At least 901 records · Page 50

Solidification and Liquation Cracking Behavior of Dual-Phase Steel DP600

In this work, the solidification and liquation cracking behavior of a dual-phase steel DP600 was examined using longitudinal Varestraint testing and hot ductility testing. Varestraint tests showed only limited cracking even at 4 pct augmented strain. Hot ductility tests showed that the nil-strength temperature of the steel was 1459 °C, while the nil-ductility and the ductility-recovery temperatures were 1435 °C and 1420 °C, respectively. The brittleness temperature range was found to be 39 °C, and the DP600 steel was highly resistant to both weld metal solidification cracking and heat-affected zone liquation cracking. The reasons for the high hot cracking resistance of dual-phase steel DP600 are discussed.

36 MATERIALS SCIENCE↗

Crack Detection in High-Velocity Oxygen-Fuel-Sprayed Al{sub 59.2}Cu{sub 25.5}Fe{sub 12.3}B{sub 3} Quasicrystalline Coatings Using Piezoelectric Active Sensors

Quasicrystals have received some attention in recent years regarding their potential usefulness as low friction and wear resistant materials. When quasicrystalline (QC) coatings are exposed to different levels of external loading or are subjected to thermal stresses, crack nucleation, and propagation become life-limiting factors. In this investigation, Al{sub 59.2}Cu{sub 25.5}Fe{sub 12.3}B{sub 3} QC coatings were deposited onto AISI-A36 steel substrates using the high-velocity oxygen-fuel (HVOF) technique. The coatings were deposited at different oxygen-to-fuel ratios. To characterize the integrity of the coatings, the active piezoceramic excitation technique was applied to detect the propagation of cracks during three-point bending tests. The piezoelectric transducer signal was processed using wavelet transformation analysis. The results revealed that the coated samples displayed different densities of cracks depending on the oxygen-to-fuel. The crack density was found higher for coatings formed using a slightly oxidizing flame. The opening of the pre-existing cracks in the coating was the main reason of signal attenuation during piezoelectric excitation. The HVOF-sprayed AlCuFeB quasicrystalline coating, with thickness between 150 and 180 μm, withstands a flexural stress as high as 340 MPa. To the best of our knowledge, this study is the first that provides a quantitative assessment of the viability of QC coatings in mechanical applications in spite of their intrinsic brittleness.

36 MATERIALS SCIENCE↗

The Influence of Residual Stress on Fatigue Crack Growth Rates in Stainless Steel Processed by Different Additive Manufacturing Methods

The properties and microstructure of Type 304L stainless steel produced by two additive manufacturing (AM) methods—directed energy deposition (DED) and powder bed fusion (PBF)—are evaluated and compared. Localized heating and steep temperature gradients of AM processes lead to significant residual stress and distinctive microstructures, which may be process-specific and influence mechanical behavior. Test data show that materials produced by DED and PDF have small differences in tensile strengths but clear differences in residual stress and microstructural features. Measured fatigue crack growth rates (FCGRs) for cracks propagating parallel to and perpendicular to the build directions differ between the two AM materials. To separate the influences of residual stress and microstructure, K-control test procedures with decreasing and constant stress intensity factor ranges are used to measure FCGRs in the near-threshold regime (crack growth rates ≤ 1 × 10 −8 m/cycle). Residual stress is quantified by the residual stress intensity factor, K res , measured by the online crack compliance method. Correcting the FCGR data for differences in K res brings results for specimens of the two AM materials into agreement with each other and with results for wrought specimens, when the latter are corrected for crack closure. Differences in microstructure and tensile strength have an insignificant influence on FCGRs in these tests.

additive manufacturing↗

Investigation of fatigue crack initiation from a non-metallic inclusion via high energy x-ray diffraction microscopy

Crack initiation at inclusions is a dominant, unavoidable and life-limiting failure mechanism of important structural materials. Fatigue progresses in a complex manner to find the ‘weakest link’ in the microstructure, leading to crack nucleation. In this study, fully 3-D characterization methods using high-energy synchrotron x-rays are combined with in-situ mechanical testing to study the crack initiation mechanism in a Ni-based superalloy specimen. The specimen was produced via powder metallurgy and seeded with a non-metallic inclusion. Two x-ray techniques were employed: absorption contrast computed micro-tomography (μ-CT) to determine the morphology of the inclusion and its location in the gauge section of the specimen; and far-field high-energy diffraction microscopy (FF-HEDM) to resolve the centroids, average orientations, and lattice strains of the individual grains comprising the microstructure surrounding the inclusion. Sequential μ-CT and FF-HEDM scans were carried out at both peak and zero applied stress following schedules of cyclic deformation. The µ-CT data showed the onset and location of crack initiation, and the FF-HEDM data provided temporal and spatial evolution of the intergranular strains. Strain partitioning and the associated stress heterogeneities that develop are shown to stabilize within a few loading cycles. Elasto-viscoplastic fast Fourier transform simulations were utilized to supplement interpretation of the experimental stress distributions and compared with the experimental stress distributions. In conclusion, appropriate conditions for crack nucleation in the form of stress gradients were demonstrated and created by virtue of the inclusion, specifically the residual stress state and local bonding state at the inclusion-matrix interface.

