Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SiC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 901 records · Page 50

Stacking fault analysis for the early-stages of PVT growth of 4H-SiC crystals

Here, four types of stacking fault formation mechanisms are identified and discussed for early stage PVT growth of 4H-SiC crystals: Type 1: Shockley / double Shockley stacking fault formation inside the facet; Type 2: Stacking fault formation via 2D nucleation; Type 3: Frank + Shockley (S) stacking fault formation due to deflection of threading mixed dislocation (TMD) by macrosteps; Type 4: “Carrot” defect formation related to overgrowth of the terrace formed by separation of 3c/4 and c/4 step risers after deflection of a TMD by vicinal steps. The results help further reduction of defect generation in 4H-SiC substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Atom-scale covalent electrochemical modification of single-layer graphene on SiC substrates by diaryliodonium salts

Owing to its high conductivity, graphene holds promise as an electrode for energy devices such as batteries and photovoltaics. However, to this end, the work function and doping levels in graphene need to be precisely tuned. One promising route for modifying graphene’s electronic properties is via controlled covalent electrochemical grafting of molecules. We show that by employing diaryliodonium salts instead of the commonly used diazonium salts, spontaneous functionalization is avoided. This then allows for precise tuning of the grafting density. Moreover, by employing bis(4-nitrophenyl)iodonium(III) tetrafluoroborate (DNP) salt calibration curves, the surface functionalization density (coverage) of glassy carbon was controlled using cyclic voltammetry in varying salt concentrations. These electro-grafting conditions and calibration curves translated directly over to modifying single layer epitaxial graphene substrates (grown on insulating 6H-SiC (0 0 0 1)). In addition to quantifying the functionalization densities using electrochemical methods, samples with low grafting densities were characterized by low-temperature scanning tunneling microscopy (LT-STM). We show that the use of buffer-layer free graphene substrates is required for clear observation of the nitrophenyl modifications. Furthermore, atomically-resolved STM images of single site modifications were obtained, showing no preferential grafting at defect sites or SiC step edges as supposed previously in the literature. Most of the grafts exhibit threefold symmetry, but occasional extended modifications (larger than 4 nm) were observed as well.

74 ATOMIC AND MOLECULAR PHYSICS↗

Nucleation and growth of vacancy clusters in β-SiC during irradiation

Molecular dynamics and molecular static calculations have been performed using the empirical many-body interatomic potential to obtain the formation and binding energies of relaxed configuration of vacancy clusters in β-SiC, which are necessary when the nucleation and growth process of clusters is investigated. The formation energy of vacancy clusters in β-SiC depends on the size, vacancy composition, and vacancy configuration of clusters. When the size and vacancy composition of clusters are given, the vacancy configuration of clusters with the lowest formation energy is primarily given so as to take the smallest number of dangling bonds. Especially when the fraction of the number of silicon vacancies to the number of carbon vacancies in clusters is quite high or quite low, the formation property of antisite defects in clusters becomes a key factor to determine the stable configuration of clusters.

36 MATERIALS SCIENCE↗

Molecular dynamics modeling of atomic displacement cascades in 3C-SiC: Comparison of interatomic potentials

We used molecular dynamics modeling of atomic displacement cascades to characterize the nature of primary radiation damage in 3C-SiC. We demonstrated that the most commonly used interatomic potentials are inconsistent with ab initio calculations of defect energetics. Both the Tersoff potential used in this work and a modified embedded-atom method potential reveal a barrier to recombination of the carbon interstitial and carbon vacancy which is much higher than the density functional theory (DFT) results. The barrier obtained with a newer potential by Gao and Weber is closer to the DFT result. This difference results in significant differences in the cascade production of point defects. We have completed both 10 keV and 50 keV cascade simulations in 3C-SiC at a range of temperatures. In contrast to the Tersoff potential, the Gao-Weber potential produces almost twice as many C vacancies and interstitials at the time of maximum disorder (~0.2 ps) but only about 25% more stable defects at the end of the simulation. Only about 20% of the carbon defects produced with the Tersoff potential recombine during the in-cascade annealing phase, while about 60% recombine with the Gao-Weber potential.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Atomistic structures of nano-engineered SiC and radiation-induced amorphization resistance

In this paper, nano-engineered 3C–SiC thin films, which possess columnar structures with high-density stacking faults and twins, were irradiated with 2 MeV Si ions at cryogenic and room temperatures. From cross-sectional transmission electron microscopy observations in combination with Monte Carlo simulations based on the Stopping and Range of Ions in Matter code, it was found that their amorphization resistance is six times greater than bulk crystalline SiC at room temperature. High-angle bright-field images taken by spherical aberration corrected scanning transmission electron microscopy revealed that the distortion of atomic configurations is localized near the stacking faults. Finally, the resultant strain field probably contributes to the enhancement of radiation tolerance of this material.

