Microstructural development in DED stainless steels: applying welding models to elucidate the impact of processing and alloy composition

Austenitic stainless steel microstructures produced by directed energy deposition (DED)are analogous to those developed during welding, particularly high energy density welding. To better understand microstructural development during DED, theories of microstructural evolution,which have been established to contextualize weld microstructures, are applied in this study to microstructural development in DED austenitic stainless steels. Phenomenological welding models that describe the development of oxide inclusions, compositional microsegregation, ferrite,matrix austenite grains, and dislocation substructures are utilized to clarify microstructural evolution during deposition of austenitic stainless steels. Two different alloys, 304L and 316L, arecompared to demonstrate the broad applicability of this framework for understanding microstmctural development during the DED process. Despite differences in grain morphology and solidification mode for these two alloys (which can be attributed to compositional differences),similar tensile properties are achieved. It is the fine-scale compositional segregation and dislocation structures that ultimately determine the strength of these materials. The evolution of microsegregation and dislocation structures is shown to be dependent on the rapid solidification and thermomechanical history of the DED processing method and not the composition of the starting material.

36 MATERIALS SCIENCE↗

Experimental Investigation of Mechanical Performance and Printability of Gamma-Irradiated Additively Manufactured ABS

The work presented in this paper investigates the effects of gamma radiation on ABS in forms of irradiated 3D-printed parts, and irradiated filament used to later 3D-printed parts, using a cobalt-60 gamma irradiator. Tensile and flexural test samples were fabricated using off-the-shelf FDM 3D printers and irradiated at different dosages. Mechanical properties including elastic and flexure moduli, ultimate and flexural strength, % elongation at break, and surface hardness were evaluated, and results were compared to a control group. Evidence of cross-linking and chain scission and signs of possible oxidation of polymer caused by irradiation were found in both test groups which led to changes in mechanical properties. Moreover, it was found that ABS filament retains its printability after absorbing 15 kGy of gamma radiation and that its mechanical performance is very similar to those of irradiated samples at the same dose. Obtained results show promise for using ABS to fabricate sterile surgical instruments.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Strain Rate on the Tensile Behavior of CoCrFeNi and CoCrFeMnNi High-Entropy Alloys

High-entropy alloys (HEAs), a novel class of metal alloys, have been receiving increasing attention from the scientific community. HEAs have the potential to be used in critical load-bearing applications in replacement of conventional alloys such as stainless steel and nickel-base superalloys. Tensile experiments at quasi-static to dynamic strain rates (10{sup −4}-10{sup 3} s{sup −1}) were performed on two single-phase face-centered cubic HEAs, CoCrFeNi and CoCrFeMnNi. Electron backscatter diffraction was used to study the microstructure of the samples before the experiments, and transmission electron microscopy was performed postmortem. The dominant deformation mechanisms were dislocation slip at quasi-static strain rates with the addition of deformation nano-twins at dynamic strain rates. Ultimate dynamic tensile strength and ductility improved with the increase in strain rate, which can be attributed to the activation of deformation nano-twins in HEAs. CoCrFeNi and CoCrFeMnNi both have low stacking fault energies, which could promote twinning at high strain rates to accommodate plastic deformation. The strain rate sensitivity of the flow stress increased with increasing strain rate, beginning with negligible strain rate sensitivity in the quasi-static range to high strain rate sensitivity in the dynamic range. CoCrFeMnNi showed greater strain rate sensitivity of flow stress. CoCrFeNi, with less configurational entropy, had higher mechanical properties and strain-hardening rates compared to CoCrFeMnNi, which was attributed to the weakening effect of the addition of Mn on the solid solution hardening.

36 MATERIALS SCIENCE↗

Parametric Studies Of Weld Quality Of Tungsten Inert Gas Arc Welding Of Stainless Steel

Effect of current and gas flow rate on quality of weld in tungsten inter gas arc welding of austenitic stainless steel has been studied in the present work through experiments and analyses. Butt welded joints have been made by using several levels of current and gas flow rate. The quality of the weld has been evaluated in terms of ultimate and breaking strengths of the welded specimens. The observed data have been interpreted, discussed and analyzed by using Grey--Taguchi methodology. Optimum parametric setting has been predicted and validated as well.

