low friction and long wear life. The use of stick lubrication via the secondary polyimide pin provided effective transfer film lubrication to self-mated 60NiTi tribological specimens. Using this approach, friction levels were equal or lower than the baseline polyimide-stainless combination and wear was higher but within data scatter observed in these preliminary tests. Based upon these results, self-mated 60NiTi gear teeth utilizing solid lubrication, is a reasonable approach for the target application.

tribology↗

Condition assessment of cable insulation materials in advanced reactor environments

While existing cable insulation materials are sufficient for use in the current reactor fleet, environmental conditions inside some advanced reactors, such as small modular reactors, will be substantially harsher. The work herein was conducted to assess the performance and overall survivability of several high-temperature, radiation resistant insulation polymers in a simulated small modular reactor environment. The materials evaluated under this research include polyether ether ketone, polyimide, and silicone rubber. These polymers were subjected to 1000 h of environmental stress exposure under two different conditions: 1) high temperature (i.e., 250 °C) in atmospheric pressure and 2) high temperature in a low-pressure vacuum (i.e., less than 2 psia). During the environmental exposure process, each insulation was periodically tested using several materials characterization techniques including Fourier transform infrared spectroscopy, oxidation induction time, and oxidation induction temperature. The objective of this testing was to assess and monitor changes that occurred in the thermal and chemical properties of the materials during the environmental exposures. The overall survivability of each insulation was assessed based on these property changes. The results of this research revealed that the polyimide and polyether ether ketone insulations had significantly better thermal and chemical stability than the silicone rubber during both the high-temperature atmospheric and vacuum exposures. Both polyimide and polyether ether ketone experienced minimal reductions in their chemical and thermal properties over the course of 1000 h in the simulated environments. Finally, based on this research, polyimide and polyether ether ketone show promise as potential base materials for small modular reactor cable insulation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Measurement of shock roughness due to phase plate speckle imprinting relevant for x-ray diffraction experiments on 3rd and 4th generation light sources

Laser-shock compression experiments at 3rd and 4th generation light sources generally employ phase plates, which are inserted into the beamline to achieve a repeatable intensity distribution at the focal plane. Here, the laser intensity profile is characterized by a high-contrast, high-frequency laser speckle. Without sufficient smoothing, these laser non-uniformities can translate to a significant pressure distribution within the sample layer and can affect data interpretation in x-ray diffraction experiments. Here, we use a combination of one- and two-dimensional velocity interferometry to directly measure the extent to which spatial frequencies within the laser focal spot intensity pattern are smoothed out during propagation within the laser plasma and a polyimide ablator. We find that the use of thicker polyimide layers results in spatially smoother shock fronts, with the greatest degree of smoothing associated with the highest spatial frequencies. Focal spots with the smallest initial speckle separation produce the most rapid smoothing. Laser systems that employ smoothing by spectral dispersion techniques to rapidly modulate the focal plane intensity distribution are shown to be the most effective ones in producing a spatially smooth shock front. We show that a simple transport model combined with the known polyimide Hugoniot adequately describes the extent of shock smoothness as a function of polyimide thickness. Finally, our results provide a description of spatial structure smoothing across a shock front, which can be used to design targets on x-ray free electron laser facilities.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Selected fretting-wear-resistant coatings for titanium - 6-percent-aluminum - 4-percent-vanadium alloy

A titanium - 6-percent-aluminum - 4-percent-vanadium alloy (Ti-6Al-4V) was subjected to fretting-wear exposures against uncoated Ti-6Al-4V as a baseline and against various coatings and surface treatments applied to Ti-6Al-4V. The coatings evaluated included plasma-sprayed tungsten carbide with 12 percent cobalt, aluminum oxide with 13 percent titanium oxide, chromium oxide, and aluminum bronze with 10 percent aromatic polyester; polymer-bonded polyimide, polyimide with graphite fluoride, polyimide with molybdenum disulfide (MoS2), and methyl phenyl silicone bonded MoS2, preoxidation surface treatment, a nitride surface treatment, and a sputtered MoS2 coating. Results of wear measurements on both the coated and uncoated surfaces after 300,000 fretting cycles indicated that the polyimide coating was the most wear resistant and caused the least wear to the uncoated mating surface.

Bill, R. C.↗

Advanced composites: Fabrication processes for selected resin matrix materials

This design note is based on present state of the art for epoxy and polyimide matrix composite fabrication technology. Boron/epoxy and polyimide and graphite/epoxy and polyimide structural parts can be successfully fabricated. Fabrication cycles for polyimide matrix composites have been shortened to near epoxy cycle times. Nondestructive testing has proven useful in detecting defects and anomalies in composite structure elements. Fabrication methods and tooling materials are discussed along with the advantages and disadvantages of different tooling materials. Types of honeycomb core, material costs and fabrication methods are shown in table form for comparison. Fabrication limits based on tooling size, pressure capabilities and various machining operations are also discussed.

Welhart, E. K.↗

Development of new addition-type composite resins

The most promising of a number of new addition type polyimides and polyaromatic melamine (NCNS) resins for use in high performance composite materials. Three different cure temperature ranges were of interest: 530-560 K (500-550 F), 475-530 K (400-500 F), and 450 K (350 F). Examined were a wide variety of polyimide precursors terminated with 5 norbornene groups and addition polymerized at 560 K similar to PMR-15 and LARC-160 polyimides. In addition, a number of lower curing cinnamal end capped polyimides and a bismaleimide were investigated but were not found promising. A group of NCNS resins were investigated and some were found to be superior to current epoxy resins in moisture resistance, oxidative aging and flame and smoke properties.