36 MATERIALS SCIENCE↗

Characterization of fatigue crack growth behavior in LENS fabricated Ti-6Al-4V using high-energy synchrotron x-ray microtomography

Laser Engineered Net Shaping (LENS) is an additive manufacturing technique that belongs to the ASTM standardized directed energy deposition category. To date, very limited work has been conducted towards understanding the fatigue crack growth behavior of LENS fabricated materials, which hinders the widespread adoption of this technology for high-integrity structural applications. In this study, the propagation of a 20 μm initial crack in LENS fabricated Ti-6Al-4V was captured in-situ, using high-energy synchrotron x-ray microtomography. Fatigue crack growth (FCG) data were then determined from 2D and 3D tomography reconstructions, as well as from fracture surface striation measurements using SEM. The generated data were compared to those obtained from conventional FCG tests that used compliance and direct current potential drop (DCPD) techniques to measure long and small crack growth. In conclusion, the observed agreement demonstrates that x-ray microtomography and fractographic analysis using SEM can be successfully combined to study the propagation behavior of fatigue cracks.

36 MATERIALS SCIENCE↗

Perovskite oxides for redox oxidative cracking of n -hexane under a cyclic redox scheme

Steam cracking of naphtha is a commercially proven technology for light olefin production and the primary source of ethylene in the Europe and Asia-Pacific markets. However, its significant energy consumption and high CO 2 intensity (up to 2 tons CO 2 /ton C 2 H 4 ), stemming from endothermic cracking reactions and complex product separations, make this state-of-the-art process increasingly undesirable from an environmental standpoint. We propose a redox oxidative cracking (ROC) approach as an alternative pathway for naphtha conversion. Enabled by perovskite oxide-based redox catalysts, the ROC process converts naphtha (represented by n-hexane) in an auto-thermal, cyclic redox mode. The addition of 20 wt.% Na 2 WO 4 to SrMnO 3 and CaMnO 3 created highly selective redox catalysts capable of achieving enhanced olefin yields from n-hexane oxy-cracking. This was largely attributed to the redox catalysts’ high activity, selectivity, and stability towards selective hydrogen combustion (SHC) under a redox mode. Na 2 WO 4 /CaMnO 3 demonstrated significantly higher olefin yield (55–58%) when compared to that from thermal cracking (34%) at 725 °C and 4500 h –1 . CO x yield as low as 1.7% was achieved along with complete combustion of H 2 over 25 cycles. Similarly, Na 2 WO 4 /SrMnO 3 achieved 41% olefin yield, 0.4% CO x yield, and 73% H 2 combustion at this condition. Oxygen-temperature-programmed desorption (O 2 -TPD) indicated that Na 2 WO 4 hindered gaseous oxygen release from CaMnO 3 . Low-energy ion scattering (LEIS) and X-ray photoelectron spectroscopy (XPS) revealed an outermost perovskite surface layer covered by Na 2 WO 4 , which suppressed near-surface Mn and alkaline earth metal cations. The formation of non-selective surface oxygen species was also inhibited. XPS analysis further confirmed that promotion of SrMnO 3 with Na 2 WO 4 suppressed surface Sr species by 90%, with a similar effect also observed on CaMnO 3 . Furthermore, these findings point to the promoting effect of Na 2 WO 4 and the potential of promoted SrMnO 3 and CaMnO 3 as selective redox catalysts for efficient production of light olefins from naphtha via the ROC process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The significance of crack-resistance curves to the mixed-mode fracture toughness of human cortical bone

The majority of fracture mechanics studies on the toughness of bone have been performed under tensile loading. However, it has recently been shown that the toughness of human cortical bone in the transverse (breaking) orientation is actually much lower in shear (mode II) than in tension (mode I); a fact that is physiologically relevant as in vivo bone is invariably loaded multiaxially. Since bone is a material that derives its fracture resistance primarily during crack growth through extrinsic toughening mechanisms, such as crack deflection and bridging, evaluation of its toughness is best achieved through measurements of the crack-resistance or R-curve, which describes the fracture toughness as a function of crack extension. Accordingly, in this study, we attempt to measure for the first time the R-curve fracture toughness of human cortical bone under physiologically relevant mixed-mode loading conditions. We show that the resulting mixed-mode (mode I + II) toughness depends strongly on the crack trajectory and is the result of the competition between the paths of maximum mechanical driving force and 'weakest' microstructural resistance.