36 MATERIALS SCIENCE↗

SiC layer microstructure in AGR-1 and AGR-2 TRISO fuel particles and the influence of its variation on the effective diffusion of key fission products

Tristructural isotropic (TRISO) coated particle fuel is a promising fuel form for advanced reactor concepts such as high temperature gas-cooled reactors (HTGR) and is being developed domestically under the US Department of Energy’s Nuclear Reactor Technologies Initiative in support of Advanced Reactor Technologies. The fuel development and qualification plan includes a series of fuel irradiations to demonstrate fuel performance from the laboratory to commercial scale. The first irradiation campaign, AGR-1, included four separate TRISO fuel variants composed of multiple, laboratory-scale coater batches. The second irradiation campaign, AGR-2, included TRISO fuel particles fabricated by BWX Technologies with a larger coater representative of an industrial-scale system. The SiC layers of as-fabricated particles from the AGR-1 and AGR-2 irradiation campaigns have been investigated by electron backscatter diffraction (EBSD) to provide key information about the microstructural features relevant to fuel performance. The results of a comprehensive study of multiple particles from all constituent batches are reported. The observations indicate that there were microstructural differences between variants and among constituent batches in a single variant. Finally, insights on the influence of microstructure on the effective diffusivity of key fission products in the SiC layer are also discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase stability, swelling, microstructure and strength of Ti 3 SiC 2 -TiC ceramics after low dose neutron irradiation

In this study, M n+1 AX n (MAX) phase Ti 3 SiC 2 materials were neutron irradiated at ~400, ~630, and 700 °C to a fluence of ~2 × 10 25 n/m 2 (E > 0.1 MeV). After irradiation at ~400 °C, anisotropic c-axis dilation of ~1.5% was observed. Room temperature strength was reduced from 445 ± 29 MPa to 315 ± 33 MPa and the fracture surfaces showed flat facets and transgranular cracks instead of typical kink-band deformation and bridging ligaments. XRD phase analysis indicated an increase of 10–15 wt% TiC. After irradiation at ~700 °C there were no lattice parameter changes, ~5 wt% decomposition to TiC occurred, and strength was 391 ± 71 MPa and 378 ± 31 MPa. The fracture surfaces indicated kink-band based deformation but with lesser extent of delamination than as-received samples. Finally, Ti 3 SiC 2 appears to be radiation tolerant at ~400 °C, and increasingly radiation resistant at ~630–700 °C, but a higher temperature may be necessary for full recovery.

36 MATERIALS SCIENCE↗

A nanomechanical Raman spectroscopy based assessment of stress distribution in irradiated and corroded SiC

Silicon carbide (SiC) composites are under consideration for cladding and structural materials in various types of reactors. The effects of ion irradiation and corrosion on stress distribution due to mechanical loading on chemical vapor deposited (CVD) SiC were investigated here in this paper by using nanomechanical Raman spectroscopy (NMRS). The stress distribution was analyzed as a function of the oxide formation on a corroded specimen and as a function of ion-induced irradiation damage in an irradiated specimen. A finite element method (FEM) based model was developed based on local mechanical properties measured using nanoindentation to predict the NMRS measured stress distribution. The stress distribution was also predicted theoretically by using a stress concentration factor, which is a function of sample geometry and boundary conditions. The maximum stress obtained theoretically was in good agreement with the FEM model and NMRS based measurements. FEM results captured the stress variation trends and maximum stress value in the analyzed samples. NMRS measurements predicted that corrosion had a greater influence on increasing the maximum value of stress in comparison to ion irradiation. The increase in stress attributed to corrosion in comparison to ion irradiated samples was approximately 10%–20%.