36 MATERIALS SCIENCE↗

Manufacturing process modeling for composite materials and structures, Sandia blade reliability collaborative

The increased use and interest in wind energy over the last few years has necessitated an increase in the manufacturing of wind turbine blades. This increase in manufacturing has in many ways out stepped the current understanding of not only the materials used but also the manufacturing methods used to construct composite laminates. The goal of this study is to develop a list of process parameters which influence the quality of composite laminates manufactured using vacuum assisted resin transfer molding and to evaluate how they influence laminate quality. Known to be primary factors for the manufacturing process are resin flow rate and vacuum pressure. An incorrect balance of these parameters will often cause porosity or voids in laminates that ultimately degrade the strength of the composite. Fiber waviness has also been seen as a major contributor to failures in wind turbine blades and is often the effect of mishandling during the lay-up process. Based on laboratory tests conducted, a relationship between these parameters and laminate quality has been established which will be a valuable tool in developing best practices and standard procedures for the manufacture of wind turbine blade composites.

Guest, Daniel A.↗

Task 1, Milestone 1 - Alloy Selection

The selection of a nickel-base alloy from candidate materials, Alloy X, INCONEL® 740H®, Alloy 230, Alloy 617 and Haynes® 282®, for which to investigate the creep-fatigue properties and assess applicable creep-fatigue design rules, has involved consideration of the availability of creep-fatigue and creep property data and alloy strength as well as other factors. Ultimately, the higher tensile and creep strength combined with a large, available database of creep properties and a single step ageing treatment lead to the selection of INCONEL® 740H for further creep-fatigue study.

14 SOLAR ENERGY↗

The Integrity of ACSR Full Tension Single-Stage Splice Connector at Higher Operation Temperature

Due to increases in power demand and limited investment in new infrastructure, existing overhead power transmission lines often need to operate at temperatures higher than those used for the original design criteria. This has led to the accelerated aging and degradation of splice connectors. It is manifested by the formation of hot-spots that have been revealed by infrared imaging during inspection. The implications of connector aging is two-fold: (1) significant increases in resistivity of the splice connector (i.e., less efficient transmission of electricity) and (2) significant reductions in the connector clamping strength, which could ultimately result in separation of the power transmission line at the joint. Therefore, the splice connector appears to be the weakest link in electric power transmission lines. This report presents a protocol for integrating analytical and experimental approaches to evaluate the integrity of full tension single-stage splice connector assemblies and the associated effective lifetime at high operating temperature.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Improving the Fracture Toughness and Ductility of Liquid-Phase Sintered WNiFe Tungsten Heavy Alloys by High-Temperature Annealing

Tungsten heavy alloys (WHAs) are candidates for use in fusion reactor divertors. Here, we characterize liquid-phase sintered WHAs with 90, 92.5, 95, and 97 (wt.%) tungsten (W), with a balance of a 0.7Ni–0.3Fe ductile phase. These WHAs show remarkable room temperature (RT) fracture toughness at the maximum load, K Jm , ranging from ≈ 38 to 107 MPa√m, compared to a monolithic W toughness of ≈ 8 MPa√m. In most cases, the fracture of WHAs occurs through stable crack tearing. However, the 97W WHA has the lowest toughness and fracture elastically in all but the smallest specimens. As lower Ni contents are desirable for fusion application, we explore the potential for improving the ductility and K Jm of WHAs using vacuum annealing at 1300 °C for 24 h. The microstructural observations reveal negligible changes in the WHA microstructure and constituent compositions. While annealing reduces the Vickers microhardness (HV), it does not significantly change the RT yield (σ y ) and ultimate (σ u ) strengths but results in beneficial increases in total elongation in the 95 and 97W WHAs by a factor of 2. RT tests on the precracked three-point-bend (3PB) bars show that annealing increases the K Jm of these WHAs, and in the case of the 97W WHA, the increase is from 42 to 92%, depending on the size of the specimen. Toughening is due to enhanced crack tip process zone microcracking and dilatation.