36 MATERIALS SCIENCE↗

Effect of environmental exposure on autogenous self-healing of cracked cement-based materials

Despite abundant literature on self-healing of cement-based materials, there is dearth of information on how environmental exposure affects self-healing. In this study, self-healing of cracks in cement mortar under different environmental exposure was investigated. Pre-cracked mortar specimens were submerged in water, while identical specimens were exposed to cyclic temperature and relative humidity. Change in crack width was examined using optical microscopy. SEM coupled with energy dispersive X-ray analysis was used to identify healing compounds. Mercury Intrusion Porosimetry, water absorption and permeability were employed to assess porosity. X-ray computed tomography was deployed to explore healing of internal cracks. No significant self-healing occurred in specimens exposed to cyclic T and RH. Although crack self-healing was identified in submerged specimens, X-ray μCT demonstrated that it was limited to exposed surface of specimens. This warrants further research to bridge the gap between laboratory findings on self-healing and actual field performance of ageing civil infrastructure.

36 MATERIALS SCIENCE↗

Water penetration through cracks in self-healing cementitious materials with superabsorbent polymers studied by neutron radiography

SuperAbsorbent Polymers (SAPs) are a promising admixture to obtain self-sealing and self-healing cementitious materials. They are able to physically block water penetration through cracks due to their swelling ability. This is very useful in a cementitious material which is prone to cracking leading to a reduced durability. The effectiveness of counteracting water penetration is of concern. Neutron radiography was performed in order to investigate the influence of SAPs on the water permeability through healed cracks with respect to a reference material without SAPs. The gravimetrically measured capillary absorption corresponded with the obtained results after image analysis and a quantitative analysis could be made. SAPs enhance the water impermeability and are able to seal and heal a crack effectively up to 100 μm. The healing was a main factor to impede water movement through cracks. This will lead to less water ingress in building infrastructures and a possible longer service life.

36 MATERIALS SCIENCE↗

Alkali-silica reaction products and cracks: X-ray micro-tomography-based analysis of their spatial-temporal evolution at a mesoscale

In this study, we propose a laboratory-scale methodology, based on X-ray micro-tomography and caesium (Cs) as a contrast agent, to advance the understanding of cracking due to alkali-silica reaction (ASR) in concrete. The methodology allows achieving a completely non-destructive and time-lapse characterization of the spatial-temporal patterns of both the cracks and the ASR products. While Cs addition slightly accelerated the ASR kinetics, the crack patterns, with and without Cs addition, were statistically equivalent. Cracks with ASR products appeared first in the aggregates, close to the interface with the cement paste. They propagated afterwards towards the aggregates interior. Some products were then extruded for several mm into air voids and cracks in the cement paste. This process suggests that, in the early stage, the ASR products may be a low-viscosity gel that can flow away from the source aggregate and may settle later elsewhere as a rigid phase, upon calcium uptake.

36 MATERIALS SCIENCE↗

Experimental and theoretical study of the restrained shrinkage cracking of early age well cement

The shrinkage cracking occurring in oil & gas well cement material is a major factor that reduces the cement sheath integrity and impairs the durability of an underground well. Shrinkage mainly takes place in the early hydration period of the cement, and the resulting restrained shrinkage cracking can form a leaking network for oil & gas or carbon dioxide stored in an underground reservoir. It is thus important to understand the early age behavior of well cement and the leaking pathway formation in the well. This study describes the application of the digital image correlation (DIC) method as a tool to measure the strain development and crack distributions of well cement in the lab during early phase changes. A theoretical model is presented to calculate the stress distribution built up in the cement sheath during early ages of well cement hydration, which helps to interpret the experimental observations and determine the major factors influencing the cracking sequences. This study presents the whole hydration – drying shrinkage – and cracking mechanism of early age well cement under restrained ring conditions experimentally and theoretically. Finally, the results offer useful insights on the key material and geometric parameters which control the fracture of a well cementing structure.