36 MATERIALS SCIENCE↗

Distribution of defect clusters in the primary damage of ion irradiated 3C-SiC

We report a statistical analysis of sizes and compositions of clusters produced in cascades during irradiation of SiC. The results are obtained using molecular dynamics (MD) simulations of cascades caused by primary knock-on atoms (PKAs) with energies between 10 eV and 50 keV. The results are averaged over six crystallographic directions of the PKA and integrated over PKA energy spectrum derived from the Stopping and Range of Ions in Matter (SRIM) code. Specific results are presented for 1 MeV Kr ion as an example of an impinging particle. We find that distributions of cluster size n for both vacancies and interstitials obey a power law f = A/n S and these clusters are dominated by carbons defects. The fitted values of A and S are different than values reported for metals, which can be explained through different defect energetics and cascade morphology between the two classes of materials. In SiC, the average carbon ratio for interstitial clusters is 91.5%, which is higher than the ratio of C in vacancy clusters, which is 85.3%. Size and composition distribution of in-cascade clusters provide a critical input for long-term defect evolution models.

36 MATERIALS SCIENCE↗

Role of microstructure on CO corrosion of SiC layer in UO₂-TRISO fuel

The Advanced Gas Reactor Fuel Qualification and Development (AGR) program has focused on qualification of UCO kernel tristructural-isotropic (TRISO) particle fuel relative to UO₂ kernel TRISO particle fuel. However, a UO₂ kernel variant was included in the second AGR irradiation experiment (AGR-2) for comparison and to connect to historic fuel irradiation data. The development of a multiscale, post-irradiation examination (PIE) analysis approach through the AGR Program has allowed for a comprehensive understanding of individual particle failure. This approach has been applied to gain an understanding of SiC layer failure in UO₂ kernel TRISO fuel from AGR-2 after safety testing at 1600–1700 °C. Particle failure by intergranular CO corrosion, facilitated by a compromised inner pyrolytic carbon layer, has been confirmed through the combined application of modern x-ray computed tomography and electron microscopy techniques. In addition, a relationship between grain boundary character and CO corrosion has been identified. This finding provides an opportunity to develop mitigating strategies to improve the resilience of the SiC layer to CO corrosion in UO₂ TRISO fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hydrothermal corrosion of laser printed SiC fibers under extreme environment

We report SiC/SiC fiber composites are proposed cladding materials to improve the accident tolerance of commercial light water nuclear reactor fuel. To evaluate their viability, understanding the kinetics of corrosion under irradiation and high-temperature, high-pressure aqueous environment is critical. In the present work, the microstructure and mechanical properties of novel SiC fibers manufactured by Laser Chemical Vapor Deposition (LCVD) are introduced. The LCVD technology has control over microstructure and stoichiometry while allowing for high purity manufacturing, all key qualities needed in search of an optimum SiC fiber for nuclear energy applications. The isolated hydrothermal corrosion of commercially available carbon-rich Hi-Nicalon Type-S fibers is compared to the LCVD stoichiometric and LCVD silicon-rich fibers. Autoclave testing was carried out at 310°C and 14 MPa in the absence of irradiation. In a separate study, the effect of gamma irradiation on the fibers in the room-temperature environment was analyzed. It was observed from the experiments that the dissolution of the fibers was highly dependent on the stoichiometric ratio, fiber surface morphology and thermal pre-treatment of fibers. Contrary to previous findings, fiber dissolution was also visible under low-temperature gamma irradiation in aqueous environment with LCVD fibers showing lower dissolution.

36 MATERIALS SCIENCE↗

Irradiation stability and thermomechanical properties of 3D-printed SiC

Neutron irradiation tests were carried out on 3D-printed SiC derived from binderjet additive manufacturing and chemical vapor infiltration. Irradiation was carried to 2.3 dpa over a temperature range of 400–850 °C. Anisotropy that had been observed in the thermal conductivity of 3D-printed SiC prior to irradiation vanished after irradiation as the irradiation defect thermal resistivity accumulated in the material. No degradation in strength was observed in the material before or after irradiation, at various temperatures, or in different orientations. Electron microscopy of the microstructure after neutron irradiation showed distinct defect morphologies in the heterogenous material, but no evidence for irradiation-induced cracking or degradation in the microstructure was observed.

