Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Tensile testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 901 records · Page 50

Master Curve Fracture Toughness Characterization of Eurofer97 Steel Variants Using Miniature Multi-Notch Bend Bar Specimens for Fusion Applications

In this study, we performed fracture toughness testing of ten Eurofer97 steel variants using precracked miniature multi-notch bend bar (M4CVN) specimens based on the Master Curve method in the ASTM E1921 standard. Additional Vickers microhardness and room temperature tensile testing complemented the fracture toughness testing. Compared with standard Eurofer97, the ten variants didn’t show a comprehensive improvement of mechanical properties. The Master Curve method was found to yield a reasonable prediction of fracture toughness results obtained from M4CVN specimens with most valid fracture toughness data within the 2% and 98% tolerance boundaries of the Master Curve. The three-parameter Weibull distribution with Weibull exponent b = 4 also yielded excellent prediction of the relationship between fracture toughness results KJc and the cumulative probability for failure pf for one steel variant.

Chen, Xiang↗

Investigation of thermal aging effects on the tensile properties of Alloy 617 by in-situ synchrotron wide-angle X-ray scattering

The nickel-base Alloy 617 has been considered as the lead candidate structural material for the intermediate heat exchanger (IHX) of the Very-High-Temperature Reactor (VHTR). In order to assess the long-term performance of Alloy 617, thermal aging experiments up to 10,000 h in duration were performed at 1000 degrees C. Subsequently, in-situ synchrotron wide-angle X-ray scattering (WAXS) tensile tests were carried out at ambient temperature. M23C6 carbides were identified as the primary precipitates, while a smaller amount of M6C was also observed. The aging effects were quantified in several aspects: (1) macroscopic tensile properties, (2) volume fraction of the M23C6 Phase, (3) the lattice strain evolution of both the matrix and the M23C6 precipitates, and (4) the dislocation density evolution during plastic deformation. The property-microstructure relationship is described with a focus on the evolution of the M23C6 phase. For aging up to 3000 h, the yield strength (YS) and ultimate tensile strength (UTS) showed little variation, with average values being 454 MPa and 787 MPa, respectively. At 10,000 h, the YS and UTS reduced to 380 MPa and 720 MPa, respectively. The reduction in YS and UTS is mainly due to the coarsening of the M23C6 Precipitates. After long term aging, the volume fraction of the M23C6 phase reached a plateau and its maximum internal stress was reduced, implying that under large internal stresses the carbides were more susceptible to fracture or decohesion from the matrix. Finally, the calculated dislocation densities were in good agreement with transmission electron microscopy (TEM) measurements. The square roots of the dislocation densities and the true stresses displayed typical linear behavior and no significant change was observed in the alloys in different aging conditions.

Alloy 617↗

Cold work study on a 316LN modified alloy for the ITER TF coil conduit

The primary structural component of the cable-in-conduit conductor (CICC) magnets, such as the ITER TF coils is the conduit. This function creates requirements for 4 K strength, toughness, fatigue crack resistance, and ductility after exposure to the superconductor's reaction heat treatment. The tensile ductility of a steel is a quality factor related to fatigue and fracture resistance that can be evaluated more economically with tensile tests rather than fatigue and fracture tests. We subject 316LN modified base metal and welds to a range of cold work from 0% to 20% and a subsequent Nb 3 Sn reaction heat treatment to evaluate the effects on the tensile properties. With the addition of cold work, the 4 K yield strength increases while tensile elongation decreases in both the base metal and weld. Our results are compared to previously published data on the same alloy to evaluate the use of tensile ductility parameters as a materials qualification specification in magnet design.

36 MATERIALS SCIENCE↗

Material property for designing, analyzing, and fabricating space structures

An analytical study was made of plasma assisted bullet projectile. The finite element analysis and the micro-macromechanic analysis was applied to an optimum design technique for the multilayered graphite-epoxy composite projectile that will achieve hypervelocity of 6 to 10 Km/s. The feasibility was determined of dialectics to monitor cure of graphite-epoxies. Several panels were fabricated, cured, and tested with encouraging results of monitoring the cure of graphite-epoxies. The optimum cure process for large structures was determined. Different orientation were used and three different curing cycles were employed. A uniaxial tensile test was performed on all specimens. The optimum orientation with the optimum cure cycle were concluded.