36 MATERIALS SCIENCE↗

In situ synchrotron X-ray tomography of 304 stainless steels undergoing chlorine-induced stress corrosion cracking

To understand the mechanisms behind chlorine-induced stress corrosion cracking (CISCC) in 304 stainless steel, synchrotron high energy x-rays were used to perform in-situ x-ray microtomography on a pre-cracked sample under load in a corrosive simulated marine environment. The tomography scans showed the crack morphology evolving into a branching crack around the surface of the sample. Finite element analysis and stress intensity analysis are conducted to explain the observed crack branching.

304 Stainless Steel↗

Fatigue crack growth mechanisms at the microstructure scale in as-fabricated and heat treated Ti-6Al-4V ELI manufactured by electron beam melting (EBM)

Electron beam melting (EBM) is a metal powder bed fusion additive manufacturing (AM) technology that fabricates parts by selectively scanning consecutive powder layers with an electron beam. Additive manufacturing technologies are increasing in importance for aerospace and medical applications, where the demand for a fundamental understanding and predictability of static and dynamic material properties are high. Ti-6Al-4V is the most widely used and studied alloy for this technology, and is the focus of this work in its Extra Low Interstitial (ELI) variation. The layered manufacturing of metallic components by EBM creates a unique directional microstructure, and consequently, anisotropic properties. Microstructure evolution, and its influence on mechanical properties of the alloy in the as-fabricated condition, has been documented by various researchers. However, fatigue crack propagation and the effects of the directional structure have not been sufficiently studied, imposing a barrier for this technology’s potential extension to high-integrity applications. Here in this study, fatigue crack growth (FCG) both parallel and perpendicular to the build directions was studied for different stress ratios and crack growth stages. The interaction between the directional as-fabricated EBM microstructure and FCG was investigated and compared to that of the equiaxed β annealed microstructure obtained by annealing above the β transus temperature. Finally, the FCG threshold, ΔK th , was analytically modeled for the two relative crack propagation directions at different stress ratios, and FCG microstructural mechanisms were established for all three regions of crack propagation.

36 MATERIALS SCIENCE↗

A path-dependent fatigue crack propagation model under non-proportional modes I and III loading conditions

It has been well established that fatigue damage process is load-path dependent under non-proportional multi-axial loading conditions. Most of studies to date have been focusing on interpretation of S-N based test data by constructing a path-dependent fatigue damage model. Our paper presents a two-parameter mixed-mode fatigue crack growth model which takes into account of crack growth dependency on both load path traversed and a maximum effective stress intensity attained in a stress intensity factor plane (e.g.,KI-KIII plane). Furthermore, by taking advantage of a path-dependent maximum range (PDMR) cycle definition (Dong et al., 2010; Wei and Dong, 2010), the two parameters are formulated by introducing a moment of load path (MLP) based equivalent stress intensity factor range (ΔKNP) and a maximum effective stress intensity parameter KMax incorporating an interaction term KI·KIII. To examine the effectiveness of the proposed model, two sets of crack growth rate test data are considered. The first set is obtained as a part of this study using 304 stainless steel disk specimens subjected to three combined non-proportional modes I and III loading conditions (i.e., with a phase angle of 0°, 90°, and 180°). The second set was obtained by Feng et al. (2007) using 1070 steel disk specimens subjected to similar types of non-proportional mixed-mode conditions. Once the proposed two-parameter non-proportional mixed-mode crack growth model is used, it is shown that a good correlation can be achieved for both sets of the crack growth rate test data.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Irradiation-assisted cracking of SA508-304L weldments with 308L groove filler and 309L butter in hot water immersion constant rate extension tests