36 MATERIALS SCIENCE↗

Fission gas retention of densely packed uranium carbonitride tristructural-isotropic fuel particles in a 3D printed SiC matrix

The Transformational Challenge Reactor (TCR) fuel form was designed to contain large, densely packed uranium carbonitride (UCN) tristructural-isotropic (TRISO) fuel particles within a 3D printed SiC matrix, increasing the uranium density compared to conventional TRISO fuel forms and offering full geometric freedom for core design. Here, this work summarizes initial low-burnup, high-power irradiation testing of TCR fuel materials, including loose UCN TRISO particles and integral fuel compacts with ~55% TRISO particles by volume, to evaluate fission gas retention. Fission gasses were fully retained in all loose particle tests and in integral compacts irradiated at low (<250 °C) surface temperatures. Initial testing at higher (~700–750 °C) fuel surface temperatures showed fission gas release (FGR) and complete fracture of three compacts, but no FGR was observed in later high temperature tests (~300–750 °C) of both fueled compacts and loose TRISO particles. Calculated thermal stresses in the failed compacts were far less than the measured strength of the SiC matrix and the stresses in some failed compacts were less than those in compacts that did not show FGR. Thermal stress-induced matrix cracks also would not cause complete fracture because the tensile stresses transition to compression in the higher temperature regions. Therefore, fuel failure was likely not caused by thermal stresses and may have been related to leakage currents from the electrical heaters and erratic fuel surface temperatures that were only observed in the test for which failure was observed. In any case, the matrix cracks propagated through the coatings of TRISO particles located in the high-density matrix regions on the peripheries of the compacts, resulting in measurable fission gas release. The discussion focuses on the importance of understanding matrix density distributions and the particle-matrix interface properties to prevent matrix cracks from causing TRISO particle failures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Synthesis and structural characterization of Al{sub 4}SiC{sub 4}-homeotypic aluminum silicon oxycarbide, [Al{sub 4.4}Si{sub 0.6}][O{sub 1.0}C{sub 2.0}]C

A new quaternary layered oxycarbide, [Al{sub 4.39(5)}Si{sub 0.61(5)}]{sub S}IGMA{sub 5}[O{sub 1.00(2)}C{sub 2.00(2)}]{sub S}IGMA{sub 3}C, has been synthesized and characterized by X-ray powder diffraction, transmission electron microscopy and energy dispersive X-ray spectroscopy (EDX). The title compound was found to be hexagonal with space group P6{sub 3}/mmc, Z=2, and unit-cell dimensions a=0.32783(1) nm, c=2.16674(7) nm and V=0.20167(1) nm{sup 3}. The atom ratios Al:Si were determined by EDX, and the initial structural model was derived by the direct methods. The final structural model showed the positional disordering of one of the three types of Al/Si sites. The maximum-entropy methods-based pattern fitting (MPF) method was used to confirm the validity of the split-atom model, in which conventional structure bias caused by assuming intensity partitioning was minimized. The reliability indices calculated from the MPF were R{sub wp}=3.73% (S=1.20), R{sub p}=2.94%, R{sub B}=1.04% and R{sub F}=0.81%. The crystal was an inversion twin. Each twin-related individual was isostructural with Al{sub 4}SiC{sub 4} (space group P6{sub 3}mc, Z=2). - Graphical abstract: A new oxycarbide discovered in the Al-Si-O-C system, Al{sub 4}SiC{sub 4}-homeotypic [Al{sub 4.4}Si{sub 0.6}][O{sub 1.0}C{sub 2.0}]C. The crystal is an inversion twin, and hence the structure is represented by a split-atom model. The three-dimensional electron density distributions are determined by the maximum-entropy methods-based pattern fitting, being consistent with the disordered structural model.