Kolkailah, Faysal A.↗

Determination of cleavage planes and fracture characterization of Ni-based single crystal superalloys

The room temperature fracture behavior of the Ge Rene N-4, CMSX-2, and CMSX-4C single crystal Ni-based superalloys was studied. All crystals were grown along the (001) direction and tensile tested in both helium and hydrogen atmospheres. A stereoscopic technique developed for use with a scanning electron microscope was applied to determine cleavage planes. Planar gamma(') morphologies also were examined to help determine cleavage planes. Helium charged specimens failed on a number of planes including the (111), (110), and (320). In most cases planes of the (111)-type initiated at the notch region and became smaller and smaller as they moved in radially. Tensile strengths in helium averaged 1000 MPa higher than that of the hydrogen charged specimens. Specimens tested in hydrogen generally failed on (100)-type planes originating from the notch region. This (100) region comprised 60 to 80 percent of the total fracture surface on most samples and appeared as large flat planes perpendicular to the growth direction of the crystal. The interior regions contained (100)-type planes as well as (321), (320), (210), and (111)-types. Hydrogen charged specimens also showed a high percentage of large cracks oriented at 90 deg to one another, indicative of the (100)-type fracture. The Ge Rene N4 and the CMSX-4C samples contained 3-5 percent gamma/gamma(') eutectic, while the CMSX-2 samples had little or no gamma/gamma(') eutectic. The relationship between gamma/gamma(') eutectic and the fracture surface has not been fully determined, but it is thought that the gamma/gamma(') eutectic may serve as a possible trapping site for hydrogen.

Merrill, John M.↗

Effect of Ce addition on the microstructure and properties of Al-Cu-Mn-Mg-Fe lithium battery shell alloy

Highlights: • Al{sub 6}(Mn, Fe) particles could be remarkably refined by Ce alloying. • Ce addition to the alloy promoted precipitation of S' phase. • Ce-containing alloy had higher tensile strength than that of Ce-free alloy. • Ce-containing alloy had positive corrosion potential and lower corrosion current density. - Abstract: Effect of Ce addition on the microstructures, mechanical properties and electrochemical properties of Al-Cu-Mn-Mg-Fe lithium battery alloy was investigated by optical microscope (OM), X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), tensile testing and electrochemical testing. Experimental results indicate that Ce addition resulted in the formation of Al{sub 8}Cu{sub 4}Ce phase in the Al-Cu-Mn-Mg-Fe alloy. The Ce-containing precipitates nucleated and grew up along the surface of Al{sub 6}(Mn, Fe) precipitates. Al{sub 6}(Mn, Fe) precipitates could be remarkably refined by Ce alloying. The aging precipitation behavior of S' phases could be promoted after Ce addition to the alloy. In comparison with Ce-free alloy, the Ce-containing alloy had higher tensile strength at both low temperature and elevated temperature. Especially at 200 °C, the yield strength and tensile strength of Ce-containing alloy substantially increased by 23.4% and 27.08%, respectively. Potentiodynamic polarization testing indicated that the Ce-containing alloy had a more positive corrosion potential and a lower corrosion current density.

36 MATERIALS SCIENCE↗

The Effects of Fiber Orientation and Adhesives on Tensile Properties of Carbon Fiber Reinforced Polymer Matrix Composite with Embedded Nickel-Titanium Shape Memory Alloys

Tensile tests of Nickel-titanium (NiTi) shape memory alloys (SMA) embedded within carbon fiber reinforced polymer matrix composite (CFRP/PMC) laminates were evaluated with simultaneous monitoring of modal acoustic emissions (MAE). Three different layup configurations utilizing two different thin film adhesives were applied to bond the materials. Ultimate tensile strengths, strains, and moduli were obtained along with cumulative AE energy of events and specimen failure location. Scanning electron microscopy was used to examine the break areas of the specimens post-test. Microscopy was used to validate failure locations revealed from MAE analysis. A unique finding within this research showed that 90° plies in the outer ply gave the strongest acoustic signals as well as the cleanest fracture of the specimens tested. Overlapping 0° ply layers surrounding the SMA was found to be the best scenario to prevent failure of the specimen itself.

