Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fracturing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 901 records · Page 50

On surface energy and the continuum thermodynamics of brittle fracture

When a separating body is viewed as a nonequilibrium thermodynamic process, the full thermodynamic nature of the surface energy induced by crack propagation becomes apparent. Within such a general framework it is no longer possible to view the surface energy as a material constant. For the self-propagating crack the induced surface energy is shown to depend explicitly on the square of the crack propagation speed. It is also shown that a separating body produces entropy even though the mechanical response of the solid may be elastic. The introduction of surface quantities such as surface energy into the continuum description of the fracture process forces a major departure from the mechanics appropriate to the nonseparating body. Local equations of balance are no longer obtainable as derived consequences of postulated global balance equations. They must instead be imposed as separate additional postulates.

Eftis, J.↗

Fracture in macro-molecules

Techniques available for the observation of molecular bond rupture during fracture of polymers are briefly outlined. Additional pertinent information can also often be inferred from microscopic and macroscopic measures.

Devries, K. L.↗

A study of the effect of subcritical crack growth on the geometry dependence on nonlinear fracture toughness parameters

The effect of subcritical crack growth on the geometry dependence of nonlinear fracture toughness parameters was studied by comparing the toughness values for different specimen geometries at the onset of subcritical crack growth and at the initiation of unstable crack propagation. Center-cracked thin sheet specimens of 2024-T3 and 7075-T6 aluminum alloys were tested by varying the specimen length L, width w, and crack length-to-width ratio c/w. When the onset of unstable crack propagation was selected as the critical point, the nonlinear energy toughness and the R curve toughness increased with increasing w and decreasing L and c/w. However, when the onset of subcritical crack growth was taken as the critical point, energy toughness and the linear toughness values were independent of these geometrical variables.

Jones, D. L.↗

The role of fracture mechanics in the design of fuel tanks in space vehicles

With special reference to design of fuel tanks in space vehicles, the principles of fracture mechanics are reviewed. An approximate but extremely simple relationship is derived among the operating stress level, the length of crack, and the number of cycles of failure. Any one of the variables can be computed approximately from the knowledge of the other two, if the loading schedule (mission of the tank) is not greatly altered. Two sample examples illustrating the procedures of determining the allowable safe operating stress corresponding to a set of assumed loading schedule are included. The selection of sample examples is limited by the relatively meager available data on the candidate material for various stress ratios in the cycling.

Denton, S. J.↗

Three dimensional finite-element analysis of finite-thickness fracture specimens

The stress-intensity factors for most of the commonly used fracture specimens (center-crack tension, single and double edge-crack tension, and compact), those that have a through-the-thickness crack, were calculated using a three dimensional finite-element elastic stress analysis. Three-dimensional singularity elements were used around the crack front. The stress intensity factors along the crack front were evaluated by using a force method, developed herein, that requires no prior assumption of either plane stress or plane strain. The calculated stress-intensity factors from the present analysis were compared with those from the literature whenever possible and were generally found to be in good agreement. The stress-intensity factors at the midplane for all specimens analyzed were within 3 percent of the two dimensional plane strain values. The stress intensity factors at the specimen surfaces were considerably lower than at the midplanes. For the center-crack tension specimens with large thickness to crack-length ratios, the stress-intensity factor reached a maximum near the surface of the specimen. In all other specimens considered the maximum stress intensity occurred at the midplane.

Raju, I. S.↗

Monitoring crack extension in fracture toughness tests by ultrasonics

An ultrasonic method was used to observe the onset of crack extension and to monitor continued crack growth in fracture toughness specimens during three-point bend tests. A 20-MHz transducer was used with commercially available equipment to detect average crack extension less than 0.09 mm. The material tested was a 300-grade maraging steel in the annealed condition. A crack extension resistance curve was developed to demonstrate the usefulness of the ultrasonic method for minimizing the number of tests required to generate such curves.

Klima, S. J.↗

Effect of water and ice on strength and fracture toughness of intermittently bonded boron-epoxy composites

The effects of water and ice on the strength and fracture toughness of boron-epoxy composites with polyurethane intermittent bonding have been investigated. Neither simple soaking in water nor soaking followed by freezing and thawing have marked effects on the strength of the fully-coated composites, but they have disastrous effects on the uncoated composites. Toughness is affected only marginally, with some small reductions in the fully-coated samples, and with essentially no effect on the uncoated composites. An analysis is presented which explains adequately the experimental strength and toughness results obtained, and which is based on an argument that water absorption reduces the interfacial shear strength only of the uncoated areas and not those regions coated by the polyurethane varnish. The results indicate that the advantages of appropriate intermittent bonding (i.e., high strength combined with high toughness) are retained in wet conditions so that such composites may be favorably used in such adverse environmental conditions.

Atkins, A. G.↗

Estimating plane strain fracture toughness of high strength aluminum alloys from crack arrest toughness

A comparison is made between fracture toughness KIc as measured by recommended ASTM procedures and crack arrest toughness KIa as measured on more than 100 bolt-loaded double-cantilever beam (DCB) specimens from 7075, 7050, and 7049 alloy plates. Close agreement was found between the two values, KIa being on the average less than KIc over a specified range. This indicates that a simplified test based on a bolt-loaded DCB specimen could be used for quality control, lot release, and screening purposes. Measurements of crack length and specimen deflection are all that are required. The specimens do not have to be fatigue precracked, nor is a tensile machine needed.