36 MATERIALS SCIENCE↗

Protoplanetary Disks as (Possibly) Viscous Disks

Protoplanetary disks are believed to evolve on megayear timescales in a diffusive (viscous) manner as a result of angular momentum transport driven by internal stresses. Here we use a sample of 26 protoplanetary disks resolved by ALMA with measured (dust-based) masses and stellar accretion rates to derive the dimensionless α-viscosity values for individual objects, with the goal of constraining the angular momentum transport mechanism. We find that the inferred values of α do not cluster around a single value, but instead have a broad distribution extending from 10{sup −4} to 0.04. Moreover, they correlate with neither the global disk parameters (mass, size, surface density) nor the stellar characteristics (mass, luminosity, radius). However, we do find a strong linear correlation between α and the central mass accretion rate M-dot . This correlation is unlikely to result from the direct physical effect of M-dot on internal stress on global scales. Instead, we suggest that it is caused by the decoupling of stellar M-dot from the global disk characteristics in one of the following ways: (1) The behavior (and range) of α is controlled by a yet-unidentified parameter (e.g., ionization fraction, magnetic field strength, or geometry), ultimately driving the variation of M-dot . (2) The central M-dot is decoupled from the global accretion rate as a result of an instability, or mass accumulation (or loss in a wind or planetary accretion) in the inner disk. (3) Perhaps the most intriguing possibility is that angular momentum in protoplanetary disks is transported nonviscously, e.g., via magnetohydrodynamic winds or spiral density waves.

79 ASTRONOMY AND ASTROPHYSICS↗

Design guidelines for use of adhesives in hybrid microcircuits

Although it is generally accepted that the use of adhesives in the assembly of hybrid microcircuits offers advantages over other bonding methods, there currently does not exist a set of guidelines for the selection of adhesives which will insure that hybrid microcircuits assembled with them will meet the long use-life, high-reliability requirements of electronic equipment for space applications. This study was directed to the identification of the properties of electrically insulative adhesives that potentially could cause problems in such an application, and to the development of evaluation tests to quantify these properties and thus form the basis for establishing suitable guidelines and, ultimately, specifications. Bond strength, outgassing after cure, and corrosivity were selected for detailed attention since they are considered to be especially critical. Introductory discussion includes enumeration and brief comments on the properties of adhesives considered to be important for the proposed application, a general review of polymeric types of adhesives, and identification of the major types of adhesives commercially available and specifically designed for microelectronic use. The specific tests developed to evaluate bond strength, outgassing after cure, and corrosivity are discussed in detail, and comparative results obtained for selected adhesives representative of the major types are given.

Caruso, S. V.↗

High-temperature, low-cycle fatigue of advanced copper-base alloys for rocket nozzles. Part 1: Narloy Z

Short-term tensile and low-cycle fatigue data are reported for Narloy Z, a centrifugally cast, copper-base alloy. Tensile tests were performed at room temperature in air and in argon at 482, 538 and 593 C using an axial strain rate of .002/sec to the -1 power. In addition tensile tests were performed at 538 C in an evaluation of tensile properties at strain rates of .004 and .01/sec to the -1 power. Ultimate and yield strength values of about 315 and 200 MN/sq m respectively were recorded at room temperature and these decreased to about 120 and 105 respectively as the temperature was increased to 593 C. Reduction in area values were recorded in the range from 40 to 50% with some indication of a minimum ductility point at 538 C.

Conway, J. B.↗

An anticorrelation between polar and equatorial rotation of the solar photosphere

Published spectroscopic measurements of solar rotation are analyzed to show that when the rotation velocity increases at high latitudes it tends to decrease at low latitudes, and that when the rotation velocity decreases at high latitudes it increases at low latitudes. The high-latitude velocities typically vary over only 20% of the range of those near the equator and the smallest variations of all occurred near latitude 60 deg during the rising portion of the previous solar cycle. The anticorrelation is consistent with a recent suggestion that differential rotation on the sun arises from photospheric wind systems whose strength is determined, ultimately, by oscillations within the sun.

Wolff, C. L.↗

Microstructure and mechanical properties of quenched and tempered 300M steel

Type 300M steel, which is being used for the landing gear on the space shuttle orbiter, was subjected to a wide range of quenched and tempered heat treatments. The plane-strain fracture toughness and the tensile ultimate and yield strengths were evaluated. Cryogenic mechanical properties were obtained for conventionally heat-treated steel. The microstructure of all heat-treated test coupons was studied both optically and by transmission electron microscopy. Fracture surfaces were studied by means of scanning electron microscopy. Results indicate that substantial improvement in toughness with no loss in strength can be accomplished in quenched and tempered steel by austenitizing at 1255 K or higher. Low fracture toughness in conventionally austenitized 300M steel (1144 K) appears to be caused by undissolved precipitates, seen both in the submicrostructure and on the fracture surface, which promote failure by quasi-cleavage. The precipitates appeared to dissolve in the range 1200 to 1255 K.