Derek Quade↗

Effect of Orientation of Weld Line on Formability of Electron Beam-Welded Dissimilar Thickness Titanium Sheets

Recently, manufacturing industries are looking forward to get insight into the influence of weld orientation on formability of tailor-welded blanks (TWBs) of titanium sheets for design and fabrication of lightweight components. Hence, commercially pure titanium (CP Ti) sheets of 1.0 and 1.2 mm thickness were joined together by electron beam welding process using accelerating voltage of 55 kV, beam current of 14.9 mA and welding speed of 865 mm/min. Two different types of TWBs with weld line perpendicular to the rolling direction (WL ⊥ RD) and weld line parallel to the rolling direction (WL || RD) were fabricated, and subsequently, the tensile test, microstructure and microhardness characterizations were conducted to ensure quality of weld. The limiting dome height (LDH) tests were carried out using laboratory-scale setup to evaluate forming behavior of both the above TWBs in terms of FLD, strain distribution, weld line movement and failure location. It was found that the tensile stress–strain response and formability performance of TWBs were significantly influenced by weld line orientation with lower ductility, ultimate tensile strength and LDH in TWB of WL || RD. Moreover, significant weld line movement and non-uniform strain distribution with necking and subsequently fracture were observed away from the weld line in thinner 1.0 mm CP Ti sheets depending on both sample geometry and weld line orientation.

36 MATERIALS SCIENCE↗

Hypervelocity impact testing of tethers

An experimental test program has been conducted to ascertain the strength losses to which representative space tether materials may be prone upon impact by hypervelocity particles of known size, density, and velocity, when the tether is under tensile loading typical of flight design loads. Twelve hypervelocity impacts were followed by tensile tests to failure to determine residual strength; relationships are established between particle velocity and strength loss due to impact damage, as well as between tether strength loss and the relationship between particle and tether diameters. Tentative design criteria are formulated in terms of a design factor allowing for strength degradation by impact.

Woodis, William R.↗

Effect of Strain Rate on Mechanical Properties of Wrought Sintered Tungsten at Temperatures above 2500 F

Specimens of wrought sintered commercially pure tungsten were made from 1/8-inch swaged rods. All the specimens were recrystallized at 4050 F for 1 hour prior to testing at temperatures from 2500 to 4000 F at various strain rates from 0.002 to 20 inches per inch per minute. Results showed that, at a constant temperature, increasing the strain rate increased the ultimate tensile strength significantly. The effects of both strain rate and temperature on the ultimate tensile strength of tungsten may be correlated by the linear parameter method of Manson and Haferd and may be used to predict the ultimate tensile strength at higher temperatures, 4500 and 5000 F. As previously reported, ductility, as measured by reduction of area in a tensile test, decreases with increasing temperature above about 3000 F. Increasing the strain rate at temperatures above 3000 F increases the ductility. Fractures are generally transgranular at the higher strain rates and intergranular at the lower strain rates.

Sikora, Paul F.↗

Effects of Long Term Exposures on PM Disk Superalloys

Turbine disks in some advanced engine applications may be exposed to temperatures above 700 C for extended periods of time, approaching 1,000 h. These exposures could affect the near-surface composition and microstructure through formation of damaged and often embrittled layers. The creation of such damaged layers could significantly affect local mechanical properties. Powder metal disk superalloys LSHR and ME3 were exposed at temperatures of 704, 760, and 815 C for times up to 2,020 h, and the types and depths of environmental attacked were measured. Fatigue tests were performed for selected cases at 704 and 760 C, to determine the impact of these exposures on fatigue life. Fatigue resistance was reduced up to 98% in both superalloys for some exposure conditions. Tensile tests were also performed to help understand fatigue responses, and showed corresponding reductions in ductility. The changes in surface composition and phases, depths of these changed layers, failure responses, and failure initiation modes were compared.