Low alloy SA508 bainitic steel is often welded to 300 series austenitic stainless steel in nuclear power plants. These dissimilar metal weldments use 309L butter applied to the low alloy steel and 308L groove filler material to join the 309L to austenite. High alloy steels (such as the 308L and 309L material used here) have been identified as having greater susceptibility to irradiation-assisted stress corrosion cracking (IASCC). Evidence is presented here of cracking under tensile loads in 309L weldment butter in LWR hydrothermal conditions that correlates irradiation induced changes at δ ferrite–γ austenite phase boundaries and γ–γ grain boundaries; specifically intergranular Cr 23 C 6 precipitates. Cracking is not observed in irradiated 308L groove filler under the same conditions. Both the 309L butter and 308L filler material have a duplex or mixed δ–γ phase microstructure due to solidification during the welding procedure. We have performed constant extension rate autoclave immersion tests in BWR normal water chemistry hot water (288 °C, 10 MPa, 2000 wt. ppb dissolved oxygen, <100 nS/cm conductivity, neutral pH) of proton irradiated (2 MeV, approximately 3 displacements per atom at a depth of 10 μm) tensile specimens. Proton irradiation to the dpa levels used here induced Cr 23 C 6 carbide precipitation at γ–γ grain boundaries and δ–γ phase boundaries in the 309L butter but not the 308L filler. Cracking was observed in the proton-irradiated volume of 309L at these interfaces in the vicinity of the Cr 23 C 6 precipitates. We hypothesis the SA508 is the source of carbon in the 309L butter. Cr depletion at γ–γ grain boundaries was also observed and may also be a root cause of cracking. Furthermore, the 309L butter is under significant tensile residual stress in the weldment that adds to applied tensile loads and this too may be a contributing factor.

309L weld butter↗

Electron backscatter diffraction characterization of fatigue crack growth in laser metal wire deposited Ti-6Al-4V

Highlights: • No difference in fatigue crack growth rate was confirmed within the material. • The tortuosity of the crack propagation could be related to the alpha colonies. • Large areas with similar crystallographic orientation were observed. - Abstract: By additive manufacturing (AM) there is a feasibility of producing near net shape components in basically one step from 3D CAD model to final product. The interest for AM is high and during the past decade a lot of research has been carried out in order to understand the influence from process parameters on the microstructure and furthermore on the mechanical properties. In the present study laser metal wire deposition of Ti-6Al-4V has been studied in detail with regard to its fatigue crack propagation characteristics. Two specimen orientations, parallel and perpendicular to the deposition direction, have been evaluated at room temperature and at 250 °C. No difference in the fatigue crack growth rate could be confirmed for the two specimen orientations. However, in the fractographic study it was observed that the tortuosity varied between certain regions on the fracture surface. The local crack path characteristic could be related to the alpha colony size and/or the crystallographic orientation. Moreover, large areas exhibiting similar crystallographic orientation were observed along the prior beta grain boundaries, which were attributed to the wide alpha colonies frequently observed along the prior beta grain boundaries.

36 MATERIALS SCIENCE↗

Effect of grain boundary character distribution on weld heat-affected zone liquation cracking behavior of AISI 316Ti austenitic stainless steel

Highlights: • Grain boundary engineered AISI 316 was produced through thermomechanical processing. • Grain boundary engineering resulted in random high angle boundary network disruption. • Liquation cracks are arrested at triple junctions having one or more CSL boundaries. • Grain boundary engineering resulted in improvement in liquation cracking resistance. - Abstract: In this work, the role of grain boundary engineering (GBE) on the weld heat-affected-zone (HAZ) liquation cracking resistance of austenitic stainless steel AISI 316Ti was investigated. Standard wrought-processed alloy 316Ti was cold rolled to 5% strain and subsequently annealed at 1373 K for 30 min to achieve the optimum grain boundary character distribution (GBCD). The GBE samples were found to consist of a significantly higher fraction (72%) of low Ʃ coincident site lattice (CSL) boundaries as compared to the as received (AR) samples (45%). To study the liquation cracking behavior, single-track longitudinal varestraint tests was performed on AR and GBE samples. Microstructural examination revealed that the grain coarsening and the liquation events were less prominent in the GBE samples as compared to the AR samples. It is believed that the reduced segregation of impurities to the special boundaries (coherent Ʃ3 twins, in particular) present in the GBE samples is responsible for the observed improvement in the HAZ liquation cracking resistance.

36 MATERIALS SCIENCE↗

Dislocation arrangements within slip bands during fatigue cracking

Highlights: • Dislocation cells form near early slip bands fatigue cracks in wavy-slip materials. • Lattice rotates severely and grain boundaries form between neighboring cells. • The walls of dislocation cells are preferential sites for fatigue cracking. - Abstract: Microstructures and dislocations associated with the slip band (SB) fatigue cracks were investigated in Cu single crystal and bicrystal. It is found that there are high strain localizations with abundant dislocation cells around the cracked SBs. Due to the high local strain and slip irreversibility, the lattice rotates severely leading to large misorientation and hence low- or high- angle grain boundaries could form between the neighboring cells. Moreover, the dislocation walls can serve as preferential sites for nucleation and propagation of fatigue cracks with high density of dislocations, vacancies and high strain incompatibility.