Kray, R. J.↗

Polymer research at NASA Langley Research Center

Polymer synthesis programs involve the development of Novel thermoplastics, pseudothermoplastics, and thermosets. These systems are prepared to elucidate structure-property relationships involving thermal capabilities, toughness, processability and environmental stability. Easily processable polyimides, solvent-resistant polysulfones and polyphenylquinoxalines, and tougher high and intermediate temperature polymers were developed. Characterization efforts included high pressure liquid chromatography methodology, the development of toughness tests for fiber reinforced composites, a study of electrical properties of metal ion filled polyimides, and a study of the mutagenicity of aromatic diamines. Also the mechanism of cure/degradation of experimental polymers was studied by rheology, mechanical behavior, separation techniques and spectroscopy. The degradative crosslinking of alkyl-containing polyimides, the separation and identification of crosslinked phenylquinoxalines, the rheological behavior of hot-melt polyimides, and the elucidation of the cure of norbornene endcapped imides were also studied.

Terry L. St. Clair↗

Matrix resin development at NASA Langley Research Center

The polymer program at NASA Langley Research Center involves exploratory studies in polymer science. These include the synthesis of novel polymers and their characterization. Polymer synthesis programs involve the development of novel thermoplastics, pseudothermoplastics, and thermosets. Recent investigations have led to the development of more easily processable polyimides, solvent-resistant polysulfones and polyphenylquinoxalines, and tougher high and intermediate-temperature polymers. Characterization efforts have included high-pressure liquid chromatography methodology, the development of toughness tests for fiber-reinforced composites, a study of electrical properties of metal-ion-filled polyimides, and a study of the mutagenicity of aromatic diamines. Also the mechanism of cure/degradation of experimental polymers has been studied by rheology, mechanical behavior, separation techniques and spectroscopy. Some of these programs have involved the degradation crosslinking of alkyl-containing polyimides, the separation and identification of crosslinked phenylquinoxalines, the rheological behavior of hot-melt polyimides, and the elucidation of the cure of norbornene endcapped imides.

St.clair, T. L.↗

Thermal History Of PMRs Via Pyrolysis-Gas Chromatography

Pyrolysis-gas chromatography (PY-GC) useful as analytical technique to determine extents of cure or postcure of PMR-15 polyimides and to lesser extent, cumulative thermal histories of PMR-15 polyimides exposed to high temperatures. Also applicable for same purposes to other PMR polyimides and to composite materials containing PMR polyimides. Valuable in reducing costs and promoting safety in aircraft industry by helping to identify improperly cured or postcured PMR-15 composite engine and airframe components and helping to identify composite parts nearing ends of their useful lives.

Gluyas, Richard E.↗

Method of Forming a Hot Film Sensor System on a Model

A method of forming a hot film sensor directly on a model is provided. A polyimide solution is sprayed onto the model. The model so sprayed is then heated in air. The steps of spraying and heating are repeated until a polyimide film of desired thickness is achieved on the model. The model with the polyimide film thereon is then thoroughly dried in air. One or more hot film sensors and corresponding electrical conducting leads are then applied directly onto the polyimide film.

Tran, Sang Q.↗

Evaluation of Space Power Materials Flown on the Passive Optical Sample Assembly

Evaluating the performance of materials on the exterior of spacecraft is of continuing interest, particularly in anticipation of those applications that will require a long duration in low Earth orbit. The Passive Optical Sample Assembly (POSA) experiment flown on the exterior of Mir as a risk mitigation experiment for the International Space Station was designed to better understand the interaction of materials with the low Earth orbit environment and to better understand the potential contamination threats that may be present in the vicinity of spacecraft. Deterioration in the optical performance of candidate space power materials due to the low Earth orbit environment, the contamination environment, or both, must be evaluated in order to propose measures to mitigate such deterioration. The thirty two samples of space power materials studied here include solar array blanket materials such as polyimide Kapton H and SiO(x) coated polyimide Kapton H, front surface aluminized sapphire, solar dynamic concentrator materials such as silver on spin coated polyimide and aluminum on spin coated polyimide, CV 1144 silicone, and the thermal control paint Z-93-P. The physical and optical properties that were evaluated prior to and after the POSA flight include mass, total, diffuse, and specular reflectance, solar absorptance, and infrared emittance. Additional post flight evaluation included scanning electron microscopy to observe surface features caused by the low Earth orbit environment and the contamination environment, and variable angle spectroscopic ellipsometry to identify contaminant type and thickness. This paper summarizes the results of pre- and post-flight measurements, identifies the mechanisms responsible for optical properties deterioration, and suggests improvements for the durability of materials in future missions.

Jaworske, Donald A.↗

Formation of Metallic Nanophases in Polymeric Matrices for Space Applications

There are a select number of polyimides which are soluble in organic media. Incorporation of hexafluoroisopropylidene groups is a route to achieving solubility. Such fluorinated polyimides have desirable properties for processing and electronic purposes; however, they often have linear coefficients of thermal expansion (CTE) which are well above those for metals and inorganic oxides or ceramics with which they might be bonded. We have developed a synthesis of composite inorganic-polyimide films using diaquotris(2,4-pentane-dionato)lanthanam(III) as the inorganic precursor and two soluble polyimides formed from 2,2-bis(3,4- dicarboxyphenyl)hexafluoro-propane (6FDA) and 1,3-bis(3-aminophenoxy)benzene (APB) or 2,2-bis[4-(4-aminophenoxy)phenyllhexafluoropropane (4-BDAF). A primary goal of our work was to control the linear CTE in these fluorinated polymer composites without adversely affecting mechanical or other thermal properties.

Orwoll, Robert A.↗