Heat resistant allos↗

Evolving Density and Static Mechanical Properties in Plutonium from Self-Irradiation

Plutonium, because of its self-irradiation by alpha decay, ages by means of lattice damage and helium in-growth. These integrated aging effects result in microstructural and physical property changes. Because these effects would normally require decades to measure, studies are underway to assess the effects of extended aging on the physical properties of plutonium alloys by incorporating roughly 7.5 weight % of highly specific activity isotope {sup 238}Pu into the {sup 239}Pu metal to accelerate the aging process. This paper presents updated results of self-irradiation effects on {sup 238}Pu-enriched alloys measured by immersion density, dilatometry, and tensile tests. After nearly 90 equivalent years of aging, both the immersion density and dilatometry show that the enriched alloys continue to decreased in density by {approx}0.002% per year, without void swelling. Quasi-static tensile measurements show that the aging process increases the strength of plutonium alloys.

36 MATERIALS SCIENCE↗

Space Environmental Effects on Additively Manufactured (AM) Parts on MISSE-9/10

The Materials on International Space Station Experiment (MISSE) experiments have made a continuous presence on the ISS and allowed for testing of performance and durability of materials exposed to the Low Earth Orbit (LEO) space environment. Additive Manufacturing (AM) has been included on several MISSE flights, and many companies (Made in Space and Stratasys) and NASA centers wanted to test various AM material samples. The goal of studying Space Environmental Effects on AM Parts with MISSE 9/10 was to fly promising metal and polymer AM material samples (dogbones) that could have future manufacturing capabilities in space and conduct post-flight analysis of these materials via mechanical and optical properties. On these flights, MISSE-9 contained three Inconel and 12 polymer samples and MISSE-10 included three Inconel and 16 polymer samples. Before flying to the ISS, all the samples underwent thermal vacuum bakeout (at 60°C for 24 hours and 10-6 torr). After bakeout, control and flight experiments were weighed, and optical properties were taken. Optical properties such as solar absorptance and infrared emittance were taken on the control samples and the flight samples (preflight and postflight). To understand more about the mechanical properties of the AM samples, tensile testing was conducted on the samples to determine the yield and ultimate tensile strength of the dogbone samples against the control. Lastly, the torque on the fasteners securing the dogbone samples were loosened and measured using a torque wrench, and they were compared to their preflight torque specification required. Optical properties and masses were recorded before flight, and the postflight results were recorded and collected in June 2022 to study the effects. With the postflight analysis, NASA engineers can now better characterize how UV radiation and thermal cycling affect the material properties.

Materials on International Space Station Experimen↗

Fatigue strength of a single lap joint SPR-bonded

In the last years, hybrid joints, meaning with this the joints which consist in combining a traditional mechanical joint to a layer of adhesive, are gradually attracting the attention of various sectors of the construction of vehicles and transportation industries, for their better performance compared to just mechanical joints (self-piercing riveting SPR, riveting, and so on) or just to bonded joints.The paper investigates the fatigue behavior of a single lap joint self-piercing riveted (SPR) and bonded throughout fatigue tests. The considered geometric configuration allowed the use of two rivets placed longitudinally; an epoxy resin was used as adhesive. In the first part of the work static characterization of the joints was carried out through tensile tests. Then fatigue tests were made with the application of different levels of load. The fatigue curves were also obtained at the varying the distance between the two rivets in order to better assess the joint strength for a given length of overlap.