Youngblood, J. L.↗

Study of high performance alloy electroforming

The first series of heat treated nickel manganese alloys are tested for mechanical properties at temperatures of 148.9 C (300 F) and 260 C (500 F). All material receives the same heat treatment in order to provide a common basis for comparison of results. Mechanical property performance improves with increasing manganese content in the alloy. Although all manganese bearing alloy is significantly superior to conventional electroformed nickel, samples containing over 3000 ppm manganese display outstanding ultimate and yield strengths while maintaining reasonably satisfactory ductility. Alloy containing over 6000 ppm of manganese is very competitive to Inconel 718 (mill annealed and age hardened) at all temperatures of interest, although ductility is not as great in the electrodeposited counterpart.

Malone, G. A.↗

Study of high performance alloy electroforming

More panels electroformed with intentional variations of pulse plating parameters are being made. Pulse plating frequency was noted to have a significant effect regarding mechanical properties. The use of a high pulse frequency (assuming fixed duty cycles) results in an increase in ductility and a decrease in ultimate and yield strengths. Electroforming to intermediate frequencies is being done to obtain the best possible combination of ductility and strength. Results of some tests from high frequency specimens are tabulated.

Malone, G. A.↗

High-temperature properties of ceramic fibers and insulations for thermal protection of atmospheric entry and hypersonic cruise vehicles

Multilayer insulations (MIs) which will operate in the 500 to 1000 C temperature range are being considered for possible applications on aerospace vehicles subject to convective and radiative heating during atmospheric entry. The insulations described consist of ceramic fibers, insulations, and metal foils quilted together with ceramic thread. As these types of insulations have highly anisotropic properties, the total heat transfer characteristics must be determined. Data are presented on the thermal diffusivity and thermal conductivity of four types of MIs and are compared to the baseline Advanced Flexible Reusable Surface Insulation currently used on the Space Shuttle Orbiter. In addition, the high temperature properties of the fibers used in these MIs are discussed. The fibers investigated included silica and three types of aluminoborosilicate (ABS). Static tension tests were performed at temperatures up to 1200 C and the ultimate strain, tensile strength, and tensile modulus of single fibers were determined.

Kourtides, Demetrius A.↗

High temperature properties of ceramic fibers and insulations for thermal protection of atmospheric entry and hypersonic cruise vehicles

Multilayer insulations (MIs) which will operate in the 500 to 1000 C temperature range are being considered for possible applications on aerospace vehicles subject to convective and radiative heating during atmospheric entry. The insulations described consist of ceramic fibers, insulations, and metal foils quilted together with ceramic thread. As these types of insulations have highly anisotropic properties, the total heat transfer characteristics must be determined. Data are presented on the thermal diffusivity and thermal conductivity of four types of MIs and are compared to the baseline Advanced Flexible Reusable Surface Insulation currently used on the Space Shuttle Orbiter. In addition, the high temperature properties of the fibers used in these MIs are discussed. The fibers investigated included silica and three types of aluminoborosilicate (ABS). Static tension tests were performed at temperatures up to 1200 C and the ultimate strain, tensile strength, and tensile modulus of single fibers were determined.

Kourtides, Demetrius A.↗

Polymer derived Nicalon/Si-C-O composites - Processing and mechanical behavior

Ceramic matrix composites fabricated using Nicalon fiber and several polysilsesquioxane-derived Si-C-O matrices were characterized by optical and SEM and in four-point bending. In the matrix material linear shrinkages of up to 19 percent were observed for the vinylmethyl copolymer pyrolyzed to 1200 C, and up to 13 percent for the phenylmethyl material pyrolyzed to the same temperature, resulting in considerable matrix cracking. Under four-point loading, most composite samples fractured in a brittle manner as the result of strong fiber-matrix bonding. Flexural strengths, moduli, and ultimate strain varied with fiber sizing and processing parameters. Testing and analysis is being applied to promote more fibrous pullout during fracture.

Hurwitz, Frances I.↗