36 MATERIALS SCIENCE↗

Characterization of tribo-layer formed during sliding wear of SiC ball against nanocrystalline diamond coatings

Tribo-layer formation and frictional characteristics of the SiC ball were studied with the sliding test against nanocrystalline diamond coating under atmospheric test conditions. Unsteady friction coefficients in the range of 0.04 to 0.1 were observed during the tribo-test. Friction and wear characteristics were found to be influenced by the formation of cohesive tribo-layer (thickness ∼ 1.3 μm) in the wear track of nanocrystalline diamond coating. Hardness of the tribo-layer was measured using nanoindentation technique and low hardness of ∼ 1.2 GPa was observed. The presence of silicon and oxygen in the tribo-layer was noticed by the energy dispersive spectroscopy mapping and the chemical states of the silicon were analyzed using X-ray photoelectron spectroscopy. Large amount of oxygen content in the tribo-layer indicated tribo-oxidation wear mechanism. - Highlights: • Sliding wear and friction characteristics of SiC were studied against NCD coating. • Silicon oxide tribo-layer formation was observed in the NCD coating wear track. • Low hardness 1.2 GPa of tribo-layer was measured using nanoindentation technique. • Chemical states of silicon were analyzed using X-ray photoelectron spectroscopy.

36 MATERIALS SCIENCE↗

Fractographical characterization of hot pressed and pressureless sintered AlN-doped ZrB{sub 2}–SiC composites

In this paper, ZrB{sub 2}–SiC composites doped with 0–5 wt.% AlN were prepared by a low pressure hot pressing as well as a pressureless sintering methods at 1900 °C for 2 h. The influence of aluminum nitride addition on the sinterability and microstructure development of such ceramic composites was studied by a fractographical approach. The results revealed that only 1 wt.% AlN can aid the densification process of the hot pressed ceramic composite via the liquid phase sintering mechanism due to the formation of nano-scale metakaolinite spinel layers. In the pressureless sintering method, adding more AlN can increase the formation of gaseous products which raised the amount of porosities in the final microstructure. The formation of nano-graphite phase in the hot pressing process, the formation of Al{sub 2}OC in the pressureless sintering process, and the formation of BN in the both processes were disclosed by X-ray diffraction, SEM and TEM analyses. - Highlights: • The effect of AlN addition on densification of ZrB{sub 2}–SiC composites was studied. • AlN promotes the densification in hot pressed samples by liquid phase formation. • A fully dense composite was obtained by adding 1 wt.% AlN in hot pressing process. • In pressureless sintering, more AlN content intensifies the formation of porosities.

36 MATERIALS SCIENCE↗

Three dimensional (3D) microstructure-based finite element modeling of Al-SiC nanolaminates using focused ion beam (FIB) tomography

Al-SiC nanolaminate composites show promise as high performance coating materials due to their combination of strength and toughness. Although a significant amount of modeling effort has been focused on materials with an idealized flat nanostructure, experimentally these materials exhibit complex undulating layer geometries. This work utilizes FIB tomography to characterize this nanostructure in 3D and finite element modeling to determine the effect that this complex structure has on the mechanical behavior of these materials. A sufficiently large volume was characterized such that a 1 × 2 μm micropillar could be generated from the dataset and compared directly to experimental results. The mechanical response from this nanostructure was then compared to pillar models using simplified structures with perfectly flat layers, layers with sinusoidal waviness, and layers with arc segment waviness. The arc segment based layer geometry showed the best agreement with the experimentally determined structure, indicating it would be the most appropriate geometry for future modeling efforts. - Highlights: •FIB tomography was used to determine the structure of an Al-SiC nanolaminate in 3D. •FEM was used to compare the deformation of the nanostructure to experimental results. •Idealized structures from literature were compared to the FIB determined structure. •Arc segment based structures approximated the FIB determined structure most closely.

36 MATERIALS SCIENCE↗

Characterisation of amorphous silica in air-oxidised Ti 3 SiC 2 at 500-1000 °C using secondary-ion mass spectrometry, nuclear magnetic resonance and transmission electron microscopy

In this paper we have described the use of secondary-ion mass spectrometry (SIMS), solid state {sup 29}Si magic-angle-spinning (MAS) nuclear magnetic resonance (NMR) and transmission electron microscopy (TEM) to detect the existence of amorphous silica in Ti{sub 3}SiC{sub 2} oxidised at 500-1000 C. The formation of amorphous SiO{sub 2} and growth of crystalline TiO{sub 2} with temperature was monitored using dynamic SIMS and synchrotron radiation diffraction. A duplex structure with an outer TiO{sub 2}-rich layer and an inner mixed layer of SiO{sub 2} and TiO{sub 2} was observed. Results of NMR and TEM verified for the first time the direct evidence of amorphous silica formation during the oxidation of Ti{sub 3}SiC{sub 2} at the temperature range 500-1000 C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