36 MATERIALS SCIENCE↗

Imide modified epoxy matrix resins

Results of a program designed to develop tough imide modified epoxy (IME) resins cured by bisimide amine (BIA) hardeners are presented. State of the art epoxy resin, MY720, was used. Three aromatic bisimide amines and one aromatic aliphatic BIA were evaluated. BIA's derived from 6F anhydride (3,3 prime 4,4 prime-(hexafluoro isopropyl idene) bis (phthalic anhydride) and diamines, 3,3 prime-diam nodiphenyl sulfone (3,3 prime-DDS), 4,4 prime-diamino diphenyl sulfone (4,4 prime-DDS), 1.12-dodecane diamine (1,12-DDA) were used. BIA's were abbreviated 6F-3,3 prime-DDS, 6F-4,4 prime-DDS, 6F-3,3 prime-DDS-4,4 prime DDS, and 6F-3,3 prime-DDS-1,12-DDA corresponding to 6F anhydride and diamines mentioned. Epoxy resin and BIA's (MY720/6F-3,3 prime-DDS, MY720/6F-3,3 prime-DDS-4,4 prime-DDS, MY720/6F-3,3 prime-DDS-1,12-DDA and a 50:50 mixture of a BIA and parent diamine, MY720/6F-3,3 prime-DDS/3,3 prime-DDS, MY720/6F-3,3 prime-DDS-4,4 prime-DDS/3,3 prime-DDS, MY720/6F-3,3 prime-DDS-1,12-DDA/3,3 prime-DDS were studied to determine effect of structure and composition. Effect of the addition of two commercial epoxies, glyamine 200 and glyamine 100 on the properties of several formulations was evaluated. Bisimide amine cured epoxies were designated IME's (imide modified epoxy). Physical, thermal and mechanical properties of these resins were determined. Moisture absorption in boiling water exhibited by several of the IME's was considerably lower than the state of the art epoxies (from 3.2% for the control and state of the art to 2.0 wt% moisture absorption). Char yields are increased from 20% for control and state of the art epoxies to 40% for IME resins. Relative toughness characteristics of IME resins were measured by 10 deg off axis tensile tests of Celion 6000/IME composites. Results show that IME's containing 6F-3,3 prime-DDS or 6F-3,3 prime-DDS-1,12-DDA improved the "toughness" characteristics of composites by about 35% (tensile strength), about 35% (intralaminar shear strength), and about 78% (shear strain to failure) relative to the control composite.

Scola, D. A.↗

Degradation of Teflon(tm) FEP Following Charged Particle Radiation and Rapid Thermal Cycling

During the Second Servicing Mission (SM2) of the Hubble Space Telescope (HST) severe degradation was observed on the outer layer of the thermal control blankets. Astronaut observations and photographs revealed large cracks in the metallized Teflon FEP (fluorinated ethylene propylene), the outer layer of the multi-layer insulation (MLI), in many locations around the telescope. In an effort to understand what elements of the space environment might cause such damage, pristine Teflon' FEP was tested for durability to radiation and thermal cycling. Specimens were subjected to electron and proton fluences comparable to those experienced by HST and were subsequently thermal cycled in a custom-built rapid thermal cycle chamber. Tensile tests of the specimens showed that radiation followed by thermal cycling significantly reduced the ultimate strength and elongation of Teflon FEP.

Townsend, Jacqueline A.↗

Degradation of Teflon(tm) FEP Following Charged Particle Radiation and Rapid Thermal Cycling

During the Second Servicing Mission (SM2) of the Hubble Space Telescope (HST) severe degradation was observed on the outer layer of the thermal control blankets. Astronaut observations and photographs revealed large cracks in the metallized Teflon' FEP (fluorinated ethylene propylene), the outer layer of the multi-layer insulation (MLI), in many locations around the telescope. In an effort to understand what elements of the space environment might cause such damage, pristine Teflon(registered trademark) FEP was tested for durability to radiation and thermal cycling. Specimens were subjected to electron and proton fluences comparable to those experienced by HST and were subsequently thermal cycled in a custom-built rapid thermal cycle chamber. Tensile tests of the specimens showed that radiation followed by thermal cycling significantly reduced the ultimate strength and elongation of Teflon(registered trademark) FEP.

Townsend, Jacqueline A.↗

Degradation of Teflon(tm) FEP Following Charged Particle Radiation and Rapid Thermal Cycling

During the Second Servicing Mission (SM2) of the Hubble Space Telescope (HST) severe degradation was observed on the outer layer of the thermal control blankets. Astronaut observations and photographs revealed large cracks in the metallized Teflon(R) FEP (fluorinated ethylene propylene), the outer layer of the multi-layer insulation (MLI), in many locations around the telescope. In an effort to understand what elements of the space environment might cause such damage, pristine Teflon(R) FEP was tested for durability to radiation and thermal cycling. Specimens were subjected to electron and proton fluences comparable to those experienced by HST and were subsequently thermal cycled in a custom-built rapid thermal cycle chamber. Tensile tests of the specimens showed that radiation followed by thermal cycling significantly reduced the ultimate strength and elongation of Teflon(R) FEP.

Townsend, Jacqueline↗