Dorward, R. C.↗

Basic principles of material selection in fracture-critical applications

A concept of material characterization which shows the relation between initial crack size, stress range, and life to failure is presented. This presentation is used to determine if a particular application is fracture-critical and to choose a suitable material. The influence of design stress inaccuracies on the material selection is assessed.

Elber, W.↗

Room temperature crack growth rates and -20 deg F fracture toughness of welded 1 1/4 inch A-285 steel plate

Data are presented which were developed in support of a structural assessment of NASA-LEWIS' 10-foot by 10-foot supersonic wind tunnel, critical portions of which are fabricated from rolled and welded 1 1/4 inch thick A-285 steel plate. Test material was flame cut from the tunnel wall and included longitudinal and circumferential weld joints. Parent metal, welds, and weld heat affected zone were tested. Tensile strength and fracture toughness were determined at -20 F, the estimated lowest tunnel operating temperature. Crack growth rates were measured at room temperature, where growth rates in service are expected to be highest.

Shannon, J. L., Jr.↗

The influence of composition, annealing treatment, and texture on the fracture toughness of Ti-5Al-2.5Sn plate at cryogenic temperatures

The plane strain fracture toughness K sub Ic and conventional tensile properties of two commercially produced one-inch thick Ti-5Al-2.5Sn plates were determined at cryogenic temperatures. One plate was extra-low interstitial (ELI) grade, the other normal interstitial. Portions of each plate were mill annealed at 1088 K (1500 F) followed by either air cooling or furnace cooling. The tensile properties, flow curves, and K sub Ic of these plates were determined at 295 K (room temperature), 77 K (liquid nitrogen temperature), and 20 K (liquid hydrogen temperature).

Vanstone, R. H.↗

The effects of eccentricities on the fracture of off-axis fiber composites

Finite element analyses were performed to investigate theoretically the effects of in-plane and out-of-plane eccentricities, bending or twisting, and thickness nonuniformity on the axial stress and strain variations across the width of off-axis specimens. The results are compared with measured data and are also used to assess the effects of these eccentricities on the fracture stress of off-axis fiber composites. Guidelines for detecting and minimizing the presence of eccentricities are described.

Chamis, C. C.↗

The effect of minor additions of titanium on the fracture toughness of Fe-12Ni alloys at 77K

Titanium additions ranging from 0.18 to 0.99 atomic percent and heat treatments of 2 hours at 550, 685 and 820 C respectively followed by a water quench were considered. Cubic and rectangular shaped inclusions were noted in the SEM fractographs of the alloys with the Ti additions. A fine precipitate was observed by TEM for the Fe-12Ni-0.18Ti alloys heat treated at 550 C; this precipitate was not observed for the 685 and 820 C heat treatments of the same alloy. Auger mappings of the fracture surfaces indicated a weak to moderate association of the interstitials C, N and O with Ti, the degree of which depended on the particular interstitial and the heat treatment temperature.

Conrad, H.↗

Fatigue and fracture

The effects of the load/temperature environment of the shuttle on the fatigue life of the body-flap were investigated by conducting real time and accelerated flight-by-flight tests up to 500 flights on coupons containing holes. On the fracture side, much is known about the sensitivity of the tensile strengths of composites to holes and other flaws, predominantly at room temperature. The effects of notches were assessed for graphite/polyimides at the expected temperature extremes of the body-flap: 117K (-250 F) to 589K (600 F). Results indicate that the shuttle temperature extremes may affect fatigue properties HTS/PMR-15. There is no significant effect of temperature on notch-strength. Tensile strengths for specimens with holes and slots are equal.

Illg, W.↗

The effects of eccentricities on the fracture of off-axis fiber composites

Finite element analyses were performed to investigate theoretically the effects of in-plane and out-of plane eccentricities, bending or twisting, and thickness nonuniformity on the axial stress and strain variations across the width of off-axis specimens. The results are compared with measured data and are also used to access the effects of these eccentricities on the fracture stress of off-axis fiber composites. Guidelines for detecting and minimizing the presence of eccentricities are described.

Chamis, C. C.↗

Fracture resistance of Ti-5Al-2.5Sn extra-low interstitial castings

Fracture toughness and cyclic crack propagation data for Ti-5Al-2.5Sn extra-low interstitial (ELI) castings, 0.51 and 2.54 cm (0.20 and 1.00 in.) thick, at 394, 294, 77, and 20 K (250, 70, -320, and -423 F), are presented. Both surface flaw and compact tension geometries were tested. Comparison is made with other titanium alloys in both wrought and cast forms. Crack propagation resistance is comparable to wrought Ti-5Al-2.5Sn ELI, even with the extremely coarse as-cast grain size encountered.

Fiftal, C. F.↗

A correlative study between analysis and experiment on the fracture behavior of graphite/epoxy composites

The paper compares the fracture behavior of a composite material by using the analytical models of Waddoups et al. (1971), Whitney and Nuismer (1974, 1975), and Snyder and Cruse (1975) with experimental results from tests performed on center-notched tensile strips. Laminate configurations of (0 deg)8s, (0 deg/90 deg)4s, (+ and -45 deg)4s, and (0 deg/+ and -45 deg/0 deg)2s from T300/934 graphite/epoxy are tested. These particular configurations are used so that the effect of various degrees of anisotropy can be studied. The procedure adopted uses the results from one test for crack size aspect ratio to predict the results of tests of other aspect ratios. For those methods that use a characteristic dimension, predictions are made by assuming the magnitude of this dimension to be constant. The validity of this assumption for a laminate is assessed by comparing predicted and experimental results. Analytical models using a characteristic dimension are compared to the model developed by Cruse (1973).

Yeow, Y. T.↗